Thin film inductor and method of manufacturing the same

By using PCB pattern transfer technology to fabricate thin-film inductors, the problems of complexity and high cost of traditional processes are solved, enabling flexible magnetic performance design and mass production, and meeting the demand for ultra-thin thin-film inductors.

CN116864300BActive Publication Date: 2026-11-24DONGGUAN SHENGYI ELECTRONICS
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202311023648.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-08-14
Publication Date
2026-11-24
Estimated Expiration
2043-08-14

AI Technical Summary

Technical Problem

Existing thin-film inductors have complex manufacturing processes, high costs, and limited magnetic performance design, making it difficult to meet the demand for ultra-thin and lightweight designs.

Method used

The coil is fabricated using pattern transfer technology from the PCB industry, and copper foil and magnetic film are laminated together to form a thin-film inductor. This avoids the use of a vacuum environment and magnetron sputtering equipment, enabling flexible magnetic performance design.

Benefits of technology

It reduces process complexity and cost, increases the flexibility of coil design, is suitable for mass production, and meets the size and performance requirements of thin-film inductors.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN116864300B_ABST
    Figure CN116864300B_ABST
Patent Text Reader

Abstract

This invention relates to the field of inductor devices and discloses a thin-film inductor and its fabrication method. The fabrication method includes: providing a first copper foil, a second copper foil, a third copper foil, a first magnetic film, and a second magnetic film, wherein the first magnetic film has a window; using the first copper foil to form a coil and a conductive connection portion protruding at the end of the coil; sequentially stacking and pressing the second copper foil, the first magnetic film, the coil, the second magnetic film, and the third copper foil together, with the conductive connection portion protruding on the coil embedded in the window area of ​​the first magnetic film; and using the second copper foil to form an electrode connected to the conductive connection portion, thus forming a thin-film inductor. This invention significantly reduces process complexity, manufacturing difficulty, and manufacturing cost while achieving high-precision coil pattern fabrication; the specific shape and size of the coil pattern can be flexibly adjusted according to different needs, enabling various magnetic performance design requirements to be met; the process flow is simple and suitable for mass production.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of inductors, and more particularly to a thin-film inductor and its fabrication method. Background Technology

[0002] As wearable and portable electronic devices continue to evolve towards thinner and more multifunctional designs, power supply components, as electronic devices, are also constantly being miniaturized. This has led to the demand for extremely thin and light inductors, a key functional component of power supply components, giving rise to thin-film inductors.

[0003] Thin-film inductors are inductors manufactured using vacuum thin-film technology. They are highly reliable, easy to integrate and surface mount, making them ideal for automated surface mount technology (SMT). Due to their advantages such as small size and good high-frequency characteristics, they have become a research hotspot both domestically and internationally.

[0004] Currently, the design requirements for thin-film inductors have reached below 0.3mm in thickness and below 2*5mm in size (conventional discrete inductors and magnetic core inductors cannot meet these requirements). For thin-film inductors with a thickness of less than 0.3mm, the mainstream manufacturing process currently used is magnetic film sputtering: conductive lines are fabricated on a magnetic thin film using magnetron sputtering (the principle is to use the magnetic thin film as a target cathode, and use argon ions to bombard the target material to generate cathode sputtering, sputtering the target material atoms onto the workpiece to form a deposition layer). Then, an insulating layer and a magnetic film layer are laminated on the conductive lines to finally form the inductor.

[0005] However, the aforementioned magnetic film sputtering process has drawbacks such as high manufacturing cost, complex manufacturing process, inflexible coil design, limited magnetic performance design, and poor economic benefits in mass production because it requires the use of special magnetic film sputtering equipment in a vacuum environment to complete the fabrication of the wires. Summary of the Invention

[0006] The purpose of this invention is to provide a thin-film inductor and its fabrication method, so as to overcome the defects of traditional magnetic film sputtering processes, such as complex processes, high costs and limited magnetic performance design.

[0007] To achieve this objective, the present invention adopts the following technical solution:

[0008] A method for fabricating a thin-film inductor, comprising:

[0009] A first copper foil, a second copper foil, a third copper foil, a first magnetic film, and a second magnetic film are provided, wherein the first magnetic film has a window;

[0010] The first copper foil is used to make a coil and a conductive connection portion protruding from the end of the coil;

[0011] The second copper foil, the first magnetic film, the coil, the second magnetic film and the third copper foil are sequentially stacked and pressed together, and the conductive connection portion protruding on the coil is embedded in the window area of ​​the first magnetic film;

[0012] The second copper foil is made into an electrode that is connected to the conductive connection portion to form a thin-film inductor.

[0013] Optionally, the method of using the first copper foil to form a coil and a conductive connection portion protruding from the end of the coil includes:

[0014] A first anti-electroplating etching dry film is applied to one side of the surface of the first copper foil;

[0015] The first anti-electroplation etch dry film on the surface of the conductive connection area of ​​the first copper foil is removed by exposure and development.

[0016] Electroplating is performed on the conductive connection area of ​​the first copper foil to obtain a conductive connection protruding from the surface of the first copper foil.

[0017] A second anti-electroplating and etching dry film is attached to the outer layer of the first anti-electroplating and etching dry film and the conductive connection portion;

[0018] By exposure and development, the first and second anti-electroplating etch dry films on the surface of the non-coil pattern fabrication area of ​​the first copper foil are removed.

[0019] The non-coil pattern area of ​​the first copper foil is etched away, and then the first and second anti-electroplating etch dry films are removed to obtain the coil and the conductive connection portion protruding from the end of the coil.

[0020] Optionally, the method of forming the second copper foil into an electrode connected to the conductive connection portion includes:

[0021] A third anti-electroplating etch dry film is coated on the surface of the electrode fabrication area of ​​the second copper foil, and the electrode fabrication area covers the conductive connection fabrication area;

[0022] Etching removes the non-electrode fabrication area of ​​the second copper foil, so that the electrode fabrication area of ​​the second copper foil is formed as the electrode;

[0023] Remove the third anti-electroplating etch dry film to expose the electrode.

[0024] Optionally, the manufacturing method further includes: before the lamination and pressing, bonding a layer of low-temperature sintered copper paste to the surface of the conductive connection portion.

[0025] Optionally, the thickness of the low-temperature sintered copper paste is 10 micrometers to 20 micrometers.

[0026] Optionally, the window area of ​​the first magnetic film is 2mil-4mil larger on one side than the conductive connection portion.

[0027] Optionally, the thickness of the coil ranges from 70 micrometers to 150 micrometers.

[0028] Optionally, the coil is a planar wound coil.

[0029] Optionally, the first magnetic film and the second magnetic film are magnetic thin films coated with a non-conductive binder and containing more than 90% soft magnetic powder particles.

[0030] A thin-film inductor, said thin-film inductor being manufactured according to any one of the methods described above.

[0031] Compared with the prior art, the beneficial effects of the present invention are as follows:

[0032] In this embodiment of the invention, the coil is first fabricated using the patterning process in the PCB field. Then, the second copper foil, the first magnetic film, the coil, the second magnetic film, and the third copper foil are sequentially stacked and pressed together. Finally, electrodes are fabricated on the outer layer to obtain a thin-film inductor that meets the manufacturing requirements.

[0033] Compared with traditional magnetic film sputtering processes, the coil in this embodiment of the invention is made using a pattern transfer process in the PCB field, and the first and second magnetic films are laminated onto the surface of the coil. The manufacturing process does not require the construction of a vacuum manufacturing environment, nor does it require the application of specific high-end equipment such as magnetron sputtering equipment. Therefore, this embodiment of the invention can greatly reduce the complexity, difficulty and cost of the process while achieving the manufacturing of high-precision coils. Moreover, the specific shape and size of the coil can be flexibly adjusted according to different needs, which can realize various magnetic performance design requirements. The process flow is simple and suitable for mass production. Attached Figure Description

[0034] To more clearly illustrate the technical solutions in the embodiments of the present invention or the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.

[0035] Figure 1 A flowchart illustrating the fabrication method of a thin-film inductor provided in an embodiment of the present invention;

[0036] Figure 2 This is a schematic diagram of the overall fabrication process of a thin-film inductor provided in an embodiment of the present invention;

[0037] Figure 3 A schematic diagram of the manufacturing process of the coil and conductive connection provided in an embodiment of the present invention;

[0038] Figure 4 A schematic diagram of the electrode manufacturing process provided in an embodiment of the present invention;

[0039] Figure 5 This is a structural view of the thin-film inductor of the electrode provided in an embodiment of the present invention.

[0040] Illustration:

[0041] 1. First copper foil 2. Second copper foil 3. Third copper foil 4. First magnetic film 5. Second magnetic film 6. Coil 7. Conductive connection part 8. Electrode 9. First anti-electroplating and etching dry film 10. Third anti-electroplating and etching dry film 11. Low-temperature sintering copper paste 12. Detailed Implementation

[0042] To make the objectives, features, and advantages of this invention more apparent and understandable, the technical solutions of the embodiments of this invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the embodiments described below are only some embodiments of this invention, and not all embodiments. Based on the embodiments of this invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of this invention.

[0043] Example 1

[0044] For details, please refer to Figure 1 and Figure 2 This invention provides a method for fabricating a thin-film inductor, comprising the following steps:

[0045] S1. Provide a first copper foil 1, a second copper foil 2, a third copper foil 3, a first magnetic film 4, and a second magnetic film 5. The first magnetic film 4 has a window.

[0046] The first copper foil 1 contains the coil 6, a key component for making the thin-film inductor, and the conductive connection portion 7 protruding from the end of the coil 6. The thickness of the first copper foil 1 can be consistent with the designed thickness of the coil 6.

[0047] The second copper foil 2 will be used to make another component of the thin-film inductor, the electrode 8, which is connected to the coil 6 via the conductive connection 7.

[0048] The first magnetic film 4 and the second magnetic film 5 can be magnetic films formed by coating a non-conductive binder with a content of more than 90% of soft magnetic characteristic powder particles (such as iron powder, iron-aluminum-silicon, iron-nickel alloy, carbonyl iron powder, etc.).

[0049] The opening on the first magnetic film 4 is used to avoid the conductive connection portion 7 protruding from the end of the coil 6. For example, the opening area of ​​the first magnetic film 4 is 2mil-4mil larger than the conductive connection portion 7 on one side.

[0050] S2. Using graphic transfer technology, a coil 6 and a conductive connection part 7 protruding from the end of the coil 6 are made using a first copper foil 1.

[0051] S3. The second copper foil 2, the first magnetic film 4, the coil 6, the second magnetic film 5 and the third copper foil 3 are sequentially stacked and pressed together, and the conductive connection part 7 protruding on the coil 6 is embedded in the window area of ​​the first magnetic film 4.

[0052] It is understandable that during the process of pressing the first magnetic film 4 and the second magnetic film 5, the first magnetic film 4 and the second magnetic film 5 will simultaneously fill the gap between the coils 6 from the opposite upper and lower directions and bond with the coils 6 as one unit.

[0053] S4. The second copper foil 2 is made into an electrode 8 connected to the conductive connection portion 7 to form a thin-film inductor, such as... Figure 5 As shown.

[0054] In summary, the embodiments of the present invention first utilize the pattern manufacturing process in the PCB field to fabricate the coil 6, then sequentially stack and press the second copper foil 2, the first magnetic film 4, the coil 6, the second magnetic film 5, and the third copper foil 3, and then fabricate the electrode 8 on the outer layer, thus obtaining a thin-film inductor that meets the manufacturing requirements.

[0055] Compared with traditional magnetic film sputtering processes, the coil 6 in this embodiment of the invention is manufactured using a pattern transfer process in the PCB field. The first magnetic film 4 and the second magnetic film 5 are laminated onto the surface of the coil 6. The manufacturing process does not require the construction of a vacuum manufacturing environment or the application of specific high-end equipment such as magnetron sputtering equipment. Therefore, this embodiment of the invention can greatly reduce the complexity, difficulty, and cost of the process while achieving the fabrication of high-precision coil 6. Moreover, the specific shape and size of the coil 6 can be flexibly adjusted according to different needs, which can realize various magnetic performance design requirements. The process flow is simple and suitable for mass production.

[0056] For details, please refer to Figure 3 The method of using the first copper foil 1 to form the coil 6 and the conductive connection portion 7 protruding from the end of the coil 6 in step S2 includes:

[0057] S21. A first anti-electroplation etching dry film 9 is applied to one side of the surface of the first copper foil 1.

[0058] For ease of description, the entire area of ​​the copper foil is divided into: the coil pattern making area covered by the coil 6 to be made, and the coil pattern making area other than the coil pattern making area.

[0059] Within the area for making the coil pattern of the copper foil, there is also a conductive connection area for making conductive connections 7 that will be used to connect the electrode 8 and the coil 6.

[0060] S22. By exposure and development, the first anti-electroplation etching dry film 9 on the surface of the conductive connection area of ​​the first copper foil 1 is removed.

[0061] The thickness of the first anti-electroplated etching dry film 9 can be flexibly designed and determined according to the thickness design requirements of the coil 6 of the conductive connection part 7 to be manufactured.

[0062] S23. Electroplating is performed on the conductive connection area of ​​the first copper foil 1 to obtain the conductive connection 7 protruding from the surface of the first copper foil 1.

[0063] The electroplating time is determined based on the thickness of the first anti-electroplated etching dry film 9 to ensure that the copper plating thickness in the conductive connection area meets the thickness required by the conductive connection 7.

[0064] S24. A second anti-electroplating etching dry film 10 is attached to the outer layer of the first anti-electroplating etching dry film 9 and the conductive connection portion 7.

[0065] S25. By exposure and development, the first anti-electroplating etch dry film 9 and the second anti-electroplating etch dry film 10 on the surface of the non-coil pattern fabrication area of ​​the first copper foil 1 are removed, so that the non-coil pattern fabrication area of ​​the first copper foil 1 is exposed to the outside, which is convenient for subsequent etching removal.

[0066] S26. Etch away the non-coil pattern area of ​​the first copper foil 1, then remove the first anti-electroplating etch dry film 9 and the second anti-electroplating etch dry film 10 to obtain the coil 6 and the conductive connection portion 7 protruding from the end of the coil 6.

[0067] During the etching process, since the copper layer surface of the coil pattern making area is covered with a second anti-electroplated etching dry film 10, the copper layer of the non-coil pattern making area is exposed. Therefore, only the copper layer of the non-coil pattern making area is etched away, while the copper layer of the coil pattern making area is retained to form the coil 6.

[0068] The resulting coil 6 can be a planar wound coil. It is understood that in other embodiments, the same pattern transfer technique can also be used to produce coils 6 of other arbitrary shapes and sizes.

[0069] For further details, please refer to Figure 4 The method for forming the second copper foil 2 into an electrode 8 connected to the conductive connection portion 7 in step S4 includes:

[0070] S41. A third anti-electroplating etching dry film 11 is coated on the surface of the electrode fabrication area of ​​the second copper foil 2, and the electrode fabrication area covers the conductive connection fabrication area.

[0071] S42. Etch away the non-electrode fabrication area of ​​the second copper foil 2 so that the electrode fabrication area of ​​the second copper foil 2 is formed as electrode 8.

[0072] S43. Remove the third anti-electroplating etching dry film 11 to expose the electrode 8.

[0073] Furthermore, to improve the conductivity between the conductive connection 7 and the electrode 8, in this embodiment, a layer of low-temperature sintered copper paste 12 can be bonded to the surface of the conductive connection 7 before the lamination process in step S3. The thickness of the low-temperature sintered copper paste 12 can be selected from 10 micrometers to 20 micrometers, and it can bond together with the copper foil under the action of the pressure plate in a certain low-temperature environment to form a good conductor.

[0074] Example 2

[0075] Embodiment 2 of the present invention provides a thin-film inductor, which is manufactured according to the method for manufacturing the thin-film inductor in Embodiment 1. Due to the special manufacturing process, the complexity of the process, the difficulty of manufacturing, and the manufacturing cost can be effectively reduced, and various magnetic performance design requirements can be met, making it suitable for mass production.

[0076] The above-described embodiments are only used to illustrate the technical solutions of the present invention, and are not intended to limit it. Although the present invention has been described in detail with reference to the foregoing embodiments, those skilled in the art should understand that modifications can still be made to the technical solutions described in the foregoing embodiments, or equivalent substitutions can be made to some of the technical features. Such modifications or substitutions do not cause the essence of the corresponding technical solutions to deviate from the spirit and scope of the technical solutions of the embodiments of the present invention.

Claims

1. A method for fabricating a thin-film inductor, characterized in that, include: A first copper foil (1), a second copper foil (2), a third copper foil (3), a first magnetic film (4), and a second magnetic film (5) are provided, wherein the first magnetic film (4) is provided with a window; Using pattern transfer technology, the first copper foil (1) is used to make a coil (6) and a conductive connection part (7) protruding from the end of the coil (6); The second copper foil (2), the first magnetic film (4), the coil (6), the second magnetic film (5) and the third copper foil (3) are sequentially stacked and pressed together, and the conductive connection part (7) protruding on the coil (6) is embedded in the window area of ​​the first magnetic film (4); The second copper foil (2) is made into an electrode (8) connected to the conductive connection portion (7) to form a thin film inductor.

2. The method for fabricating a thin-film inductor according to claim 1, characterized in that, The method of using the first copper foil (1) to form a coil (6) and a conductive connection portion (7) protruding from the end of the coil (6) includes: A first anti-electroplation etching dry film (9) is applied to one side of the surface of the first copper foil (1); The first anti-electroplated etch dry film (9) on the surface of the conductive connection area of ​​the first copper foil (1) is removed by exposure and development. Electroplating is performed on the conductive connection area of ​​the first copper foil (1) to obtain a conductive connection (7) protruding from the surface of the first copper foil (1); A second anti-electroplated etching dry film (10) is attached to the outer layer of the first anti-electroplated etching dry film (9) and the conductive connection portion (7); By exposure and development, the first anti-electroplating etch dry film (9) and the second anti-electroplating etch dry film (10) on the surface of the non-coil pattern fabrication area of ​​the first copper foil (1) are removed. The non-coil pattern area of ​​the first copper foil (1) is removed by etching, and then the first anti-electroplating etch dry film (9) and the second anti-electroplating etch dry film (10) are removed to obtain the coil (6) and the conductive connection portion (7) protruding from the end of the coil (6).

3. The method for fabricating a thin-film inductor according to claim 1, characterized in that, The method of forming the second copper foil (2) into an electrode (8) connected to the conductive connection portion (7) includes: A third anti-electroplating etching dry film (11) is coated on the surface of the electrode fabrication area of ​​the second copper foil (2), and the electrode fabrication area covers the conductive connection fabrication area; The non-electrode fabrication area of ​​the second copper foil (2) is etched away so that the electrode fabrication area of ​​the second copper foil (2) is formed as the electrode (8); Remove the third anti-electroplated etching dry film (11) to expose the electrode (8).

4. The method for fabricating a thin-film inductor according to claim 1, characterized in that, The manufacturing method further includes: before the lamination and pressing, bonding a layer of low-temperature sintered copper paste (12) to the surface of the conductive connection part (7).

5. The method for fabricating a thin-film inductor according to claim 4, characterized in that, The thickness of the low-temperature sintered copper paste (12) is 10 micrometers to 20 micrometers.

6. The method for fabricating a thin-film inductor according to claim 1, characterized in that, The window area of ​​the first magnetic film (4) is 2mil-4mil larger on one side than the conductive connection part (7).

7. The method for fabricating a thin-film inductor according to claim 1, characterized in that, The thickness of the coil (6) ranges from 70 micrometers to 150 micrometers.

8. The method for fabricating a thin-film inductor according to claim 1, characterized in that, The coil (6) is a planar wound coil.

9. The method for fabricating a thin-film inductor according to claim 1, characterized in that, The first magnetic film (4) and the second magnetic film (5) are magnetic thin films coated with a non-conductive binder mixed with soft magnetic powder particles containing more than 90% of the powder.

10. A thin-film inductor, characterized in that, The thin-film inductor is manufactured according to the method for manufacturing a thin-film inductor according to any one of claims 1 to 9.

Citation Information

Patent Citations

  • Coil manufacturing method, chip component and manufacturing method of chip component

    CN105405638A

  • Thin-film inductor and manufacturing method therefor, integrated circuit and terminal device

    CN113016043A