Construction method of energy deformation compaction pile composite foundation of microbial solidified construction waste filler

By using microbial solidification of construction waste filler, combined with specific bacterial strains and cementing liquid, an energy deformation compaction pile composite foundation is formed, which solves the problem of insufficient pile structural strength and achieves efficient and environmentally friendly utilization of construction waste resources and improvement of bearing capacity.

CN116676951BActive Publication Date: 2026-11-24HAINAN UNIV
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202310632906.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-05-31
Publication Date
2026-11-24
Estimated Expiration
2043-05-31

AI Technical Summary

Technical Problem

With the improvement of engineering quality requirements, the existing composite foundation technology of carrier piles has insufficient pile structural strength, making it difficult to effectively improve bearing capacity. In addition, the traditional CFG pile composite foundation has high cost and cannot effectively utilize construction waste resources.

Method used

Microbial solidified construction waste filler is used. By adding bacterial solutions and cementing solutions of Bacillus uric acid oxidizing, Providencia reticularis, and Bacillus pasteurellis, and combining them with construction waste filler of different particle sizes, an energy deformation compaction pile composite foundation is formed, which improves the structural strength and bearing capacity of the pile body.

Benefits of technology

It significantly improves the bearing capacity of composite foundations and the strength of pile structures, and is simple to construct, environmentally friendly and efficient, saving engineering costs and conforming to the concept of green development.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0004258891910000071
    Figure BDA0004258891910000071
  • Figure BDA0004258891910000081
    Figure BDA0004258891910000081
Patent Text Reader

Abstract

This invention provides a construction method for an energy deformation compaction pile composite foundation using microbial-solidified construction waste filler. The method uses construction waste as filler, which is inserted into the pile hole along with a mixture of bacterial solution and cementing liquid. The construction waste filler is made from crushed waste concrete blocks and consists of two sizes of construction waste with particle sizes of 15-25 mm and 3-5 mm, respectively. The bacterial solution is prepared from *Arthrobacter urate-oxidizing*, *Providensia rubella*, and *Bacillus pasteurellii*. This invention, by using construction waste fillers of different particle sizes as raw materials and employing *Arthrobacter urate-oxidizing*, *Providensia rubella*, and *Bacillus pasteurellii* to solidify the construction waste filler, effectively improves the microbial solidification effect and enhances the bearing capacity of the resulting composite foundation.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of compaction piles, and in particular to a construction method for a composite foundation of energy-deformable compaction piles using microbial solidified construction waste fillers. Background Technology

[0002] Construction waste, including discarded concrete and blocks, arises from both the demolition of existing structures and the construction of new buildings, as well as from damage caused by disasters such as earthquakes and fires. If this construction waste can be transformed into valuable resources, the greatest benefit is the protection of the ecological environment, reducing the exploitation of natural sand and gravel resources, thereby achieving the goal of sustainable development.

[0003] The carrier pile composite foundation is a composite foundation treatment technology that uses plain carrier piles as reinforcement to achieve joint load-bearing between piles and soil. This technology can be applied to both building foundation treatment (rigid foundation) and roadbed treatment (flexible foundation). In buildings, the carrier pile composite foundation includes: a rigid foundation, a cushion layer, plain carrier piles, and soil between piles; in roadbeds, it includes: geotextiles, a cushion layer, plain carrier piles, and soil between piles. By adjusting the pile-soil displacement at the pile top through the cushion layer, joint load-bearing between piles and soil is achieved, maximizing the single pile bearing capacity while making rational use of the soil between piles. To fully utilize the high single pile bearing capacity of the carrier piles, the pile top is expanded within a certain depth range, transferring more of the upper load to the deeper soil layers through the single pile.

[0004] Compared to traditional CFG pile composite foundations, composite foundations have higher bearing capacity due to the high single-pile bearing capacity of carrier piles. The pile top expands within a certain range, transferring more load to the soil at the pile tip. The soil at the pile tip has higher bearing capacity and modulus than shallow soil, effectively reducing foundation settlement. Costs are 10-30% lower than with CFG piles. However, as engineering quality requirements continue to increase, the structural strength of the piles also needs further improvement. Summary of the Invention

[0005] In view of this, the present invention proposes a construction method for a composite foundation of energy deformation compaction piles using microbial solidified construction waste fillers, thereby solving the above-mentioned problems.

[0006] The technical solution of this invention is implemented as follows:

[0007] A construction method for an energy deformation compaction pile composite foundation using microbial solidified construction waste filler is disclosed. Construction waste is used as filler material, which is inserted into the holes at the pile locations. Simultaneously, a mixture of bacterial solution and cementing liquid is added. The construction waste filler material is made from crushed waste concrete blocks and consists of two specifications of construction waste with particle sizes of 15–25 mm and 3–5 mm, respectively. The bacterial solution is prepared from *Arthrobacter urate-oxidizing bacteria*, *Providencia rettgeri*, and *Sporosarcina pasteurii*.

[0008] Preferably, the mass ratio of the two particle sizes of 15-25mm and 3-5mm in the construction waste filler is 1:0.3-0.5.

[0009] Preferably, by weight, for every 1 part of construction waste filler, 0.3 to 0.4 parts of a mixture of bacterial solution and cementing solution are added.

[0010] Preferably, the ratio of bacterial solution to cementing solution in the bacterial solution and cementing solution mixture is 0.4-0.6:0.8-1.2.

[0011] Preferably, the viable bacterial concentrations of Arthrobacter urate-oxidizing bacteria, Providencia reticularis, and Bacillus pasteurellii in the bacterial solution are (4.5–5.5) × 10⁻⁶. 8 cfu / g, (2-4)*10 8 cfu / g, (1.5~2.5)*10 8 cfu / g.

[0012] Preferably, the cementing solution is prepared from the following raw materials: calcium chloride, urea, coconut husk powder, coconut shell powder, ammonium carbonate, sodium hexametaphosphate, and water.

[0013] Preferably, the cementing solution is prepared from the following raw materials in parts by weight: 8-12 parts calcium chloride, 4-6 parts urea, 0.1-0.2 parts sodium chloride, 1.4-1.6 parts coconut husk powder, 0.8-1.2 parts coconut shell powder, 0.2-0.4 parts ammonium carbonate, 0.1-0.2 parts sodium hexametaphosphate, and 80-85 parts water.

[0014] Preferably, the coconut husk powder is made by crushing waste coconut husks to 80-100 mesh.

[0015] Preferably, the coconut shell powder is made by crushing waste coconut shells to 30-50 mesh.

[0016] Compared with the prior art, the beneficial effects of the present invention are:

[0017] (1) The present invention uses construction waste fillers of different particle sizes as raw materials and employs Bacillus uric acid oxidizing, Providencia reticularis and Bacillus pasteurellis microorganisms to solidify the construction waste fillers, which effectively improves the microbial solidification effect and enhances the bearing capacity of the resulting composite foundation.

[0018] (2) This invention is for construction waste filler, and uses a combination of Arthrobacter urate-oxidizing bacteria, Providencia reticularis and Bacillus pasteurellis, which has higher and more stable urease activity, improves the quality of microbial solidification and enhances the structural strength of piles.

[0019] (3) The present invention uses calcium chloride, urea, coconut outer skin powder, coconut shell powder, ammonium carbonate, sodium hexametaphosphate and water to prepare a cementing solution, which, combined with the compound bacterial solution of the present invention, effectively promotes the solidification effect of microorganisms and helps to improve the bearing capacity of the pile.

[0020] (3) The composite foundation formed by the present invention has strong bearing capacity and high use value; the construction process is simple and easy to implement, with a high construction quality assurance rate; the construction efficiency is high, the construction period is short and the speed is fast; during the construction process, no mud is generated and the filling material is construction waste, which has the advantages of turning waste into treasure, being environmentally friendly, saving project costs, and conforming to my country's green development concept. Detailed Implementation

[0021] To better understand the technical content of this invention, specific embodiments are provided below to further illustrate the invention.

[0022] Unless otherwise specified, the experimental methods used in the embodiments of this invention are all conventional methods.

[0023] Unless otherwise specified, all materials and reagents used in the embodiments of this invention are commercially available.

[0024] All bacterial strains used in this invention were purchased, wherein,

[0025] Sporosarcina pasteurii: Guangdong Provincial Microbial Culture Collection Center, strain number GDMCC NO.:1.803;

[0026] Providencia rettgeri: Brand ATCC, Product No. ATCC29944;

[0027] Arthrobacter uratoxydans: Brand ATCC, Product No.: ATCC 21751;

[0028] All bacterial solutions used on-site were obtained through conventional methods, including aseptic indoor culture, centrifugal concentration, low-temperature transportation, and on-site scale-up culture.

[0029] Example 1: Construction Method of Energy Deformation Compaction Pile Composite Foundation with Microbial Solidified Construction Waste Filler

[0030] (1) Preparation of construction waste filler: It is made by crushing waste concrete blocks. Two specifications of construction waste filler are prepared by crushing them separately, with particle sizes of 15-25mm and 3-5mm respectively. The two particle sizes of construction waste filler are mixed at a mass ratio of 1:0.4 to obtain the target construction waste filler for later use.

[0031] (2) Preparation of bacterial suspension: A bacterial suspension was prepared by mixing three bacterial species: *Arthrobacter urate-oxidizing*, *Providendum repens*, and *Bacillus pasteurellis*. The viable cell concentrations of the three species in the bacterial suspension were 5.0 * 10⁻⁶. 8 cfu / g, 3.0*10 8 cfu / g, 2.0*10 8 cfu / g.

[0032] (3) Preparation of cementing solution: Take the following raw materials in the following weight ratio: 10g calcium chloride, 5g urea, 0.15g sodium chloride, 1.5g coconut outer skin powder, 1.0g coconut shell powder, 0.3g ammonium carbonate, 0.15g sodium hexametaphosphate and 82g water, mix them to prepare cementing solution; wherein the coconut outer skin powder is made by crushing waste coconut outer skin to 100 mesh, and the coconut shell powder is made by crushing waste coconut shell to 40 mesh.

[0033] (4) Construction technology

[0034] 1) Clean and level the site;

[0035] 2) Construction preparation, including setting out and verifying construction lines; inspecting and debugging construction equipment;

[0036] 3) Position the pile driver so that the center of the hammer is aligned with the center of the pile location;

[0037] 4) Hammer to form a hole, lift the heavy hammer and let it fall freely to impact the foundation soil to form a hole to the designed depth;

[0038] 5) Fill the hole with 0.2–0.3 m of filler. 3 The construction waste filler is then poured in, followed by 0.2–0.3 m³ of [material / material]. 3 Mix equal volumes of bacterial solution and cementing solution (mix the bacterial solution and cementing solution in a 1:1 volume ratio before use), then lift the heavy hammer and ram the filler multiple times.

[0039] 6) Under the action of standard impact energy, measure the penetration of the final blow of the hammer. If it is not greater than the design requirement, repeat step 5).

[0040] 7) Repeat steps 5) and 6) to fill the pile holes to the ground level. This ultimately forms energy-deformation compaction piles in the foundation, using microbial-solidified construction waste filler.

[0041] 8) After pile completion, the equipment is moved to the next pile;

[0042] 9) After all the piles are completed, use a plate compactor with a certain energy to compact the ground in the construction area;

[0043] 10) After compacting the ground, backfill with a layer of construction waste filler and an equal volume of bacterial solution and cementing solution mixture. The backfill elevation should be at least 0.2m higher than the ground surface. Then, lift the plate compactor to a certain height and repeatedly compact the microbial solidified construction waste filler layer until the layer is level with the ground surface.

[0044] Ultimately, a composite foundation is formed in the foundation using energy-deformed compaction piles, which are filled with construction waste and solidified by microorganisms.

[0045] Example 2: Construction Method of Energy Deformation Compaction Pile Composite Foundation with Microbial Solidified Construction Waste Filler

[0046] (1) Preparation of construction waste filler: The waste concrete blocks were crushed to obtain two specifications of construction waste filler with particle sizes of 15-25 mm and 3-5 mm, respectively. The two particle sizes of construction waste filler were mixed at a mass ratio of 1:0.3 to obtain the target construction waste filler for later use.

[0047] (2) Preparation of bacterial suspension: A bacterial suspension was prepared by mixing three bacterial species: *Arthrobacter urate-oxidizing*, *Providendum repens*, and *Bacillus pasteurellis*. The viable cell concentrations of the three species in the bacterial suspension were 4.5 × 10⁻⁶. 8 cfu / g, 4.0*10 8 cfu / g, 1.5*10 8 cfu / g.

[0048] (3) Preparation of cementing solution: Take the following raw materials in the following weight ratio: 9g calcium chloride, 6g urea, 0.1g sodium chloride, 1.4g coconut outer skin powder, 1.2g coconut shell powder, 0.2g ammonium carbonate, 0.1g sodium hexametaphosphate and 82g water, mix them to prepare cementing solution; wherein the coconut outer skin powder is made by crushing waste coconut outer skin to 100 mesh, and the coconut shell powder is made by crushing waste coconut shell to 40 mesh.

[0049] (4) The construction process is the same as that in Example 1.

[0050] Example 3: Construction Method of Energy Deformation Compaction Pile Composite Foundation Using Microbial Solidified Construction Waste Filler

[0051] (1) Preparation of construction waste filler: The waste concrete blocks were crushed to obtain two specifications of construction waste filler with particle sizes of 15-25 mm and 3-5 mm, respectively. The two particle sizes of construction waste filler were mixed at a mass ratio of 1:0.3 to obtain the target construction waste filler for later use.

[0052] (2) Preparation of bacterial suspension: A bacterial suspension was prepared by mixing three bacterial species: *Arthrobacter urate-oxidizing*, *Providendum repens*, and *Bacillus pasteurellis*. The viable cell concentrations of the three species in the bacterial suspension were 5.5 × 10⁻⁶. 8 cfu / g, 2.0*10 8 cfu / g, 2.5*10 8 cfu / g.

[0053] (3) Preparation of cementing solution: Take the following raw materials in the following weight ratio: 11g calcium chloride, 4g urea, 0.2g sodium chloride, 1.5g coconut outer skin powder, 0.8g coconut shell powder, 0.4g ammonium carbonate, 0.1g sodium hexametaphosphate and 82g water, mix them to prepare cementing solution; wherein the coconut outer skin powder is made by crushing waste coconut outer skin to 100 mesh, and the coconut shell powder is made by crushing waste coconut shell to 40 mesh.

[0054] (4) The construction process is the same as that in Example 1.

[0055] Comparative Example 1

[0056] Based on Example 1, the main adjustment is to use construction waste filler, specifically a single-size construction waste filler.

[0057] (1) Preparation of construction waste filler: Waste concrete blocks are crushed to a particle size of 8-12mm to obtain the filler for use;

[0058] (2) Preparation of bacterial suspension: A bacterial suspension was prepared by mixing three bacterial species: *Arthrobacter urate-oxidizing*, *Providendum repens*, and *Bacillus pasteurellis*. The viable cell concentrations of the three species in the bacterial suspension were 5.0 * 10⁻⁶. 8 cfu / g, 3.0*10 8 cfu / g, 2.0*10 8 cfu / g.

[0059] (3) Preparation of cementing solution: Take the following raw materials in the following weight ratio: 10g calcium chloride, 5g urea, 0.15g sodium chloride, 1.5g coconut outer skin powder, 1.0g coconut shell powder, 0.3g ammonium carbonate, 0.15g sodium hexametaphosphate and 82g water, mix them to prepare cementing solution; wherein the coconut outer skin powder is made by crushing waste coconut outer skin to 100 mesh, and the coconut shell powder is made by crushing waste coconut shell to 40 mesh.

[0060] Comparative Example 2

[0061] Based on Example 1, the main adjustment is to the bacterial culture, using a single Bacillus pasteurellium culture. The specific scheme is as follows:

[0062] (1) Preparation of construction waste filler: It is made by crushing waste concrete blocks. Two specifications of construction waste filler are prepared by crushing them separately, with particle sizes of 15-25mm and 3-5mm respectively. The two particle sizes of construction waste filler are mixed at a mass ratio of 1:0.4 to obtain the target construction waste filler for later use.

[0063] (2) Preparation of bacterial suspension: A single Bacillus pasteurellium bacterial suspension was used, with a viable cell concentration of 10*10. 8 cfu / g.

[0064] (3) Preparation of cementing solution: Take the following raw materials in the following weight ratio: 10g calcium chloride, 5g urea, 0.15g sodium chloride, 1.5g coconut outer skin powder, 1.0g coconut shell powder, 0.3g ammonium carbonate, 0.15g sodium hexametaphosphate and 82g water, mix them to prepare cementing solution; wherein the coconut outer skin powder is made by crushing waste coconut outer skin to 100 mesh, and the coconut shell powder is made by crushing waste coconut shell to 40 mesh.

[0065] (4) The construction process is the same as that in Example 1.

[0066] Comparative Example 3

[0067] Based on Example 1, the main adjustment is to the bonding solution; coconut husk powder and coconut shell powder are not added. The specific solution is as follows:

[0068] (1) Preparation of construction waste filler: It is made by crushing waste concrete blocks. Two specifications of construction waste filler are prepared by crushing them separately, with particle sizes of 15-25mm and 3-5mm respectively. The two particle sizes of construction waste filler are mixed at a mass ratio of 1:0.4 to obtain the target construction waste filler for later use.

[0069] (2) Preparation of bacterial suspension: A bacterial suspension was prepared by mixing three bacterial species: *Arthrobacter urate-oxidizing*, *Providendum repens*, and *Bacillus pasteurellis*. The viable cell concentrations of the three species in the bacterial suspension were 5.0 * 10⁻⁶. 8 cfu / g, 3.0*10 8 cfu / g, 2.0*10 8 cfu / g.

[0070] (3) Preparation of cementing solution: Take the following raw materials in the following weight ratio: 10g calcium chloride, 5g urea, 0.1g sodium chloride, 2.6g straw powder, 0.3g ammonium carbonate, 0.15g sodium hexametaphosphate and 82g water, mix them to prepare cementing solution.

[0071] (4) The construction process is the same as that in Example 1.

[0072] Comparative Example 4

[0073] Based on Example 1, the main adjustment is to the bonding solution, specifically the amounts of coconut husk powder, coconut shell powder, ammonium carbonate, and sodium hexametaphosphate added. The specific scheme is as follows:

[0074] (1) Preparation of construction waste filler: It is made by crushing waste concrete blocks. Two specifications of construction waste filler are prepared by crushing them separately, with particle sizes of 15-25mm and 3-5mm respectively. The two particle sizes of construction waste filler are mixed at a mass ratio of 1:0.4 to obtain the target construction waste filler for later use.

[0075] (2) Preparation of bacterial suspension: A bacterial suspension was prepared by mixing three bacterial species: *Arthrobacter urate-oxidizing*, *Providendum repens*, and *Bacillus pasteurellis*. The viable cell concentrations of the three species in the bacterial suspension were 5.0 * 10⁻⁶. 8 cfu / g, 3.0*10 8 cfu / g, 2.0*10 8 cfu / g.

[0076] (3) Preparation of cementing solution: Take the following raw materials in the following weight ratio: 10g calcium chloride, 5g urea, 0.15g sodium chloride, 1.0g coconut outer skin powder, 1.7g coconut shell powder, 0.05g ammonium carbonate, 0.4g sodium hexametaphosphate and 82g water, mix them to prepare cementing solution; wherein the coconut outer skin powder is made by crushing waste coconut outer skin to 100 mesh, and the coconut shell powder is made by crushing waste coconut shell to 40 mesh.

[0077] (4) The construction process is the same as that in Example 1.

[0078] Test case

[0079] (1) Structural strength test of cemented soil samples

[0080] Penetration tests were conducted on cemented soil samples from Examples 1-3 and Comparative Examples 1-4 using an ultra-miniature penetrator SMP-1. The end resistance of the probe during penetration reflected the structural strength of the soil. Before penetration, water was allowed to permeate from bottom to top through a hole in the bottom of the mold to saturate the sample. Three rounds of penetration tests were conducted on each sample at different points (at intervals of more than 2 cm), with each penetration depth being 2 cm. The results were then averaged.

[0081] The results are shown in Table 1 below:

[0082]

[0083]

[0084] The above results show that the methods of Examples 1-3 of this invention significantly improve the penetration stress of cemented soil samples, which helps to improve the structural strength of foundation soil. Among them, compared with Example 1, the penetration stress of soil samples in Comparative Examples 1-4 decreased. The use of construction waste fillers with different particle sizes, the compound bacterial solution of this invention, and the cementing solution of this invention all contribute to improving the structural strength of foundation soil.

[0085] (2) Bearing capacity test of compacted pile composite foundation

[0086] The bearing capacity of the compacted pile composite foundation formed after construction using the method in Example 1 was tested. A static load test of the vertical compressive strength of a single pile was conducted in accordance with JGJ106-2014, "Technical Specification for Testing of Building Foundation Piles".

[0087] The results are shown in Table 2 below:

[0088] Single pile bearing capacity / KN Example 1 816.5

[0089] As can be seen from Table 2, the compaction piles obtained by the construction method of the present invention have a significant increase in single pile bearing capacity.

[0090] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of the present invention should be included within the protection scope of the present invention.

Claims

1. A construction method for a composite foundation of energy deformation compaction piles using microbial-solidified construction waste fillers, characterized in that, Construction waste is used as filler material. The construction waste filler material is filled into the hole of the pile location, and a mixture of bacterial solution and cementing liquid is added at the same time. The construction waste filler material is made by crushing waste concrete blocks. The construction waste filler material is composed of two specifications of construction waste with particle sizes of 15~25mm and 3~5mm respectively. The mass ratio of the two particle sizes of 15~25mm and 3~5mm in the construction waste filler material is 1:0.3~0.

5. The bacterial solution was prepared from *Arthrobacter urate-oxidizing*, *Providendum repens*, and *Bacillus pasteurellis*; the viable cell concentrations of *Arthrobacter urate-oxidizing*, *Providendum repens*, and *Bacillus pasteurellis* in the bacterial solution were (4.5~5.5)×10⁻¹⁰, respectively. 8 cfu / g, (2~4)×10 8 cfu / g, (1.5~2.5)×10 8 cfu / g; The cementing solution is prepared from the following raw materials in parts by weight: 8-12 parts calcium chloride, 4-6 parts urea, 0.1-0.2 parts sodium chloride, 1.4-1.6 parts coconut husk powder, 0.8-1.2 parts coconut shell powder, 0.2-0.4 parts ammonium carbonate, 0.1-0.2 parts sodium hexametaphosphate, and 80-85 parts water; the coconut husk powder is made by crushing waste coconut husks to 80-100 mesh; the coconut shell powder is made by crushing waste coconut shells to 30-50 mesh. By volume, for every 1 part of construction waste filler, add 0.8 to 1.2 parts of a mixture of bacterial solution and cementing solution; The volume ratio of the bacterial solution to the cementing solution in the mixture is 1:0.8~1.2.

Citation Information

Patent Citations

  • Isoenergetic deformation composite foundation for solidifying aggregate through microorganisms, and construction method