Elliptical beam spot ion beam-based two-dimensional shaping method for x-ray mirrors
By combining elliptical beam spot ion beam with first-level coarse correction and second-level fine correction, the problem of high-efficiency and high-precision two-dimensional mirror surface shape correction in existing one-dimensional ion beam equipment is solved. By optimizing the number and spacing of correction lines using elliptical beam spot, high-efficiency and high-precision mirror surface shape correction is achieved.
Patent Information
- Application Number
- CN202311252425.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-09-26
- Publication Date
- 2026-11-24
- Estimated Expiration
- 2043-09-26
AI Technical Summary
In the existing technology, conventional one-dimensional ion beam equipment can only achieve unidirectional surface correction, making it difficult to maintain high precision and high efficiency in two-dimensional mirror surface correction with fewer etching lines, especially the surface correction accuracy in the meridional direction is insufficient.
By employing an elliptical beam ion beam combined with first-level coarse correction and second-level fine correction, and by designing a special mask, the traditional circular Gaussian beam spot is replaced with an elliptical beam spot with the sagittal direction greater than the meridional direction. The number and spacing of correction lines are optimized to achieve high-efficiency and high-precision two-dimensional surface correction.
High-precision mirror surface correction was achieved with fewer etching lines, improving correction speed and efficiency and meeting the processing accuracy requirements of X-ray mirrors.
Smart Images

Figure CN117293004B_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of optical processing, and in particular to a method for reshaping an X-ray mirror based on an elliptical beam spot ion beam. Background Technology
[0002] X-ray strip mirrors are crucial optical components of synchrotron radiation beamlines, playing a vital role in X-ray transmission and focusing. Operating under grazing incidence conditions, the X-ray beam on the mirror surface is elongated, ranging from tens to hundreds of millimeters in length but only a few millimeters in width; hence, X-ray mirrors are typically designed in an elongated shape. Advanced synchrotron radiation sources have a large coherence length. For surface shape errors with periods greater than the coherence length, height errors introduce phase shifts, affecting beam distortion and broadening; slope errors affect the direction of light propagation, causing beam distortion and broadening after long-distance propagation through the beamline. Advanced synchrotron radiation sources require mirror height errors to be within several nanometers to sub-nanometers, and slope errors to be within hundreds to tens of nanoarcs. Because the X-ray beam spot is elongated, the accuracy requirements in the meridional direction are generally significantly higher than those in the sagittal direction.
[0003] Currently, computer-controlled ion beam shaping is the mainstream process for fabricating X-ray long strip mirrors. Ion beam shaping utilizes the physical sputtering effect that occurs when an ion beam emitted from an ion source bombards an optical mirror surface to remove surface material from optical components. Numerous commercially available two-dimensional ion beam shaping systems are now available. For example, the PVT-IBF developed by Brookhaven National Laboratory in the United States has a cavity size of 1.0*0.6*0.6m and is equipped with a three-axis linkage motion system. Its path repeatability is RMS several μm within a 400mm movement range, enabling the fabrication of 80mm long samples with sub-nanometer surface accuracy. The Trim200 ion beam shaping system from Scia in Germany has dimensions of 2.8*1.4*2.2m and a four-axis linkage motion system with 50μm displacement accuracy, enabling the fabrication of 300mm diameter samples with several nanometer precision. The aforementioned small-scale two-dimensional correction equipment typically processes mirrors no larger than 300mm, and the equipment cost is relatively low. Larger devices, such as the IBF-2000 from NTG in Germany, measure 3.9*3.9*2.6m and have an XYZ three-axis linkage motion system, capable of processing samples with a maximum diameter of 2000mm and an accuracy of a few nanometers; the Finish1500 from Scia in Germany measures 3.6*7.7*3.4m and can process 1.5-meter mirrors with sub-nanometer accuracy, but it is very expensive, costing several times more than the aforementioned small ion beam devices.
[0004] In existing technologies, conventional one-dimensional ion beam equipment is relatively inexpensive, but it only has one-way correction capability, enabling surface correction in only one direction and is only suitable for very narrow mirror surfaces. Although two-dimensional surface correction of such mirrors can be achieved using a one-dimensional ion beam reshaping device in conjunction with a mask, several problems exist: existing methods use multiple circular holes to obtain several correction lines, and then process them multiple times by moving the positions of the correction lines. However, this method may introduce new positioning errors due to the increase in correction lines, and it also makes the process more complex and time-consuming. In addition, there are also problems when the number of correction lines is small. To cover the entire surface, the ion beam spot needs to be large enough, but an excessively large ion beam spot reduces the reshaping accuracy. Therefore, a processing method is needed that can maintain the highest possible reshaping accuracy, especially the surface correction accuracy in the meridional direction, while achieving high correction efficiency, even with a small number of etching lines. Summary of the Invention
[0005] The purpose of this invention is to overcome the defects of the prior art and provide a method for reshaping an X-ray mirror based on an elliptical beam spot ion beam.
[0006] The objective of this invention can be achieved through the following technical solutions:
[0007] This invention discloses a method for reshaping an X-ray mirror based on an elliptical spot ion beam, comprising the following steps:
[0008] Step 1: Obtain the amount of material to be removed from the surface of the component to be shaped;
[0009] Step 2: Use a large-diameter circular beam spot with first-level correction to perform first-level correction on the surface of the element to be corrected. After first-level correction, determine whether the target accuracy of first-level correction is met.
[0010] If the target accuracy of the first-level correction is not met, return to step 1;
[0011] If satisfied, proceed to the next step;
[0012] Step 3: Determine the number and spacing of the elliptical ion beam spot for secondary correction and the correction lines for secondary correction based on the one-dimensional ion beam shaping equipment and the element to be shaped;
[0013] Step 4: Design the spatial positions of the mask and the element to be shaped based on the equipment and the elliptical ion beam spot;
[0014] Step 5: Use an elliptical ion beam spot to perform secondary correction on the surface of the component to be corrected, and determine whether the processing accuracy is met after the secondary correction;
[0015] If the machining accuracy requirements are not met, repeat step 5 for iterative secondary correction machining;
[0016] If the machining accuracy requirements are met, the machining is complete.
[0017] Furthermore, the Gaussian parameter σ of the large-diameter circular beam spot mentioned in step 2... x =σ y , σ x The value range is 4–15 mm;
[0018] Step 2 includes: etching the element to be shaped along each correction line of the first-level correction using a large-diameter circular beam spot, wherein the number of correction lines ranges from m. L The range is 5 to 9.
[0019] Furthermore, the target accuracy for the first-level correction in step 2 is a two-dimensional surface height error RMS(h) ≤ 5nm.
[0020] Furthermore, the elliptical ion beam spot mentioned in step 3 is generated by a mask and an ion beam system, and the beam spot satisfies an ideal elliptical Gaussian removal function:
[0021]
[0022] Among them, V p σ represents the peak removal rate. x With σ y These are the Gaussian distribution parameters of the meridional and sagittal directions of the elliptic Gaussian removal function, respectively, σ y >σ x .
[0023] Furthermore, the cutoff frequency f for surface shape error correction in the meridional direction of the element to be modified is... cx With σ x The relationship satisfies:
[0024]
[0025] Cutoff frequency f for surface shape error correction in the sagittal direction of the element to be modified cy With σ x The relationship satisfies:
[0026]
[0027] Further, the determination of the elliptical ion beam spot for secondary correction in step 3 includes: etching elliptical vias in a mask, using a linear particle transport model, and simulating the simulated beam spot f generated by the ion beam passing through the elliptical vias on the surface of the element to be corrected on a computer. simu By adjusting the shape of the elliptical through-hole and the distance between the mask and the surface of the component to be shaped, the simulated beam spot f is made. simu By approximating the ideal elliptical Gaussian removal function f, an elliptical ion beam spot is obtained.
[0028] Furthermore, the number m of the correction lines mentioned in step 3 L The number m of correction lines is determined based on the device and the surface of the component to be corrected. L The range is 7 to 20;
[0029] The spacing ΔL of the correction lines mentioned in step 3 y The maximum is the half-width of the elliptic Gaussian removal function's arc vector. Half of it, which satisfies the following formula:
[0030]
[0031] Each correction line affects the surface shape of the element to be modified within a radius of 3σ on both sides. y The distance, and the correction line spacing, satisfy the following formula:
[0032]
[0033] Post-style and By combining the equations, we can obtain the direction σ of the arc sagitta. y satisfy:
[0034] σ y ≥b0 / (1.177m L -4.823).
[0035] Further, step 5 includes: calculating the residence time of the elliptical ion beam on the correction line using the elliptical ion beam and the amount to be removed; determining the movement speed of the element to be shaped based on the time; the device drives the element to be shaped to move along the meridional direction of the element to be shaped; changing the mask plate to change the position of the elliptical ion beam spot in the sagittal direction; and etching the element to be shaped along each correction line in sequence by the elliptical ion beam spot to complete the secondary correction.
[0036] Furthermore, the one-dimensional ion beam shaping device uses a wide-beam ion source with a width ranging from 50 to 400 mm, and the size of the ion beam emitted by the ion source can cover the position of the correction line.
[0037] Furthermore, the elements to be shaped in the above method are all elongated reflectors, and the meridional length a0 of the reflector ranges from 300 to 1000 mm, and the sagittal width b0 ranges from 10 to 90 mm.
[0038] Compared with the prior art, the present invention has the following beneficial effects:
[0039] (1) This invention uses a one-dimensional ion beam device and a specially designed mask to replace the traditional circular Gaussian beam spot with an elliptical beam spot with a sagittal direction greater than the meridional direction. By optimizing and matching the major axis-minor axis dimensions of the elliptical beam spot with the surface shape error characteristics of the mirror in the sagittal-meridional direction, and selecting an appropriate elliptical beam spot size and the number of correction lines, high-efficiency and high-precision mirror surface shape correction can be achieved with fewer lines.
[0040] (2) The present invention first uses a larger circular ion beam spot for rough correction (first-level processing), and then uses second-level etching for fine correction (second-level processing). This has a faster correction speed, reduces the number of etched lines, and meets the processing accuracy requirements, thus improving the efficiency of two-dimensional surface correction using one-dimensional ion beam shaping equipment. Attached Figure Description
[0041] Figure 1 This is a schematic diagram of the method flow of the present invention;
[0042] Figure 2 This is a schematic diagram of the secondary correction process of the present invention;
[0043] Figure 3 This is a schematic diagram of the etching apparatus in an embodiment of the present invention;
[0044] Figure 4 This is a schematic diagram of the ellipse removal function, grid, and correction line in an embodiment of the present invention;
[0045] Figure 5 The σ=10mm circular spot used for primary machining (left) and the σ=10mm circular spot used for secondary machining. x =1mm,σ y =5mm elliptical spot (right) schematic diagram;
[0046] Figure 6 The initial surface shape of the target area is modified;
[0047] Figure 7 The target correction area has undergone primary processing with a circular spot pattern of σ=10mm. The surface shape of the area to be further corrected is shown in the image.
[0048] Figure 8 The simulation of the target correction area using a circular spot with σ=5mm and 13 etching lines spaced 5mm apart is shown in the secondary processing effect diagram.
[0049] Figure 9 The simulation of the secondary processing effect using a circular spot with σ=1mm and 13 etching lines spaced 5mm apart in the target correction area is shown in the figure.
[0050] Figure 10 The simulation of the target correction area using a circular spot with σ=1mm and 47 etching lines spaced 1mm apart is shown in the secondary processing effect diagram.
[0051] Figure 11 σ is used to simulate the target correction region. x =1mm,σ y =5mm elliptical cluster spot, 13 etching lines spaced 5mm apart, secondary processing effect diagram.
[0052] Figure label:
[0053] Figure 3 1. Ion source; 2. Mask plate; 3. Long strip mirror, i.e., the substrate to be etched; 4. Mask aperture; 5. Ion beam. Detailed Implementation
[0054] The present invention will now be described in detail with reference to the accompanying drawings and specific embodiments. These embodiments are based on the technical solution of the present invention and provide detailed implementation methods and specific operating procedures. However, the scope of protection of the present invention is not limited to the following embodiments.
[0055] Example
[0056] like Figure 1 As shown, this embodiment provides a method for reshaping an X-ray mirror based on an elliptical beam spot ion beam. The method specifically includes the following steps:
[0057] Step 1: As Figure 3 As shown, the element to be corrected in this embodiment is a long strip-shaped reflector surface to be corrected, with a meridional length a0 = 380 mm and a sagittal width b0 = 40 mm.
[0058] Obtain the amount to be removed from the surface of the component to be corrected, such as... Figure 6 As shown, Figure 6 The initial surface shape of the target correction region has an average meridional slope error of 970 nrad and an average sagittal slope error of 1429 nrad.
[0059] Step 2: Perform primary processing using a large-diameter circular beam spot ion beam for primary correction. For example... Figure 5 As shown on the left, with a circular spot of σ = 10mm, a circular Gaussian removal function with a Gaussian parameter σ = 10mm is selected based on the mirror width. The number of correction lines for the first-level correction is m. L =7, Correction line spacing ΔL y =12mm. For example... Figure 7 As shown, after primary processing with 7-line σ=10mm circular beams, the average meridional slope error of the entire plane is 483nrad, the average sagittal slope error is 711nrad, and the target accuracy of primary correction is RMS(h)≤5nm.
[0060] Step 3: Determine the number and spacing of the elliptical ion beam spot and correction lines for secondary correction based on the one-dimensional ion beam shaping equipment and the elongated mirror. Specifically, the elliptical ion beam spot is generated using a mask and the ion beam system. A linear particle transport model is used to simulate the beam spot generated by the ion beam passing through an elliptical aperture on the optical surface to be etched on a computer. By adjusting the shape of the elliptical aperture and the spacing between the mask and the mirror surface, the simulated beam spot f is optimized. simu The Gaussian removal function f should be as close as possible to the ideal elliptic.
[0061] like Figure 4 and 5 As shown, the elliptical ion beam spot satisfies an ideal elliptical Gaussian removal function, which is:
[0062]
[0063] Specifically, V p σ represents the peak removal rate. x With σ y These are the Gaussian distribution parameters of the ellipse removal function in the meridional and sagittal directions, respectively, and the Gaussian parameters in the meridional and sagittal directions are different.
[0064] In this embodiment, the number m of the second-order correction lines is... L =13.
[0065] Based on the specified conditions:
[0066]
[0067] In this embodiment, the spacing ΔL of the correction line is taken. y =5mm, Gaussian parameter σ in the sagittal direction y =5mm, based on the cutoff frequency and machining accuracy requirements, adjust the Gaussian parameter σ according to the simulated etching. x In this embodiment, σ is taken. x =1mm.
[0068] Step 4: Figure 3 This is a schematic diagram of the etching apparatus in an embodiment of the present invention. The shape of the aperture in the mask and the spatial position of the mask and mirror are designed based on a one-dimensional ion beam shaping device and an elliptical ion beam spot. Using a linear transmission model, the Monte Carlo method is used to simulate the shape of the ion beam spot on the surface to be etched on the mirror after the elliptical aperture is created in the mask, passing through the mask. The major and minor axis lengths of the elliptical aperture mask and the distance between the mask and the mirror are modified to maximize its two-dimensional correlation with the Gaussian shape, and the fitted Gaussian parameters are made as close as possible to the ideal elliptical Gaussian removal function. Masks with different positions in the sagittal direction are manufactured to correspond to different etching lines. To generate σ... x =1mm, σy =5mm beam spot, using an elliptical aperture size of φ x =1.6mm, φ y =14mm, the distance between the mask and the reflector is 15mm.
[0069] Step 5: As Figure 2 As shown, a two-stage processing is performed. The dwell time on the correction line is calculated based on the elliptical ion beam spot and the amount to be removed. During the shaping process, the one-dimensional ion beam shaping device moves the reflector along the meridional (length) direction, and the mask is changed to alter the position of the ion beam spot in the sagittal direction, allowing the ion beam spot to etch the reflector sequentially along each correction line. If the result does not meet the processing accuracy requirements, iterative processing can be performed.
[0070] In this embodiment, a circular spot with σ = 5mm was first used for correction, and 13 correction lines spaced 5mm apart were used as a control group. The results are as follows. Figure 8 As shown, the average meridional slope error of the entire plane is 260 nrad, the average sagittal slope error is 292 nrad, and the time is 0.94 h. The height error and meridional slope error of the residual surface shape are not ideal.
[0071] In addition, a control group was set up, using a circular spot correction with σ = 1 mm and 13 correction lines spaced 5 mm apart. This did not satisfy the sampling theorem, and the results were as follows. Figure 9 As shown, due to the excessively large spacing, the etching causes a wavy pattern in the sagittal direction of the surface, which actually worsens the surface shape, resulting in a large number of groove errors in the sagittal direction that cannot be removed. Therefore, when using a removal function with σ = 1 mm, 47 correction lines are required to satisfy the sampling theorem, such as... Figure 10 As shown, the correction accuracy is very high at this time, with an average meridional slope error of 29 nrad and an average sagittal slope error of 29 nrad for the entire plane. However, the processing time is very long, at 9.6 hours, and too many correction lines are difficult to implement on a one-dimensional motion device, which will also increase the positioning error, making the processing far from achieving the simulation accuracy.
[0072] This embodiment uses σ x =1mm,σ y For an ellipse removal function of σ=5mm, the same 13 correction lines, spaced 5mm apart, can be used as for a circular spot with σ=5mm. For example... Figure 11 As shown, the average meridional slope error in the simulation results is 172 nrad, the average sagittal slope error is 282 nrad, and the simulation time is only 2.8 hours. In this embodiment, the slope error is calculated by taking the standard deviation of the average rate of change of surface height over a 2mm distance along a line.
[0073] Compared to the correction result of the circular spot with σ=5mm, the residual meridional slope error was reduced from 260nrad to 172nrad, a reduction of 34%. Compared to the circular spot with σ=1mm, although the error accuracy is higher, the etching efficiency is higher, and the number of etching lines required is reduced from 47 to 13, showing an overall comprehensive advantage.
[0074] Additionally, if σ is used x =1mm,σ y If an elliptical beam spot of 5 mm is used to directly etch and correct the initial surface shape, the etching time will exceed 11 hours. Therefore, a two-stage etching process is used. Before fine finishing (secondary processing), a larger ion beam spot is used for rough finishing (first-stage processing) to reduce the etching time.
[0075] The preferred embodiments of the present invention have been described in detail above. It should be understood that those skilled in the art can make numerous modifications and variations based on the concept of the present invention without creative effort. Therefore, all technical solutions that can be obtained by those skilled in the art based on the concept of the present invention through logical analysis, reasoning, or limited experimentation on the basis of existing technology should be within the scope of protection defined by the claims.
Claims
1. A method for reshaping an X-ray mirror based on an elliptical spot ion beam, characterized in that: Includes the following steps: Step 1: Obtain the amount of material to be removed from the surface of the component to be shaped; Step 2: Use a large-diameter circular beam spot with first-level correction to perform first-level correction on the surface of the element to be corrected. After first-level correction, determine whether the target accuracy of first-level correction is met. If the target accuracy of the first-level correction is not met, return to step 1; If satisfied, proceed to the next step; Step 3: Determine the number and spacing of the elliptical ion beam spot for secondary correction and the correction lines for secondary correction based on the one-dimensional ion beam shaping equipment and the element to be shaped; Step 4: Design the spatial positions of the mask and the element to be shaped based on the equipment and the elliptical ion beam spot; Step 5: Use an elliptical ion beam spot to perform secondary correction on the surface of the component to be corrected, and determine whether the processing accuracy is met after the secondary correction; If the machining accuracy requirements are not met, repeat step 5 for iterative secondary correction machining; If the machining accuracy requirements are met, the machining is complete.
2. The method for reshaping an X-ray mirror based on an elliptical beam spot ion beam according to claim 1, characterized in that, The Gaussian parameter σ of the large-diameter circular beam spot mentioned in step 2 x =σ y , σ x The value range is 4–15 mm; Step 2 includes: etching the element to be shaped along each correction line of the first-level correction using a large-diameter circular beam spot, wherein the number of correction lines ranges from m. L The range is 5 to 9.
3. The method for reshaping an X-ray mirror based on an elliptical beam spot ion beam according to claim 1, characterized in that, In step 2, the target accuracy for the first-level correction is a two-dimensional surface height error RMS(h) ≤ 5nm.
4. The method for reshaping an X-ray mirror based on an elliptical beam spot ion beam according to claim 1, characterized in that, The elliptical ion beam spot described in step 3 is generated by a mask and an ion beam system, and the beam spot satisfies the ideal elliptical Gaussian removal function: Among them, V p σ represents the peak removal rate. x With σ y These are the Gaussian distribution parameters of the meridional and sagittal directions of the elliptic Gaussian removal function, respectively, σ y >σ x .
5. The method for reshaping an X-ray mirror based on an elliptical beam spot ion beam according to claim 4, characterized in that, The cutoff frequency f for surface shape error correction in the meridional direction of the component to be shaped cx With σ x The relationship satisfies: Cutoff frequency f for surface shape error correction in the sagittal direction of the element to be modified cy With σ x The relationship satisfies:
6. The method for reshaping an X-ray mirror based on an elliptical beam spot ion beam according to claim 4, characterized in that, Step 3, determining the elliptical ion beam spot for secondary correction, includes: etching elliptical vias in a mask, using a linear particle transport model, and simulating the simulated beam spot f generated by the ion beam passing through the elliptical vias on the surface of the element to be corrected on a computer. simu By adjusting the shape of the elliptical through-hole and the distance between the mask and the surface of the component to be shaped, the simulated beam spot f is made. simu By approximating the ideal elliptical Gaussian removal function f, an elliptical ion beam spot is obtained.
7. The method for reshaping an X-ray mirror based on an elliptical beam spot ion beam according to claim 4, characterized in that, The number m of correction lines mentioned in step 3 L The number m of correction lines is determined based on the device and the surface of the component to be corrected. L The range is 7 to 20; The spacing ΔL of the correction lines mentioned in step 3 y The maximum is the half-width of the elliptic Gaussian removal function's arc vector. Half of it, which satisfies the following formula: Each correction line affects the surface shape of the element to be modified within a radius of 3σ on both sides. y The distance, and the correction line spacing, satisfy the following formula: Post-style and By combining the equations, we can obtain the direction σ of the arc sagitta. y satisfy: s y ≥b0 / (1.177m L -4.823).
8. The method for reshaping an X-ray mirror based on an elliptical beam spot ion beam according to claim 4, characterized in that, Step 5 includes: calculating the residence time of the elliptical ion beam on the correction line using the elliptical ion beam and the amount to be removed; determining the movement speed of the element to be shaped based on the time; the device drives the element to be shaped to move along the meridional direction of the element to be shaped; changing the mask plate to change the position of the elliptical ion beam spot in the sagittal direction; and etching the element to be shaped along each correction line in sequence to complete the secondary correction.
9. The method for reshaping an X-ray mirror based on an elliptical beam spot ion beam according to claim 1, characterized in that: The one-dimensional ion beam shaping device uses a wide-beam ion source with a width ranging from 50 to 400 mm, and the size of the ion beam emitted by the ion source can cover the position of the correction line.
10. A method for reshaping an X-ray mirror based on an elliptical beam spot ion beam according to any one of claims 1 to 9, characterized in that, The element to be shaped is a long strip-shaped reflector, the meridional length a0 of which ranges from 300 to 1000 mm, and the sagittal width b0 of which ranges from 10 to 90 mm.
Citation Information
Patent Citations
Two-dimensional surface shape correction method of reflector for synchrotron radiation isobeam line station
CN116305639A
Specimen observation method and device, and inspection method and device using the method and device
WO2009125603A1