Controllable self-assembly method of long strip-shaped film and device

By constructing anchor points on the elongated thin film to control the film roll-up direction, the problem of controllable self-assembly of elongated self-rolling thin film devices is solved, resulting in a significant reduction in device footprint and simplification of process, supporting heterogeneous integration.

CN116471917BActive Publication Date: 2026-11-20XI AN JIAOTONG UNIV
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202310536437.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-05-12
Publication Date
2026-11-20
Estimated Expiration
2043-05-12

AI Technical Summary

Technical Problem

Existing technologies for controllable self-assembly of elongated self-rolling thin-film devices are complex and costly, making it difficult to further reduce the device footprint.

Method used

By depositing a sacrificial layer and a thin film layer with a lattice strain gradient on a substrate, an elongated self-assembled pattern with anchor points is etched and formed. The curling direction of the thin film is controlled by wet etching, and the thin film is released segment by segment by the anchor points to realize a self-curling functional device of microtube structure.

Benefits of technology

It enables controllable self-assembly of thin-film devices, reduces device footprint, simplifies process flow, lowers costs, and supports heterogeneous integration with semiconductor substrates.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure HDA0004226426100000011
    Figure HDA0004226426100000011
  • Figure HDA0004226426100000012
    Figure HDA0004226426100000012
  • Figure HDA0004226426100000013
    Figure HDA0004226426100000013
Patent Text Reader

Abstract

The application discloses a controllable self-assembly method of long strip-shaped film and a device, which comprises the following steps: depositing a sacrificial layer on a substrate; depositing a film layer on the sacrificial layer; etching the film layer to form a long strip-shaped self-assembly pattern; the long strip-shaped self-assembly pattern comprises a long strip-shaped film and a plurality of anchor points symmetrically connected to two long sides of the long strip-shaped film; the length of a short side of the long strip-shaped film is W0, the distance between at least one short side of the long strip-shaped film and the nearest anchor point is L1, and L1<=W0; wet etching the sacrificial layer, and with the wet etching, the long strip-shaped film is curled along the direction of the long side from the at least one short side, and the connection between the anchor points and the long strip-shaped film is sequentially broken in the curling process. The application releases the film from the substrate in sections by constructing the anchor points, controls the curling direction of the film, and obtains a device with a microtubular structure.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of electronic device technology and relates to a controllable self-assembly method and device for a long strip thin film. Background Technology

[0002] To develop compact, multifunctional thin-film electronic devices, self-rolling technology has been widely applied to metals, polymers, and oxide materials. This technology utilizes internal stresses generated during thin-film growth, such as strain gradients within monolayer films or interlayer lattice strain differences within bilayer / multilayer films, to achieve self-rolling as the film detaches from the substrate. A series of micro-thin-film electronic devices based on the self-rolling phenomenon have been reported in the literature, for example, those made of Ni… 80 Fe 20 Self-curved vector magnetic sensors made of ferromagnetic metal materials (Science Advances, 2019, 5(12), eaay7459), self-curved capacitors with polycrystalline oxides such as Al2O3 as dielectric layers (Advanced Energy Materials, 2014, 4(9), 1301631), self-curved inductors made of polymers and metals (Advanced Electronic Materials, 2018, 4(11), 1800298), and self-curved inductors made of metallic Ni and SiN X Self-curling 3D transformers made from materials (Nature Electronics, 2018, 1(5):305-313), etc. Taking the above capacitor as an example, the area occupied by the device after self-curling is reduced from 0.5 mm². 2 Reduced to 0.008mm 2 The lateral area is reduced by two orders of magnitude. However, elongated (high aspect ratio) self-rolling films are easy to roll up from the long side, and the controllable self-assembly of elongated self-rolling film devices becomes crucial to further reduce the device footprint.

[0003] Current controllable self-assembly methods for self-rolling thin film devices have the following defects and shortcomings: (1) The traditional windowing method (Advanced Energy Materials, 2014, 4(9), 1301631) involves exposing a window at the initial roll-up position on the surface of the thin film with the etched shape to be rolled up, allowing the thin film at that position to roll up first, thereby controlling the roll-up direction. This method involves multiple photolithography and etching steps, making the process complex. (2) The emerging method of controlling the self-rolling direction using an external magnetic field (Nature Communications, 2019, 10(1), 3013) involves adding a magnetic layer to the thin film and using an external magnetic field to control the magnetic layer to achieve controllable self-rolling of the thin film. This method involves complex external magnetic field equipment, resulting in high costs. Currently, no simple, low-cost, and easy-to-operate controllable self-assembly method for elongated self-rolling thin film devices has been proposed. Summary of the Invention

[0004] To address the problems of the prior art, the present invention provides a controllable self-assembly method and device for elongated thin films, which is simple in process, low in cost and easy to operate.

[0005] This invention is achieved through the following technical solution:

[0006] A method for controllable self-assembly of a strip-shaped thin-film device includes the following steps:

[0007] S1, deposit a sacrificial layer on the substrate;

[0008] S2, depositing a thin film layer with a lattice strain gradient on the sacrificial layer;

[0009] S3, etch the thin film layer to form a strip-shaped self-assembled pattern; the strip-shaped self-assembled pattern includes a strip-shaped thin film and multiple anchor points symmetrically connected to the two long sides of the strip-shaped thin film; the length of the short side of the strip-shaped thin film is W0, and the distance between at least one short side of the strip-shaped thin film and its nearest anchor point is L1, and L1 and W0 satisfy L1≤W0.

[0010] S4, wet etching is performed on the sacrificial layer. As the wet etching proceeds, the elongated film curls up along the direction of the long side starting from at least one short side. During the curling process, the connection between the anchor point and the elongated film breaks down in sequence.

[0011] Preferably, the distance between two adjacent anchor points on the same long side of the elongated film is L3, and L3≈W0; the length of the connection between the anchor point and the elongated film is L2, and 1μm≤L2≤5μm.

[0012] Preferably, the anchor point is trapezoidal, with the base of the trapezoid connected to the long side of the elongated film.

[0013] Furthermore, the angle α between the waist of the anchor point and the long side of the elongated film is 30° to 60°.

[0014] Preferably, the other short side of the elongated film is connected with several strips.

[0015] Furthermore, the strip length is L5, the width is W1, and 10μm≤W1≤60μm, with L5 being equal to the curling diameter of the elongated film.

[0016] Furthermore, the distance between the short side of the long strip connecting strip and its nearest anchor point is L4, and L4≈W0.

[0017] Preferably, S3 further includes: etching away the thin film layer and sacrificial layer at the edge of the substrate to expose the substrate surface; and using photoresist to press the thin film layer around the elongated self-assembled pattern together with the exposed substrate surface.

[0018] Preferably, the thin film layer is a single-layer thin film or a multi-layer thin film.

[0019] The device obtained using the above-described preparation method.

[0020] Compared with the prior art, the present invention has the following beneficial effects:

[0021] The controllable self-assembly method of the thin film of the present invention utilizes the self-rolling characteristics of the thin film. By constructing anchor points, the thin film is released segment by segment from the substrate. The roll-up direction of the thin film is controlled by the anchor points, thereby obtaining a self-rolling functional device with a microtube structure, which greatly reduces the footprint of the device. The advantages of the present invention include: (1) This method overcomes the roll-up characteristics of long strip self-rolling thin films that are easy to roll up from the long side, making the roll-up direction of the thin film controllable, and can control the roll-up direction of the thin film to be along the long side; (2) Compared with traditional self-assembly methods such as windowing, this method is simple, low-cost and easy to operate; (3) The multilayer roll prepared by this method can be transferred to any substrate to achieve heterogeneous integration with semiconductor substrates such as silicon, and can be compatible with CMOS technology; (4) After the thin film self-rolls, the footprint is reduced by one or even several orders of magnitude, and large-scale integration can be achieved; (5) This method can be widely applied to the preparation of various long strip self-rolling thin films, thereby constructing functional devices with microtube structures, realizing the integrated preparation and large-area integration of thin film devices.

[0022] Furthermore, after edge etching, the thin film layer around the elongated self-assembled pattern is pressed together with the substrate surface exposed after etching to prevent excess film from rolling up along with the film to be rolled up during the self-rolling process, and also to make the anchor point easier to break. Attached Figure Description

[0023] Figure 1A flowchart illustrating a controllable self-assembly method for a long strip thin film;

[0024] Figure 2 It features multi-layer single-roll structure etching and edge pressing patterns;

[0025] Figure 3 This is a photograph of the actual process of curling the multi-layer single-roll structure in Example 1;

[0026] Figure 4 The double-roll structure etching and edge pressing pattern in Example 2;

[0027] Figure 5 This is a photograph of the actual process of curling the double-roll structure in Example 2. Detailed Implementation

[0028] To further understand the present invention, the present invention will be described below with reference to embodiments. These descriptions are only for further explaining the features and advantages of the present invention and are not intended to limit the claims of the present invention.

[0029] This invention provides a controllable self-assembly method for elongated thin films, such as... Figure 1 As shown, it includes the following steps:

[0030] First, a sacrificial layer is epitaxially deposited on a single-crystal substrate.

[0031] Then, a thin film layer with a lattice strain gradient is grown on the sacrificial layer. The thin film layer can be a single-layer thin film or a multilayer thin film.

[0032] Then, a strip-shaped self-assembled pattern with anchor points is formed on the surface of the thin film layer by a combination of photolithography and dry etching, and the thin film layer and sacrificial layer around the edges of the substrate are removed.

[0033] Long strip self-assembly pattern with anchor points, such as Figure 2 As shown, the device includes a long strip of film to be rolled up and multiple anchor points connected to the two long sides of the film, with the anchor points symmetrically arranged on the two long sides. The shaded area represents the portion of the film layer and sacrificial layer to be removed; the length of the long strip of film to be rolled up is L0, and the width is W0; the rolling direction is from right to left (e.g., ...). Figure 2(As indicated by the middle arrow); the anchor point is trapezoidal, with the base of the trapezoid connected to the long side of the strip film, and the angle α between the waist of the anchor point and the long side of the strip film is 30° to 60°; the distance between the first anchor point and the initial roll-up position of the strip film is L1, and L1 ≤ W0 must be satisfied, because the self-rolling film has the characteristic of being easy to roll up from the long side; the length of the connection between the anchor point and the strip film is L2, L2 is much smaller than L1 and 1μm ≤ L2 ≤ 5μm; the distance between two adjacent anchor points on the same long side is L3, and L3 ≈ W0; the distance between the last anchor point and the end of the roll-up position is L4, and L4 ≈ W0. The rolled-up end of the elongated thin film is connected to two strips. By selectively disrupting these strips, the multilayer roll can be transferred to other substrates, thereby achieving heterogeneous integration. The strips are L5 in length and W1 in width, where W1 is much smaller than W0 and 10 μm ≤ W1 ≤ 60 μm. L5 is equal to the rolled-up diameter of the elongated thin film. Parts of the film are etched around the perimeter of the sample; this area is for subsequent edge-clamping operations, and the etching width can be determined as needed.

[0034] Alternatively, elongated self-assembling patterns with anchor points, such as Figure 4 As shown, the device includes a long strip of film to be rolled up and multiple anchor points connected to the two long sides of the film, with the anchor points symmetrically arranged on the two long sides. The shaded area represents the portion where the film layer and sacrificial layer need to be removed; the length of the long strip of film to be rolled up is L0, and the width is W0; the rolling direction is from both ends to the middle (e.g., ...). Figure 4 (As indicated by the middle arrow); the anchor point is trapezoidal, and the included angle α between the anchor point and the elongated film is 30° to 60°; the distance between the first anchor point on the two short sides of the film and the initial roll-up position is L1, and L1 ≤ W0 must be satisfied between L1 and W0, because the self-rolling film has the characteristic of being easy to roll up from the long side; the length of the connection between the anchor point and the elongated film is L2, L2 is much smaller than L1 and 1μm≤L2≤5μm; the distance between two adjacent anchor points on the same long side is L3, and L3≈W0; part of the film is etched around the edges of the sample, and this area is for subsequent edge pressing operations, and its etching width can be determined as needed.

[0035] Then, the etched film surface is pressed (fixed) using photolithography, such as... Figure 2 and 4 As shown in the dashed box, SU-8 photoresist is used to press the thin film layer around the elongated self-assembled pattern together with the substrate surface exposed after etching. This is to prevent excess film from being rolled up along with the film to be rolled up during the self-rolling process, and also to make the anchor point easier to break.

[0036] Then, the obtained sample is immersed in the corresponding solution, and the sacrificial layer is wet etched. As the sacrificial layer dissolves, the elongated film will roll up from the short side. The internal stress of the elongated film rolling will cause the anchor point and the connection of the elongated film to break in sequence, so that the film rolls up continuously along the long side.

[0037] Finally, by selectively breaking the two strips at the ends of the coil using a micromanipulator, the multilayer roll is transferred to another substrate (e.g., a silicon (Si) or polydimethylsiloxane (PDMS) flexible substrate) using the micromanipulator and micromanipulation needle, thus achieving heterogeneous integration.

[0038] The technical solutions of this invention will be clearly and completely described below with reference to the embodiments thereof. Obviously, the described embodiments are only a part of the embodiments of this invention, and not all of them. All other embodiments obtained by those skilled in the art based on the embodiments of this invention without creative effort are within the scope of protection of this invention.

[0039] Example 1: Nickel ferrite (NiFe2O4) / lead zirconate titanate (Pb(Zr,Ti)O3) single crystal thin film multilayer single roll structure

[0040] The nickel ferrite (NiFe2O4) / lead zirconate titanate (Pb(Zr,Ti)O3) single crystal thin film multilayer single roll structure provided in this embodiment consists of, from bottom to top, a SrTiO3 substrate, a Sr3Al2O6 sacrificial layer, a NiFe2O4 ferromagnetic thin film layer, and a Pb(Zr,Ti)O3 ferroelectric thin film layer.

[0041] The implementation steps of this embodiment are as follows:

[0042] Step 1: Using Sr3Al2O6 as the target material, a first layer is deposited on the surface of the SrTiO3 substrate using pulsed laser deposition to form a Sr3Al2O6 sacrificial layer.

[0043] 1.1) The SrTiO3 substrate has a crystal plane orientation of (001).

[0044] 1.2) Sr3Al2O6, as a sacrificial layer, can be completely dissolved in water at room temperature, thereby completely releasing the upper functional film.

[0045] 1.3) Set the distance between the SrTiO3 substrate and the Sr3Al2O6 target to 6 cm; heat the SrTiO3 substrate to 760 °C, and grow a Sr3Al2O6 sacrificial layer on the upper surface of the SrTiO3 substrate using pulsed laser deposition under the conditions of laser energy of 0.8 W, frequency of 3 Hz and oxygen partial pressure of 15 Pa. The deposition time is 5 min, and a Sr3Al2O6 sacrificial layer with a thickness of 10-30 nm is obtained.

[0046] Step 2: Using NiFe2O4 as the target material, a second deposition is performed on the surface of the Sr3Al2O6 sacrificial layer using pulsed laser deposition to form a NiFe2O4 ferromagnetic thin film layer.

[0047] 2.1) The NiFe2O4 ferromagnetic thin film has a cubic spinel structure with a lattice constant of The lattice constant of cubic Sr3Al2O6 is because NiFe2O4 ferromagnetic thin films can be epitaxially grown on Sr3Al2O6 sacrificial layers.

[0048] 2.2) Set the substrate temperature to 650℃, and under the conditions of laser energy of 1W, frequency of 5Hz and oxygen partial pressure of 5Pa, use NiFe2O4 target to grow a NiFe2O4 ferromagnetic layer on the upper surface of the Sr3Al2O6 sacrificial layer obtained in step one. The deposition time is 10min, and a NiFe2O4 ferromagnetic thin film layer is obtained.

[0049] Step 3: Using Pb(Zr,Ti)O3 as the target material, a third deposition is performed on the surface of the NiFe2O4 ferromagnetic thin film layer using pulsed laser deposition method to form a Pb(Zr,Ti)O3 ferroelectric thin film layer.

[0050] 3.1) The Pb(Zr,Ti)O3 ferroelectric thin film has a tetragonal phase structure and a lattice constant of . The lattice constant of cubic NiFe2O4 is 8.339. Since 8.339 / 2 > 4.024, the Pb(Zr,Ti)O3 ferroelectric thin film layer can be epitaxially grown on the NiFe2O4 ferromagnetic thin film layer, and the lattice mismatch provides a self-curling strain gradient for the bilayer film.

[0051] 3.2) Set the substrate temperature to 625℃, and under the conditions of laser energy of 1W, frequency of 5Hz and oxygen partial pressure of 26Pa, use Pb(Zr,Ti)O3 target to grow a Pb(Zr,Ti)O3 ferroelectric thin film layer on the upper surface of the NiFe2O4 ferromagnetic thin film layer obtained in step two. The deposition time is 10min, and a ferroelectric oxide thin film layer is obtained.

[0052] Step four: A long, strip-shaped self-assembled pattern with anchor points is formed on the surface of the thin film layer using a combination of photolithography and ion beam etching (e.g., ...). Figure 2 (as shown), and remove the thin film layer and sacrificial layer around the edges of the substrate.

[0053] Long strip self-assembly pattern with anchor points, such as Figure 2As shown, the film includes a long strip of film to be rolled up and multiple anchor points connected to the two long sides of the film. The shaded area represents the portion where the film layer and sacrificial layer need to be removed; the length of the long strip of film to be rolled up is L0 = 3.2 mm, and the width is W0 = 410 μm; the rolling direction is from right to left (e.g., ...). Figure 2 (As indicated by the middle arrow); the anchor point is trapezoidal, and the angle α between the anchor point and the elongated film is 45°; the distance between the first anchor point and the initial roll-up position is L1 = 130 μm, and L1 ≤ W0 must be satisfied between L1 and W0, because the self-rolling film has the characteristic of being easy to roll up from the long side; the length of the connection between the anchor point and the elongated film is L2 = 10 μm; the distance between two adjacent anchor points on the same long side is L3 = 410 μm; the distance between the last anchor point and the end of the roll-up position is L4 = 400 μm; the length of the two strips at the end of the roll-up of the elongated film is L5 = 70 μm, and the width is W1 = 40 μm, with L5 being approximately equal to the roll-up diameter of the film; a portion of the film is etched around the four edges of the sample, and this area is for subsequent edge pressing operations, the etching width of which can be determined as needed.

[0054] 4.1) Spin-coat three layers of photoresist onto the thin film surface, and then expose the area to be etched by photolithography. The three layers of photoresist form the etching pattern on one hand, and prevent the photoresist from deteriorating due to excessively high temperature during the etching process, making subsequent photoresist removal impossible.

[0055] 4.2) Ion beam etching is performed on the photolithographically etched film. Different etching times are set according to different film thicknesses to etch away the NiFe2O4 / Pb(Zr,Ti)O3 bilayer film and Sr3Al2O6 sacrificial layer in the area not covered by photoresist.

[0056] 4.3) Place the etched film into an acetone solution to completely dissolve the photoresist in the acetone (an ultrasonic cleaner with a power of less than 20W can be used to accelerate the dissolution of the photoresist). Then rinse the surface of the film with clean flowing acetone and finally dry it with nitrogen.

[0057] Step 5: Apply an edge clamping technique to the etched film surface using photolithography, such as... Figure 2 As shown in the dashed box, SU-8 photoresist is used to press the thin film layer around the elongated self-assembled pattern together with the substrate surface exposed after etching. This is to prevent excess film from being rolled up along with the film to be rolled up during the self-rolling process, and also to make the anchor point easier to break.

[0058] Step six involves immersing the sample in deionized water to wet-etch the Sr3Al2O6 sacrificial layer. Due to the lattice mismatch strain gradient of NiFe2O4 / Pb(Zr,Ti)O3, the film will curl up from the short side as the sacrificial layer dissolves. The internal stress from the self-curling will cause the anchor points and the connections to the elongated film to break sequentially, thus forming a multilayer single-roll structure, such as... Figure 3 As shown.

[0059] Step 7: Selectively break the two strips at the end of the coil using a micromanipulator, and use the micromanipulator and micromanipulation needle to transfer the multilayer single-roll structure to another substrate (e.g., silicon (Si) or polydimethylsiloxane (PDMS) flexible substrate) to achieve heterogeneous integration.

[0060] Example 2: Nickel ferrite (NiFe2O4) / lead zirconate titanate (Pb(Zr,Ti)O3) single-crystal thin film double-roll structure

[0061] The nickel ferrite (NiFe2O4) / lead zirconate titanate (Pb(Zr,Ti)O3) single crystal thin film double roll structure provided in this embodiment consists of, from bottom to top, a SrTiO3 substrate, a Sr3Al2O6 sacrificial layer, a NiFe2O4 ferromagnetic thin film layer, and a Pb(Zr,Ti)O3 ferroelectric thin film layer.

[0062] The implementation steps of this embodiment are as follows:

[0063] Steps one, two, and three are completely identical to those in Example 1.

[0064] Step four: A long, strip-shaped self-assembled pattern with anchor points is formed on the surface of the thin film layer using a combination of photolithography and ion beam etching (e.g., ...). Figure 4 (as shown), and remove the thin film layer and sacrificial layer around the edges of the substrate.

[0065] Long strip self-assembly pattern with anchor points, such as Figure 4 As shown, the device includes a long strip of film to be rolled up and multiple anchor points connected to the two long sides of the film, with the anchor points symmetrically arranged on the two long sides. The shaded area represents the portion where the film layer and sacrificial layer need to be removed; the length of the long strip of film to be rolled up is L0 = 1.52 mm, and the width is W0 = 620 μm; the rolling direction is from both ends to the middle (e.g., ...). Figure 4(As indicated by the middle arrow); the anchor point is trapezoidal, and the angle α between the anchor point and the elongated film is 45°; the distance between the first anchor point on the two short sides of the film and the initial roll-up position is L1 = 190 μm, and L1 ≤ W0 must be satisfied between L1 and W0, because the self-rolling film has the characteristic of being easy to roll up from the long side; the length of the connection between the anchor point and the elongated film is L2 = 20 μm; the distance between two adjacent anchor points on the same long side is L3 = 1100 μm; part of the film is etched around the edges of the sample, and this area is for subsequent edge pressing operations. The etching width can be determined as needed, such as 100 μm.

[0066] 4.1) Spin-coat three layers of photoresist onto the thin film surface, and then expose the area to be etched by photolithography. The three layers of photoresist form the etching pattern on one hand, and prevent the photoresist from deteriorating due to excessively high temperature during the etching process, making subsequent photoresist removal impossible.

[0067] 4.2) Ion beam etching is performed on the photolithographically etched film. Different etching times are set according to different film thicknesses to etch away the NiFe2O4 / Pb(Zr,Ti)O3 bilayer film and Sr3Al2O6 sacrificial layer in the area not covered by photoresist.

[0068] 4.3) Place the etched film into an acetone solution to completely dissolve the photoresist in the acetone (an ultrasonic cleaner with a power of less than 20W can be used to accelerate the dissolution of the photoresist). Then rinse the surface of the film with clean flowing acetone and finally dry it with nitrogen.

[0069] Step 5: Apply an edge clamping technique to the etched film surface using photolithography, such as... Figure 4 As shown in the dashed box, SU-8 photoresist is used to press the thin film layer around the elongated self-assembled pattern together with the substrate surface exposed after etching. This is to prevent excess film from being rolled up along with the film to be rolled up during the self-rolling process, and also to make the anchor point easier to break.

[0070] Step six involves immersing the sample in deionized water to wet-etch the Sr3Al2O6 sacrificial layer. Due to the lattice mismatch strain gradient of NiFe2O4 / Pb(Zr,Ti)O3, the film will curl up from the short side as the sacrificial layer dissolves. The internal stress from the self-curling will cause the anchor points and the connections to the elongated film to break sequentially, thus forming a double-curled structure, such as... Figure 5 As shown.

[0071] Step 7: The self-rolled composite thin film double roll structure is transferred to another substrate (e.g., silicon (Si) or polydimethylsiloxane (PDMS) flexible substrate) using a micromanipulator and micromanipulation needle to achieve heterogeneous integration.

Claims

1. A controllable self-assembly method for a strip-shaped thin-film device, characterized in that, Includes the following steps: S1, deposit a sacrificial layer on the substrate; S2, depositing a thin film layer with a lattice strain gradient on the sacrificial layer; S3, etch the thin film layer to form a strip-shaped self-assembled pattern; the strip-shaped self-assembled pattern includes a strip-shaped thin film and multiple anchor points symmetrically connected to the two long sides of the strip-shaped thin film; the length of the short side of the strip-shaped thin film is W0, and the distance between at least one short side of the strip-shaped thin film and its nearest anchor point is L1, and L1 and W0 satisfy L1≤W0. S4, wet etching is performed on the sacrificial layer. As the wet etching proceeds, the elongated film curls up along the direction of the long side starting from at least one short side. During the curling process, the connection between the anchor point and the elongated film breaks down in sequence.

2. The controllable self-assembly method for elongated thin-film devices according to claim 1, characterized in that, The distance between two adjacent anchor points on the same long side of the elongated film is L3, and L3≈W0; the length of the connection between the anchor point and the elongated film is L2, and 1μm≤L2≤5μm.

3. The controllable self-assembly method for elongated thin-film devices according to claim 1, characterized in that, The anchor point is trapezoidal, and the base of the trapezoid is connected to the long side of the strip-shaped film.

4. The controllable self-assembly method for the elongated thin-film device according to claim 3, characterized in that, The angle α between the waist of the anchor point and the long side of the elongated film is 30° to 60°.

5. The controllable self-assembly method for a strip-shaped thin-film device according to claim 1, characterized in that, The other short side of the long strip film is connected to several strips.

6. The controllable self-assembly method for the elongated thin-film device according to claim 5, characterized in that, strip length The diameter of the strip film is L5, the width is W1, and 10μm≤W1≤60μm. L5 is equal to the curling diameter of the strip film.

7. The controllable self-assembly method for a strip-shaped thin-film device according to claim 5, characterized in that, The distance between the short side of the long strip connecting the strip and its nearest anchor point is L4, and L4≈W0.

8. The controllable self-assembly method for a strip-shaped thin-film device according to claim 1, characterized in that, S3 also includes: etching away the thin film layer and sacrificial layer at the edge of the substrate to expose the substrate surface; and using photoresist to press the thin film layer around the elongated self-assembled pattern together with the exposed substrate surface.

9. The controllable self-assembly method for a strip-shaped thin-film device according to claim 1, characterized in that, The thin film layer can be a single-layer thin film or a multi-layer thin film.

10. A device obtained by the controllable self-assembly method according to any one of claims 1-9.

Citation Information

Patent Citations

  • Method for reducing diameter of self-crimping micron tube by virtue of metal nanoparticles

    CN104555899A

  • Topography minimization of neutral layer overcoats in directed self-assembly applications