Resistance change memory element and method for manufacturing the same
By designing an upper electrode structure layer with gradually decreasing nitrogen content, the problem of metal atom consumption and diffusion in resistive switching memory elements was solved, improving device reliability, simplifying the fabrication process, and reducing costs.
Patent Information
- Application Number
- CN202310463167.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-04-26
- Publication Date
- 2026-11-20
- Estimated Expiration
- 2043-04-26
AI Technical Summary
Existing resistive switching memory elements gradually consume metal atoms due to the generation and erasure of conductive filaments, resulting in fewer metal atoms available to form conductive filaments, decreased device reliability, and the possibility of metal atoms diffusing outwards.
The upper electrode structure is designed to consist of two or more nitrogen-containing metal layers, with the nitrogen content gradually decreasing along the direction away from the upper electrode layer. Each layer is formed using a physical vapor deposition process, and the nitrogen content gradient is controlled by adjusting parameters such as nitrogen flow rate, current magnitude, and negative bias voltage.
This improved the reliability and resistance control capability of the device, simplified the fabrication process, and reduced costs.
Smart Images

Figure CN116456813B_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of semiconductor device technology, and in particular to a resistive switching memory element and its fabrication method. Background Technology
[0002] Resistive random access memory (RRAM) is a non-volatile memory fabricated by utilizing the reversible switching characteristic of the resistance of non-conductive materials between high-resistance and low-resistance states under the influence of an applied electric field. Compared to other non-volatile memory technologies, RRAM has advantages such as fast read speed and is considered to have the potential to replace the current mainstream Flash memory, thus becoming an important research direction for new memory technologies.
[0003] The resistance change of resistive switching memory elements is due to the formation of conductive filaments (transition from a high-resistance state to a low-resistance state) and erasure (transition from a low-resistance state to a high-resistance state). In the existing structure, the metal / metal nitride of the upper plate of the memory provides conductive metal atoms for the resistive switching layer. However, the formation and erasure of conductive filaments gradually consume metal atoms, and metal atoms may also diffuse outward, resulting in fewer metal atoms available to form conductive filaments and a decrease in device reliability.
[0004] It should be noted that the above introduction to the technical background is only for the purpose of providing a clear and complete explanation of the technical solutions of this application and facilitating understanding by those skilled in the art. It should not be assumed that these technical solutions are known to those skilled in the art simply because they have been described in the background section of this application. Summary of the Invention
[0005] In view of the shortcomings of the prior art described above, the purpose of this invention is to provide a resistive switching memory element and its preparation method, which solves the problems of existing resistive switching memory elements where the generation and erasure of conductive wires gradually consume metal atoms, and the metal atoms may also diffuse outwards, resulting in fewer metal atoms available to form conductive wires and a decrease in device reliability.
[0006] To achieve the above and other related objectives, the present invention provides a resistive switching memory element, the resistive switching memory element comprising a lower electrode layer, a resistive switching layer, an upper electrode layer and an upper electrode structure layer stacked sequentially, wherein the upper electrode structure layer comprises two or more nitrogen-containing metal layers stacked sequentially, and the nitrogen content in the two or more nitrogen-containing metal layers gradually decreases in the direction away from the upper electrode layer.
[0007] Optionally, the materials of the lower electrode layer and the upper electrode layer include one or more of Cu, Pt, Ag, Fe, Co, Ni, W, Ti, Ta, Hf, Zr, Nb, Y, Zn, Al, graphene, and n-Si.
[0008] Optionally, the resistive switching layer is made of one or more of binary or higher metal oxides, graphene oxides, and metal nitrides.
[0009] Optionally, the resistive switching layer may be made of one or more of the following materials: NiOx, TiOx, ZnOx, ZrOx, HfOx, TaOx, PrCaMnO3, SrTiO3, AlN, ZnTe, and ZnS.
[0010] Optionally, an adhesion metal layer is further provided between the upper electrode plate layer and the upper electrode structure layer.
[0011] Optionally, the nitrogen-containing metal layer of the upper electrode structure layer has at least three layers, and the nitrogen content in each nitrogen-containing metal layer decreases in a gradient or gradually.
[0012] Optionally, each nitrogen-containing metal layer of the upper electrode structure layer contains the same metal element.
[0013] The present invention also provides a method for fabricating a resistive switching memory element, the method comprising forming a resistive switching memory element as described in any of the above embodiments using a physical vapor deposition process.
[0014] Optionally, the preparation method includes employing one or more of the following methods during the preparation of the upper electrode structure layer, such that the nitrogen content in the two or more nitrogen-containing metal layers of the upper electrode structure layer gradually decreases in the direction away from the upper electrode layer: adjusting the nitrogen flow rate, adjusting the current magnitude, and adjusting the negative bias voltage.
[0015] Optionally, the preparation method includes the step of performing a surface nitriding treatment on the upper electrode layer to obtain a nitrogen-containing metal layer as the bottom layer of the upper electrode structure layer.
[0016] As described above, the resistive switching memory element and its fabrication method of the present invention have the following beneficial effects: The improved structural design of the present invention makes it easy to control the resistance value of the upper electrode structure layer while having good blocking ability, which helps to improve the reliability of the device. The resistive switching memory element provided by the present invention has a simple structure, is easy to fabricate, and helps to reduce its manufacturing cost. Attached Figure Description
[0017] Figure 1 The diagram shown is an exemplary cross-sectional view of the resistive switching memory element provided in Embodiment 1 of the present invention.
[0018] Figure 2The diagram shown is an exemplary cross-sectional view of the resistive switching memory element provided in Embodiment 2 of the present invention. Detailed Implementation
[0019] The following specific examples illustrate the embodiments of the present invention. Those skilled in the art can easily understand other advantages and effects of the present invention from the content disclosed in this specification. The present invention can also be implemented or applied through other different specific embodiments, and various details in this specification can be modified or changed based on different viewpoints and applications without departing from the spirit of the present invention. For ease of explanation, when detailing the embodiments of the present invention, the cross-sectional views showing the device structure are partially enlarged, not according to the general scale, and the schematic diagrams are merely examples and should not limit the scope of protection of the present invention. Furthermore, in actual manufacturing, the three-dimensional spatial dimensions of length, width, and depth should be included.
[0020] For ease of description, spatial relation terms such as “below,” “under,” “lower than,” “below,” “above,” and “upper” may be used herein to describe the relationship between one element or feature shown in the accompanying drawings and other elements or features. It will be understood that these spatial relation terms are intended to include directions other than those depicted in the drawings for devices in use or operation. Furthermore, when a layer is referred to as being “between” two layers, it may be the only layer between the two layers, or there may be one or more layers in between.
[0021] In the context of this application, the structure described above the first feature may include embodiments in which the first and second features are formed in direct contact, or embodiments in which additional features are formed between the first and second features, such that the first and second features may not be in direct contact.
[0022] It should be noted that the illustrations provided in this embodiment are only schematic representations of the basic concept of the present invention. Therefore, the drawings only show components related to the present invention and are not drawn according to the actual number, shape, and size of the components in the actual implementation. In the actual implementation, the form, quantity, and proportion of each component can be arbitrarily changed, and the layout of the components may also be more complex. To keep the illustrations as concise as possible, not all structures are shown in the figures.
[0023] Example 1
[0024] like Figure 1As shown, the present invention provides a resistive switching memory element, the resistive switching memory element comprising a lower electrode layer 12, a resistive switching layer 13, an upper electrode layer 14 and an upper electrode structure layer 15 stacked sequentially, wherein the upper electrode structure layer 15 comprises two or more nitrogen-containing metal layers stacked sequentially, and the nitrogen content in the two or more nitrogen-containing metal layers gradually decreases in the direction away from the upper electrode layer 14.
[0025] The resistive switching memory element typically also includes a substrate 11, on which the aforementioned lower electrode layer 12, resistive switching layer 13, upper electrode layer 14, and top electrode structure layer 15 are sequentially formed. The substrate 11 can be a bare wafer, such as a silicon wafer, germanium wafer, germanium-silicon wafer, silicon-on-insulator (SOI) wafer, etc. It can also be a wafer with pre-fabricated devices, such as transistors or other device structures on its surface. The lower electrode layer 12 (BE) is made of conductive material and is used to electrically connect the resistive switching memory element to transistors or other devices on the wafer. The resistive switching layer 13 (RSL) is, as the name suggests, a material layer whose resistance changes. Under an applied bias voltage, the resistive switching layer 13 switches between high and low resistance states, thereby achieving the storage of "0" and "1". The upper electrode layer 14 (TE) is also made of conductive material, providing metal atoms for the resistive switching layer 13 to form a resistance wire. The upper electrode layer 14 can be made of pure metal or metal nitride, as some metals exhibit better thermal stability and conductivity after nitriding. The upper electrode structure layer 15 is also made of a conductive material, serving not only as an electrical lead-out layer but also as an etch stop layer for the upper electrode interconnects. The conductive filaments (CFs) formed in the resistive switching layer 13 consume metal atoms during repeated generation and erasure processes, leading to the gradual depletion of metal atoms in the metal / metal nitride until insufficient metal atoms are available to form the filaments. Furthermore, in existing resistive switching memory devices, metal atoms in the metal / metal nitride diffuse outward through the upper electrode, reducing the number of metal atoms available to form the filaments and degrading device performance. This invention, however, effectively avoids these problems by improving the device structure.
[0026] Specifically, in the resistive switching memory element provided by this invention, the upper electrode structure layer 15 is designed to be composed of two or more stacked structural layers. For example... Figure 1In the example, the upper electrode structure layer 15 has a three-layer structure, defined from bottom to top as a first nitrogen-containing metal layer 151, a second nitrogen-containing metal layer 152, and a third nitrogen-containing metal layer 153, each with a different nitrogen content. The first nitrogen-containing metal layer 151, adjacent to the upper electrode layer 14, has the highest nitrogen content, and the nitrogen content gradually decreases as it moves upwards and further away from the upper electrode layer 14. Therefore, if ordered by nitrogen content, the order is: first nitrogen-containing metal layer 151 > second nitrogen-containing metal layer 152 > third nitrogen-containing metal layer 153. Preferably, the thickness of each nitrogen-containing metal layer does not exceed 100 nm. The higher the nitrogen content in the nitrogen-containing metal layer, the stronger its barrier properties. This effectively reduces the difficulty of erasing the resistance wire caused by metal diffusion from the upper electrode structure layer 15 into the resistive switching layer 13, and also reduces the degradation of device cycle performance caused by metal diffusion from the upper electrode layer 14 into the upper electrode structure layer 15, as well as the decrease in conductivity of the upper electrode structure layer 15 due to excessive nitrogen content. Therefore, this layered structure of the upper electrode structure layer 15 ensures both good barrier properties and control over its resistance, thereby contributing to improved memory reliability.
[0027] The resistive switching memory element may include multiple memory cells, each memory cell comprising a lower electrode layer 12, a resistive switching layer 13, an upper electrode layer 14, and an upper electrode structure layer 15 stacked sequentially. The multiple memory cells may be arranged in a stacked and / or parallel spacing manner. This depends on the specific design requirements and is not specifically limited.
[0028] The number of nitrogen-containing metal layers in the upper electrode structure layer 15 is at least two. In a preferred example, the upper electrode structure layer 15 has at least three nitrogen-containing metal layers, with the nitrogen content in each layer decreasing in a gradient or gradually decreasing manner, which is not limited to any specific type. From the perspective of simplifying the process, a gradual decrease is preferred. Because the elemental ratio in the final thin film is difficult to be completely consistent with the elemental ratio in the reactants due to various factors during the thin film preparation process. The nitrogen content in each nitrogen-containing metal layer can be set as needed while satisfying the requirement of gradual decrease, but it is preferred that the ratio of nitrogen to metal in each nitrogen-containing metal layer does not exceed 1:1. For example, in one example, the atomic percentage of nitrogen to metal in the first nitrogen-containing metal layer is about 0.8:1, the atomic percentage of nitrogen to metal in the second nitrogen-containing metal layer is about 0.6:1, the atomic percentage of nitrogen to metal in the third nitrogen-containing metal layer is about 0.4:1, and so on, decreasing sequentially.
[0029] The nitrogen-containing metal layers may contain the same or different metal elements, and their thicknesses may be the same or different. However, in a preferred example, the nitrogen-containing metal layers of the upper electrode structure layer 15 contain the same metal element, for example, all nitrogen-containing metal layers contain Ti (titanium), and the thickness of each nitrogen-containing metal layer is preferably the same. This helps simplify the fabrication process of the upper electrode structure layer 15, and also makes it easier to control its resistance, which helps to further improve device performance. For example, in the process of fabricating these nitrogen-containing metal layers, only the nitrogen gas flow rate needs to be adjusted, while the RF power, negative bias voltage, deposition time, and other conditions remain unchanged, thus enabling the fabrication of multiple nitrogen-containing metal layers with basically the same thickness but different nitrogen contents.
[0030] The materials of the lower electrode layer 12 and the upper electrode layer 14 can be the same or different. From the perspective of simplifying the manufacturing process, it is preferable that they are made of the same material. For example, both can be made of active metals or inert conductive materials. More specifically, both can be selected from, but are not limited to, one or more of Cu (copper), Pt (platinum), Ag (silver), Fe (iron), Co (cobalt), Ni (nickel), W (tungsten), Ti (titanium), Ta (tantalum), Hf (hafnium), Zr (chromium), Nb (niobium), Y (yttrium), Zn (zinc), Al (aluminum), graphene, and n-Si (doped polycrystalline silicon). That is, both can be a single material or a composite material. In a preferred example provided by the present invention, both the lower electrode layer 12 and the upper electrode layer 14 are titanium layers or titanium nitride layers, or both are tantalum or tantalum nitride. The thickness of the lower electrode layer 12 and the upper electrode layer 14 is preferably 20-200 nm, for example, 50 nm.
[0031] The resistive switching layer 13 can be made of a high-k dielectric material with variable resistance, including but not limited to one or more of binary or higher metal oxides, graphene oxides, and metal nitrides. More specifically, for example, it can be one or more of NiOx, TiOx, ZnOx, ZrOx, HfOx, TaOx, PrCaMnO3, SrTiO3, AlN, ZnTe, and ZnS. The resistive switching layer 13 can be a single material layer, such as a single HfOx layer, or a stack of multiple material layers. Its total thickness is preferably no more than 50 nm. When it is composed of multiple sub-resistive switching layers 13, the thickness of each sub-resistive switching layer 13 is preferably no more than 20 nm. For example, in one example, the resistive switching layer 13 includes a first sub-resistive switching layer 13 and a second sub-resistive switching layer 13 stacked vertically and having different resistive switching characteristics during resistive switching. The first sub-resistive switching layer 13 is made of a binary oxide such as TaOx. During resistive switching, it can reduce the absolute value of the Gibbs free energy of the redox reaction inside the material, thereby improving the stability of the resistive switching memory. The second sub-resistive switching layer 13 is made of a material such as HfOx. When subjected to an electric field, conductive filaments are formed inside the second sub-resistive switching layer 13. By setting the resistive switching layer 13 as a multilayer structure, local conductive filaments can be formed between multiple interconnected sub-resistive switching layers 13, which can provide uniform and reliable high and low resistance states, and help to further improve device performance.
[0032] In one example, an adhesion metal layer (not shown) is further disposed between the upper electrode layer 14 and the upper electrode structure layer 15. The adhesion metal layer enhances the adhesion between the upper electrode layer 14 and the upper electrode structure layer 15, reducing contact resistance. The thickness of the adhesion metal layer can be set as needed. If used purely as an adhesion layer, its thickness is preferably controlled within 20 nm. The material of the adhesion metal layer can be, for example, a metal such as titanium or tantalum, preferably the same as the metal element contained in the upper electrode or upper electrode structure layer 15, which will help further enhance interlayer adhesion. For example, in a preferred example, both the upper electrode layer 14 and the upper electrode structure layer 15 are TiN layers, except that the TiN layer in the upper electrode structure layer 15 has a layered structure with different nitrogen contents in each layer, while the adhesion metal layer is made of Ti.
[0033] The fabrication method of each structural layer of the resistive switching memory element can be determined according to its material. However, in a preferred example, each structural layer is formed using physical vapor deposition (PVD), thus allowing each layer to be fabricated one by one within the same process chamber by adjusting parameters such as the target material and gas flow rate. This helps simplify the fabrication process and reduce fabrication costs.
[0034] Example 2
[0035] like Figure 2As shown, this embodiment provides a resistive switching memory element with another structure. The main difference between the resistive switching memory element in this embodiment and that in Embodiment 1 is that a protective layer 16 is provided circumferentially in the lower electrode layer 12, the resistive switching layer 13, and the upper electrode layer 14. This protective layer 16 can extend upwards to the circumferential direction of the upper electrode structure layer 15. The protective layer 16 can be used to suppress the diffusion and loss of oxygen ions in the resistive switching layer 13, which helps to improve the switching characteristics of the device and its stability under high temperature operation. In addition, the protective layer 16 can also prevent the metal in the upper electrode layer 14 from diffusing outwards, which can lead to problems such as deterioration of device cycle performance, just like the upper electrode structure layer 15. The material of the protective layer 16 can be an oxide or a nitride, and it can also adopt the layered structure of the upper electrode structure layer 15, for example, it also contains multiple nitrogen-containing metal layers, and the nitrogen content in each nitrogen-containing metal layer decreases sequentially in the direction away from the center of the device.
[0036] Apart from the differences mentioned above, the other structures of the resistive switching memory element in this embodiment are the same as those in Embodiment 1. Please refer to the description in Embodiment 1 for details, which will not be repeated for the sake of brevity.
[0037] This invention also provides a method for fabricating a resistive switching memory element. This method can be used to fabricate the resistive switching memory elements described in Examples 1 and 2, therefore the foregoing content can be quoted in its entirety here, and will not be repeated for the sake of brevity. Of course, the resistive switching memory elements in Examples 1 and 2 can also be fabricated using other methods. However, compared to other methods, this invention uses physical vapor deposition to form the resistive switching memory elements as described in Examples 1 or 2, which can greatly simplify the fabrication process and reduce fabrication costs.
[0038] Specifically, the fabrication method of the resistive switching memory element provided by the present invention includes a step of cleaning the substrate 11. The cleaning process can begin by washing the substrate 11 with diluted hydrofluoric acid to remove impurities such as natural oxides from the surface of the substrate 11, followed by drying. Then, the cleaned substrate 11 is placed in a physical vapor deposition chamber, such as a magnetron sputtering chamber. By adjusting parameters such as the target material, reactive gas flow rate, and RF power, a lower electrode layer 12, a resistive switching layer 13, an upper electrode layer 14, and an upper electrode structure layer 15 are sequentially fabricated on the substrate 11. During the fabrication of the upper electrode structure layer 15, one or more of the following methods are used to gradually reduce the nitrogen content in the two or more nitrogen-containing metal layers of the upper electrode structure layer 15 away from the upper electrode layer 14: adjusting the nitrogen flow rate, adjusting the current magnitude, and adjusting the negative bias voltage. For example, if the nitrogen flow rate is adjusted, other parameters can be kept constant while the nitrogen flow rate is reduced in stages during the fabrication process, so that the nitrogen content of the fabricated nitrogen-containing metal layers decreases sequentially. By adjusting the current, the target current can be increased in stages while keeping the nitrogen flow rate constant, thereby increasing the ionization rate of the target material. This increases the metal ion content in each nitrogen-containing metal layer, achieving the same effect of reducing nitrogen content. Furthermore, increasing the negative bias voltage allows argon ions to generate more metal ions upon impact with the target, which also helps increase the target ionization rate, leading to an increase in the metal ion content in each nitrogen-containing metal layer and achieving the same effect of reducing nitrogen content. Among these methods, adjusting the nitrogen flow rate is preferred because it is simpler to adjust and causes the least damage to the equipment.
[0039] If the resistive switching memory element of the aforementioned embodiment 2 is to be prepared, a mask covering the upper electrode layer 14 can be formed after the upper electrode layer 14 is prepared, and then a protective layer 16 located in the circumferential direction of the lower electrode layer 12, the resistive switching layer 13 and the upper electrode layer 14 can be formed. After that, the mask is removed and the upper electrode structure layer 15 is finally formed. Alternatively, the upper electrode structure layer 15 can be formed first, and then the protective layer 16 can be prepared with the help of a mask. There are no strict limitations on this.
[0040] In one example, the upper electrode layer 14 is a metal layer, and therefore the fabrication method includes the step of performing a surface nitriding treatment on the upper electrode layer 14 to obtain a nitrogen-containing metal layer as the bottom layer of the upper electrode structure layer 15. In other examples, if an adhesion metal layer, such as a Ti layer, is also provided between the upper electrode layer 14 and the upper electrode structure layer 15, the nitrogen-containing metal layer as the bottom layer of the upper electrode structure layer 15 can be obtained by performing a nitriding treatment on the adhesion metal layer. Ammonia and / or pure nitrogen can be used during the nitriding treatment, with a flow rate of, for example, 200-500 sccm, a nitriding temperature of 200℃ to 400℃, a radio frequency power of 500-700 W, and a nitriding time of 10s to 30s. The nitrogen-containing metal layer at the bottom of the upper electrode structure layer 15, prepared by nitriding, effectively eliminates lattice defects and releases stress within the original metal film. This not only results in a nitrogen-containing metal layer with excellent density and surface flatness but also exhibits excellent adhesion to the upper electrode layer 14, the adhering metal layer, and subsequent nitrogen-containing metal layers, thus improving interlayer stress and further enhancing device performance. After forming the bottom nitrogen-containing metal layer of the upper electrode structure layer through nitriding, other nitrogen-containing metal layers with different nitrogen contents are sequentially prepared using the aforementioned physical vapor deposition method, adjusting gas flow rate, negative bias voltage, and RF power during the preparation process.
[0041] In summary, this invention provides a resistive switching memory element and its fabrication method. The resistive switching memory element comprises a lower electrode layer, a resistive switching layer, an upper electrode layer, and an upper electrode structure layer stacked sequentially. The upper electrode structure layer comprises two or more nitrogen-containing metal layers stacked sequentially, with the nitrogen content in the two or more nitrogen-containing metal layers gradually decreasing away from the upper electrode layer. The improved structural design of this invention allows the upper electrode structure layer to have good blocking ability while easily controlling its resistance value, thus contributing to improved device reliability. The resistive switching memory element provided by this invention has a simple structure, is easy to fabricate, and helps reduce its manufacturing cost. Therefore, this invention effectively overcomes various shortcomings of the prior art and has high industrial applicability.
[0042] The above embodiments are merely illustrative of the principles and effects of the present invention and are not intended to limit the invention. Any person skilled in the art can modify or alter the above embodiments without departing from the spirit and scope of the present invention. Therefore, all equivalent modifications or alterations made by those skilled in the art without departing from the spirit and technical concept disclosed in the present invention should still be covered by the claims of the present invention.
Claims
1. A resistive switching memory element, characterized in that, The resistive switching memory element includes a lower electrode layer, a resistive switching layer, an upper electrode layer, and an upper electrode structure layer stacked sequentially. The upper electrode layer provides metal atoms to the resistive switching layer to form a resistance wire. The material of the upper electrode layer includes one or more of Cu, Ag, Pt, Fe, Co, Ni, W, Ti, Ta, Hf, Zr, Nb, Y, Zn, and Al. The upper electrode structure layer serves not only as an electrical lead-out layer but also as an etch stop layer for interconnecting the upper electrodes. The upper electrode structure layer includes two or more nitrogen-containing metal layers stacked sequentially, with the nitrogen content in the two or more nitrogen-containing metal layers gradually decreasing in the direction away from the upper electrode layer.
2. The resistive switching memory element according to claim 1, characterized in that, The material of the lower electrode layer includes one or more of Cu, Ag, Pt, Fe, Co, Ni, W, Ti, Ta, Hf, Zr, Nb, Y, Zn, Al, graphene, and n-Si.
3. The resistive switching memory element according to claim 1, characterized in that, The resistive switching layer is made of one or more of binary or higher metal oxides, graphene oxides, and metal nitrides.
4. The resistive switching memory element according to claim 1, characterized in that, The resistive switching layer is made of NiO. X TiO X ZnO X ZrO X HfO X TaO X One or more of PrCaMnO3, SrTiO3, AlN, ZnTe and ZnS.
5. The resistive switching memory element according to claim 1, characterized in that, An adhesion metal layer is also provided between the upper electrode plate layer and the upper electrode structure layer.
6. The resistive switching memory element according to claim 1, characterized in that, The upper electrode structure layer has at least three nitrogen-containing metal layers, and the nitrogen content in each nitrogen-containing metal layer decreases in a gradient or gradually.
7. The resistive switching memory element according to any one of claims 1 to 6, characterized in that, The nitrogen-containing metal layers of the upper electrode structure layer contain the same metal element.
8. A method for fabricating a resistive switching memory element, characterized in that, The preparation method includes forming a resistive switching memory element as described in any one of claims 1 to 7 using a physical vapor deposition process.
9. The method for fabricating a resistive switching memory element according to claim 8, characterized in that, The preparation method includes employing one or more of the following methods during the preparation of the upper electrode structure layer, so that the nitrogen content in the two or more nitrogen-containing metal layers of the upper electrode structure layer gradually decreases in the direction away from the upper electrode layer: adjusting the nitrogen flow rate, adjusting the current magnitude, and adjusting the negative bias voltage.
10. The preparation method according to claim 8 or 9, characterized in that, The preparation method includes the step of performing surface nitriding treatment on the upper electrode layer to obtain the nitrogen-containing metal layer as the bottom layer of the upper electrode structure layer.
Citation Information
Patent Citations
Changing nitrogen content in a switching layer of a
CN115142032A
Resistive Random Access Memory (RRAM) Cell with a Composite Capping Layer
US20160276586A1