A method for converting carbonylation residues into high-activity carbonylation feedstocks

By using a steel belt conveyor atmosphere furnace for segmented activation treatment, hydrogen and hydrogen sulfide gases are used to activate carbonyl slag, changing its elemental composition and morphology. This solves the problem of low activity in carbonyl slag, achieves efficient carbonylation reaction and waste reuse, and reduces production costs.

CN116574993BActive Publication Date: 2026-11-24JINCHUAN GROUP NICKEL COBALT CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202310570360.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-05-19
Publication Date
2026-11-24
Estimated Expiration
2043-05-19

AI Technical Summary

Technical Problem

In existing technologies, carbonyl slag has a high nickel content and is not activated, resulting in low efficiency of re-entry into the reactor for reaction, high production costs, low recovery rate of precious metals, and difficulty in effectively utilizing accumulated carbonyl slag.

Method used

A steel belt conveyor atmosphere furnace is used for segmented activation treatment. By combining hydrogen and hydrogen sulfide gases, the carbonyl slag is activated in stages to change its elemental composition and morphology, transforming it into a highly active carbonyl raw material. This includes introducing hydrogen and hydrogen sulfide gases at 900-1200℃, controlling the gas flow rate and purity, and carrying out a three-stage reaction.

Benefits of technology

It significantly improved the activity of carbonyl slag, reduced the nickel content from 22% to below 5.5%, improved the carbonylation reaction efficiency, reduced production costs, and enabled the reuse of waste materials.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

This invention provides a method for converting carbonylation slag into highly active carbonylation raw materials. The method involves reacting the carbonylation slag in stages with hydrogen and hydrogen sulfide in a steel belt conveyor atmosphere furnace at a specific temperature. The technical concept of this invention is based on the fact that when hydrogen reacts with nickel sulfide, hydrogen atoms in the hydrogen combine with nickel atoms on the nickel sulfide to form nickel hydride. This reaction requires heating and can therefore be carried out at 900-1200℃ as follows: 2H₂ + NiS₂ → 2Ni + 2H₂S. The reaction rate increases with increasing temperature. The activated nickel readily undergoes a carbonylation reaction with CO under medium pressure. This invention provides a simple and effective method for converting carbonylation slag into highly active carbonylation raw materials through activation treatment. It allows for the reuse of incompletely carbonylated waste. After testing, the metal content in the activated material, after a second carbonylation reaction, decreased from 22% to 5.5%.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of mining and metallurgical technology, and relates to a method for converting carbonyl slag into highly active carbonyl raw materials. Background Technology

[0002] Currently, nickel carbonylation is produced in an intermittent manner. The activity and composition of the raw materials directly affect the efficiency of the carbonylation reaction. Due to the inherent characteristics of the raw materials, the carbonylation reaction becomes increasingly difficult as the reaction time progresses.

[0003] Considering production costs, when the material yield is lower than a specified value, the reactor is subjected to replacement and slag removal operations. However, at this point, the nickel content in the carbonyl slag is still over 20%. Re-entering the reactor without activation results in similarly low yield, with production costs 10-15 times higher than normal production. The long-term accumulation of carbonyl slag hinders cash flow and significantly reduces the recovery rate of precious metals. Therefore, there is an urgent need to develop a process to convert high-nickel carbonyl slag into carbonyl raw materials. Summary of the Invention

[0004] The purpose of this invention is to address the problems existing in the prior art by providing a method for converting carbonyl slag into highly active carbonyl raw materials. This invention employs a segmented activation technique using hydrogen and hydrogen sulfide gases to activate the carbonyl slag, thereby altering the elemental composition and form of the carbonyl slag and converting it into a carbonyl raw material for recycling. This method solves the problem of low direct recovery rate of high-nickel carbonyl slag during the production process, which leads to low economic benefits.

[0005] Therefore, the present invention adopts the following technical solution: A method for converting carbonyl residue into a highly active carbonyl feedstock includes the following steps: a. Nitrogen gas is introduced into the steel belt conveyor atmosphere furnace to purge oxygen; b. Heating the furnace chamber of the steel belt conveyor atmosphere furnace, wherein the furnace temperature is controlled at 900-1200℃; c. Open the first-stage hydrogen valve and the second-stage hydrogen sulfide valve to introduce activation gas into the furnace, forming an activation atmosphere. The hydrogen and hydrogen sulfide in the atmosphere furnace are applied to the material in three stages. The first stage is the hydrogen reduction stage, with a hydrogen flow rate of 25-80 Nm³. 3 / h, hydrogen purity >98%; the second stage is the hydrogen sulfide activation stage, hydrogen sulfide flow rate 2.5-5.5Nm 3 / h, hydrogen sulfide purity >60%; the third stage is the hydrogen protection stage, hydrogen flow rate 25-50Nm 3 / h, hydrogen purity >80%, the remainder includes but is not limited to nitrogen, argon or other rare gases; In this invention, carbonyl slag is subjected to a phased reaction with hydrogen and hydrogen sulfide in a steel belt conveyor atmosphere furnace at a certain temperature. The main components of the carbonyl slag, NiS2, CuS, and Cu2S, undergo redox reactions, resulting in changes in elemental composition and increased activity of the carbonyl slag. d. Control the steel belt moving speed of the belt conveyor atmosphere furnace to 5m / h.

[0006] Furthermore, the furnace pressure of the atmosphere furnace is 2-5 kPa.

[0007] Furthermore, in step c, the material is reduced in the furnace for 5-7 hours.

[0008] The beneficial effects of this invention are as follows: 1. The technical concept of this invention is based on the fact that when hydrogen reacts with nickel sulfide, hydrogen atoms in the hydrogen gas combine with nickel atoms on the nickel sulfide to form nickel hydride. This reaction requires heating to occur, so it can be carried out at 900-1200℃: 2H2 + NiS2 → 2Ni + 2H2S. Nickel sulfide is a stable substance, so the reaction is highly sensitive to temperature. The reaction rate increases with increasing temperature. The activated nickel readily undergoes a carbonylation reaction with CO under medium pressure. 2. In the second stage of process control, the present invention introduces hydrogen sulfide at a flow rate of 2.5-5.5 Nm. 3 / h, purity >60%, this gas is used as a raw material activator. In the process, the exposed nickel metal is contacted with the surface of hydrogen sulfide in proportion to activate and precipitate elemental sulfur, ultimately achieving the purpose of catalytic carbonylation reaction. 3. In this invention, the carbonyl slag is treated with hydrogen and hydrogen sulfide in a belt conveyor atmosphere furnace and then used at a flow rate of 20-50 Nm³. 3 / h, hydrogen protection with a purity of >80% to prevent active materials from being passivated again; 4. This invention is simple to operate, has obvious effects, is easy to implement, and can realize the reuse of waste materials. After testing, the metal content in the carbonyl residue after the second carbonylation reaction decreased from 22% to 5.5%, which is quite effective. Detailed Implementation

[0009] In this invention, carbonyl slag is subjected to a phased contact reaction with hydrogen and hydrogen sulfide in a steel belt conveyor atmosphere furnace at a certain temperature, and the activation reaction is carried out under certain temperature, gas flow rate and activation time.

[0010] The technical solution of the present invention will be described below in conjunction with the implementation method.

[0011] Example 1 A method for converting carbonyl residue into a highly active carbonyl feedstock includes the following steps: a. Nitrogen gas is introduced into the steel belt conveyor atmosphere furnace to purge oxygen; b. Heating the furnace chamber of the steel belt conveyor atmosphere furnace, wherein the furnace temperature is controlled at 700℃; c. Place carbonyl slag with a nickel content of 22% and a material layer thickness of 5cm into an atmosphere furnace. Open the first hydrogen valve and the second hydrogen sulfide valve to introduce activation gas into the furnace, forming an activation atmosphere. The hydrogen and hydrogen sulfide in the atmosphere furnace act on the material in three stages. The first stage is the hydrogen reduction stage, with a hydrogen flow rate of 30 Nm³. 3 / h, hydrogen purity >98%; the second stage is the hydrogen sulfide activation stage, hydrogen sulfide flow rate 5Nm 3 / h, hydrogen sulfide purity >60%, the rest includes but is not limited to nitrogen, argon or other rare gases, the material is reduced in the furnace for 5 hours, and the nickel content in the carbonyl slag after the final carbonylation reaction is 18.63%.

[0012] Example 2 A method for converting carbonyl residue into a highly active carbonyl feedstock includes the following steps: a. Nitrogen gas is introduced into the steel belt conveyor atmosphere furnace to purge oxygen; b. Heating the furnace chamber of the steel belt conveyor atmosphere furnace, wherein the furnace temperature is controlled at 800℃; c. Place carbonyl slag with a nickel content of 22% and a material layer thickness of 5cm into an atmosphere furnace. Open the first hydrogen valve and the second hydrogen sulfide valve to introduce activation gas into the furnace, forming an activation atmosphere. The hydrogen and hydrogen sulfide in the atmosphere furnace act on the material in three stages. The first stage is the hydrogen reduction stage, with a hydrogen flow rate of 30 Nm³. 3 / h, hydrogen purity >98%; the second stage is the hydrogen sulfide activation stage, hydrogen sulfide flow rate 5Nm 3 / h, hydrogen sulfide purity >60%, the remainder includes but is not limited to nitrogen, argon or other rare gases, the material is reduced in the furnace for 5 hours, and the nickel content in the carbonyl slag after the final carbonylation reaction is 13.88%.

[0013] Example 3 A method for converting carbonyl residue into a highly active carbonyl feedstock includes the following steps: a. Nitrogen gas is introduced into the steel belt conveyor atmosphere furnace to purge oxygen; b. Heating the furnace chamber of the steel belt conveyor atmosphere furnace, wherein the furnace temperature is controlled at 900℃; c. Place carbonyl slag with a nickel content of 22% and a material layer thickness of 5cm into an atmosphere furnace. Open the first hydrogen valve and the second hydrogen sulfide valve to introduce activation gas into the furnace, forming an activation atmosphere. The hydrogen and hydrogen sulfide in the atmosphere furnace act on the material in three stages. The first stage is the hydrogen reduction stage, with a hydrogen flow rate of 30 Nm³.3 / h, hydrogen purity >98%; the second stage is the hydrogen sulfide activation stage, hydrogen sulfide flow rate 5Nm 3 / h, hydrogen sulfide purity >60%, the rest includes but is not limited to nitrogen, argon or other rare gases, the material is reduced in the furnace for 5 hours, and the nickel content in the carbonyl slag after the final carbonylation reaction is 10.02%.

[0014] Example 4 A method for converting carbonyl residue into a highly active carbonyl feedstock includes the following steps: a. Nitrogen gas is introduced into the steel belt conveyor atmosphere furnace to purge oxygen; b. Heating the furnace chamber of the steel belt conveyor atmosphere furnace, wherein the furnace temperature is controlled at 900℃; c. Place carbonyl slag with a nickel content of 22% and a material layer thickness of 5cm into an atmosphere furnace. Open the first hydrogen valve and the second hydrogen sulfide valve to introduce activation gas into the furnace, forming an activation atmosphere. The hydrogen and hydrogen sulfide in the atmosphere furnace act on the material in three stages. The first stage is the hydrogen reduction stage, with a hydrogen flow rate of 45 Nm³. 3 / h, hydrogen purity >98%; the second stage is the hydrogen sulfide activation stage, hydrogen sulfide flow rate 5Nm 3 / h, hydrogen sulfide purity >60%, the remainder includes but is not limited to nitrogen, argon or other rare gases, the material is reduced in the furnace for 5 hours, and the nickel content in the carbonyl slag after the final carbonylation reaction is 8.34%.

[0015] Example 5 A method for converting carbonyl residue into a highly active carbonyl feedstock includes the following steps: a. Nitrogen gas is introduced into the steel belt conveyor atmosphere furnace to purge oxygen; b. Heating the furnace chamber of the steel belt conveyor atmosphere furnace, wherein the furnace temperature is controlled at 900℃; c. Place carbonyl slag with a nickel content of 22% and a material layer thickness of 5cm into an atmosphere furnace. Open the first hydrogen valve and the second hydrogen sulfide valve to introduce activation gas into the furnace, forming an activation atmosphere. The hydrogen and hydrogen sulfide in the atmosphere furnace act on the material in three stages. The first stage is the hydrogen reduction stage, with a hydrogen flow rate of 45 Nm³. 3 / h, hydrogen purity >98%; the second stage is the hydrogen sulfide activation stage, hydrogen sulfide flow rate 4.5Nm 3 / h, hydrogen sulfide purity >60%, the remainder includes but is not limited to nitrogen, argon or other rare gases, the material is reduced in the furnace for 5 hours, and the nickel content in the carbonyl slag after the final carbonylation reaction is 5.5%.

[0016] Example 6 A method for converting carbonyl residue into a highly active carbonyl feedstock includes the following steps: a. Nitrogen gas is introduced into the steel belt conveyor atmosphere furnace to purge oxygen; b. Heating the furnace chamber of the steel belt conveyor atmosphere furnace, wherein the furnace temperature is controlled at 900℃; c. Place carbonyl slag with a nickel content of 22% and a material layer thickness of 5cm into an atmosphere furnace. Open the first hydrogen valve and the second hydrogen sulfide valve to introduce activation gas into the furnace, forming an activation atmosphere. The hydrogen and hydrogen sulfide in the atmosphere furnace act on the material in three stages. The first stage is the hydrogen reduction stage, with a hydrogen flow rate of 55 Nm³. 3 / h, hydrogen purity >98%; the second stage is the hydrogen sulfide activation stage, hydrogen sulfide flow rate 4.5Nm 3 / h, hydrogen sulfide purity >60%, the rest includes but is not limited to nitrogen, argon or other rare gases, the material is reduced in the furnace for 5 hours, and the nickel content in the carbonyl slag after the final carbonylation reaction is 7.2%.

[0017] Example 7 A method for converting carbonyl residue into a highly active carbonyl feedstock includes the following steps: a. Nitrogen gas is introduced into the steel belt conveyor atmosphere furnace to purge oxygen; b. Heating the furnace chamber of the steel belt conveyor atmosphere furnace, wherein the furnace temperature is controlled at 900℃; c. Place carbonyl slag with a nickel content of 22% and a material layer thickness of 5cm into an atmosphere furnace. Open the first hydrogen valve and the second hydrogen sulfide valve to introduce activation gas into the furnace, forming an activation atmosphere. The hydrogen and hydrogen sulfide in the atmosphere furnace act on the material in three stages. The first stage is the hydrogen reduction stage, with a hydrogen flow rate of 45 Nm³. 3 / h, hydrogen purity >98%; the second stage is the hydrogen sulfide activation stage, hydrogen sulfide flow rate 7Nm 3 / h, hydrogen sulfide purity >60%, the remainder includes but is not limited to nitrogen, argon or other rare gases, the material is reduced in the furnace for 5 hours, and the nickel content in the carbonyl slag after the final carbonylation reaction is 7.33%.

[0018] As shown in Table 1, under the premise of constant nickel content, material layer thickness, and furnace reaction time, the temperature of the atmosphere reduction furnace is controlled at 900℃, and the hydrogen flow rate is controlled at 45 Nm. 3 / h, hydrogen sulfide flow rate controlled at 4.5 Nm 3 The activated material produced at a rate of / h showed the greatest reduction in nickel content in the carbonylation slag after the carbonylation reaction, reaching 5.5%, indicating the highest carbonylation rate. This is most beneficial for nickel metal recovery in the carbonylation metallurgical production line. It also shows that under certain conditions, a higher hydrogen sulfide flow rate is not necessarily better; it should be maintained at a hydrogen flow rate of 25-50 Nm³ / h.3 / h, hydrogen sulfide flow rate 2.5-5.5 Nm 3 / h.

[0019] Table 1 .

Claims

1. A method for converting carbonyl slag into highly active carbonyl raw materials, characterized in that, Includes the following steps: a. Nitrogen gas is introduced into the steel belt conveyor atmosphere furnace to purge oxygen; b. Heating the furnace chamber of the steel belt conveyor atmosphere furnace, wherein the furnace temperature is controlled at 900-1200℃; c. Place the carbonyl slag into an atmosphere furnace, open the first hydrogen valve and the second hydrogen sulfide valve, and introduce activation gas into the furnace to form an activation atmosphere. The hydrogen and hydrogen sulfide in the atmosphere furnace act on the carbonyl slag in three stages. The first stage is the hydrogen reduction stage, with a hydrogen flow rate of 30-55 Nm³ / h and a hydrogen purity >98%; the second stage is the hydrogen sulfide activation stage, with a hydrogen sulfide flow rate of 4.5-5 Nm³ / h and a hydrogen sulfide purity >60%; the third stage is the hydrogen protection stage, with a hydrogen flow rate of 25-50 Nm³ / h and a hydrogen purity >80%. The remaining part includes nitrogen, argon, or other rare gases. The reduction time of carbonyl slag in the furnace is 5-7 hours; d. Control the steel belt moving speed of the belt conveyor atmosphere furnace to 5m / h.

2. The method for converting carbonyl slag into highly active carbonyl raw materials according to claim 1, characterized in that, The furnace pressure of the atmosphere furnace is 2-5 kPa.

Citation Information

Patent Citations

  • Improvements in the recovery of nickel from lateritic ores

    GB782242A

  • Apparatus and process for making high purity nickel

    US20080267810A1