Plasma etching techniques

By using an oxygen-free plasma etching process with a mixture of fluorine, nitrogen, and hydrogen gases to form a nitride passivation layer on the Ge layer surface, the problem of selective etching of the Si layer is solved, resulting in higher etching selectivity and better device surface quality.

CN116897414BActive Publication Date: 2026-11-20TOKYO ELECTRON LTD +1
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202280017300.3
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2021-01-28
Filing Date
2022-01-24
Publication Date
2026-11-20
Estimated Expiration
2042-01-24

AI Technical Summary

Technical Problem

Existing technologies make it difficult to selectively etch the Si layer without significantly etching the Ge layer in semiconductor manufacturing, especially when forming 3D vertical nanowire or nanosheet devices. Conventional etching techniques result in excessive consumption of the oxide protective layer of the Ge layer or poor surface roughness.

Method used

An oxygen-free plasma etching process is employed, using a mixture of fluorine, nitrogen, and hydrogen gases to form a nitride passivation layer on the Ge layer surface to suppress etching, while selectively etching the Si layer to create a recess.

Benefits of technology

It improves the selectivity and etching profile of Si layer etching, reduces Ge layer loss, improves surface roughness, provides clearer device edges, and enhances the stability of nanowires.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN116897414B_ABST
    Figure CN116897414B_ABST
Patent Text Reader

Abstract

In certain embodiments, a method for processing a semiconductor substrate includes receiving a semiconductor substrate including a film stack. The film stack includes first and second germanium-containing layers and a first silicon layer positioned between the first and second germanium-containing layers. The method includes selectively etching the first silicon layer by exposing the film stack to a plasma including a fluorine agent and a nitrogen agent. The plasma etches the first silicon layer and causes a passivation layer to form on exposed surfaces of the first and second germanium-containing layers to inhibit etching of the first and second germanium-containing layers during exposure of the film stack to the plasma.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] Cross-references to related applications

[0002] This disclosure claims the benefit of U.S. non-provisional application No. 17 / 161,199, entitled “PLASMA ETCHING TECHNIQUES”, filed January 28, 2021, the contents of which are incorporated herein by reference in their entirety. Technical Field

[0003] This disclosure generally relates to semiconductor manufacturing, and in some embodiments, to plasma etching techniques. Background Technology

[0004] The integrated circuit (IC) manufacturing industry strives to increase device density to improve speed, performance, and cost. To continue shrinking to smaller node sizes, device architectures have evolved from two-dimensional (2D) planar structures to three-dimensional (3D) vertical structures, such as transistors with nanowires or vertical orientation. Insufficient control of the conductive channel by the gate potential has fueled expectations for this change. The short-channel effect (SCE) can become too significant as gate size shrinks and becomes even more pronounced when no voltage is applied to the gate (I0). 关闭 This can increase current conduction. Changes in device architecture can allow for better electrostatic control of the gate, reducing SCE and power loss. Fabricating nanowire devices can present 3D etching challenges, where highly selective isotropic etching processes are beneficial. For example, exposed material layers may need to be etched relative to each other to create indentations in the film stack. Summary of the Invention

[0005] In some embodiments, a method for processing a semiconductor substrate includes receiving a semiconductor substrate comprising a film stack. The film stack includes first and second germanium (Ge) layers and a first silicon (Si) layer located between the first and second Ge-containing layers. The method includes selectively etching the first Si layer by exposing the film stack to a plasma comprising a fluorine agent and a nitrogen agent. The plasma etching of the first Si layer causes a passivation layer to be formed on the exposed surfaces of the first and second Ge-containing layers to suppress etching of the first and second Ge-containing layers during plasma exposure of the film stack.

[0006] In some embodiments, the method for processing a semiconductor substrate includes positioning the semiconductor substrate in a plasma chamber of a plasma tool. The semiconductor substrate includes a film stack comprising alternating Si layers and Ge-containing layers, having at least two Si layers and at least two Ge-containing layers. The method includes generating a plasma comprising a fluorine agent, a nitrogen agent, and a hydrogen agent in the plasma chamber of the plasma tool. The plasma is generated without intentionally introducing oxygen-containing gas into the plasma chamber. The method includes exposing the film stack to plasma in the plasma chamber of the plasma tool. The plasma causes a nitride passivation layer to be formed on the exposed surface of the Ge-containing layers, and selectively etches opposite exposed ends of the Si layers to form recesses in the Si layers relative to the opposite exposed ends of the Ge-containing layers. The nitride passivation layer inhibits etching of the Ge-containing layers by the plasma.

[0007] A method for processing a semiconductor substrate includes positioning the semiconductor substrate in a plasma chamber of a plasma tool. The semiconductor substrate includes a film stack comprising a first layer of a first material and a second layer of a second material arranged in alternating stacked layers. The first material is Si. The method includes generating plasma for selectively etching the first layer of the first material. Generating the plasma includes introducing a gas comprising fluorine and nitrogen into the plasma chamber and maintaining a temperature on the semiconductor substrate at approximately -40°C to approximately 40°C. The method includes exposing the film stack to plasma in the plasma chamber for a period of time. The plasma selectively etches opposite exposed ends of the first layer of the first material to form recesses in the first layer of the first material relative to opposite exposed ends of the second layer of the second material. Attached Figure Description

[0008] To gain a more complete understanding of this disclosure and its advantages, reference is made to the following description taken in conjunction with the accompanying drawings, in which:

[0009] Figure 1A-1D A cross-sectional view of an example semiconductor substrate during an example process for processing a semiconductor substrate, according to certain embodiments of this disclosure;

[0010] Figure 2 This illustrates example methods for processing a semiconductor substrate according to certain embodiments of this disclosure;

[0011] Figure 3 This illustrates example methods for processing a semiconductor substrate according to certain embodiments of this disclosure;

[0012] Figure 4 Example devices illustrating certain embodiments of this disclosure include substrates comprising alternating film stacks with recesses; and

[0013] Figure 5A block diagram illustrating an example plasma tool according to certain embodiments of this disclosure. Detailed Implementation

[0014] There are various techniques for selectively etching one material relative to another. In some cases, the two materials are chemically different enough to allow the use of a plasma selectively etching one material without concern for etching the other. In other cases, determining the appropriate etching scheme for selective etching is more difficult because the materials may have similar chemical properties, or the available etching processes may be limited by other factors. Certain materials present more challenging selective etching challenges, where it is desirable to etch one material while barely etching the other. Conventional processes for this type of selective etching may not be able to achieve selective etching of one material relative to another, or may fail to meet process requirements such as selectivity, etching profile (e.g., local uniformity and / or surface roughness), etc.

[0015] Selective challenges can arise when forming nanowires or nanosheets to serve as channel regions in the 3D vertical structure of semiconductor devices such as gate-all-around (GAA) devices. Forming such nanowires may involve forming a film stack on a substrate layer comprising alternating layers of Si and Ge or Si-Ge (SiGe) alloys. Part of this process may include etching recesses in the film stack at opposite ends of the Si layers while minimizing etching of the Ge-containing layers to expose the ends of the Ge-containing layers for later use as conductive devices. Conventional etching techniques may be unsatisfactory due to various challenges, including native oxide (NOL) layers and / or other residues (e.g., reactive ion etching (RIE) residues) present on the surface of the film stack.

[0016] For example, some conventional techniques employ a single etching step using a plasma containing nitrogen trifluoride (NF3) (or another etchant) and oxygen (O2). Fluorine radicals in this plasma etch the Si layer, while oxygen reacts with Ge in the Ge-containing layer to form a germanium oxide (e.g., GeO2) protective layer on the Ge-containing layer. However, the resulting structure after etching typically exhibits unacceptable levels of surface roughness along the exposed surfaces of both the Si and Ge-containing layers, partly due to the etching by NOL. Furthermore, although the GeO2 protective layer facilitates selective etching of the Si layer, it consumes a significant portion of the Ge-containing layer.

[0017] As another example, some conventional techniques use wet or dry processes to remove NOL before performing plasma etching to form recesses in the film stack. Diluted hydrogen fluoride (HF) acid or chemical oxide removal processes can be used to treat the film stack. However, removing NOL from both the Si layer and the Ge-containing layer surfaces reduces the selectivity of subsequent recess plasma etching processes (e.g., using NF3 and O2) in etching the Si layer with minimal to no etching of the Ge-containing layer.

[0018] The embodiments provided below describe various methods of selective etching. For example, the embodiments can be used to selectively etch portions of a substrate (e.g., a film stack comprising alternating Si layers and Ge-containing layers). It is desirable to selectively etch recesses (or may completely remove) in the edge portions of the Si layers to form nanowires containing Ge layers.

[0019] In some embodiments, oxygen-free plasma is used to form recesses or depressions in a film stack comprising alternating Si layers and Ge-containing layers. The oxygen-free plasma allows for the formation of a passivation layer (e.g., a germanium nitride passivation layer) on the exposed surface of the Ge-containing layer. Before exposing the substrate to the oxygen-free plasma, a suitable dry or wet etching process can be used to substantially remove the barrier layer (e.g., NOL) from the exposed surface of the film stack.

[0020] Figure 1A-1D The illustration shows a cross-sectional view of an example substrate 102 during an example process 100 for processing substrate 102 according to certain embodiments of this disclosure. In some embodiments, process 100 incorporates an oxygen-free plasma etching process to etch portions of certain layers of the film stack of substrate 102, resulting in substrate 102 having a recessed film stack after performing process 100. It should be understood that oxygen-free does not necessarily mean the removal of all oxygen from process 100, but rather reflects that oxygen-containing gases, such as O2 and CO2, are not intentionally introduced as part of the plasma etching process.

[0021] like Figure 1AAs shown, substrate 102 is a semiconductor substrate including a film stack 104 disposed on a base layer 106. The film stack 104 includes Si layers 108 and Ge-containing layers 110 arranged in an alternating stacked configuration. The film stack 104 may have any suitable shape and include any suitable number of layers. As an example, the vertical thickness of the Si layer 108 and the Ge-containing layer 110 may each be from about 10 nm to about 25 nm, and as a specific example, may be about 10 nm or about 20 nm. Furthermore, the Si layers 108 may have the same thickness or may have different thicknesses relative to each other, and the Ge-containing layers 110 may have the same thickness or may have different thicknesses relative to each other. In a specific example, both the Si layer 108 and the Ge-containing layer 110 have substantially the same thickness.

[0022] For example, the material of the Si layer 108 may be pure Si or silicon nitride (SiN). In some embodiments, all Si layers 108 comprise the same material; however, if desired, the Si layers 108 may comprise different materials.

[0023] For example, the material containing the Ge layer 110 may be pure Ge or a SiGe alloy. As a specific example, the Ge layer 110 may include an appropriate ratio (e.g., Si0.7Ge) for the desired etching characteristics of a given application or for the desired performance of a semiconductor device formed using a portion of process 100. 0.3 Si 0.75 Ge 0.25 SiGe alloys (mixtures), etc. In some embodiments, all Ge-containing layers 110 comprise the same material; however, if desired, the Ge-containing layers 110 may comprise different materials.

[0024] The substrate 106 can be any suitable material, and in one example includes a Ge or SiGe alloy. In a particular example, the film stack 104 is formed by growing alternating heteroepitaxial layers of Si (e.g., Si layer 108) and Ge or SiGe (e.g., Ge-containing layer 110) on top of the substrate 106.

[0025] An optional hard mask 112 may be included on top of the film stack 104. For example, in a prior etching process, a hard mask 112 may be used to form the structure of the film stack 104. In some embodiments, the hard mask 112 is SiN, but may include any suitable material.

[0026] Barrier layer 114 is formed on film stack 104 (including hard mask 112), and in this example on substrate layer 106. Barrier layer 114 may be generated by a previous fabrication step (e.g., RIE) applied to substrate 102, or by other treatments of substrate 102 (e.g., exposure to ambient air during transfer between processing tools). As a specific example, barrier layer 114 may include NOL, RIE residue, or both. NOL may be, for example, a thin layer of SiO2 (or other suitable material) about 1 nm to about 2.0 nm thick, formed on the surface of substrate 102, such as when substrate 102 is exposed to ambient air containing O2 and H2O. For example, the surfaces of substrate layer 106, Si layer 108, Ge-containing layer 110, and hard mask 112 may interact with ambient air, which may generate barrier layer 114 at these surfaces. As another example, the surfaces of the substrate 106, Si layer 108, Ge-containing layer 110, and hard mask 112 may include residues produced by the previous RIE step.

[0027] The barrier layer 114 may have different etch characteristics than the layers located beneath it. Although shown as having a substantially uniform coverage over the film stack 104 (including the hard mask 112) and the substrate layer 106, the barrier layer 114 may or may not have uniform coverage.

[0028] As shown, when viewed from a cross-sectional perspective, each layer in the film stack 104 has a pair of exposed surfaces at opposite ends. That is, each Si layer 108 has an (opposite) exposed surface 116, and each Ge-containing layer 110 has an (opposite) exposed surface 118. Furthermore, in Figure 1A In the state shown, because the substrate 102 includes a barrier layer 114, the exposed surface 116 of the Si layer 108 and the exposed surface 118 containing the Ge layer 110 include the barrier layer 114.

[0029] like Figure 1BAs shown, barrier layer 114 is etched to remove some or all of barrier layer 114 from the exposed surface 116 of Si layer 108, the exposed surface 118 of Ge-containing layer 110, and the exposed surfaces of substrate layer 106 and hard mask 112. Barrier layer 114 can be removed using any suitable process, including any suitable wet or dry etching process. In some embodiments, substrate 102 is treated with dilute HF acid or chemical oxide removal processes to remove some or all of barrier layer 114. The process used to etch barrier layer 114 may or may not remove some or all of hard mask 112, but for the purposes of this example, hard mask 112 is shown as not being removed or otherwise etched. However, removing barrier layer 114 from the exposed surface 116 of Si layer 108 and the exposed surface 118 of Ge-containing layer 110 reduces the selectivity of subsequent conventional oxygen-based recessed plasma etching processes (e.g., using NF3 and O2) attempting to etch Si layer 108 with minimal to no etching of Ge-containing layer 110.

[0030] like Figure 1C As shown, in the plasma step 120 of process 100, substrate 102 is exposed to plasma 122 to selectively etch the Si layer 108. For example, substrate 102 may be exposed to plasma 122, which is an oxygen-free plasma, to selectively etch the exposed surface 116 of the Si layer 108 to form a recess 136 in the film stack 104, with opposite ends of the Si layer 108 in an intermediate state of removal / etching relative to the adjacent Ge-containing layer 110. In some embodiments, plasma step 120 is an isotropic etching process.

[0031] Plasma step 120 can be performed in the plasma chamber 123 of the plasma tool. The plasma tool can be any suitable type, including inductively coupled plasma (ICP) tools, capacitively coupled plasma (CCP) tools, surface wave plasma (SWP) tools, etc. See below for reference. Figure 5 Describe an example plasma tool.

[0032] In some embodiments, plasma step 120 is an oxygen-free plasma etching process to etch portions of certain layers of the film stack on substrate 102, thereby giving substrate 102 a recessed or sunken film stack after performing process 100. It should be understood that oxygen-free does not necessarily mean the elimination of all oxygen from plasma step 120, but rather reflects that oxygen-containing gas is not intentionally introduced as part of plasma step 120. Removing all oxygen from plasma chamber 123 can be difficult or impossible, and therefore some oxygen may still remain during some of the steps described below.

[0033] During the exposure of substrate 102 to plasma 122 and to facilitate selective etching of Si layer 108, plasma 122 may cause a passivation layer 124 to be formed on the exposed surface 118 of Ge-containing layer 110. Plasma 122 may cause the passivation layer 124 to be formed on the exposed surface 118 of Ge-containing layer 110 by removing and replacing or otherwise modifying portions of the exposed surface 118 of Ge-containing layer 110. In some embodiments, passivation layer 124 may also be formed on the exposed surface of substrate 106, such as when substrate 106 is pure Ge or includes Ge (e.g., SiGe substrate 106).

[0034] During the exposure of substrate 102 to plasma 122, a passivation layer 124 on the exposed surface 118 of the Ge-containing layer 110 (and, in the illustrated example, on the exposed surface of the base layer 106) inhibits the etching of the Ge-containing layer 110 (and, in the illustrated example, the base layer 106). In other words, plasma 122 selectively etches the Si layer 108 at least in part due to the formation and presence of the passivation layer 124 on the exposed surface 118 of the Ge-containing layer 110 (and on the exposed surface of the base layer 106).

[0035] While the passivation layer 124 can have any suitable thickness, in some embodiments it is thinner, such as 2 nm or less. The passivation layer 124 can be, for example, a monolayer. In some embodiments, the passivation layer 124 is a nitride, such as germanium nitride (e.g., Ge3N4).

[0036] As plasma 122 etches the Si layer 108, an additional surface 138 containing the Ge layer 110 is exposed. That is, due to the selective etching of the Si layer 108, a recess 136 or depression is formed in the film stack 104, exposing the additional surface 138 containing the Ge layer 110. Plasma 122 may continue to form a passivation layer 124 on the additional surface 138. The passivation layer 124 formed on the additional surface 138 may also be a nitride, such as germanium nitride (e.g., Ge3N4). In other words, as the Si layer 108 is etched above, below, and / or between the Ge layer 110, the passivation layer 124 is further formed on the newly exposed surface of the Ge layer 110 (e.g., the additional surface 138). The passivation layer 124 on the additional surface 138 inhibits etching of the Ge layer 110 at the additional surface 138, while the passivation layer 124 at the exposed surface 118 of the Ge layer 110 inhibits etching of the Ge layer 110 at the exposed surface 118.

[0037] Plasma 122 may include a fluorine agent 126, a hydrogen agent 128, and a nitrogen agent 130. Fluorine agent 126 may primarily act as an etchant for etching the Si layer 108 at its exposed surface 116. Hydrogen agent 128 may act as a reducing agent, promoting etching of the Si layer 108 at its exposed surface 116 in the presence of fluorine agent 126. Furthermore, if applicable, depending on the gas used to generate plasma 122, hydrogen agent 128 may further decompose certain compounds of fluorine and nitrogen to produce fluorine agent 126 and nitrogen agent 130. Nitrogen agent 130 reacts with Ge at the exposed surface 118 containing the Ge layer 110 to form a nitride layer (e.g., a germanium nitride layer, such as Ge3N4) at the exposed surface 118. For example, atomic nitrogen (N) generated in plasma 122 can react with Ge molecules at the exposed surface 118 of the Ge-containing layer 110 (and the exposed surface of the substrate 106) to form a passivation layer 124 (e.g., a nitride layer) on the exposed surface 116 of the Ge-containing layer 110 (and on the exposed surface of the substrate 106).

[0038] In some embodiments, plasma 122 may be generated by a gas including fluorine, nitrogen, and hydrogen. As several examples, the fluorine-containing gas used to generate plasma 122 may include NF3, sulfur hexafluoride (SF6), or carbon tetrafluoride (CF4). Furthermore, although fluorine has been described, other halogens may also be used to facilitate the etching process.

[0039] In some embodiments, oxygen-containing gas is not intentionally introduced as part of the gas generating plasma 122. As a specific example, the gas used to generate plasma 122 may include a suitable combination of NF3, N2, and H2. As another specific example, the gas may include NF3, ammonia (NH3), and N2. In some embodiments, N2 may be replaced by an inert gas such as argon (Ar) or krypton (Kr), or such inert gases may be used in combination with N2. As a specific example, gas / gas combinations used to generate plasma 122 may include N2 / H2 / NF3, N2 / NH3 / NF3, Ar / NH3 / NF3, N2 / H2 / Ar / NF3, NF3 / NH3, NF3 / H2, or N2 / H2 / NH3 / NF3.

[0040] When the Si layer 108 and the Ge-containing layer 110 are exposed to a plasma (e.g., plasma 122) comprising a fluorine agent 126 and a nitrogen agent 130 (and possibly a hydrogen agent 128), the reaction of the fluorine agent 126 with Si (e.g., at the exposed surface 116 of the Si layer 108) is faster than the reaction of the hydrogen agent 128 or the nitrogen agent 130 with Si, resulting in the etching of the Si layer 108. Furthermore, although the fluorine agent 126 is generally considered more reactive than the hydrogen agent 128 or the nitrogen agent 130, when the Ge-containing layer 110 is exposed to plasma 122 comprising a fluorine agent 126 and a nitrogen agent 130 (and possibly a hydrogen agent 128), the reaction of the hydrogen agent 128 and / or the nitrogen agent 130 with Ge (e.g., at the exposed surface 118 and additional surface 138 of the Ge-containing layer 110) is faster than the reaction of the fluorine agent 126 with Ge, thereby forming a passivation layer 124 (e.g., germanium nitride). Furthermore, since the reaction of hydrogen agent 128 and / or nitrogen agent 130 with Ge is largely responsible for the formation of passivation layer 124 on the exposed surface 118 and additional surface 138 of Ge-containing layer 110, a higher concentration of Ge in Ge-containing layer 110 may increase the likelihood of forming passivation layer 124 on the exposed surface 118 and additional surface 138 of Ge-containing layer 110.

[0041] In examples where the gases used to generate plasma 122 include NF3 and N2, the NF3 to N2 ratio may be a suitable consideration. In some embodiments, plasma 122 includes more nitrogen than fluorine to ensure that the passivation layer 124 forms quickly enough to reduce or eliminate etching of the Ge-containing layer 110 by fluorine, and because fluorine is a more reactive chemical in plasma 122. A suitable ratio (or range of ratios) may depend on a variety of factors, including other process parameters and the Ge concentration in the Ge-containing layer 110. In some embodiments, a higher percentage of Ge in the Ge-containing layer 110 may result in faster formation of the passivation layer 124 and better results. H2 may be added to help drive the reactions occurring in plasma chamber 123, including etching the Si layer 108 and forming the passivation layer 124 on the exposed surface 118 and additional surface 138 of the Ge-containing layer 110. Example ranges for the NF3 to H2 ratio may include from NF3:H2 = 1:1.5 to NF3:H2 = 1:3. Examples of the NF3:N2 ratio range may include NF3:N2 = 1:2.5 to NF3:N2 = 1:10.

[0042] Other process parameters used to generate plasma 122 include gas flow rate, pressure, plasma source power, plasma bias power, time, and temperature. The gas used to form plasma 122 can be provided at any suitable flow rate. In some embodiments, the etchant source gas flow rate is NF3 = 20-50 sccm, H2 = 30-150 sccm, and N2 = 50-500 sccm. In some embodiments, plasma step 120 can be performed at intermediate pressures (e.g., about 100 mTorr to about 500 mTorr, and in one example about 300 mTorr to about 350 mTorr) and intermediate source power (e.g., about 100 W to about 400 W, and in one example about 200 W to about 300 W). The exposure time for plasma step 120 can be any suitable time. In some embodiments, the exposure time can be as short as about five seconds or less, ten seconds or less, fifteen seconds or less, or twenty seconds or less. In a particular embodiment, the exposure time is about fifteen seconds. In some embodiments, plasma step 120 is performed at a temperature of approximately -40°C to approximately 20°C, and in one example, at approximately 0°C. It should be understood that the specific values ​​and ranges provided herein are for illustrative purposes only.

[0043] An example formulation of the oxygen-free etching process 120 includes the following: a pressure of 350 mTorr; a source power (inductively coupled plasma) of 300 W; a bias power of 0 W; a wafer processing temperature of 0 °C; and flow rates of NF3, H2, and N2 of 30 sccm, 55 sccm, and 250 sccm, respectively. Another example formulation may include: a pressure of 300 mTorr; a source power (inductively coupled plasma) of 300 W; a bias power of 0 W; a wafer processing temperature of 0 °C; and flow rates of NF3, H2, and N2 of 20 sccm, 36 sccm, and 250 sccm, respectively.

[0044] Figure 1D Substrate 102 is shown after plasma step 120. Figure 1D In the illustrated state, the membrane stack 104 includes recesses 136 (two examples are labeled). Furthermore, due to the formation of the recesses 136, an exposed end 141 containing a Ge layer 110 can be formed (one example is labeled).

[0045] Figure 1DSome measurements of the resulting substrate 102 are shown, such as the exposed end spacing 142 and the etch width 144. For example, the exposed end spacing 142 indicates the remaining width of the Si layer 108 (each of these sections) by measuring each Si layer 108 from a first exposed surface 116 on a first side of the film stack 104 to an opposite second exposed surface 116 on a second side of the film stack 104. In some embodiments, the exposed end spacing 142 may be less than 20 nm, and in one embodiment it is between 2 nm and 20 nm. The exposed end spacing may also refer to the spacing of the exposed ends before etching. The etch width 144 measures how much of a particular Si layer 108 is removed from a particular end of a particular Si layer 108. In other words, the etch width 144 measures the amount of recess 136 in the Si layer 108. In some embodiments, the etch width 144 is from about 5 nm to about 15 nm. However, depending on the given application, the exposed end spacing 142 and the etch width 144 may be outside these ranges.

[0046] Subsequent processing can then be performed on substrate 102. For example, a plasma step 120 can be integrated into a process for forming the Ge-containing layer 110 into a corresponding nanowire for a channel region of a semiconductor device such as a GAA device. In such devices, subsequent processing may include filling the recess 136 with an insulator, removing the remainder of the Si layer 108, providing a gate oxide around the Ge-containing layer 110, and other associated steps, all of which are provided merely for illustrative purposes. In such devices, the exposed end 141 of the Ge-containing layer 110 can be used as a conductive contact to a channel region formed in the region of the film stack 104.

[0047] Process 100 offers one or more technological advantages. Compared to conventional techniques that selectively etch Si layers containing Ge layers, it utilizes plasma chemistry comprising an etchant (e.g., fluorine) and oxygen (e.g., NF3 / O2 or CF4 / O2) (referred to as F / O-based plasma). Such F / O-based plasma can oxidize the surface of the Ge-containing layer to form germanium dioxide (GeO2) or germanium oxynitride (GeO2) on the Ge-containing layer. x N y Etch-stop layer. While this etch-stop layer inhibits the etchant's ability to etch the Ge-containing layer, it can be thick and thus replace a significant portion of the Ge-containing layer, reducing its thickness by an undesirable amount. As device dimensions shrink, this loss can become a significant percentage of the Ge-containing layer in the channel region (and ultimately, the nanowire / nanofaft). Furthermore, the timing of this etch-stop layer formation allows the etchant to erode areas where the etch-stop layer has not yet formed. Additionally, the oxide etch-stop layer can be water-soluble.

[0048] Furthermore, F / O-based plasmas can etch other materials on semiconductor substrates, such as silicon dioxide (SiO2), silicon nitride (Si3N4), oxides, and low-k dielectric materials, which may be undesirable. In other words, such oxygen-containing plasmas (e.g., F / O-based plasmas) are not selective for SiO2, Si3N4, oxides, and low-k dielectric materials.

[0049] According to an embodiment of process 100, the passivation layer 124 formed on the Ge-containing layer 110 may include a nitride (e.g., germanium nitride) that is thinner than the etch stop layer formed by oxidizing the Ge-containing layer according to conventional techniques. In some embodiments, the thickness of the Ge-containing layer 110 is reduced by less than about 2.0 nm by selectively etching the Si layer 108 by exposing the substrate 102 (including the film stack 104) to plasma 122. Therefore, process 100 reduces the loss of the Ge-containing layer 110 during the selective etching of the Si layer 108 compared to the losses incurred using conventional techniques.

[0050] Furthermore, the film stack 104 may have an improved etch profile, at least in part due to the high selectivity of plasma 122 for the Ge-containing layer 110, and at least in part due to the rapid formation of the passivation layer 124 on the exposed surface 118 and additional surface 138 of the Ge-containing layer 118. The improved etch profile may include a reduction in surface roughness along the surface 116 of the Si layer 108 after the plasma step 120 (to the extent that the Si layer 108 is not completely removed), and particularly along the exposed surface 118 and the remaining surface 138 of the Ge-containing layer. Additionally or alternatively, the improved etch profile may include a sharp edge and square profile at the exposed end 141 of the Ge-containing layer after the plasma step 120. In some embodiments, the plasma process 120, including the use of plasma 122, provides a relatively straight Si etch front along the surface 116 of the Si layer 108 (to the extent that the Si layer 108 is not completely removed) and good local uniformity regarding the amount of Si removed from each Si layer 108 of the film stack 104.

[0051] The nitride (e.g., germanium nitride) passivation layer 124 is insoluble in water, allowing it to act as a diffusion barrier for O2 and H2O, thereby improving the stability of the nanowires formed from the Ge-containing layer 110. In addition to being selective for Ge and SiGe, the plasma 122 (e.g., a fluorine, hydrogen, and nitrogen-containing plasma) is also selective for SiO2, Si3N4, oxides, and low-k dielectric materials because the plasma 122 lacks the oxygen that would cause conventional F / O-based plasma etching of these materials. Furthermore, removing the barrier layer 114 prior to recessed etching reduces surface roughness; however, the plasma 122 also exhibits improved selectivity for etching the Si layer 108 relative to the Ge-containing layer 110 due to the increased rate of passivation layer 124 formation relative to the oxide etch stop layer.

[0052] Figure 2 An example method 200 for processing a substrate 102 according to certain embodiments of this disclosure is illustrated. Method 200 begins at step 202. At step 204, the substrate 102 is received. The substrate 102 has a film stack 104 comprising Si layers 108 and Ge-containing layers 110 arranged in an alternating stacked configuration. That is, the film stack 104 may comprise alternating Si layers 108 and Ge-containing layers 110 (e.g., as shown in the diagram). Figure 1A (As shown). The barrier layer 114 (e.g., NOL) may be present on the surface of the film stack 104, such as on the exposed surface 116 of the Si layer 108, the exposed surface 118 of the Ge layer 110, and the exposed surfaces of the substrate layer 106 and the hard mask 112.

[0053] In step 206, the barrier layer 114 on the surface of the film stack 104 is etched to remove the barrier layer 114 from, for example, the exposed surface 116 of the Si layer 108, the exposed surface 118 of the Ge layer 110, and the exposed surfaces of the substrate layer 106 and the hard mask 112. The barrier layer 114 can be removed using any suitable process (e.g., wet etching or dry etching process).

[0054] In step 208, the Si layer 108 is selectively etched by exposing the substrate 102 (including the film stack 104) to plasma 122. Plasma 122 may include a fluorine agent 126 and a nitrogen agent 130. In some embodiments, plasma 122 further includes a hydrogen agent 128. Plasma 122 etches the Si layer 108 and forms a passivation layer 124 on the exposed surface 118 containing the Ge layer 110 to suppress etching of the Ge layer 110 during exposure of the semiconductor device 102 (including the film stack 104) to plasma 122. In some embodiments, step 208 is an isotropic etching process.

[0055] In some embodiments, plasma 122 is generated by a gas comprising NF3 gas, and fluorinating agent 126 comprises fluorine dissociated from NF3 gas. In some embodiments, plasma 122 is generated by a gas comprising N2 gas, and nitrogen agent 130 comprises nitrogen gas. As a specific example, plasma 122 is generated by a combination of gases comprising: NF3 and NH3; NF3, NH3 and N2; NF3, NH3 and Ar; NF3 and H2; NF3, H2 and N2; or NF3, H2, NH3 and N2. In some embodiments, passivation layer 124 formed on the exposed surface 118 containing Ge layer 110 comprises germanium nitride (Ge3N4).

[0056] Selectively etching the Si layer 108 may include selectively etching the ends of the Si layer 108 to form a recess 136 in the film stack 104 above, below, or between the Ge-containing layer 110. As the Si layer 108 is selectively etched, an additional surface 138 of the Ge-containing layer 110 is exposed, and plasma 122 forms a passivation layer 124 on the additional surface 138. In some embodiments, selectively etching the Si layer 108 includes selectively removing substantially all of the Si layer 108, thereby releasing the Ge-containing layer 110. In some embodiments, selectively etching the Si layer 108 by exposing the substrate 102 (including the film stack 104) to plasma 122 reduces the thickness of the Ge-containing layer 110 by less than about 2.0 nm.

[0057] In step 210, additional manufacturing steps are performed. (See above for reference.) Figure 1D The description of potential additional processing steps is incorporated by reference. For example, in some embodiments, step 208 is integrated into a process for forming a corresponding nanowire containing the Ge layer 110 as a channel region of a semiconductor device such as a GAA device. At step 212, the method ends.

[0058] Figure 3 An example method 300 for processing a substrate 102 according to certain embodiments of this disclosure is illustrated. Method 300 begins at step 302. In step 304, the substrate 102 is positioned in the plasma chamber 123 of a plasma tool. The substrate 102 has a film stack 104 comprising alternating Si layers 108 and Ge-containing layers 110 (e.g., as shown in the image). Figure 1A (As shown).

[0059] In step 306, plasma 122 is generated in plasma chamber 123 of the plasma tool. Plasma 122 includes a fluorine agent 126, a nitrogen agent 130, and a hydrogen agent 128. Plasma 122 can be generated without intentionally introducing oxygen-containing gas into plasma chamber 123. Plasma 122 can be generated by a gas including fluorine-containing gases such as NF3, SF6, or CF4. Fluorine agent 126 may include fluorine dissociated from the fluorine-containing gas. In some embodiments, plasma 122 is generated by a gas including nitrogen-containing gas, and the nitrogen-containing gas includes NH, NH2, or NH3, and nitrogen agent 130 includes nitrogen dissociated from the nitrogen-containing gas.

[0060] In some embodiments, plasma 122 is generated by a gas comprising N2 and H2, a nitrogen agent 130 comprising nitrogen, and a hydrogen agent 128 comprising hydrogen. As a specific example, plasma 122 may be generated by a combination of gases including: NF3 and NH3; NF3, NH3, and N2; NF3, NH3, and Ar; NF3 and H2; NF3, H2, and N2; or NF3, H2, NH3, and N2.

[0061] In step 308, substrate 102 (including film stack 104) is exposed to plasma 122 in plasma chamber 123. Plasma 122 causes a passivation layer 124, which may be a nitride layer, to be formed on the exposed surface 118 of the Ge-containing layer 110 and an additional surface 138. In some embodiments, passivation layer 124 comprises germanium nitride (Ge3N4). Plasma 122 also selectively etches the exposed surface 116 (e.g., the opposite exposed end) of Si layer 108 to form a recess 136 in Si layer 108 relative to the exposed surface 118 (e.g., the opposite exposed end) of Ge-containing layer 110. Passivation layer 124 inhibits etching of Ge-containing layer 110 by plasma 122. In some embodiments, step 308 is an isotropic etching process.

[0062] In step 310, additional manufacturing steps are performed. (See above for reference.) Figure 2 The discussion of the potential additional processing steps described in step 210 is incorporated by reference. In step 312, the method ends.

[0063] Figure 4 Example device 400, comprising a substrate with alternating film stacks having recesses, is shown according to certain embodiments of this disclosure. At least a portion of device 400 may be formed using any of the processes and methods described herein.

[0064] Device 400 includes a substrate 402 comprising a channel material 404 (e.g., Ge or SiGe) and a gate material 406 (e.g., SiGe or Si). At some point after process 100, the channel material 404 may correspond to a Ge-containing layer 110 of the substrate 102. Device 400 may be a GAA device as shown herein, or any other device such as a FinFET. Device 400 may also include an isolation region 408. In some embodiments, the isolation region 408 is a shallow trench isolation (STI).

[0065] Device 400 can be fabricated by first forming a recessed alternating film stack 410 (which may correspond to film stack 104 after process 100 and may have additional subsequent processes) and then depositing additional gate material 406 on the recessed alternating film stack 410. Specifically, device 400 can be formed by heteroepitaxial growth of alternating Si and Ge or SiGe layers, and then patterning these layers and vertically recessing them to laterally expose the Ge or SiGe layers.

[0066] The embodiments described herein are advantageously suited as optimal solutions for 5nm, 3nm, or lower nodes. For example, the GAA device architecture is suitable for scaling beyond 7nm nodes. The GAA device architecture addresses the short-channel effect found in some FinFET architectures by wrapping the gate around the entire channel instead of just three sides. This reduces or eliminates current leakage under the gate of the FinFET, thereby reducing non-active power losses.

[0067] Figure 5 A block diagram illustrating an example plasma tool 500 according to certain embodiments of this disclosure is provided. Although a particular plasma tool 500 is shown and described, any suitable type of plasma tool can be used. The plasma tool 500 can be used to perform the reference... Figure 1A-1D and Figure 2-4 The plasma process 120 is described.

[0068] Plasma tool 500 includes a plasma chamber 123 in which a semiconductor substrate (e.g., substrate 102) is treated using plasma (e.g., plasma 122). Plasma chamber 123 includes a substrate stage 502 configured to support substrate 102 during processing. In some embodiments, substrate 102 is... Figure 1BIn the indicated state, for example after removing the barrier layer 114, the substrate is positioned on the substrate stage 502 for performing plasma step 120 using plasma 122. Plasma (e.g., plasma 122) is injected through the nozzle 504 of the plasma tool 500, selectively etching the material of the Si layer 108 of the film stack 104 of the substrate 102 within the plasma chamber 123 (e.g., as shown above in the reference). Figure 1A-1D (Described). Nozzle 504 may include a single mixing reaction chamber filled with a precursor gas, a mixed gas, and a carrier gas mixed to form plasma 122, and a set of outlet orifices for distributing plasma 122 toward substrate 102.

[0069] Plasma chamber 123 includes and / or is otherwise coupled to a vacuum pump 506, which is coupled to a vacuum line 508 to remove residual precursor gas from plasma chamber 123, and in some embodiments may also include and / or be otherwise coupled to a pressure system to maintain a target pressure. Plasma chamber 123 may further include mechanical tools, such as a heater 510 and a temperature sensor 512, for heating substrate 102 and controlling the temperature within plasma chamber 123 and / or substrate 102.

[0070] The plasma tool 500 includes a precursor gas line 514, a mixed gas line 516, and a carrier gas line 518 coupled to a nozzle 504. In some embodiments, the precursor gas supplied through the precursor gas line 514 may include a fluorine-based precursor, such as fluorine or NF3, the mixed gas supplied through the mixed gas line 516 may include hydrogen, and the carrier gas supplied through the carrier gas line 518 may include nitrogen or an inert gas, such as argon or krypton.

[0071] In some embodiments, the plasma tool 500 may include a mass flow controller and sensor system for controlling gas flow rates (e.g., mass flow rates). Therefore, the plasma tool 500 may include a first flow controller 520, a second flow controller 522, a third flow controller 524, a vacuum pump 506, a heater 510, a temperature sensor 512, a voltage-current (VI) sensor 526, and substrate sensors 528, 530, 532, and 534 (528-534). A precursor gas line 514, a mixed gas line 516, and a carrier gas line 518 are coupled to and controlled by the first flow controller 520, the second flow controller 522, and the third flow controller 524, respectively.

[0072] Plasma tool 500 may include controller 536 to control aspects of plasma step 120. Controller 536 may be implemented in any suitable manner. For example, controller 536 may be a computer. As another example, controller 536 may include one or more programmable ICs programmed to provide the functions described herein. In a particular example, one or more processors (e.g., microprocessors, microcontrollers, central processing units, etc.), programmable logic devices (e.g., complex programmable logic devices, field-programmable gate arrays, etc.), and / or other programmable ICs are programmed using software or other programming instructions to implement the functions described herein with respect to controller 536. The software or other programming instructions may be stored in one or more non-transitory computer-readable media (e.g., memory storage devices, flash memory, dynamic random access memory, reprogrammable storage devices, hard disk drives, floppy disks, DVDs, CD-ROMs, etc.), and the software or other programming instructions, when executed by the programmable IC, cause the programmable IC to perform the operations described herein.

[0073] Machine components such as heater 510 and temperature sensor 512 of plasma chamber 123, as well as flow controllers 520, 522 and 524, vacuum pump 506 and other components outside plasma chamber 123 are coupled to and controlled by controller 536.

[0074] Equipment sensors measure equipment parameters, such as the temperature of the substrate stage 502, heater current, vacuum pump speed and temperature, and provide signals to ensure proper equipment operation. Various process sensors measure process parameters, such as process temperature, process pressure, plasma density, gas flow rate, and gas composition, and provide signals to ensure proper process operation. Data from the equipment and process sensors continuously provides feedback to the controller 536 throughout the plasma step 120. The controller 536 can adjust in real time to keep the equipment and process close to specifications.

[0075] The controller 536 receives data from sensors and controls the process parameters of the plasma chamber 123 based on the sensor data. The controller 536 can analyze the data collected by the sensors to determine when to modify or terminate one or more steps of the plasma step 120, and provide feedback to control the process parameters of the components of the plasma chamber 123.

[0076] The controller 536 can be connected to the VI sensor 526 and the substrate sensors 528-534 to monitor the plasma 122 when the substrate 102 is exposed to the plasma 122, thereby providing real-time status of the plasma 122 and optional composition and thickness data. This feedback data can be used by the controller 536 to continuously adjust the plasma step 120 when selectively etching the substrate 102 using the plasma 122, and, for example, to shut down the plasma step 120 when a target recess (e.g., etch width 144) is reached.

[0077] Specifically, the measurement data from the substrate sensors 528-534 and the temperature sensor 512 can be received by the controller 536, and the controller 536 generates control signals that are sent to the first flow controller 520, the second flow controller 522, the third flow controller 524, the vacuum pump 506, and the heater 510.

[0078] Controller 536 can receive measurement or metrological data acquired at multiple points on substrate 102 from substrate sensors 528-534 to measure, in situ and in real time, the thickness and composition of passivation layer 124 (formed by exposing substrate 102 to plasma 122), the exposed end spacing 142, and / or the target recess (e.g., etch width 144). For example, multiple trans-substrate sensors in a multi-substrate plasma tool can be used to monitor and adjust the thickness and composition of passivation layer 124 (formed by exposing substrate 102 to plasma 122), the exposed end spacing 142, and / or the target recess from top to bottom of substrate 102 (e.g., etch width 144). Multiple trans-substrate sensors in a single-substrate plasma tool can be used to monitor and adjust the thickness and composition of passivation layer 124 (formed by exposing substrate 102 to plasma 122), the exposed end spacing 142, and / or the target recess from the center to the edge of substrate 102 (e.g., etch width 144).

[0079] Substrate sensors 528-534 may be coupled to and / or located within plasma chamber 123 for monitoring various parameters of substrate 102, plasma tool 500, and / or plasma step 120. Substrate sensors 528-534 may include various types of sensors, including but not limited to optical sensors (such as cameras, lasers, light, reflectometers, spectrometers, ellipsometers, etc.), capacitive sensors, ultrasonic sensors, gas sensors, or other sensors capable of monitoring the state of substrate 102, plasma 122, and / or plasma tool 500. In some embodiments, one or more optical sensors may be used to measure in real time (during plasma step 120) the thickness and refractive index of the material at the surface of the Ge-containing layer 118 and the surface of the substrate layer 106 (e.g., where the passivation layer 124 is being formed), the exposed end spacing 142, and / or the etch width 144a (or another suitable measurement) at the surface of the substrate layer 106 (e.g., where the passivation layer 124 is being formed). As another example, a spectrometer can be used in real time (during plasma step 120) to measure the film thickness, exposed end spacing 142, and / or etch width 144a (or another suitable measurement) of the material at the surface 118 containing the Ge layer and the surface of the substrate layer 106 (e.g., where the passivation layer 124 is being formed). In yet another embodiment, a residual gas analyzer (RGA) can be used in real time (during plasma step 120) to detect precursor decomposition for real-time chemical reaction completion detection.

[0080] The controller 536 can receive user-inputted process parameters, including, for example, etch rate, conformality, profile, and deposition rate based on standard plasma etch parameters (e.g., for passivation layer 124), such as chamber pressure, room temperature, RF source power, RF bias power, RF waveform (e.g., continuous wave RF, pulsed RF, square pulse, sawtooth pulse, etc.), etch time, and the composition and flow rate of various process gases and carrier gases. Advantageously, the user can adjust the plasma 122 to meet a target local critical dimensional uniformity (LCDU).

[0081] Based on data from substrate sensors 528-534 and user-inputted process parameters, controller 536 generates control signals to temperature sensor 512 and heater 510 to regulate the heat within plasma chamber 123. When heater 510 heats plasma chamber 123, controller 536 continuously or periodically monitors temperature sensor 512 to track the temperature of plasma chamber 123, sending control signals to heater 510 to maintain the temperature within plasma chamber 123.

[0082] Once controller 536 determines, based on data provided by temperature sensor 512, that the target temperature of plasma chamber 123 has been reached, controller 536 generates control and data signals to activate first flow controller 520, second flow controller 522, and third flow controller 524. Based on user-input process parameters, controller 536 provides target flow rates for the precursor gas to first flow controller 520, for the mixed gas to second flow controller 522, and for the carrier gas to third flow controller 524. Once controller 536 determines that the corresponding flow rates have been established, controller 536 provides power to plasma chamber 123 to supply power to plasma 122 through bias and source electrodes. The power supplied to bias and source electrodes is adjustable based on measurements from VI sensor 526. First flow controller 520, second flow controller 522, and third flow controller 524 can each be a closed-loop control system connected to a flow rate sensor and an adjustable proportional valve, allowing each flow controller to continuously or periodically monitor and internally maintain the target flow rate for each gas via the flow rate sensor and adjustable proportional valve.

[0083] In some embodiments, once the controller 536 determines, based on user-input data, that the etching process time has been met, the controller 536 generates a control signal to deactivate the first flow controller 520, the second flow controller 522, and the third flow controller 524, which may be deactivated at the same or different times, depending on the circumstances.

[0084] Controller 536 may use or analyze substrate sensor data to determine when to end plasma step 120. For example, controller 536 may receive data from a residual gas analyzer to detect the end of plasma step 120. In another example, controller 536 may use elliptic polarization spectroscopy to detect the average film thickness of passivation layer 124, the exposed end 141 of Ge layer 110, and / or the exposed end spacing 142 during plasma step 120, and indicate changes during plasma step 120. In yet another example, controller 536 may use elliptic polarization spectroscopy to detect the refractive index of the material at the surface 118 of Ge layer and the surface of substrate layer 106 (e.g., where passivation layer 124 is being formed) during plasma step 120, and indicate changes in film composition during plasma step 120. Controller 536 may automatically end plasma step 120 when the exposed end spacing 142 and / or etch width 144a (or another suitable measurement) target is achieved. In some embodiments, controller 536 may automatically adjust one or more parameters, such as the ratio of NF3 to H2 and / or the ratio of NF3 to N2, for example, during plasma step 120, to achieve a desired etch profile of the film stack 104. Data from controller 536 and substrate sensors 528-534 can also be used to achieve a desired semiconductor substrate yield target. Further, data from controller 536 and substrate sensors 528-534 can be used to achieve a desired etch profile and composition of the film stack 104, as well as a desired semiconductor substrate yield, or alternatively, a combination thereof.

[0085] Although described for a specific application of forming nanowires / nanofa sheets for GAA devices, this disclosure can be used for any type of isotropic etching of Si with selective Ge-containing layers. Furthermore, while the etching performed is primarily described as forming recesses in the film stack 104 by removing portions of the Si layer 108 at opposite ends, processes 100 and 400 can be used to remove substantially all portions of the Si layer 108, which may be referred to as releasing the Ge-containing layer 110.

[0086] Although this disclosure describes particular process / method steps as occurring in a specific order, this disclosure contemplates process steps occurring in any suitable order. While this disclosure has been described with reference to illustrative embodiments, this description is not intended to be construed in a limiting sense. Various modifications and combinations of the illustrative embodiments and other embodiments of this disclosure will be apparent to those skilled in the art under the referenced description. Therefore, the appended claims are intended to cover any such modifications or embodiments.

Claims

1. A method for processing a semiconductor substrate, the method comprising: A semiconductor substrate comprising a film stack comprising a first germanium-containing layer, a second germanium-containing layer, and a first silicon layer located between the first germanium-containing layer and the second germanium-containing layer is received. as well as The first silicon layer is selectively etched by exposing the film stack to a plasma containing fluorine and nitrogen, while the plasma etches the first silicon layer, causing passivation layers to form on the exposed surfaces of the first germanium-containing layer and the second germanium-containing layer to inhibit the etching of the first germanium-containing layer and the second germanium-containing layer during the exposure of the film stack to the plasma. The plasma is generated without intentionally introducing oxygen-containing gas into the plasma chamber, and the passivation layer formed on the exposed surfaces of the first germanium-containing layer and the second germanium-containing layer contains germanium nitride Ge3N4.

2. The method as described in claim 1, wherein, The plasma further contains hydrogen.

3. The method as described in claim 1, wherein, The plasma is generated by a gas containing nitrogen trifluoride (NF3) gas, and the fluorinating agent contains fluorine dissociated from the NF3 gas.

4. The method of claim 1, wherein, The plasma is generated by a gas containing N2 gas, and the nitrogen agent is nitrogen gas.

5. The method of claim 1, wherein, This plasma is generated by a combination of gases including: Nitrogen trifluoride (NF3) and ammonia (NH3); NF3, NH3 and nitrogen N2; NF3, NH3, and argon (Ar); NF3 and hydrogen (H2); NF3, H2, and N2; or NF3, H2, NH3 and N2.

6. The method of claim 1, wherein, Both the first germanium-containing layer and the second germanium-containing layer are germanium layers or both are silicon-germanium layers.

7. The method of claim 1, wherein, One of the first germanium-containing layer and the second germanium-containing layer is a germanium layer, and the other of the first germanium-containing layer and the second germanium-containing layer is a silicon-germanium layer.

8. The method of claim 1, wherein, Selectively etching the first silicon layer includes selectively etching the ends of the first silicon layer to form a recess in the film stack between the first germanium-containing layer and the second germanium-containing layer.

9. The method of claim 1, wherein, As the first silicon layer is selectively etched to expose additional surfaces of the first germanium-containing layer and the second germanium-containing layer, the plasma forms the passivation layer on these additional surfaces.

10. The method of claim 1, wherein, Selectively etching the first silicon layer includes selectively removing all of the first silicon layer between the first germanium-containing layer and the second germanium-containing layer.

11. The method of claim 1, wherein, Before selectively etching the first silicon layer: A natural oxide layer exists on the surface of the film stack; and The method further includes etching the natural oxide layer.

12. The method of claim 1, wherein: The film stack further includes a second silicon layer and a third germanium-containing layer, the second silicon layer being located between the second germanium-containing layer and the third germanium-containing layer; and The method includes selectively etching the second silicon layer by exposing the film stack to the plasma, the plasma forming the passivation layer on the exposed surface of the third germanium-containing layer to suppress the etching of the third germanium-containing layer during the exposure of the film stack to the plasma.

13. A method for processing a semiconductor substrate, the method comprising: A semiconductor substrate is positioned in the plasma chamber of a plasma tool. The semiconductor substrate includes a film stack comprising silicon layers and germanium-containing layers arranged in an alternating stacked manner, having at least two silicon layers and at least two germanium-containing layers. The plasma tool generates a plasma containing fluorine, nitrogen and hydrogen in the plasma chamber without intentionally introducing oxygen-containing gas into the plasma chamber. as well as In the plasma chamber of the plasma tool, the film stack is exposed to plasma, which causes a nitride passivation layer to be formed on the exposed surface of the germanium-containing layer while selectively etching the opposite exposed end of the silicon layer to form a recess in the silicon layer relative to the opposite exposed end of the germanium-containing layer. The nitride passivation layer inhibits the etching of the germanium-containing layer by the plasma. The nitride passivation layer formed on the exposed surface of the germanium-containing layer contains germanium nitride Ge3N4.

14. The method of claim 13, wherein: The plasma is generated by a gas containing fluorine, specifically nitrogen trifluoride (NF3), sulfur hexafluoride (SF6), or carbon tetrafluoride (CF4); and The fluorinating agent contains fluorine that dissociates from the fluorine-containing gas.

15. The method of claim 13, wherein: The plasma is generated by a gas containing nitrogen, including N2, NF3, or NH3; and The nitrogen agent contains nitrogen dissociated from the nitrogen-containing gas.

16. The method of claim 13, wherein: The plasma is generated by a gas containing nitrogen (N2) and hydrogen (H2). This nitrogen agent contains nitrogen gas; and This hydrogen agent contains hydrogen gas.

17. The method of claim 13, wherein, This plasma is generated by a combination of gases including: Nitrogen trifluoride (NF3) and ammonia (NH3); NF3, NH3 and nitrogen N2; NF3, NH3, and argon (Ar); NF3 and hydrogen (H2); NF3, H2, and N2; or NF3, H2, NH3 and N2.

18. A method for processing a semiconductor substrate, the method comprising: A semiconductor substrate is positioned in the plasma chamber of a plasma tool. The semiconductor substrate includes a film stack comprising a first layer of a first material and a second layer of a second material arranged in an alternating stacked configuration. The first material is silicon and the second material is germanium. A plasma is generated for selectively etching a first layer of the first material. Generating the plasma involves introducing a gas comprising fluorine and nitrogen into the plasma chamber and maintaining a temperature on the semiconductor substrate at -40°C to 40°C. The plasma is generated without intentionally introducing oxygen-containing gas into the plasma chamber, and the plasma comprises a greater amount of nitrogen than fluorine. as well as The film stack is exposed to plasma in the plasma chamber for a period of time. The plasma selectively etches the opposite exposed end of the first layer of the first material to form a recess in the first layer of the first material relative to the opposite exposed end of the second layer of the second material. The plasma also causes a passivation layer containing germanium nitride (Ge3N4) to be formed on the exposed surface of the second layer.

Citation Information

Patent Citations

  • ETCH suppression with germanium

    US20150126039A1

  • Method for Selective Etching at an Interface Between Materials

    US20200266070A1