Large-scale dissimilar metal structure gap self-adaptive adjustment welding method

By using L-shaped lug plates and submerged arc welding technology in the welding of dissimilar metal large gears, the problem of gap changes caused by thermal expansion and contraction of the wheel rim was solved, achieving flexible connection and dimensional accuracy assurance of large bimetallic structural parts, and improving production efficiency and weld quality.

CN117300312BActive Publication Date: 2026-11-20CITIC HEAVY INDUSTRIES CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202311513223.3
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-11-14
Publication Date
2026-11-20
Estimated Expiration
2043-11-14

AI Technical Summary

Technical Problem

In the welding process of dissimilar metal large gears, the gap change caused by thermal expansion and contraction of the gear rim leads to welding cracks and failure to meet positioning requirements, making it difficult to guarantee dimensional accuracy.

Method used

L-shaped lugs are used to fix the spokes to the rim. The gap is adaptively adjusted by the free movement of the lugs during heating. Combined with submerged arc welding technology, the center consistency between the spokes and the rim is ensured, and weld cracking is avoided.

Benefits of technology

It enables flexible connection of large bimetallic structural components under different temperature gradients, ensuring weld quality and dimensional accuracy, improving production efficiency, and avoiding problems such as welding cracks and inaccurate positioning.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117300312B_ABST
    Figure CN117300312B_ABST
Patent Text Reader

Abstract

The application discloses a large-scale heterogeneous metal structure gap self-adaptive adjustment welding method. Due to different thermal expansion coefficients of metals, with the change of temperature, the metals expand and contract, leading to the change of the gap between the two. The L-shaped ear hanging plate is used in the welding of the large-scale double-metal structure, and the self-adaptive adjustment of the assembly gap between the heterogeneous metals is realized through the L-shaped ear hanging plate. The self-adaptive adjustment of the gap of the spoke in the horizontal direction under different temperature gradients is realized, the cracking of the spot welding seam between the rim and the spoke caused by the thermal expansion of the rim is avoided, the positioning precision of the spoke is ensured, the appearance of the inner surface defects of the rim caused by the cracking of the spot welding seam is prevented, the product quality of the large-scale forged and welded gear structure is ensured through reasonable groove forms and welding specifications, the effective guarantee of the size precision of the large-scale gear is realized, and meanwhile, the operation is simple, and the production efficiency is doubled.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of welding technology, specifically to a welding method for adaptive adjustment of gaps in large dissimilar metal structural components. Background Technology

[0002] Welding technology can produce gears with larger diameters and higher transmission ratios. Compared with cast gears, forged and welded gears not only save on materials and production costs, but are also more environmentally friendly and energy-efficient, which is in line with future development trends.

[0003] The forged and welded large gear comprises multiple layers from the outside in, including the rim and spokes. The rim is a forging, while the spokes are steel plates. The rim and spokes are connected by welding, a type of dissimilar bimetallic welding. The rim material is generally medium-carbon quenched and tempered steel. The base material has a high carbon content and alloying elements, resulting in poor weldability and a tendency to weld cracks. Therefore, thorough preheating is essential before welding, typically reaching temperatures as high as 250℃. Due to the large coefficient of thermal expansion of the rim, high-temperature preheating before welding causes thermal expansion and contraction. If the rim and spokes are spot-welded together beforehand, the rim will expand due to heat, increasing the gap between them. This leads to cracking of the spot weld on the rim side, making welding cracks highly likely. Furthermore, the spokes will move up and down inside the rim, compromising the flatness and dimensional accuracy of the spokes.

[0004] Therefore, it is necessary to design an effective method to avoid the gap change caused by the thermal expansion and contraction of the gear rim, so as to enable the gap of the dissimilar metal large gear structure to be freely adjusted, ensure its dimensional accuracy, and meet the product requirements. Summary of the Invention

[0005] To address the shortcomings of existing technologies, this invention provides a welding method for adaptively adjusting the gap of large dissimilar metal structural components. This welding method enables a flexible and effective connection of the gap between the rim and spokes of a large gear under different temperature gradients.

[0006] To achieve the above objectives, the specific solution adopted by the present invention is as follows: A welding method for adaptively adjusting the gap of large dissimilar metal structural components, wherein the welding method is used to weld wheel rims and spokes into a single component, mainly including the following steps: S1. Make several L-shaped ear-hanging plates, each L-shaped ear-hanging plate including a horizontal part and a vertical part; S2. Make a bevel on the circumferential sidewall of the spoke; S3. The vertical parts of several L-shaped ear plates are evenly welded onto the spoke plate to obtain the first joint; wherein the inner corner of each L-shaped ear plate is away from the center of the spoke plate. S4. Assemble the first connecting piece with the wheel rim. The horizontal part of the L-shaped lug plate overlaps the upper end surface of the wheel rim to effectively fix the spokes in the corresponding position inside the wheel rim, forming the intermediate piece. S5. Hoist the intermediate part onto the flat turntable and adjust it so that the center of the wheel rim, the spokes and the flat turntable are aligned. Use a heater to fully heat the outer circle of the wheel rim. During heating, the gap between the wheel rim and the spokes changes. As the gap changes, the L-shaped lug plate can move freely relative to the wheel rim. After heating, inspect and fine-tune the intermediate part to keep the center of the wheel rim and the spokes aligned. S6. Perform multi-layer, multi-pass welding on the wheel rim and spokes. Once the welding is complete, the integral part is obtained, and the L-shaped lug plate is removed.

[0007] Furthermore, in step S2, the bevel on the spoke is a K-type bevel with an angle of 40-60°.

[0008] Furthermore, in step S5, the heating temperature is not lower than 250°C.

[0009] Furthermore, the rim material is 34CrNi1Mo, and the spoke material is Q355B.

[0010] Furthermore, in step S6, the welding process specifically includes: S61. Perform base welding on both sides. After welding, remove the L-shaped ear plate. For the root pass welding on both sides, use 4mm H10Mn2 welding wire, with a current of 450-500A, a voltage of 27-30V, and a welding speed of 250-400mm / min. S62, Perform front and back filler welding. In the front and back filler welding, 4mm H10Mn2 welding wire is used, the current is 500-650A, the voltage is 28-34V, and the welding speed is 300-420mm / min; S63. Perform front and back cover welding. For welding the front and back cover surfaces, use 4mm H10Mn2 welding wire, with a current of 500-650A, a voltage of 28-34V, and a welding speed of 300-420mm / min.

[0011] Furthermore, submerged arc welding is used for root pass welding, filler welding, or cover welding on both sides.

[0012] Furthermore, in step S6, the flatness of the spokes is monitored in real time during the welding process.

[0013] Furthermore, in step S6, during the welding process, when the deformation of the spokes is detected to exceed 3mm, the following operation should be performed: first, flip the intermediate part over, and then weld the opposite sides.

[0014] Furthermore, the maximum gap between the rim and the spokes shall not exceed 12 mm.

[0015] Beneficial effects:

[0016] This invention uses several L-shaped lug plates, one end of which is rigidly fixed (welded) to the spoke plate, and the other end is evenly arranged and freely overlapped on the upper surface of the rim. As the rim 1 is heated to the target temperature, the diameter of the rim changes continuously with the temperature gradient due to thermal expansion and contraction. This results in a gap change between the rim and the spoke plate, allowing the L-shaped lug plates to move freely. This enables the spoke plate to adaptively adjust in the horizontal (diameter direction) direction as the gap changes, maintaining the relative position of the spoke plate and the rim in the height direction (perpendicular to the diameter direction) and completing the welding of the rim and the spoke plate. This invention applies the method of effective connection using L-shaped lug plates to the manufacturing of large bimetallic structural components such as large gears with non-uniform expansion coefficients. It achieves adaptive adjustment of the gap between the spokes in the horizontal (diameter direction) direction under different temperature gradients. At the same time, it avoids the impact of cracking of the spot weld between the rim and the spokes due to thermal expansion of the rim, which affects the dimensional positioning accuracy of the spokes, and the occurrence of defects on the inner surface of the rim due to cracking of the spot weld. This improves the weld quality and effectively ensures the dimensional accuracy of large bimetallic structural components. In addition, it is easy to operate and doubles the production efficiency. Attached Figure Description

[0017] Figure 1 This is a structural diagram of the middleware.

[0018] Figure 2 for Figure 1 A sectional view.

[0019] The diagram shows the following markings: 1. Wheel rim, 2. Spoke, 3. L-shaped lug plate, 4. K-shaped bevel. Detailed Implementation

[0020] The technical solution of the present invention will be clearly and completely described below with reference to specific embodiments. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the protection scope of the present invention.

[0021] A welding method for adaptive adjustment of gaps in large dissimilar metal structural components, wherein the welding method is used to weld a wheel rim 1 and a spoke 2 into an integral component, mainly including the following steps: S1. Make several L-shaped ear hangers 3. The size of the L-shaped ear hanger 3 is determined according to the size between the wheel rim and the spoke. The L-shaped ear hanger 3 includes a horizontal part and a vertical part. In the L-shaped ear hanger 3, the length of the lower end face of the horizontal part from the bottom end of the vertical part should be consistent with the target distance between the upper surface of the spoke 2 and the upper end face of the wheel rim 1. S2. Make a K-shaped bevel 4 on the circumferential sidewall of the spoke plate 2. The bevel angle is 30-60°. The bevel angles on both sides can be equal or unequal, depending on the actual situation. It should be noted that the use of the K-shaped bevel can ensure that the root of the weld is fully penetrated after the back side of the weld is cleaned, so that the welding heat source can penetrate into the root of the joint to ensure the quality of the joint weld. S3. Evenly weld the vertical parts of several L-shaped ear plates 3 onto the spoke plate 2 to obtain the first joint. Please refer to [reference needed]. Figure 1 and Figure 2 Among them, the inner corner of each L-shaped ear plate 3 is away from the center of the spoke plate 2; S4. Assemble the first connecting piece with the wheel rim 1, wherein the horizontal part of the L-shaped lug plate 3 overlaps the upper end surface of the wheel rim 1 to support the spoke plate 2 in the corresponding position inside the wheel rim 1, forming an intermediate piece; S5. Hoist the intermediate part onto the flat turntable and adjust it so that the center of the wheel flange 1, the spoke 2, and the flat turntable are aligned. Use a heater to fully heat the wheel flange 1 to a temperature not lower than 250℃. During heating, the gap between the wheel flange 1 and the spoke 2 changes. As the gap changes, the L-shaped lug plate 3 can move freely relative to the wheel flange 1. After heating, inspect and fine-tune the intermediate part to ensure that the center of the wheel flange 1 and the spoke 2 are aligned. The medium carbon quenched and tempered steel 34CrNi1Mo has a carbon equivalent as high as 0.89% and poor weldability. By taking preheating before welding and heat preservation and slow cooling after welding, the hardness and brittleness of the heat-affected zone of the weld can be reduced, while accelerating the outward diffusion of hydrogen in the weld, thereby avoiding hydrogen-induced cracking in the weld. S6. Weld the rim 1 and the spoke 2. The specific welding process is as follows: S61. Use submerged arc welding for the front and back root passes. After welding, remove the L-shaped ear plate 3. For the root pass welding on both sides, use 4mm H10Mn2 welding wire, with a current of 450-500A, a voltage of 27-30V, and a welding speed of 250-400mm / min. S62. Submerged arc welding is used for filler welding on both sides; In the front and back filler welding, 4mm H10Mn2 welding wire is used, the current is 500-650A, the voltage is 28-34V, and the welding speed is 300-420mm / min; S63. Submerged arc welding is used for front and back cover welding; For welding the front and back covers, use Φ4mm H10Mn2 welding wire, current of 500-650A, voltage of 28-34V, and welding speed of 300-420mm / min.

[0022] Table 1. Submerged arc welding process parameters in step S6

[0023] It should be noted that during the welding process, the flatness of the spoke 2 needs to be monitored in real time. When the deformation of the spoke 2 exceeds 3mm, the following operations should be performed: first, flip the intermediate part over, and then weld the opposite sides. For example, when performing front fill welding, if the deformation of the spoke 2 exceeds 3mm, it should be flipped over immediately for reverse fill welding. When the deformation of the reverse fill welding exceeds 3mm, it should be flipped over again for front welding. If no deformation exceeds the limit during the reverse welding process, the reverse welding should be completed halfway, and then the spokes should be flipped over again for front welding, leaving a deformation allowance for the front welding.

[0024] In this invention, one end of several L-shaped lug plates 3 is rigidly fixed, i.e., welded to the spoke plate 2, while the other end is evenly arranged and freely overlapped on the upper surface of the rim 1. As the rim 1 is heated to the target temperature, the diameter of the rim 1 changes continuously with the temperature gradient due to thermal expansion and contraction. This results in a change in the gap between the rim 1 and the spoke plate 2, allowing the L-shaped lug plates 3 to move freely. This enables the spoke plate 2 to adaptively adjust in the horizontal (diameter direction) direction as the gap changes, maintaining the relative position of the spoke plate 2 and the rim 1 in the height direction (perpendicular to the diameter direction) and completing the welding of the rim 1 and the spoke plate 2.

[0025] The technical solution of this application will be described in detail below with reference to specific embodiments.

[0026] Example 1

[0027] In the forged and welded large gear, a component of a large dissimilar metal structure, the rim 1 is made of 34CrNi1Mo, and the spokes 2 are made of Q355B. Before welding, the inner diameter of rim 1 is Φ6908mm, the outer diameter is Φ7210mm, the wall thickness is approximately 151mm, and the height is 706mm. The spokes 2 have a thickness of 85mm, an inner diameter of Φ4930mm, and an outer diameter of Φ6906mm. The welding method is described below: S1. Design and manufacture several L-shaped ear-hanging plates 3; S2. A K-shaped bevel 4 is made on the circumferential sidewall of the spoke 2, with the upper bevel angle being 40° and the lower bevel angle being 50°. S3. The vertical parts of several L-shaped ear plates 3 are evenly welded onto the spoke plate 2, and one piece is arranged every 1.5 meters to obtain the first joint; wherein, the inner corner of each L-shaped ear plate 3 is away from the center of the spoke plate. S4. Assemble the first connecting piece with the wheel rim 1. The horizontal part of the L-shaped lug plate 1 overlaps the upper surface of the wheel rim 1 to support the spoke plate 2 inside the wheel rim 1, forming an intermediate piece. S5. Hoist the intermediate component onto the flat turntable and adjust it so that the centers of the rim 1, spokes 2, and the turntable are aligned. Use a ring heater to fully heat the outer circumference of the rim until the preheating temperature reaches 250℃. During the entire heating process, the gap between the rim 1 and spokes 2 continuously increases, allowing the spokes 2 and rim 1 to move freely with the gap adapting to its own movement. The gap increases from the initial 0mm to a maximum of approximately 12mm. After ensuring the gap between the rim 1 and spokes 2 is uniform and the positions of spokes 2 and rim 1 are checked to ensure they meet the requirements, proceed with electric welding after passing the inspection. S6. First, submerged arc welding is used for the root pass. After the root pass is completed, the L-shaped lug plate 3 is removed. Then, submerged arc welding is used for the fill and cover passes. Submerged arc welding is performed using a manipulator, and multi-layer, multi-pass welding is employed. Welding parameters are shown in Table 2. During the welding process, the flatness of the spoke 2 is monitored in real time. When the deformation exceeds 3mm, the intermediate part is flipped over, and its opposite side is welded until the welding is completed, thus obtaining the integral part.

[0028] Table 2. Submerged arc welding process parameters in step S6

[0029] By using the above-mentioned adaptive adjustment welding method for the gap of large dissimilar metal structural components, the L-shaped lug plate 3 is freely moved on the upper end face of the rim 1 for flexible adjustment, ensuring that the height position between the spoke plate 2 and the rim 1 remains unchanged, avoiding spot weld cracks, and solving the manufacturing technical problem of large bimetallic structural components with high thermal expansion and contraction. The problem of weld cracking is solved by reasonable bevel form and welding specifications, realizing the precise positioning and efficient welding of the rim 1 and spoke plate 2 of the large gear. Finally, the weld passed the flaw detection on the first attempt, the flatness of the spoke plate 2 was controlled within 3mm, and all performance met the design requirements.

[0030] The above description is merely a preferred embodiment of the present invention and is not intended to limit the scope of the invention in any way. All equivalent transformations or modifications made in accordance with the essence of the present invention should be covered within the protection scope of the present invention.

Claims

1. A welding method for adaptive adjustment of gaps in large dissimilar metal structural components, wherein the welding method is used to weld wheel rims and spokes into a single integral component, characterized in that, The main steps include the following: S1. Make several L-shaped ear-hanging plates, each L-shaped ear-hanging plate including a horizontal part and a vertical part; S2. Make a bevel on the circumferential sidewall of the spoke; S3. The vertical parts of several L-shaped ear plates are evenly welded onto the spoke plate to obtain the first joint; wherein the inner corner of each L-shaped ear plate is away from the center of the spoke plate. S4. Assemble the first connecting piece with the wheel rim. The horizontal part of the L-shaped lug plate overlaps the upper end surface of the wheel rim to effectively fix the spokes in the corresponding position inside the wheel rim, forming the intermediate piece. S5. Hoist the intermediate part onto the flat turntable and adjust it so that the center of the wheel rim, the spokes and the flat turntable are aligned. Use a heater to fully heat the outer circle of the wheel rim. During heating, the gap between the wheel rim and the spokes changes. As the gap changes, the L-shaped lug plate can move freely relative to the wheel rim. After heating, inspect and fine-tune the intermediate part to keep the center of the wheel rim and the spokes aligned. S6. Perform multi-layer, multi-pass welding on the wheel rim and spokes. Once the welding is complete, the integral part is obtained, and the L-shaped lug plate is removed.

2. The method for adaptively adjusting the gap of large dissimilar metal structural components according to claim 1, characterized in that, In step S2, the bevel on the spoke is a K-type bevel with an angle of 40-60°.

3. The method for adaptively adjusting the gap of large dissimilar metal structural components according to claim 1, characterized in that, In step S5, the heating temperature shall not be lower than 250°C.

4. The method for adaptively adjusting the gap of large dissimilar metal structural components according to claim 1, characterized in that, The rim is made of 34CrNi1Mo, and the spokes are made of Q355B.

5. The method for adaptively adjusting the gap of large dissimilar metal structural components according to claim 4, characterized in that, In step S6, the welding process is as follows: S61. Perform base welding on both sides. After welding, remove the L-shaped ear plate. For the front and back root welding, use Φ4mm H10Mn2 welding wire and a current of 450-500A.

6. Voltage: 27-30V; Welding speed: 250-400mm / min; S62, Perform front and back filler welding. In the front and back filler welding, Φ4mm H10Mn2 welding wire is used, the current is 500-650A, the voltage is 28-34V, and the welding speed is 300-420mm / min; S63. Perform front and back cover welding. For welding the front and back covers, use Φ4mm H10Mn2 welding wire, current of 500-650A, voltage of 28-34V, and welding speed of 300-420mm / min.

7. The method for adaptively adjusting the gap of large dissimilar metal structural components according to claim 5, characterized in that, Submerged arc welding is used for root pass welding, filler welding, or cover welding on both sides.

8. The method for adaptively adjusting the gap of large dissimilar metal structural components according to claim 1, characterized in that, In step S6, the flatness of the spokes is monitored in real time during the welding process.

9. A method for adaptively adjusting the gap of large dissimilar metal structural components according to claim 7, characterized in that, In step S6, during the welding process, when the deformation of the spokes exceeds 3mm, the following operation should be performed: first, flip the intermediate part over, and then weld the opposite sides.

10. A welding method for adaptive adjustment of gaps in large dissimilar metal structural components according to claim 1, characterized in that, The maximum gap between the rim and the spokes shall not exceed 12 mm.

Citation Information

Patent Citations

  • Main platform ear plate fast assembling tooling and ear plate assembling method

    CN104439849A

  • Method for welding hollow main shaft and solid shaft head

    WO2016173314A1