一种燃机空气管的聚酰亚胺耐磨带更换方法及维修方法

By melting adhesive tape on the gas turbine air pipe to form an adhesive film and bonding polyimide wear-resistant tape, the problem of unsuitable clearance between the air pipe and the compressor rotor hub was solved, thus improving the normal operation and replacement efficiency of the gas turbine.

CN116922790BActive Publication Date: 2026-07-17PIPECHINA SOUTH CHINA CO +1
View PDF 2 Cites 0 Cited by

Patent Information

Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
PIPECHINA SOUTH CHINA CO
Filing Date
2023-07-28
Publication Date
2026-07-17

AI Technical Summary

Technical Problem

During gas turbine operation, abnormal noise and vibration occur due to the detachment of polyimide wear-resistant tape in the fit clearance between the air pipe and the compressor rotor hub. Existing replacement methods are complex and it is difficult to guarantee the appropriate thickness, which affects the operation of the gas turbine.

Method used

The adhesive tape is melted and extruded at 85℃-95℃ to form an adhesive film. The new polyimide wear-resistant tape is then bonded to the end of the air pipe. The thickness of the adhesive film is controlled to be below 0.12mm. Replacement is completed by air cooling molding.

Benefits of technology

It enables rapid replacement of polyimide wear-resistant belts, ensures appropriate clearance between air pipes and compressor rotor hubs, ensures normal operation of gas turbine, simplifies replacement process and improves efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN116922790B_ABST
    Figure CN116922790B_ABST
Patent Text Reader

Abstract

本发明涉及燃机维修技术,具体而言,涉及一种燃机空气管的聚酰亚胺耐磨带更换方法及维修方法。该更换方法先将粘接胶带熔化,再挤压至所述空气管端部,形成胶膜;将新的聚酰亚胺耐磨带通过所述胶膜粘接至所述空气管端部;所述粘接胶带熔化的温度为85℃ˉ95℃,所述胶膜的厚度小于0.12mm。该方法无需对更换后的聚酰亚胺耐磨带厚度进行单独调整,从而实现对空气管端部脱落的聚酰亚胺耐磨带进行快速的更换,并且能够保证更换后的聚酰亚胺耐磨带符合工作要求,特别是厚度上能够保证空气管与压气机转子毂配合间隙适宜,保证燃机的正常运行。
Need to check novelty before this filing date? Find Prior Art

Citation Information

Patent Citations

  • Extrusion-type interelectrode sulfuration forming and encapsulating method for researching flexible sensor sensitive element

    CN102023064A

  • Method for repairing conveyor rubber belt by using high-molecular wear-resistant belt

    CN111016225A