Method for manufacturing electronic device with reduced substrate warpage

By setting active and peripheral regions on the substrate and adjusting the bevel angle and thickness of the insulating layer, a multi-layer structure is formed, which solves the substrate warping problem and improves the substrate utilization and mass production efficiency.

CN117238771BActive Publication Date: 2026-11-24INNOLUX CORP
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202210645917.1
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-06-08
Publication Date
2026-11-24
Estimated Expiration
2042-06-08

AI Technical Summary

Technical Problem

In existing fan-out panel-level packaging technologies, substrate warpage is a serious problem, affecting the efficiency of automated production.

Method used

By setting active and peripheral regions on the substrate and adjusting the bevel angle and thickness of the insulating layer, a multi-layer structure is formed, reducing substrate warping.

Benefits of technology

It effectively reduces substrate warpage, improves substrate utilization, and meets mass production requirements.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117238771B_ABST
    Figure CN117238771B_ABST
Patent Text Reader

Abstract

This invention discloses a method for manufacturing an electronic device to reduce substrate warpage, comprising providing a substrate, providing an interposer layer on the substrate, and providing an insulating layer on the interposer layer. The substrate includes an active region and a peripheral region, wherein the peripheral region is adjacent to the active region, and the ratio of the area of ​​the active region to the area of ​​the substrate surface is between 75% and 92%. The insulating layer includes a first surface and at least one bevel. The first surface of the insulating layer is disposed corresponding to the active region, and the at least one bevel is disposed corresponding to the peripheral region, forming a first angle with the substrate surface.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to a method for manufacturing an electronic device, and more particularly to a method for manufacturing an electronic device that can reduce substrate warpage. Background Technology

[0002] In fan-out packaging technology for electronic components, fan-out wafer-level packaging (FOWLP) involves manufacturing electronic components on a wafer and then packaging and dicing them. However, since the diameter of commonly used large-size wafers is only about 300 millimeters, the number of electronic components that can be packaged on a wafer simultaneously is limited. Therefore, the industry has developed fan-out panel-level packaging (FOPLP) technology to replace wafer-level packaging technology.

[0003] In existing fan-out panel-level packaging technologies, a multi-layer structure, including conductive and insulating layers, is typically fabricated on a substrate. The conductive and insulating layers are stacked to form a redistribution layer. To achieve mass production efficiency, the redistribution layer is usually coated to cover the entire substrate as much as possible to improve substrate utilization. However, this method easily leads to excessive substrate warpage, which is detrimental to automated production. Therefore, it is necessary to propose a method for manufacturing electronic devices that can reduce substrate warpage. Summary of the Invention

[0004] In view of this, the object of the present invention is to provide a method for manufacturing an electronic device that can reduce substrate warping.

[0005] To achieve the above objectives, according to an embodiment of the present invention, a method for manufacturing an electronic device is provided, comprising providing a substrate, providing an interposer layer on the substrate, and providing a first insulating layer on the interposer layer. The substrate includes an active region and a peripheral region, wherein the peripheral region is adjacent to the active region, and the ratio of the extent of the active region to the area of ​​a surface of the substrate is between 75% and 92%. The first insulating layer includes a first surface and at least one first bevel, wherein the first surface is correspondingly disposed in the active region, the at least one first bevel is correspondingly disposed in the peripheral region, and the at least one first bevel forms a first angle with the surface of the substrate. Attached Figure Description

[0006] Figure 1 This is a flowchart illustrating a method for manufacturing an electronic device according to an embodiment of the present invention.

[0007] Figure 2 This is a top view of the substrate in an embodiment of the present invention.

[0008] Figures 3 to 10 This is a schematic cross-sectional view of each stage of manufacturing the electronic device in an embodiment of the present invention.

[0009] Explanation of reference numerals in the attached figures: 110 - substrate; 120 - interposer; 131 - first insulating layer; 132 - second insulating layer; OP1 - first opening; OP2 - second opening; 141 - first conductive structure; 142 - second conductive structure; 150, 151 - microbumps; 151b - bottom surface of microbumps; 160 - chip; ST1~ST12 - steps; AR - active region; PR - peripheral region; SF0 - substrate area; SF1 - first surface; SF2 - second surface; TS1~TS4 - beveled edge; TS5, TS6 - bottom edge; L1, L2 - extension lines; t1~t4 - thickness. Detailed Implementation

[0010] The contents of this invention can be understood by those skilled in the art through reference to the detailed description below and in conjunction with the accompanying drawings. It should be noted that, for the sake of simplicity and to facilitate understanding by those skilled in the art, specific elements in the drawings are not drawn to scale. Furthermore, the number and dimensions of the elements in the drawings are for illustrative purposes only and are not intended to limit the scope of the invention.

[0011] Certain terms are used in this specification and claims to refer to specific elements. Those skilled in the art will understand that electronic device manufacturers may use different names to refer to the same elements. This document is not intended to distinguish between elements that have the same function but different names. In the claims and the following specification, words such as “comprising,” “including,” and “having” are open-ended terms and should therefore be interpreted as “containing but not limited to…”.

[0012] When a component or membrane is described as "disposed on another component or membrane" or "connected to another component or membrane," it can mean that the component or membrane is directly disposed on or directly connected to another component or membrane, or that there may be other intermediary components or membranes between them. In contrast, when a component is described as "directly disposed on another component or membrane" or "directly connected to another component or membrane," there are no intermediary components or membranes between them.

[0013] Electronic devices according to embodiments of the present invention may include display devices, light-emitting elements, antenna devices, or packaging elements, but are not limited thereto. In embodiments of packaging elements, the electronic device may be a chip-first / face-down or redistribution layer-first (RDL first) fan-out package, but is not limited thereto.

[0014] Without departing from the spirit of the invention, the technical features in the different embodiments described below may be substituted, rearranged, or mixed with each other to form other embodiments.

[0015] Figure 1 This is a flowchart illustrating a method for manufacturing an electronic device according to an embodiment of the present invention. Figure 1 The flowchart shown includes the following steps:

[0016] Step ST1: Provide a substrate 110.

[0017] Step ST2: Provide an interposer layer 120 on substrate 110.

[0018] Step ST3: Provide a first insulating layer 131 on the interlayer 120.

[0019] Step ST4: Form at least one first opening OP1 on the first insulating layer 131.

[0020] Step ST5: Provide a first conductive structure 141 within each first opening OP1.

[0021] Step ST6: Provide a second insulating layer 132 on the first insulating layer 131.

[0022] Step ST7: Form at least one second opening OP2 on the second insulating layer 132.

[0023] Step ST8: Provide a second conductive structure 142 within each second opening OP2.

[0024] Step ST9: Provide a microbump 150 on at least one second conductive structure 142.

[0025] Step ST10: Place a chip 160 on at least one microbump 150.

[0026] Step ST11: Remove the structure located within the peripheral region PR of the first insulating layer 131.

[0027] Step ST12: Remove the interposer layer 120 and provide another microbump 151 on the side of the corresponding first conductive structure 141 away from the microbump 150.

[0028] First, the present invention provides a substrate 110 in step ST1. Figure 2 This is a top view of the substrate 110 in an embodiment of the present invention. Figure 2As shown, the substrate surface of substrate 110 includes an active region AR and a peripheral region PR, with the peripheral region PR adjacent to the active region AR. In this embodiment of the invention, the length and width of substrate 110 may each be 300 mm, wherein the ratio of the range of the active region AR to the substrate area SF0 of substrate 110 is between 75% and 92%. In this embodiment of the invention, substrate 110 may be a glass substrate, but this does not limit the scope of the invention.

[0029] Please see Figure 2 As shown, in a top-view direction, the area SF0 of substrate 110 can be the integral result of the substrate's length (along the X direction) and width (along the Y direction), where the X and Y directions are perpendicular to each other. The area of ​​the active region AR can be the integral result of this projected area. A ratio between the area of ​​the active region AR and the substrate area SF0 of substrate 110 is between 75% and 92% to effectively reduce warpage. According to some embodiments, the substrate and the active region AR can be circular, trapezoidal, or other arbitrary shapes, and the integration method of the substrate area and the active region AR area will be selected according to their shapes.

[0030] In this invention, the active region AR includes a partially redistributable layer electrically connected to the chip. More specifically, the active region AR is a partially redistributable layer electrically connected to a known good die (KGD). In some embodiments, the active region AR may be considered as a region overlapping with the chip, but this does not limit the scope of the invention.

[0031] In this invention, the peripheral region PR is located outside the active region AR, adjacent to or surrounding the active region AR, and may include areas that are not electrically connected to the chip, such as test dummy areas or alignment marks. In some embodiments, the peripheral region PR may be considered as an area that does not overlap with the chip, but this does not limit the scope of the invention. For example, the substrate 110 includes the active region AR and the peripheral region PR. A test signal is provided from the peripheral region PR, and the conductive lines of the peripheral region PR are used to test whether the conductive lines of the active region AR are normal, for example, to test whether there are defects such as short circuits or open circuits in the conductive lines of the active region AR. Then, the known good areas in the active region AR will be electrically connected to the known good chip.

[0032] Figures 3 to 10 For the present invention Figure 1 The illustrated embodiment shows schematic cross-sectional views of various stages in the fabrication of the electronic device.

[0033] like Figure 1 and Figure 10As shown, the present invention provides an interposer layer 120 on the substrate 110. The interposer layer 120 can serve as a material layer for temporary bonding / peeling on both sides in an electronic device. Its material can be determined according to the coating method, application process and tools required in the electronic device production line, but does not limit the scope of the present invention.

[0034] like Figure 1 and Figure 10 As shown, the present invention provides a first insulating layer 131 on the interposer 120. The first insulating layer 131 can serve as an insulating layer, a passivation layer, a buffer inner coating, or a dielectric material between multiple metal layers. In embodiments of the present invention, the material of the first insulating layer 131 may include insulating materials such as polyimide (PI), photosensitive polyimide (PSPI), benzocyclobutene (BCB), polybenzoxazole (PBO), silicon oxide (SiOx), silicon nitride (SiNx), silicon oxide nitride (SiOxNy), and ABF (Ajinomoto Build-up Film), but this does not limit the scope of the present invention. According to some embodiments, a conductive layer may be selectively provided between the interposer 120 and the first insulating layer 131 to facilitate the preparation of subsequent film layers, wherein the conductive layer may comprise a single-layer or multi-layer structure, but this does not limit the scope of the present invention.

[0035] In this embodiment of the invention, the first insulating layer 131 includes a first surface SF1 and at least one bevel TS1. The first surface SF1 is disposed in the active region AR, for example, the first surface SF1 is disposed on the upper surface of the first insulating layer 131 in the active region AR. The bevel TS1 is disposed in the peripheral region PR, for example, the bevel TS1 is disposed on the side surface of the first insulating layer 131 in the peripheral region PR. The bevel TS1 and the substrate surface form an angle θ1, wherein the value of angle θ1 is less than 90 degrees. According to some embodiments, the value of angle θ1 is less than or equal to 30 degrees. According to some embodiments, the value of angle θ1 is less than or equal to 10 degrees.

[0036] In one embodiment, the present invention may use a coating process, a deposition process, or other suitable process to form the first insulating layer 131 on the interposer 120, but is not limited thereto. For example, when using a coating process, the parameters of the equipment can be adjusted to make the first insulating layer 131 include at least one bevel TS1 and adjust the size of the angle θ1. For example, when forming the first insulating layer 131, the ejection rate P1 of the glue applicator can be adjusted to provide the material of the first insulating layer 131 onto the interposer 120, or the glue applicator can be adjusted to apply the material of the first insulating layer 131 at a coating rate V1 to form it on the interposer 120. Since the insulating layer 131 is flowable, the thickness t2 of the first insulating layer 131 in the peripheral region PR can be made smaller than the thickness t1 in the active region AR. The thickness referred to in the present invention is the insulating layer thickness measured along the normal direction of the electronic device in a cross-sectional view. The thickness referred to in the present invention is not the thickness at the boundary between the active region AR and the peripheral region PR. Furthermore, the present invention can also achieve at least one beveled edge TS1 in the structure of the first insulating layer 131 within the peripheral region PR by using weak exposure and photomask design.

[0037] like Figure 1 and Figure 10 As shown, the present invention forms one or more first openings OP1 on the first insulating layer 131. Each first opening OP1 includes at least one bevel TS2, and each bevel TS2 forms an angle θ2 with the substrate surface SF0, wherein the value of angle θ2 is greater than the value of angle θ1 and less than 90 degrees. According to some embodiments, the value of angle θ2 is greater than or equal to 45 degrees and less than 90 degrees. According to some embodiments, the value of angle θ2 is greater than or equal to 60 degrees and less than 90 degrees. According to some embodiments, the value of angle θ3 is greater than or equal to 70 degrees and less than 90 degrees. By designing that the value of angle θ2 is greater than or equal to 45 degrees and less than 90 degrees, the adhesion between the conductive structure and the insulating layer can be improved, for example, but is not limited thereto.

[0038] like Figure 1 and Figure 10 As shown, the present invention provides a first conductive structure 141 within at least one first opening OP1. The first conductive structure 141 may comprise a single-layer or multi-layer structure. In embodiments of the present invention, the material of the first conductive structure 141 may include copper, titanium, or other suitable metal materials, and it is formed within the first opening OP1 by photolithography, deposition, electroplating, or other suitable processes, but this does not limit the scope of the present invention.

[0039] like Figure 1 and Figure 10As shown, the present invention provides a second insulating layer 132 on a first insulating layer 131. The second insulating layer 132 can serve as an insulating layer, a passivation layer, a buffer inner coating, or a dielectric material between multiple metal layers. In embodiments of the present invention, the material of the second insulating layer 132 may include insulating materials such as PI, BCB, PBO, SiOx, SiNx, SiOxNy, or ABF, but this does not limit the scope of the present invention. According to some embodiments, the materials of the first insulating layer 131 and the second insulating layer 132 may be the same or different.

[0040] In this embodiment of the invention, the second insulating layer 132 includes a second surface SF2 and at least one bevel TS3, wherein the second surface SF2 is disposed in the active region AR, and the bevel TS3 is disposed in the peripheral region PR. The bevel TS3 and the substrate surface SF0 form an angle θ3, wherein the value of angle θ3 is less than 90 degrees. According to some embodiments, the value of angle θ3 is less than or equal to 60 degrees. According to some embodiments, the value of angle θ3 is less than or equal to 30 degrees. According to some embodiments, the value of angle θ3 is less than or equal to 10 degrees.

[0041] In one embodiment, the present invention can use a coating process, a deposition process, or other suitable process to form the second insulating layer 132 on the first insulating layer 131, for example, by adjusting the parameters of the equipment to make the second insulating layer 132 include at least one bevel TS3 and adjusting the size of the angle θ3. For example, when forming the second insulating layer 132, the ejection rate P2 of the glue applicator can be adjusted to provide the material of the second insulating layer 132 onto the first insulating layer 131, or the glue applicator can be adjusted to apply the material of the second insulating layer 132 at a spreading rate V2 to form it on the first insulating layer 131. Since the insulating layer 131 is fluid, the thickness t4 of the second insulating layer 132 in the peripheral region PR can be made smaller than the thickness t3 in the active region AR along the normal direction of the electronic device. In addition, the present invention can also use weak exposure and photomask design to make the structure of the second insulating layer 132 in the peripheral region PR exhibit at least one bevel TS3. The spray rate P1 and spray rate P2 referred to in this invention may be the same or different, and the application rate V1 and application rate V2 may be the same or different. A better thickness can be obtained by adjusting the parameters to reduce warping, but this is not a limitation.

[0042] like Figure 1 and Figure 10As shown, the present invention forms one or more second openings OP2 on the second insulating layer 132. Each second opening OP2 includes at least one bevel TS4, and each bevel TS4 forms an angle θ4 with the substrate surface SF0, wherein the value of angle θ4 is greater than the value of angle θ3 and less than 90 degrees. According to some embodiments, the value of angle θ4 is greater than or equal to 45 degrees and less than 90 degrees. According to some embodiments, the value of angle θ4 is greater than or equal to 60 degrees and less than 90 degrees. According to some embodiments, the value of angle θ4 is greater than or equal to 70 degrees and less than 90 degrees.

[0043] like Figure 1 and Figure 10 As shown, the present invention provides a second conductive structure 142 within at least one second opening OP2. The second conductive structure 142 is used for electrically connecting to the first conductive structure 141, but is not limited thereto. The second conductive structure 142 may comprise a single-layer or multi-layer structure. In embodiments of the present invention, the material of the second conductive structure 142 may include copper, titanium, or other suitable metals, and it is formed within the second opening OP2 by photolithography, deposition, electroplating, or other suitable processes, but this does not limit the scope of the present invention.

[0044] like Figure 1 and Figure 10 As shown, the present invention provides microbumps 150 on at least one second conductive structure 142 for subsequent connection. The material of the microbumps 150 may include tin, nickel, copper, or other suitable metals, and they can be directly formed or bonded to the second conductive structure 142 by printing, deposition, or other suitable processes, but this does not limit the scope of the invention. According to some embodiments, microbumps 150 may be provided on at least one first conductive structure 141 for subsequent connection, and then the chip 160 is disposed on the microbumps 150, and the structure of the first insulating layer 130 in the peripheral area is removed, but this is not a limitation.

[0045] like Figure 1 and Figure 10 As shown, the present invention bonds chip 160 to at least one microbump 150. In one embodiment, the present invention may selectively fill a primer (not shown) between the surfaces of the substrate 110 of chip 160, and then perform a heat treatment to resolder the microbump 150, but this does not limit the scope of the present invention.

[0046] like Figure 1 and Figure 10 As shown, the present invention removes structures located within the peripheral region PR of the first insulating layer 131 and the second insulating layer 132. In one embodiment, the present invention can remove structures located within the peripheral region PR of the first insulating layer 131 and the second insulating layer 132 through an etching process, a cutting process, or other suitable processes, but this does not limit the scope of the present invention.

[0047] like Figure 1 and Figure 10 As shown, the present invention removes the interposer 120 and provides at least one more microbump 151 on the side of the corresponding first conductive structure 141 away from the microbump 150. In one embodiment, after removing the interposer 120, the present invention may further remove a portion of the structure of the first insulating layer 131, such that the first insulating layer 131 includes a bottom edge TS5 and another bottom edge TS6 on the side away from the microbump 150, wherein the bottom edge TS5 is, for example, located between two adjacent microbumps 151, and the other bottom edge TS6 is, for example, located between the microbump 151 and the first extension line L1 of the side of the first insulating layer 131 and the second insulating layer 132. According to some embodiments, at least one of the bottom edge TS5 and the other bottom edge TS6 may have an arcuate surface, but is not limited thereto. According to some embodiments, the roughness of the bottom edge TS5 and the other bottom edge TS6 is greater than the roughness of the surface of the second insulating layer 132, but is not limited thereto. A second extension line L2 passes through the bottom surface 151b of at least one of two adjacent microbumps 151. The bottom surface 151b may, for example, be located in the normal direction N of the electronic device, at the surface furthest from the package chip 160. According to some embodiments, the distance between the bottom surface TS5 and the second extension line L2 along the normal direction N of the electronic device is different from the distance between the other bottom edge TS6 and the second extension line L2. For example, the distance between the bottom edge TS5 and the second extension line L2 may be greater than the distance between the other bottom edge TS6 and the second extension line L2. The normal direction N of the electronic device is, for example, the Z direction, the extension direction of the first extension line L1 is, for example, the Z direction, and the extension direction of the second extension line L2 is, for example, the Z direction. Figure 2 The X or Y direction is shown, wherein the X, Y, and Z directions are perpendicular to each other, and the normal direction N (Z direction) of the electronic device is perpendicular to the surface of the substrate 110. Figure 2 (The XY plane shown).

[0048] According to some embodiments, the electronic device may further include a protective layer packaged chip 160, or a protective layer packaged chip 160, microbumps 150, an insulating layer 131, and a conductive structure layer 141. The protective layer reduces the impact of moisture on the reliability of the electronic device, but does not limit the scope of the invention. According to some embodiments, insulating layers 131, 132, and conductive structure layers 141 and 142 are staggered along the Z-direction to form a redistribution layer, wherein conductive structure layers 141 and 142 are electrically connected. The packaged chip 160 can be electrically connected to other electronic components or achieve a circuit fan-out effect through the redistribution layer. The redistribution layer may further include active or passive components such as thin-film transistors and capacitors to improve the performance of the electronic device, but this does not limit the scope of the invention.

[0049] In summary, the present invention adjusts the contour of the insulating layer in the peripheral area of ​​the substrate, thereby reducing warpage without changing the substrate coating area.

[0050] The above description is merely an embodiment of the present invention and is not intended to limit the invention. Those skilled in the art will recognize that the present invention can have various modifications and variations. Any modifications, equivalent substitutions, or improvements made within the spirit and principles of the present invention should be included within the scope of protection of the present invention.

Claims

1. A method for manufacturing an electronic device that reduces substrate warpage, characterized in that, Include: A substrate is provided, the substrate comprising an active region and a peripheral region, wherein the peripheral region is adjacent to the active region, and the ratio of the extent of the active region to an area of ​​a surface of the substrate is between 75% and 92%. An intermediate layer is provided on the substrate; A first insulating layer is provided on the interposer layer, the first insulating layer comprising: A first surface, which is correspondingly disposed in the active region; as well as At least one first inclined edge is disposed in the peripheral area, and the at least one first inclined edge and the surface of the substrate form a first angle; At least one first opening is formed on the first insulating layer, wherein the at least one first opening includes at least one second inclined side, and the at least one second inclined side forms a second angle with the substrate surface, and the second angle is greater than the first angle; A first conductive structure is provided within the at least one first opening, wherein the first conductive structure comprises a single layer or multiple layers of metallic material; A second insulating layer is provided on the first insulating layer, the second insulating layer comprising: A second surface, the second surface being disposed correspondingly in the active region; and At least one third inclined edge, wherein the at least one third inclined edge is disposed in the peripheral area, and the at least one third inclined edge and the substrate surface form a third angle, and the second angle is greater than the third angle; At least one second opening is formed on the second insulating layer, wherein the at least one second opening includes at least one fourth bevel, and the at least one fourth bevel and the surface of the substrate form a fourth angle, and the fourth angle is greater than the third angle; A second conductive structure is provided within the at least one second opening, wherein the second conductive structure comprises a single layer or multiple layers of metallic material; At least one first microbump is provided on the second conductive structure; A chip is disposed on the at least one first microbump; Remove the structures located in the peripheral region of the first and second insulating layers; Remove the intermediary layer; as well as At least one second microbump is provided on the side of the first conductive structure away from the at least one first microbump.

2. The method as described in claim 1, characterized in that, The thickness of the first insulating layer in the peripheral region is less than the thickness in the active region.

3. The method as described in claim 1, characterized in that, Also includes: The structure of the first insulating layer in the surrounding area is made to exhibit the at least one first bevel by means of a weak exposure and a photomask design.

4. The method as described in claim 1, characterized in that, The thickness of the second insulating layer in the peripheral region is less than the thickness in the active region.

5. The method as described in claim 1, characterized in that, Also includes: The structure of the second insulating layer in the surrounding area is made to exhibit the at least one third bevel by means of a weak exposure and a photomask design.

6. The method as described in claim 1, characterized in that, Also includes: After removing the interposer layer, a portion of the structure of the first insulating layer is removed, such that the first insulating layer includes a first bottom edge and a second bottom edge on the side away from the at least one first microbump, wherein: A first extension line passes through one side of the first insulating layer and the second insulating layer and extends along a normal direction of the electronic device; The first bottom edge is located between two adjacent second micro-bumps; and The second bottom edge is located between the at least one second micro-bump and the first extension line.

7. The method as described in claim 6, characterized in that: A second extension line passes through the bottom surface of the at least one second micro-bump; and The distance between the first bottom edge and the second extension line is greater than the distance between the second bottom edge and the second extension line.