Method for preparing grid-shaped photodetecting device by using tin-doped gallium oxide microwire

By fabricating a grid-like photodetector device using tin-doped gallium oxide microwires, the complex fabrication problem of gallium oxide photodetector arrays was solved, achieving low-cost, high-efficiency photoelectric performance and imaging applications.

CN116632114BActive Publication Date: 2026-11-24ZHENGZHOU UNIV
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202310700258.1
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-06-14
Publication Date
2026-11-24
Estimated Expiration
2043-06-14

AI Technical Summary

Technical Problem

In the existing technology, the photodetector arrays made of gallium oxide materials have the problems of complex fabrication process and high equipment requirements, which hinders their development in integrated and miniaturized photodetectors.

Method used

A photoelectric detection device with an N×N grid structure is formed by using tin-doped gallium oxide microwires and fabricating patterned electrodes by magnetron sputtering, which are then cross-laid and fixed on a sapphire substrate.

Benefits of technology

It realizes a low-cost, simple-to-operate photoelectric detection device with good structural stability and high-density integration, fast individual response speed, and is suitable for imaging components.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN116632114B_ABST
    Figure CN116632114B_ABST
Patent Text Reader

Abstract

A method for fabricating a grid-like photodetector using tin-doped gallium oxide microwires includes the following steps: fabricating microwires → preparing a sapphire substrate for meshing → sputtering patterned electrodes → wire selection and transfer → cross-laying and fixing the microwires on the substrate, etc., finally obtaining the tin-doped gallium oxide microwire-fabricated grid-like photodetector. Each detection unit is formed by the intersection of two tin-doped gallium oxide microwires, and the entire microwire array consists of multiple photodetector units formed by the intersection of multiple warp and weft microwires. This detection device exhibits good structural stability, and the fabrication method has the advantages of low cost, simple operation steps, short development cycle, and low equipment requirements. Experimental verification shows that the measured current changes significantly depending on the light projection position of the detection unit, making it suitable for imaging detection.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the technical field of optoelectronic components, and in particular to a method for preparing a grid-like photodetector using tin-doped gallium oxide microwires. Background Technology

[0002] A photodetector is a device that converts light radiation signals into electrical signals. Its working principle is based on the photoelectric effect of semiconductors or metals. Because deep ultraviolet radiation is absorbed by ozone and particulate matter in the Earth's atmosphere, solar radiation with wavelengths between 200-280 nm cannot penetrate the atmosphere and reach the Earth's surface, forming what is known as the solar blind zone. Photodetectors operating in this region are called solar-blind photodetectors. Due to the low background noise in the atmosphere, solar-blind photodetectors typically possess advantages such as high signal-to-noise ratio, low false alarm rate, high accuracy, and high sensitivity. Therefore, photodetectors are of great significance in both civilian and military applications, including fire early warning, water purification, ultraviolet early warning, and ultraviolet countermeasures. Recently, some wide bandgap semiconductors, such as AlGaN, AlN, ZnMgO, diamond, and gallium oxide, have been developed for use in solar-blind photodetectors. Compared to other materials, gallium oxide has significant advantages: its bandgap is 4.9 eV, directly corresponding to the solar-blind band, and it has high chemical stability and lower growth costs compared to other materials. Meanwhile, one-dimensional nanowires possess quantum confinement effects and surface size effects, which can significantly improve the light absorption and carrier transport characteristics of devices.

[0003] With the trend towards integration and miniaturization of optoelectronic devices, arrayed photodetectors have become a research hotspot. A solar-blind photodetector system generally consists of three parts: a solar-blind photodetector array, a readout circuit, and a signal processing circuit. The solar-blind detector array is the main component of the detection system, serving as a crucial device for converting optical signals into electrical signals. In 2017, a detector array fabricated using gallium oxide was first proposed. Although some progress has been made, its development is still hindered by complex fabrication processes and high equipment requirements. Therefore, developing simpler fabrication methods has become a challenge for those skilled in the art. Summary of the Invention

[0004] To address the aforementioned problems and achieve excellent processability and low manufacturing cost, this invention provides a simple method for fabricating a grid-like photodetector using tin-doped gallium oxide microwires.

[0005] The technical solution of the present invention is: a method for preparing a grid-like photoelectric detection device using tin-doped gallium oxide microwires, comprising the following steps; Step 1: Fabricate tin-doped gallium oxide microwires. Step 2: Prepare the sapphire substrate for mesh fabrication. Step 3: Sputtering to create patterned electrodes Gold electrodes with specific patterns were sputtered onto a sapphire substrate with a grid using a magnetron sputtering instrument. Step 4: Line Selection and Transfer Under a microscope, select a micron-length wire and transfer the tin-doped gallium oxide micron-wire onto the sapphire substrate used for meshing after step 3. Step 5: Cross-laying and fixing the mesh Under a microscope, 2N tin-doped gallium oxide microwires are arranged crosswise on a sapphire substrate with a sputtered gold electrode pattern using tweezers. N tin-doped gallium oxide microwires serve as warp threads and N tin-doped gallium oxide microwires serve as weft threads, forming an N×N grid structure, where N≥4. At the same time, under a microscope, the two ends of the tin-doped gallium oxide microwires are fixed to the gold electrode.

[0006] Preferably, step 1 includes the following sub-steps. 101) Weigh out gallium oxide powder, activated carbon powder and tin oxide powder in a mass ratio of 1:1:2, mix them and put them into a mortar, add anhydrous ethanol until the mixed powder is submerged, and then grind them thoroughly. 102) Clean the sapphire substrate for wire fabrication, deposit a 500 nm thick gold film on the cleaned sapphire substrate for wire fabrication using magnetron sputtering, and rapidly anneal the sapphire substrate for wire fabrication with the gold film deposited; after annealing, the gold film on the sapphire substrate for wire fabrication cracks into gold particles, forming a sapphire substrate for wire fabrication with gold particles. 103) In a conventional CVD tube furnace, the mixed powder ground in step 101) is placed in the center of a rigid boat. The sapphire substrate for wire fabrication with gold particles is inverted and placed directly above the mixed powder, with the gold particles facing the powder. Ar=200sccm and O2=5sccm are set. The temperature is raised to 1160℃ after 3 hours and held for 1 hour. A large number of white tin-doped gallium oxide microwires are clearly visible to the naked eye on the sapphire substrate for wire fabrication.

[0007] Preferably, step 2 is as follows: The double-sided polished sapphire substrate was cut into 1.5cm×1.5cm squares. Then, the double-sided polished sapphire substrate was cleaned sequentially with acetone for 15min, anhydrous ethanol for 15min, and deionized water for 15min. The surface of the double-sided polished sapphire substrate was dried with nitrogen gas and used as a sapphire substrate for mesh laying.

[0008] Preferably, step 3 is as follows: A custom rigid mask is placed on a sapphire substrate for mesh fabrication. A gold electrode with a thickness of d is deposited using a magnetron sputtering instrument. The thickness is 80nm≤d≤120nm. A total of 4N inner gold electrodes are arranged in a square with N equally spaced inner gold electrodes on each side. The inner gold electrodes on opposite sides are opposite each other, and the distance between opposite sides is L.

[0009] Preferably, step 4 includes the following sub-steps. 401) The tin-doped gallium oxide microwires were transferred to a cleaned sapphire substrate using tweezers, and separated into individual microwires under a microscope. 402) Under a microscope, select 2N tin-doped gallium oxide microwires with a length of L±0.1mm, and use tweezers to transfer the selected microwires to a sapphire substrate with patterned electrodes in sequence.

[0010] Preferably, the mesh after step 5) is a plain weave with alternating warp and weft threads.

[0011] Preferably, step 5 is as follows: The steps for creating an alternating warp and weft wire mesh on a sapphire substrate under a microscope are as follows. 501) Select a micron wire as the first warp, with the two ends of the micron wire close to or in contact with the first column of gold electrodes, and then fix it with silver paste; 502) Select a micron-sized wire as the first weft wire, with the two ends of the micron-sized wire close to or in contact with the two ends of the first row of gold electrodes, and then fix it with silver paste; 503) Select a micron wire as the second warp, with the two ends of the micron wire close to or in contact with the second column of gold electrodes, and then fix it with silver paste; 504) Select a micron wire as the second micron wire, drop anhydrous ethanol onto the substrate to cover the micron wire, soften the micron wire, and pass the micron wire through the lower part of the first meridian; the two ends of the micron wire are close to or in contact with the second row of gold electrodes, and then fixed with silver paste. 505) Select a micron wire as the third warp wire, drop anhydrous ethanol onto the substrate to cover the micron wire, soften the micron wire, and pass the micron wire through the lower part of the first weft wire; the two ends of the micron wire are close to or in contact with the third column of gold electrodes, and then fixed with silver paste. 506) Select a micron wire as the third weft wire, drop anhydrous ethanol onto the substrate to cover the micron wire, soften the micron wire, and pass the micron wire through the lower part of the second warp wire and over the upper part of the first warp wire in sequence; the two ends of the micron wire are close to or in contact with the third row of gold electrodes, and then fixed with silver paste. 507) Select a micron wire as the fourth warp, drop anhydrous ethanol onto the substrate to cover the micron wire and soften it, and pass the micron wire through the lower part of the second weft wire and over the upper part of the first weft wire in sequence; the two ends of the micron wire are close to or in contact with the fourth column of gold electrodes, and then fixed with silver paste. 508) Select a micron wire as the fourth weft wire, drop anhydrous ethanol onto the substrate to cover the micron wire, soften the micron wire, pass the micron wire through the lower part of the third warp wire, cross the upper part of the second warp wire, and pass through the lower part of the first warp wire in sequence; the two ends of the micron wire are close to or in contact with the fourth row of gold electrodes, and then fixed with silver paste. Using the above method, the 5th to Nth meridians and the 5th to Nth parallels are sequentially and alternately threaded and fixed between the corresponding gold electrodes on the sapphire substrate used for meshing, forming an N×N grid-shaped photodetector.

[0012] Preferably, the silver paste fixation is specifically as follows: A small amount of silver paste is applied to both ends of the microwire and the electrode using a tungsten needle. The ends of the microwire are initially connected to the electrode. Then, the silver paste is dried on a 90°C heating stage, ultimately fixing the microwire onto the gold electrode. Preferably, N=8.

[0013] Preferably, L=4mm.

[0014] The beneficial effects of this invention are: (1) The grid-like photodetector based on tin-doped gallium oxide microwires designed in this invention has good structural stability and the preparation method has the advantages of low cost, simple operation steps, short development cycle and low equipment requirements. (2) The length of the tin-doped gallium oxide microwire prepared by the present invention can reach more than 4 mm, which provides operability for subsequent weaving into a mesh.

[0015] (3) The grid-shaped photoelectric detection device formed by this method has a fast single response speed, a high switching ratio, and high quantum efficiency. The integration of the detectors allows its photoelectric performance research to be not limited to a single device.

[0016] (4) The grid-shaped photoelectric detection device formed by this method, in the embodiment, realizes an 8×8 array in the plane, achieving high-density integration.

[0017] (4) The mesh-shaped photoelectric detector made by this method has a greater contact force at the intersection of the warp and weft of its woven structure, which can ensure the conductivity effect and facilitate the multiple and long-term use of the mesh-shaped photoelectric detector.

[0018] (5) The grid-shaped photoelectric detection device produced by this method has a large difference in the internal current data of the intersection point and the non-intersection point when the light spot is irradiated. Based on the relationship between the projection position of the light spot and the current, the device can be used for image detection and can be used as an imaging component. Attached Figure Description

[0019] Figure 1 This is the tin-doped gallium oxide microwire prepared by the present invention; Figure 2 This is a substrate image after patterning the gold electrodes in this invention; Figure 3 This is a schematic diagram of the structure of the grid-like photoelectric detection device prepared by the tin-doped gallium oxide microwires obtained in this invention; Figure 4 This is a physical image of the mesh-like photoelectric detection device structure prepared by the tin-doped gallium oxide microwires of this invention; Figure 5 yes Figure 4 A magnified image of the intersection points under a microscope; Figure 6 Micrometer-scale linear array diagram of non-cross-linked fabrication methods; Figure 7 This is a graph showing the relationship between the distance between the light spot and the intersection point and the photocurrent in this invention; Figure 8 This is the IV curve of the 8×8 array of 64 units obtained by this invention under darkness and 266nm illumination; Figure 9 This is the IT curve of the 8×8 detector unit of this invention under 30V bias voltage and 266nm illumination with a light intensity of 6mW. Figure 10 This is a photoresponse curve of the 8×8 detector unit of the present invention under different bias voltages.

[0020] Figure 3 1. Outer electrode, 2. Inner electrode, 3. Inner and outer electrode guide wires, 4. Tin-doped gallium oxide micrometer wire meridian, 5. Tin-doped gallium oxide micrometer wire parallel, 6. Longitude and parallel intersection. Detailed Implementation

[0021] The following description, in conjunction with the accompanying drawings, details the implementation methods and usage of this invention.

[0022] Example 1: A method for fabricating a grid-like photodetector using tin-doped gallium oxide microwires, comprising the following steps; Step 1: Fabrication of tin-doped gallium oxide microwires Gallium oxide powder, activated carbon powder, and tin oxide powder were weighed in a mass ratio of 1:1:2, mixed, and placed in a mortar. Anhydrous ethanol was added until the powder mixture was submerged, and then the mixture was ground thoroughly. Adding anhydrous ethanol to grind the powder mixture ensures more thorough grinding, and the volatile nature of anhydrous ethanol prevents the formation of residual impurities in the powder mixture.

[0023] 102) Clean the sapphire substrate for wire fabrication, deposit a 500 nm thick gold film on the cleaned sapphire substrate for wire fabrication using magnetron sputtering, and rapidly anneal the sapphire substrate for wire fabrication with the gold film deposited; after annealing, the gold film on the sapphire substrate for wire fabrication cracks into gold particles, forming a sapphire substrate for wire fabrication with gold particles. 103) In a conventional CVD tube furnace, the mixed powder ground in step 101) is placed in the center of a rigid boat. A sapphire substrate with gold particles for wire fabrication is inverted directly above the mixed powder, with the gold particles facing the powder. Ar=200 sccm and O2=5 sccm are set. The temperature is increased to 1160℃ after 3 hours and held for 1 hour. Numerous white tin-doped gallium oxide microwires are clearly visible to the naked eye on the sapphire substrate. See details... Figure 1 .

[0024] Step 2: Prepare the sapphire substrate for mesh fabrication. The double-sided polished sapphire substrate was cut into 1.5cm×1.5cm squares. Then, the double-sided polished sapphire substrate was cleaned sequentially with acetone for 15min, anhydrous ethanol for 15min, and deionized water for 15min. The surface of the double-sided polished sapphire substrate was dried with nitrogen gas and used as a sapphire substrate for mesh laying.

[0025] Step 3: Sputtering to create patterned electrodes A custom rigid mask is placed on a sapphire substrate for mesh fabrication. A gold electrode with a thickness of d is deposited using a magnetron sputtering instrument. The thickness is 80nm≤d≤120nm. A total of 4N inner gold electrodes are arranged in a square with four sides. Each side has N inner gold electrodes arranged at equal intervals. The inner gold electrodes on opposite sides are opposite each other, and the distance between opposite sides is L, where L=4mm. N=8.

[0026] Step 4: Line Selection and Transfer Under a microscope, select a micron-length wire and transfer the tin-doped gallium oxide micron-wire onto the sapphire substrate used for meshing as completed in step 3, as detailed below. 401) The tin-doped gallium oxide microwires were transferred to a cleaned sapphire substrate using tweezers, and separated into individual microwires under a microscope. 402) Under a microscope, select 2N tin-doped gallium oxide microwires with a length of L±0.1mm, and use tweezers to transfer the selected microwires to a sapphire substrate with patterned electrodes in sequence.

[0027] Step 5: Cross-laying and fixing the mesh Under a microscope, 2N tin-doped gallium oxide microwires are arranged crosswise on a sapphire substrate with a sputtered gold electrode pattern using tweezers. N tin-doped gallium oxide microwires serve as warp threads and N tin-doped gallium oxide microwires serve as weft threads, forming an N×N grid structure, where N=8. At the same time, under a microscope, the two ends of the tin-doped gallium oxide microwires are fixed to the gold electrode.

[0028] The specific operational details are as follows: Under a microscope, the steps for weaving an alternating warp and weft wire mesh on a sapphire substrate are as follows. 501) Select a micron wire as the first warp, with the two ends of the micron wire close to or in contact with the first column of gold electrodes, and then fix it with silver paste; 502) Select a micron-sized wire as the first weft wire, with the two ends of the micron-sized wire close to or in contact with the two ends of the first row of gold electrodes, and then fix it with silver paste; 503) Select a micron wire as the second warp, with the two ends of the micron wire close to or in contact with the second column of gold electrodes, and then fix it with silver paste; 504) Select a micron wire as the second micron wire, drop anhydrous ethanol onto the substrate to cover the micron wire, soften the micron wire, and pass the micron wire through the lower part of the first meridian; the two ends of the micron wire are close to or in contact with the second row of gold electrodes, and then fixed with silver paste. 505) Select a micron wire as the third warp wire, drop anhydrous ethanol onto the substrate to cover the micron wire, soften the micron wire, and pass the micron wire through the lower part of the first weft wire; the two ends of the micron wire are close to or in contact with the third column of gold electrodes, and then fixed with silver paste. 506) Select a micron wire as the third weft wire, drop anhydrous ethanol onto the substrate to cover the micron wire, soften the micron wire, and pass the micron wire through the lower part of the second warp wire and over the upper part of the first warp wire in sequence; the two ends of the micron wire are close to or in contact with the third row of gold electrodes, and then fixed with silver paste. 507) Select a micron wire as the fourth warp, drop anhydrous ethanol onto the substrate to cover the micron wire and soften it, and pass the micron wire through the lower part of the second weft wire and over the upper part of the first weft wire in sequence; the two ends of the micron wire are close to or in contact with the fourth column of gold electrodes, and then fixed with silver paste. 508) Select a micron wire as the fourth weft wire, drop anhydrous ethanol onto the substrate to cover the micron wire, soften the micron wire, pass the micron wire through the lower part of the third warp wire, cross the upper part of the second warp wire, and pass through the lower part of the first warp wire in sequence; the two ends of the micron wire are close to or in contact with the fourth row of gold electrodes, and then fixed with silver paste. Using the above method, the 5th to 8th warp and 5th to 8th weft wires are sequentially and alternately threaded and fixed between the corresponding gold electrodes on the sapphire substrate used for meshing, forming an 8×8 grid-shaped photodetector.

[0029] Since the tin-doped gallium oxide microwires produced in step 1 of this embodiment are not very flexible, they need to be soaked in anhydrous ethanol to make them more flexible when they need to be interlaced and braided. This makes it easier to interlac and braid. After the anhydrous ethanol evaporates, the tin-doped gallium oxide microwires return to their original flexibility. This results in a greater contact force at the intersection of warp and weft, which ensures conductivity and facilitates the repeated and long-term use of the grid-shaped photodetector.

[0030] The silver paste fixation process is as follows: a small amount of silver paste is applied to both ends of the microwire and the electrode using a tungsten needle. The ends of the microwire are initially connected to the electrode. Then, the silver paste is dried on a heating table at 90°C, thus fixing the microwire onto the gold electrode.

[0031] Example 2: This example differs from Example 1 in that, in fabricating the grid-like photodetector using tin-doped gallium oxide microwires, all the latitude lines are placed first, followed by all the longitude lines. Figure 6 As shown, with Figure 3 Compared to traditional arrays, this type of cross array has poor stability. It can be used in the early stages of preparation, but after being left for a long time or used multiple times, the intersections of the micrometer wires will not make contact due to the lack of their own pressure control. As a result, the intersections will not have conductivity or will have poor conductivity, causing the grid-like photoelectric detection device to fail.

[0032] Example 3: Based on Example 1, a mask for applying silver paste is added in step 5. The area of ​​the silver paste is controlled by the mask. Since the spacing between the inner gold electrodes is small, directly applying silver paste can easily short-circuit adjacent inner gold electrodes.

[0033] Based on Embodiment 1 or 3, the distance between two adjacent meridians and two adjacent parallels of latitude is set to 400 micrometers; the electrodes at both ends of a certain intersection point are connected to the detection device via wires, a light spot is projected onto the intersection point, and the device is moved by a displacement platform to measure the distance as shown in the figure. Figure 7The figure shows the relationship between the distance between the light spot and the intersection point and the photocurrent. The figure shows that when the distance between the light spot and the intersection point is 300 micrometers, the current differs by two orders of magnitude compared to when the light spot is illuminating the intersection point. This indicates that there is a corresponding relationship between the light irradiation position and the current, thus demonstrating that the detection device can be used for imaging.

[0034] Specific imaging application process: Using the diagonal as the dividing line, select one half of the electrodes to connect to the detection device, ensuring that both electrodes at each intersection are connected to wires. In the laboratory stage, the light forming the pattern is projected onto the grid-shaped photoelectric detection device by using a light source and a mask. By continuously changing the electrode wires connected to the detection device at each intersection, the corresponding internal current data at each intersection can be detected. Based on the current change pattern when light shines on the intersection and the parts outside the intersection in Experiment Example 1, the illumination position data of the light around each intersection can be derived in reverse. By summing up all the illumination position data, the shape of the pattern projected through the mask can be obtained.

[0035] In practical applications, this sensor can be used to switch the connection to the detection circuit at each intersection point sequentially using multiple program-controlled switches in parallel. This achieves an automated and rapid switching process, quickly detecting the shape of light.

[0036] The 64 units of the tin-doped gallium oxide microwire-based mesh photodetector fabricated in Example 1 were tested under both dark and light conditions (using a semiconductor analyzer 4200). The test results are as follows: Figure 8 As shown in the figure, each unit of the 8×8 array has good photoelectric properties, and the fabricated array has good uniformity.

[0037] Select a single detector unit for further testing, such as Figure 9 As shown, under a 30V bias and 5.5mW 266nm light illumination, the device exhibits a good on / off ratio, and the test was repeated for 8 It cycles. The device demonstrates good repeatability.

[0038] The spectral response curves of a single detector element in an 8×8 array under different bias voltages are shown below. Figure 10 As shown, there is a good response in the solar blind region, and the responsiveness increases with the increase of the applied bias voltage.

[0039] The prepared solar-blind detector array exhibits excellent photoelectric performance and good uniformity, making it suitable for array imaging.

Claims

1. A method for fabricating a grid-like photodetector using tin-doped gallium oxide microwires, comprising the following steps: Step 1: Fabricate tin-doped gallium oxide microwires. Step 2: Prepare the sapphire substrate for mesh fabrication. Step 3: Sputtering to create patterned electrodes Gold electrodes with specific patterns were sputtered onto a sapphire substrate with a grid using a magnetron sputtering instrument. Step 4: Line Selection and Transfer Under a microscope, select a micron-length wire and transfer the tin-doped gallium oxide micron-wire onto the sapphire substrate used for meshing after step 3. Step 5: Cross-laying and fixing the mesh Under a microscope, tweezers are used to arrange 2N tin-doped gallium oxide microwires in a crisscross pattern on a sapphire substrate with a sputtered gold electrode pattern. N tin-doped gallium oxide microwires are used as warp and N tin-doped gallium oxide microwires are used as weft, forming an N×N grid structure, where N≥4. At the same time, under a microscope, the two ends of the tin-doped gallium oxide microwires are fixed to the gold electrode. The mesh after weaving is a plain weave structure with alternating warp and weft threads, as detailed below: The steps for creating an alternating warp and weft wire mesh on a sapphire substrate under a microscope are as follows. 501) Select a micron wire as the first warp, with the two ends of the micron wire close to or in contact with the first column of gold electrodes, and then fix it with silver paste; 502) Select a micron-sized wire as the first weft wire, with the two ends of the micron-sized wire close to or in contact with the two ends of the first row of gold electrodes, and then fix it with silver paste; 503) Select a micron wire as the second warp, with the two ends of the micron wire close to or in contact with the second column of gold electrodes, and then fix it with silver paste; 504) Select a micron wire as the second micron wire, drop anhydrous ethanol onto the substrate to cover the micron wire, soften the micron wire, and pass the micron wire through the lower part of the first meridian; the two ends of the micron wire are close to or in contact with the second row of gold electrodes, and then fixed with silver paste. 505) Select a micron wire as the third warp wire, drop anhydrous ethanol onto the substrate to cover the micron wire, soften the micron wire, and pass the micron wire through the lower part of the first weft wire; the two ends of the micron wire are close to or in contact with the third column of gold electrodes, and then fixed with silver paste. 506) Select a micron wire as the third weft wire, drop anhydrous ethanol onto the substrate to cover the micron wire, soften the micron wire, and pass the micron wire through the lower part of the second warp wire and over the upper part of the first warp wire in sequence; the two ends of the micron wire are close to or in contact with the third row of gold electrodes, and then fixed with silver paste. 507) Select a micron wire as the fourth warp, drop anhydrous ethanol onto the substrate to cover the micron wire and soften it, and pass the micron wire through the lower part of the second weft wire and over the upper part of the first weft wire in sequence; the two ends of the micron wire are close to or in contact with the fourth column of gold electrodes, and then fixed with silver paste. 508) Select a micron wire as the fourth weft wire, drop anhydrous ethanol onto the substrate to cover the micron wire, soften the micron wire, pass the micron wire through the lower part of the third warp wire, cross the upper part of the second warp wire, and pass through the lower part of the first warp wire in sequence; the two ends of the micron wire are close to or in contact with the fourth row of gold electrodes, and then fixed with silver paste. Using the above method, the 5th to Nth meridians and the 5th to Nth parallels are sequentially and alternately threaded and fixed between the corresponding gold electrodes on the sapphire substrate used for meshing, forming an N×N grid-shaped photodetector.

2. The method for fabricating a grid-like photoelectric detection device using tin-doped gallium oxide microwires according to claim 1, characterized in that: Step 1 includes the following sub-steps. 101) Weigh out gallium oxide powder, activated carbon powder and tin oxide powder in a mass ratio of 1:1:2, mix them and put them into a mortar, add anhydrous ethanol until the mixed powder is submerged, and then grind them thoroughly. 102) Clean the sapphire substrate for wire fabrication, deposit a 500nm thick gold film on the cleaned sapphire substrate for wire fabrication using magnetron sputtering, and rapidly anneal the sapphire substrate for wire fabrication with the gold film deposited; after annealing, the gold film on the sapphire substrate for wire fabrication cracks into gold particles, forming a sapphire substrate for wire fabrication with gold particles. 103) In a conventional CVD tube furnace, the mixed powder ground in step 101) is placed in the center of a rigid boat. The sapphire substrate for wire fabrication with gold particles is inverted and placed directly above the mixed powder, with the gold particles facing the powder. Ar=200sccm and O2=5sccm are set. The temperature is raised to 1160℃ after 3 hours and held for 1 hour. A large number of white tin-doped gallium oxide microwires are clearly visible to the naked eye on the sapphire substrate for wire fabrication.

3. The method for fabricating a grid-like photoelectric detection device using tin-doped gallium oxide microwires according to claim 1, characterized in that: Step 2 is described in detail below. The double-sided polished sapphire substrate was cut into 1.5cm×1.5cm squares. Then, the double-sided polished sapphire substrate was cleaned sequentially with acetone for 15min, anhydrous ethanol for 15min, and deionized water for 15min. The surface of the double-sided polished sapphire substrate was dried with nitrogen gas and used as a sapphire substrate for mesh laying.

4. The method for fabricating a grid-like photoelectric detection device using tin-doped gallium oxide microwires according to claim 1, characterized in that: Step 3 is described in detail below. A custom rigid mask is placed on a sapphire substrate for mesh fabrication. A gold electrode with a thickness of d is deposited using a magnetron sputtering instrument. The thickness is 80nm≤d≤120nm. A total of 4N inner gold electrodes are arranged in a square with N equally spaced inner gold electrodes on each side. The inner gold electrodes on opposite sides are opposite each other, and the distance between opposite sides is L.

5. The method for fabricating a grid-like photoelectric detection device using tin-doped gallium oxide microwires according to claim 1, characterized in that: Step 4 includes the following sub-steps. 401) The tin-doped gallium oxide microwires were transferred to a cleaned sapphire substrate using tweezers, and separated into individual microwires under a microscope. 402) Under a microscope, select 2N tin-doped gallium oxide microwires with a length of L±0.1mm, and use tweezers to transfer the selected microwires to a sapphire substrate with patterned electrodes in sequence.

6. The method for fabricating a grid-like photoelectric detection device using tin-doped gallium oxide microwires according to claim 1, characterized in that: The silver paste fixation is specifically described below. A small amount of silver paste is applied to both ends of the microwire and the electrode using a tungsten needle. The ends of the microwire are initially connected to the electrode. Then, the silver paste is dried on a 90°C heating table, which finally fixes the microwire onto the gold electrode.

7. The method for fabricating a grid-like photoelectric detection device using tin-doped gallium oxide microwires according to claim 1, characterized in that: The N=8 mentioned above.

8. The method for fabricating a grid-like photodetector using tin-doped gallium oxide microwires according to claim 5, characterized in that: The L=4mm.

Citation Information

Patent Citations

  • Vertical MSM structure photoelectric imaging system based on semi-insulating 4H-SiC substrate

    CN115172509A