Method of forming flash memory
By cleaning or ashing the surface of the hard mask layer, the problem of bottom depression in the shallow trench isolation structure of flash memory is solved, thus improving the performance and reliability of flash memory.
Patent Information
- Application Number
- CN202310789623.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-06-29
- Publication Date
- 2026-11-24
- Estimated Expiration
- 2043-06-29
AI Technical Summary
The bottom of the shallow trench isolation structure of existing flash memory is prone to indentation towards the active area, which affects the performance of flash memory.
The surface of the hard mask layer is cleaned with propylene glycol monomethyl ether or propylene glycol monomethyl ether acetate, or aerated with gas to prevent the hard mask layer from reacting with the antireflective layer and avoid the formation of depressions.
This effectively prevents the shallow trench isolation structure from recessing into the active area, thus improving the performance and reliability of the flash memory.
Smart Images

Figure CN116847656B_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of semiconductor technology, and in particular to a method for forming flash memory. Background Technology
[0002] Flash memory has the advantages of large storage capacity and high write speed, and therefore has become the mainstream of non-volatile memory.
[0003] Existing flash memory technologies vary widely, but their fabrication methods typically involve providing a silicon substrate, forming an active region within the substrate, and then sequentially forming a coupling oxide layer, a floating gate polysilicon layer, a silicon nitride layer, and a hard mask layer on the substrate. Trenching is then achieved by etching the hard mask layer, silicon nitride layer, floating gate polysilicon layer, coupling oxide layer, and a portion of the active region. The trenches are then filled with oxide to form a shallow trench isolation structure, which separates the active region into multiple partitions, thereby allowing multiple devices to be formed on the substrate.
[0004] However, the inventors discovered that the bottom of the shallow trench isolation structure of some flash memory chips is recessed into the active area below the shallow trench isolation structure, which may reduce the performance of the flash memory. Summary of the Invention
[0005] The purpose of this invention is to provide a method for forming flash memory, which prevents the bottom of the shallow trench isolation structure of the formed flash memory from recessing into the active region below the shallow trench isolation structure, thereby improving the performance of the flash memory.
[0006] To achieve the above objectives, the present invention provides a method for forming flash memory, comprising:
[0007] A substrate is provided, an active region is formed in the substrate, and a coupling oxide layer, a floating gate polysilicon layer, a silicon nitride layer and a hard mask layer are sequentially formed on the substrate, wherein the hard mask layer is tetraethyl orthosilicate-based silicon dioxide;
[0008] Clean the surface of the hard mask layer with propylene glycol monomethyl ether or propylene glycol monomethyl ether acetate;
[0009] Remove any remaining propylene glycol monomethyl ether or propylene glycol monomethyl ether acetate;
[0010] An anti-reflection layer and a photoresist layer are sequentially formed on the hard mask layer;
[0011] The photoresist layer and anti-reflective layer are patterned;
[0012] The hard mask layer, silicon nitride layer, floating gate polysilicon layer, coupling oxide layer and substrate are sequentially dry etched according to the patterned photoresist layer and anti-reflection layer, and the etching inside the active region is stopped to form a shallow trench.
[0013] The shallow trenches are filled with oxide to form a shallow trench isolation structure.
[0014] Optionally, in the method for forming the flash memory, the substrate includes a wafer.
[0015] Optionally, in the method for forming the flash memory, the concentration of propylene glycol monomethyl ether is 70 wt%.
[0016] Optionally, in the method for forming the flash memory, the concentration of propylene glycol monomethyl ether acetate is 30 wt%.
[0017] Optionally, in the method for forming the flash memory, the method of cleaning the surface of the hard mask layer using propylene glycol monomethyl ether or propylene glycol monomethyl ether acetate includes:
[0018] The hard mask layer is impregnated with propylene glycol monomethyl ether or propylene glycol monomethyl ether acetate.
[0019] Optionally, in the method for forming the flash memory, the method for removing the remaining propylene glycol monomethyl ether or propylene glycol monomethyl ether acetate includes:
[0020] The remaining propylene glycol monomethyl ether or propylene glycol monomethyl ether acetate is spun dry by shaking the hard mask layer.
[0021] Optionally, in the method for forming the flash memory, the method for patterning the photoresist layer and the anti-reflection layer includes:
[0022] The photoresist layer and antireflective layer are photolithographically etched to form a patterned photoresist layer and antireflective layer, the patterned photoresist layer and antireflective layer exposing a portion of the surface of the hard mask layer.
[0023] The present invention also provides a method for forming flash memory, comprising:
[0024] A substrate is provided, an active region is formed in the substrate, and a coupling oxide layer, a floating gate polysilicon layer, a silicon nitride layer and a hard mask layer are sequentially formed on the substrate, wherein the hard mask layer is tetraethyl orthosilicate-based silicon dioxide;
[0025] The surface of the hard mask layer is ashed using gas.
[0026] An anti-reflection layer and a photoresist layer are sequentially formed on the hard mask layer;
[0027] The photoresist layer and anti-reflective layer are patterned;
[0028] The hard mask layer, silicon nitride layer, floating gate polysilicon layer, coupling oxide layer and substrate are sequentially dry etched according to the patterned photoresist layer and anti-reflection layer, and the etching inside the active region is stopped to form a shallow trench.
[0029] The shallow trenches are filled with oxide to form a shallow trench isolation structure.
[0030] Optionally, in the method for forming the flash memory, the gas includes H2N2 or CF4.
[0031] Optionally, in the method for forming the flash memory, the method for patterning the photoresist layer and the anti-reflective layer includes:
[0032] The photoresist layer and antireflective layer are photolithographically etched to form a patterned photoresist layer and antireflective layer, the patterned photoresist layer and antireflective layer exposing a portion of the surface of the hard mask layer.
[0033] In the flash memory formation method provided by the present invention, by cleaning or ashing the surface of the hard mask layer with propylene glycol monomethyl ether or propylene glycol monomethyl ether acetate, some substances in the hard mask layer are prevented from reacting with the anti-reflection layer, thereby preventing the hard mask layer from sinking. Finally, it prevents the shallow trench isolation structure from sinking into the active area below the shallow trench isolation structure, thus improving the performance of the flash memory. Attached Figure Description
[0034] Figures 1 to 3 This is a schematic diagram of existing flash memory technology;
[0035] Figure 4 This is a flowchart of the flash memory formation method according to Embodiment 1 of the present invention;
[0036] Figures 5 to 8 This is a schematic diagram of the flash memory formation method according to Embodiment 1 of the present invention;
[0037] Figure 9 This is a flowchart of the flash memory formation method according to Embodiment 2 of the present invention;
[0038] Figures 10 to 13 This is a schematic diagram of the flash memory formation method according to Embodiment 2 of the present invention;
[0039] In the diagram: 110 - Active region, 120 - Coupling oxide layer, 130 - Floating gate polysilicon layer, 140 - Silicon nitride layer, 150 - Hard mask layer, 160 - Anti-reflection layer, 170 - Photoresist layer, 180 - Shallow trench, 190 - Shallow trench isolation structure, 210 - Active region, 220 - Coupling oxide layer, 230 - Floating gate polysilicon layer, 240 - Silicon nitride layer, 250 - Hard mask layer Film layer, 260-antireflective layer, 270-photoresist layer, 280-shallow trench, 290-shallow trench isolation structure, 310-active region, 320-coupling oxide layer, 330-floating gate polysilicon layer, 340-silicon nitride layer, 350-hard mask layer, 351-recess, 360-antireflective layer, 370-photoresist layer, 380-shallow trench, 390-shallow trench isolation structure. Detailed Implementation
[0040] The specific embodiments of the present invention will now be described in more detail with reference to the accompanying drawings. The advantages and features of the present invention will become clearer from the following description. It should be noted that the drawings are all in a very simplified form and use non-precise proportions, and are only used to facilitate and clarify the illustration of the embodiments of the present invention.
[0041] In the following text, the terms “first,” “second,” etc., are used to distinguish between similar elements and are not necessarily used to describe a specific order or chronological sequence. It should be understood that these terms, as used herein, may be replaced where appropriate. Similarly, if the methods described herein comprise a series of steps, and the order of these steps presented herein is not necessarily the only possible order in which they can be performed, and some described steps may be omitted and / or other steps not described herein may be added to the method.
[0042] The inventors discovered that flash memory with a downward-facing active area recess at the bottom of the shallow trench isolation structure is mainly produced using the ArF process, where the surface has a hard mask layer. Please refer to [link / reference needed]. Figure 1 Before forming trenches by etching the hard mask layer 350, silicon nitride layer 340, floating gate polysilicon layer 330, coupling oxide layer 320, and active region 310, this type of flash memory undergoes exposure. Before exposure, an anti-reflection layer 360 and a photoresist layer 370 are coated on the hard mask layer, and the photoresist layer 370 is exposed. At this point, a cross-section of the entire structure reveals that a depression 351 appears in the anti-reflection layer 360 near the hard mask layer 350. Please refer to... Figure 2 After etching the hard mask layer 350, silicon nitride layer 340, floating gate polysilicon layer 330, coupling oxide layer 320, and active region 310 to form a shallow trench 380, cross-sectioning revealed a depression extending towards the active region 310 at the bottom of the shallow trench 380. Please refer to... Figure 3After filling the shallow trench 380 with silicon oxide, it was found that the shallow trench isolation structure 390 recessed downwards towards the active region 310. Furthermore, through multiple defective flash memory samples, it was discovered that the recesses appeared in different locations at the bottom of the shallow trench isolation structure, and their locations were irregular. This defect was not found in other types of flash memory, such as those without ethyl silicate as a hard mask layer. Therefore, after analyzing the flash memory process and flow, the inventors discovered that the surface of the ethyl silicate used as the hard mask layer contains substances that can react with the anti-reflection layer. This reaction causes a recess on the surface of the hard mask layer. Consequently, during subsequent etching, due to the characteristics of dry etching, each layer experiences downward recessing. After etching is complete, the recess appears at the bottom of the shallow trench, extending downwards towards the active region below the shallow trench. After the shallow trench is filled with silicon oxide to form the shallow trench isolation structure, the shallow trench isolation structure recesses downwards towards the active region. Therefore, to address this problem, the present invention proposes two embodiments to solve this issue.
[0043] Example 1
[0044] Please refer to Figure 4 The present invention provides a method for forming flash memory, comprising:
[0045] S11: Provide a substrate, form an active region within the substrate, and sequentially form a coupling oxide layer, a floating gate polysilicon layer, a silicon nitride layer, and a hard mask layer on the substrate. The hard mask layer is tetraethyl orthosilicate-based silicon dioxide.
[0046] S12: Clean the surface of the hard mask layer using propylene glycol monomethyl ether or propylene glycol monomethyl ether acetate;
[0047] S13: Remove the remaining propylene glycol monomethyl ether or propylene glycol monomethyl ether acetate;
[0048] S14: An anti-reflection layer and a photoresist layer are sequentially formed on the hard mask layer;
[0049] S15: Patterned photoresist layer and anti-reflective layer;
[0050] S16: Based on the patterned photoresist layer and anti-reflection layer, the hard mask layer, silicon nitride layer, floating gate polysilicon layer, coupling oxide layer and substrate are etched sequentially, and the etching stops inside the active region to form a shallow trench.
[0051] S17: Fill shallow trenches with oxides to form shallow trench isolation structures.
[0052] Specifically, first, please refer to Figure 5First, a substrate is provided, which can be a silicon substrate, for example, a wafer. Ions are implanted into the substrate to form an active region 110. Next, a coupling oxide layer 120 is formed on the substrate by depositing oxide, the coupling oxide layer 120 having a thickness of approximately 90 angstroms. Next, a floating gate polysilicon layer 130 is formed on the coupling oxide layer 120 by depositing polysilicon, the floating gate polysilicon layer 130 having a thickness of approximately 300 angstroms. Next, a silicon nitride layer 140 is formed on the floating gate polysilicon layer 130 by depositing silicon nitride, the silicon nitride layer 140 having a thickness of approximately 800 angstroms. Next, a hard mask layer 150 is formed on the silicon nitride layer 140 by depositing tetraethyl orthosilicate silicon dioxide, the hard mask layer 150 having a thickness of approximately 450 angstroms.
[0053] Next, the entire surface of the hard mask layer 150 is immersed in propylene glycol monomethyl ether or propylene glycol monomethyl ether acetate. At this point, the entire structure can be immersed in propylene glycol monomethyl ether or propylene glycol monomethyl ether acetate before being spin-coated onto the surface of the hard mask layer 150. The inventors discovered that after the anti-reflective layer is coated on the hard mask layer 150, part of the anti-reflective layer may react with impurities or other substances on the hard mask layer 150, causing depressions in the anti-reflective layer 160. Therefore, the entire surface of the hard mask layer 150 is cleaned with propylene glycol monomethyl ether or propylene glycol monomethyl ether acetate. The propylene glycol monomethyl ether or propylene glycol monomethyl ether acetate is then spun dry.
[0054] Next, please refer to Figure 6 An anti-reflection layer 160 and a photoresist layer 170 are sequentially formed on the hard mask layer 150 by deposition.
[0055] Next, please refer to Figure 7 As needed, a photoresist layer 170 and an anti-reflection layer 160 are patterned using photolithography to form a patterned photoresist layer and a patterned anti-reflection layer. Based on the patterned photoresist layer and the patterned anti-reflection layer, a dry etching method is used to perpendicularly etch the hard mask layer 150, the silicon nitride layer 140, the floating gate polysilicon layer 130, the coupling oxide layer 120, and the active region 110 in the direction of the active region 110, stopping the etching inside the active region 110 to form a shallow trench 180. Next, please refer to... Figure 8 An oxide, such as silicon dioxide, is filled into the shallow trench 180 to form a shallow trench isolation structure 190.
[0056] Example 2
[0057] Please refer to Figure 9 The present invention provides a method for forming flash memory, comprising:
[0058] S21: Provide a substrate, form an active region in the substrate, and sequentially form a coupling oxide layer, a floating gate polysilicon layer, a silicon nitride layer and a hard mask layer on the substrate. The hard mask layer is tetraethyl orthosilicate silicon dioxide.
[0059] S22: Ashing the surface of the hard mask layer using gas;
[0060] S23: An anti-reflection layer and a photoresist layer are sequentially formed on the hard mask layer;
[0061] S24: Patterned photoresist layer and anti-reflective layer;
[0062] S25: Based on the patterned photoresist layer and anti-reflection layer, the hard mask layer, silicon nitride layer, floating gate polysilicon layer, coupling oxide layer and substrate are etched sequentially, and the etching stops inside the active region to form a shallow trench.
[0063] S26: Fill shallow trenches with oxides to form shallow trench isolation structures.
[0064] Specifically, first, please refer to Figure 10 First, a substrate is provided, which can be a silicon substrate, for example, a wafer. Ions are implanted into the substrate to form an active region 210. Next, a coupling oxide layer 220 with a thickness of approximately 90 angstroms is formed on the substrate by depositing oxide. Then, a floating gate polysilicon layer 230 with a thickness of approximately 300 angstroms is formed on the coupling oxide layer 220 by depositing polysilicon. Next, a silicon nitride layer 240 with a thickness of approximately 800 angstroms is formed on the floating gate polysilicon layer 230 by depositing silicon nitride. Finally, a hard mask layer 250 with a thickness of approximately 450 angstroms is formed on the silicon nitride layer 240 by depositing tetraethyl orthosilicate silicon dioxide.
[0065] Next, the surface of the hard mask layer 250 is ashed using a gas, which can be H2N2 or CF4.
[0066] Next, please refer to Figure 11 An anti-reflection layer 260 and a photoresist layer 270 are sequentially formed on the hard mask layer 250 by deposition.
[0067] Next, please refer to Figure 12As needed, a photoresist layer 270 and an anti-reflection layer 260 are patterned using photolithography to form a patterned photoresist layer and a patterned anti-reflection layer. Based on the patterned photoresist layer and the patterned anti-reflection layer, a dry etching method is used to perpendicularly etch the hard mask layer 250, the silicon nitride layer 240, the floating gate polysilicon layer 230, the coupling oxide layer 220, and the active region 210 in the direction of the active region 210, stopping the etching inside the active region 210 to form a shallow trench 280. Next, please refer to... Figure 13 An oxide, such as silicon dioxide, is filled into the shallow trench 280 to form a shallow trench isolation structure 290.
[0068] In summary, in the flash memory formation method provided in this embodiment of the invention, by cleaning or ashing the surface of the hard mask layer with propylene glycol monomethyl ether or propylene glycol monomethyl ether acetate, some substances in the hard mask layer are prevented from reacting with the anti-reflection layer, thereby preventing the hard mask layer from becoming recessed. Finally, this prevents the shallow trench isolation structure from recessing into the active area below the shallow trench isolation structure, reducing leakage current and improving the performance of the flash memory.
[0069] The above are merely preferred embodiments of the present invention and do not constitute any limitation on the present invention. Any equivalent substitutions or modifications made by those skilled in the art to the technical solutions and content disclosed in the present invention without departing from the scope of the present invention shall be deemed to have remained within the protection scope of the present invention.
Claims
1. A method of forming a flash memory, comprising: include: A substrate is provided, an active region is formed in the substrate, and a coupling oxide layer, a floating gate polysilicon layer, a silicon nitride layer and a hard mask layer are sequentially formed on the substrate, wherein the hard mask layer is tetraethyl orthosilicate-based silicon dioxide; Clean the surface of the hard mask layer with propylene glycol monomethyl ether or propylene glycol monomethyl ether acetate; Remove any remaining propylene glycol monomethyl ether or propylene glycol monomethyl ether acetate; An anti-reflection layer and a photoresist layer are sequentially formed on the hard mask layer; The photoresist layer and anti-reflective layer are patterned; The hard mask layer, silicon nitride layer, floating gate polysilicon layer, coupling oxide layer and substrate are sequentially dry etched according to the patterned photoresist layer and anti-reflection layer, and the etching inside the active region is stopped to form a shallow trench. The shallow trenches are filled with oxide to form a shallow trench isolation structure.
2. The method of forming flash memory as claimed in claim 1, wherein, The substrate includes a wafer.
3. The method of claim 1, wherein The concentration of the propylene glycol monomethyl ether is 70 wt%.
4. The method of forming flash memory as claimed in claim 1, wherein, The concentration of propylene glycol monomethyl ether acetate is 30 wt%.
5. The method of claim 1, wherein The method of cleaning the surface of the hard mask layer using propylene glycol monomethyl ether or propylene glycol monomethyl ether acetate includes: The hard mask layer is impregnated with propylene glycol monomethyl ether or propylene glycol monomethyl ether acetate.
6. The method for forming flash memory as described in claim 1, characterized in that, Methods for removing residual propylene glycol monomethyl ether or propylene glycol monomethyl ether acetate include: The remaining propylene glycol monomethyl ether or propylene glycol monomethyl ether acetate is spun dry by shaking the hard mask layer.
7. The method for forming flash memory as described in claim 1, characterized in that, The method for patterning the photoresist layer and the anti-reflective layer includes: The photoresist layer and antireflective layer are photolithographically etched to form a patterned photoresist layer and antireflective layer, the patterned photoresist layer and antireflective layer exposing a portion of the surface of the hard mask layer.
8. A method for forming flash memory, characterized in that, include: A substrate is provided, an active region is formed in the substrate, and a coupling oxide layer, a floating gate polysilicon layer, a silicon nitride layer and a hard mask layer are sequentially formed on the substrate, wherein the hard mask layer is tetraethyl orthosilicate-based silicon dioxide; The surface of the hard mask layer is ashed using gas. An anti-reflection layer and a photoresist layer are sequentially formed on the hard mask layer; The photoresist layer and anti-reflective layer are patterned; The hard mask layer, silicon nitride layer, floating gate polysilicon layer, coupling oxide layer and substrate are sequentially dry etched according to the patterned photoresist layer and anti-reflection layer, and the etching inside the active region is stopped to form a shallow trench. The shallow trenches are filled with oxide to form a shallow trench isolation structure.
9. The method for forming flash memory as described in claim 8, characterized in that, The gas includes H2N2 or CF4.
10. The method for forming flash memory as described in claim 8, characterized in that, The method for patterning the photoresist layer and the anti-reflective layer includes: The photoresist layer and antireflective layer are photolithographically etched to form a patterned photoresist layer and antireflective layer, the patterned photoresist layer and antireflective layer exposing a portion of the surface of the hard mask layer.
Citation Information
Patent Citations
Method for reducing particle defects at edges of wafers
CN102446805A
Method for forming shallow trench isolation
CN103887224A