Plate butt welding method
By using a welding method that increases thickness in stages, the problems of low welding accuracy and short lifespan between the plate and the main pipe were solved, resulting in a stable connection structure and improved welding strength and accuracy.
Patent Information
- Application Number
- CN202311255246.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-09-26
- Publication Date
- 2026-11-20
- Estimated Expiration
- 2043-09-26
AI Technical Summary
The large difference in wall thickness between the plate and the main pipe during welding leads to low welding precision, easy deformation, and short service life.
A welding method with progressively increasing thickness is adopted. Through pretreatment, spot welding, seam welding, argon arc welding and laser welding, the transition pipe is connected to the plate and the main pipe to form a stable connection structure.
It improves the welding strength and precision between the plate and the main pipe, avoids weld burn-through, and extends service life.
Smart Images

Figure CN117245257B_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of heat exchanger technology, and more particularly to a plate-to-plate welding method. Background Technology
[0002] Plate heat exchangers are the most common type of heat exchanger. Two corrugated plates form a plate pair, through which liquid flows to complete heat exchange. To improve heat exchange efficiency, the plate pair is usually thin, while the main pipe through which the liquid flows is thicker because it needs to withstand a large flow rate. This leads to the following problems: 1. When welding the plate pair and the main pipe, the difference in wall thickness is large, and the thinner plate pair is prone to weld burn-through; 2. Welding is prone to deformation due to heat, and the thinner plate pair deforms more, resulting in poor welding precision between the plate pair and the main pipe; 3. During use, the plate pair and the main pipe are subjected to greater liquid impact, leading to a reduced service life. Summary of the Invention
[0003] The technical problem to be solved by this invention is to address the issues of difficult board-to-board welding, low welding precision, and short lifespan in existing technologies.
[0004] The technical solution adopted by this invention to solve its technical problem is: a plate-to-plate welding method, comprising: S1, pre-processing each corrugated plate; S2, setting two corrugated plates opposite each other and spot welding the four corners of the corrugated plates to fix the two corrugated plates together to form a plate pair; S3, seaming along the perimeter of the plate pair to form a receiving cavity inside the plate pair, and forming connection ports at the four corners of the plate pair, with the connection ports communicating with the receiving cavity; S4, welding a transition pipe at the connection port of the plate pair; S5, welding multiple plate pairs sequentially onto the main pipe, so that the transition pipe is welded to the opening on the main pipe and then connected together.
[0005] Furthermore, the wall thickness of the transition tube is greater than the wall thickness of the corrugated plate, and the wall thickness of the main tube is greater than the wall thickness of the transition tube.
[0006] Furthermore, the wall thickness at the connection port on the corrugated plate is 0.8 mm, the wall thickness of the transition tube is 2 mm, and the wall thickness of the main tube is 5 mm.
[0007] Furthermore, the pretreatment in S1 includes cleaning, degreasing, deburring, and drying.
[0008] Furthermore, resistance welding is used in S2 and S3. The welding current for spot welding in S2 is 9-10kA and the electrode pressure is 0.3MPa. The welding current for seam welding in S3 is 10-11kA and the electrode pressure is 0.3MPa.
[0009] Furthermore, in S4, before welding the transition pipe, the edge of the connection needs to be welded. The welding method used for the welding is argon arc welding, the welding current is 25-35A, and the diameter of the welding wire used is 1mm.
[0010] Furthermore, when welding the transition tube at the connection joint of the plate pair, the transition tube is butted with the connection joint, and the transition tube is welded and fixed to the edge of the connection joint using argon arc welding. The welding current is 130-150A and the welding wire diameter is 1.6mm.
[0011] Furthermore, after the transition tube is fixed to the connection port, laser welding is used to weld the gap between the transition tube and the connection port, with a welding power of 750-850W.
[0012] Furthermore, in S5, the connecting port, transition pipe and opening are elliptical. First, spot welding is performed on two points along the long axis between the transition pipe and the opening. The welding current is 110-140A and the diameter of the welding wire is 1.6mm. Then, the gap between the transition pipe and the opening is welded. The welding current is 80-110A and the diameter of the welding wire is 1.6mm.
[0013] Furthermore, multiple evenly spaced openings are pre-made on the main tube, and multiple plate pairs are welded to the main tube one by one from bottom to top, so that the receiving cavity inside each plate pair is connected to the inside of the main tube.
[0014] The beneficial effects of this invention are: The welding process of this invention is simple and reliable. After the plates are welded together, a transition pipe is welded at the joint between the plate and the main pipe for transition. This improves the welding strength between the plate and the main pipe and avoids the problem of the plates being welded through by using a thickness step welding method. At the same time, it effectively improves the welding accuracy between the plate and the main pipe and improves the welding effect. Attached Figure Description
[0015] The present invention will be further described below with reference to the accompanying drawings and embodiments.
[0016] Figure 1 This is a schematic flowchart of the plate-to-plate welding method in this invention.
[0017] Figure 2 This is a schematic diagram of the plate pair after step S3 of the present invention.
[0018] Figure 3 This is a schematic diagram of the welding position of the plate according to the present invention.
[0019] Figure 4 This is a schematic diagram of the welding position in step S4 of the present invention.
[0020] Figure 5This is a schematic diagram of the structure of the plate of the present invention after welding with the main tube.
[0021] Figure 6 This is a schematic diagram of the welding position in step S5 of the present invention. Detailed Implementation
[0022] The present invention will now be described in further detail with reference to the accompanying drawings. These drawings are simplified schematic diagrams, illustrating only the basic structure of the invention, and therefore only show the components relevant to the invention.
[0023] This invention discloses a plate-to-plate welding method.
[0024] Reference Figures 1 to 6 The plate-to-plate welding method includes: S1, pre-treating each corrugated plate 1; S2, setting two corrugated plates 1 opposite each other and spot welding the four corners of the corrugated plates 1 to fix the two corrugated plates 1 together to form a plate pair; S3, seaming along the perimeter of the plate pair to form a receiving cavity inside the plate pair, and forming connection ports 11 at the four corners of the plate pair, with the connection ports 11 communicating with the receiving cavity; S4, welding a transition pipe 3 at the connection port 11 of the plate pair; S5, welding multiple plate pairs sequentially onto the main pipe 2, so that the transition pipe 3 is welded to the opening 21 on the main pipe 2 and then connected together.
[0025] Furthermore, the wall thickness of the transition pipe 3 is greater than that of the corrugated plate 1, and the wall thickness of the main pipe 2 is greater than that of the transition pipe 3. Even further, the wall thickness at the connection port 11 on the corrugated plate 1 is 0.8 mm, the wall thickness of the transition pipe 3 is 2 mm, and the wall thickness of the main pipe 2 is 5 mm.
[0026] In this embodiment, the main pipe 2 is vertically arranged and needs to support multiple plate pairs. The plate pairs are parallel to each other, and the liquid flows between the plate pairs and the main pipe 2. The thickness of the corrugated plate 1 (0.8 mm) is much smaller than the wall thickness of the main pipe 2 (5 mm). During welding, the main pipe 2 may not reach the melting temperature, while the corrugated plate 1 may have already melted into a liquid state, which can easily cause the plate pairs to weld through. A 2 mm transition pipe 3 is set. One end of the transition pipe 3 is welded to the 0.8 mm corrugated plate 1, and the other end is welded to the 5 mm main pipe 2. This ensures that the plate pairs can be welded to the main pipe 2 and can improve the connection strength at the weld. It can withstand the impact of a large flow of liquid and has a longer service life.
[0027] The pretreatment in S1 includes cleaning, degreasing, deburring, and drying.
[0028] Resistance welding is used in S2 and S3. In S2, the welding current for spot welding is 9-10kA and the welding electrode pressure is 0.3MPa. In S3, the welding current for seam welding is 10-11kA and the electrode pressure is 0.3MPa.
[0029] In S2, use bolt cutters to clamp the plate. Figure 1 Spot weld corrugated plates 1 at positions A1, A2, A3, and A4, ensuring the gap around the upper and lower corrugated plates 1 is zero. The resistance welding electrode head needs to be cleaned regularly; after spot welding 20 corrugated plates 1, the electrode head should be cleaned with 120-grit sandpaper to ensure it is flat and shiny. Additionally, in S3, in... Figure 1 Seam welding is performed at the four gap positions B1, B2, B3, and B4 to ensure continuous and uninterrupted welding at each position. The upper and lower rollers of the resistance seam welding are cleaned regularly. After each 40 corrugated plates 1 are welded, the rollers should be cleaned with 240-mesh or 300-mesh sandpaper to ensure that the rollers are smooth and free of impurities.
[0030] In S4, before welding the transition pipe 3, the edge of the connection 11 needs to be additionally welded. The welding method used is argon arc welding, the welding current is 25-35A, and the diameter of the welding wire used is 1mm. Figure 3 As shown, the three positions to be welded are C1, C2, and C3. When welding, a 3mm gap is reserved at the end of the C1 and C2 positions near the connection port 11.
[0031] Based on this, when welding the transition tube 3 at the connection port 11 of the plate pair, the transition tube 3 is butted with the connection port 11, and the transition tube 3 is welded and fixed to the edge of the connection port 11 by argon arc welding. The welding current is 130-150A and the welding wire diameter is 1.6mm.
[0032] like Figure 4 As shown, the reserved 3mm gap allows the connector 11 to be deformed so that the transition tube 3 can be installed on the connector 11. At the same time, spot welding is performed at positions D1 and D2, and the reserved 3mm gap is welded to positions D1 and D2 simultaneously, thereby fixing the transition tube 3 to the edge of the connector 11.
[0033] Furthermore, after the transition tube 3 is fixed to the connector 11, laser welding is used to weld the gap between the transition tube 3 and the connector 11, with a welding power of 750-850W. Figure 4 It can be seen that laser welding is used to continuously weld the two semi-circular positions E1 and E2, so that the transition tube 3 is connected to the connection port 11.
[0034] In S5, the connecting port 11, transition pipe 3, and opening 21 are elliptical. First, spot welding is performed on two points along the major axis between transition pipe 3 and opening 21, with a welding current of 110-140A and a welding wire diameter of 1.6mm. Then, the gap between transition pipe 3 and opening 21 is welded, with a welding current of 80-110A and a welding wire diameter of 1.6mm. That is, after aligning transition pipe 3 with opening 21, spot welding is first performed on positions F1 and F2, and then continuous welding is performed on gaps G1 and G2 to connect transition pipe 3 and opening 21.
[0035] Furthermore, multiple evenly spaced openings 21 are pre-drilled on the main pipe 2, and multiple plate pairs are welded to the main pipe 2 one by one from bottom to top, so that the receiving cavity inside each plate pair is connected to the interior of the main pipe 2. By pre-drilling the openings 21, the distance between each plate pair is ensured to be uniform.
[0036] The welding process of this invention is simple and reliable. After the plates are welded together, a transition pipe 3 is welded at the connection 11 between the plate and the main pipe 2 for transition. On the one hand, this improves the welding strength between the plate and the main pipe 2. On the other hand, the use of a thickness-step welding method avoids the problem of the plates being welded through. At the same time, it effectively improves the welding accuracy between the plate and the main pipe 2 and improves the welding effect.
[0037] Based on the above-described preferred embodiments of the present invention, and through the foregoing description, those skilled in the art can make various changes and modifications without departing from the inventive concept. The technical scope of this invention is not limited to the contents of the specification, but must be determined according to the scope of the claims.
Claims
1. A plate butt welding method, characterized in that, include: S1. Preprocess each corrugated board; S2. Place the two corrugated plates opposite each other and spot weld the four corners of the corrugated plates together to fix the two corrugated plates together to form a plate pair. S3. Weld along the perimeter of the plate pair to form a receiving cavity inside the plate pair. Connecting ports are formed at the four corners of the plate pair and are connected to the receiving cavity. S4. Weld a transition tube at the joint of the plates. Before welding the transition tube, the edges of the joint need to be welded. The welding method used is argon arc welding. The welding current is 25-35A. The diameter of the welding wire is 1mm. A gap of 3mm is reserved in some positions when welding. S5. Weld multiple plates to the main pipe in sequence, so that the transition pipe is connected to the opening on the main pipe after welding. Wherein: the wall thickness at the connection port on the corrugated plate is 0.8mm, the wall thickness of the transition tube is 2mm, and the wall thickness of the main tube is 5mm.
2. The plate-to-plate welding method as described in claim 1, characterized in that: The pretreatment in S1 includes cleaning, degreasing, deburring, and drying.
3. The plate-to-plate welding method as described in claim 1, characterized in that: Resistance welding is used in S2 and S3. In S2, the welding current for spot welding is 9-10kA and the electrode pressure is 0.3MPa. In S3, the welding current for seam welding is 10-11kA and the electrode pressure is 0.3MPa.
4. The plate-to-plate welding method as described in claim 1, characterized in that: When welding the transition pipe at the connection joint of the plate pair, the transition pipe is butted with the connection joint, and the transition pipe is fixed to the edge of the connection joint by argon arc welding. The welding current is 130-150A and the welding wire diameter is 1.6mm.
5. The plate-to-plate welding method as described in claim 4, characterized in that: After the transition tube is fixed to the connection port, the gap between the transition tube and the connection port is welded by laser welding with a welding power of 750-850W.
6. The plate-to-plate welding method as described in claim 1, characterized in that: In S5, the connecting port, transition pipe and opening are elliptical. First, spot weld the two points in the long axis direction between the transition pipe and the opening. The welding current is 110-140A and the diameter of the welding wire is 1.6mm. Then weld the gap between the transition pipe and the opening. The welding current is 80-110A and the diameter of the welding wire is 1.6mm.
7. The plate-to-plate welding method as described in claim 6, characterized in that: Multiple evenly spaced openings are pre-made on the main pipe, and multiple plate pairs are welded to the main pipe one by one from bottom to top, so that the receiving cavity inside each plate pair is connected to the inside of the main pipe.
Citation Information
Patent Citations
Heat exchanger
CN112212716A
Heat exchanger
CN112212717A