Display device

By employing a flexible display panel and support substrate design in the foldable display, the gaps and flexible materials are used to buffer the impact, solving the problem of local deformation and bending of the display under point impact, and achieving a balance between impact resistance and bending performance.

CN117321659BActive Publication Date: 2026-11-20SHARP DISPLAY TECHNOLOGY CORP
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202180098303.X
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-06-23
Publication Date
2026-11-20
Estimated Expiration
2041-06-23

AI Technical Summary

Technical Problem

When subjected to point impacts, the metal film of existing foldable displays cannot flex sufficiently, resulting in ineffective shock absorption. Furthermore, the display panel is prone to localized deformation near the bending area, affecting display quality.

Method used

The design employs a flexible display panel and a support substrate, creating a gap between the display panel and the support substrate in the non-fixed area. The gap between the support substrate and the frame buffers the impact. The support substrate structure, which combines a flexible metal film and a resin film, maintains the flexibility and impact resistance of the display panel.

Benefits of technology

It achieves a balance between impact resistance to large point impacts and the bending flexibility of the display panel, avoiding local deformation and undulation of the display panel and improving the durability of the monitor.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117321659B_ABST
    Figure CN117321659B_ABST
Patent Text Reader

Abstract

A display device includes a display region (D) composed of a pair of flat portions (Fa, Fb) held flat and a bent portion (B) disposed between the pair of flat portions (Fa, Fb) and held bendable, and a frame region (N) provided around the display region (D); a support substrate (50) that supports the display panel (40) flat; and a frame (60) that supports the support substrate (50), in the display region (D), the display panel (40) and the support substrate (50) are not fixed, and a gap (G) is formed between the support substrate (50) and the frame (60).
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to a display device. Background Technology

[0002] In recent years, as a replacement for liquid crystal displays, self-emissive organic EL displays using organic electroluminescent (EL) elements have attracted much attention. Among organic EL displays, a display panel with a structure (laminate) in which organic EL elements and various thin films are stacked on a flexible resin substrate has been proposed. Organic EL displays that can be repeatedly folded are called foldable displays.

[0003] In foldable displays, flexibility is required, so rigid components such as non-flexible (rigid) covers cannot be placed on the surface. Therefore, even flexible display panels can sometimes deform locally due to impacts from objects falling onto their surface or the foldable display itself during a fall. This localized deformation can cause cracks or other defects in the inorganic film of the thin-film transistor (TFT) layer that makes up the display panel, resulting in bright spots, dark spots (dot defects), and other display problems. Thus, foldable displays have a weak resistance to impacts from drops.

[0004] Regarding the aforementioned problems, various methods have been studied to reduce the possibility of display defects. For example, Patent Document 1 discloses a foldable display that includes an impact-absorbing layer disposed between a flexible display layer (a first display area, a second display area, and a third display area) and a non-flexible first support substrate supporting the first display area, and between a non-flexible second support substrate supporting the second display area. This impact-absorbing layer has a thin metal film to improve the impact resistance of the foldable display. Existing technical documents Patent documents

[0005] Patent Document 1: International Publication No. 2020 / 203584 Summary of the Invention The technical problem to be solved by the present invention

[0006] In the folding display described in Patent Document 1, the metal film constituting the impact-absorbing layer is bonded to the entire display area as part (one layer) of a laminate constituting a flexible display layer (display panel). Therefore, in the event of a large point impact, such as a pen tip with a small ball diameter falling onto the display panel, the metal film cannot flex sufficiently, raising concerns that it may not adequately buffer point impacts.

[0007] Furthermore, in the folding display described in Patent Document 1, although it is provided with supports for the first and second display areas (non-bending areas, ... Figure 1 The first and second support substrates in the range X shown, but in the third display area (curved area) located between the first display area and the second display area. Figure 1 There is no supporting substrate on the lower side of the area Y shown. Therefore, when a point impact of a large amount, such as a pen stroke, is applied to the curved area, the display panel may be locally deformed near the curved area. In addition, even when there is a relatively thick adhesive layer between the first and second display areas and the first and second supporting substrates, if a large point impact is applied to the non-curved area, the flexible adhesive layer will be locally deformed. Therefore, the display panel may be locally deformed even in the non-curved area.

[0008] Furthermore, in the folding display described in Patent Document 1, the panel structure differs significantly between the non-bending and bending areas. Therefore, in the bending areas, there are concerns about issues such as panel undulations or creases during bending. If these problems are to be resolved, it is sometimes impossible to maintain the flexibility of the display panel.

[0009] The present invention was made in view of the above points, and its purpose is to simultaneously achieve impact resistance against large point impacts and the flexibility of the display panel. Technical solutions for solving technical problems

[0010] To achieve the above objectives, the display device of the present invention includes: a display panel having flexibility, and comprising: a display area consisting of a pair of flat portions that remain flat and a curved portion disposed between the pair of flat portions and remaining flexible; a frame area disposed around the display area; a support substrate that flatly supports the display panel; and a frame that supports the support substrate, wherein in the display area, the display panel and the support substrate are not fixed, and a gap is formed between the support substrate and the frame. Beneficial effects

[0011] According to the present invention, it is possible to balance the impact resistance to large point impacts and the flexibility of the display panel. Attached Figure Description

[0012] Figure 1 This is a perspective view showing the unfolded state of the organic EL display device according to the first embodiment of the present invention. Figure 2 This is a plan view showing the unfolded state of the organic EL display device according to the first embodiment of the present invention. Figure 3 It shows along Figure 2The image shows a cross-sectional view of the organic EL display device of the first embodiment of the present invention in its unfolded state along line III-III. Figure 4 This is a top view showing a modified example of the organic EL display device according to the first embodiment of the present invention in an unfolded state, which is equivalent to... Figure 2 The image. Figure 5 It shows along Figure 4 The enlarged cross-sectional view of a modified example 1 of the organic EL display device of the first embodiment of the present invention, folded into a U-shape, is shown in the VV line. Figure 6 This is a top view showing the unfolded state of a modified example 2 of the organic EL display device according to the first embodiment of the present invention, which is equivalent to... Figure 2 The image. Figure 7 It is along Figure 6 The enlarged cross-sectional view of the modified example 2 of the organic EL display device of the first embodiment of the present invention, folded into a U-shape, is equivalent to the VII-VII lines in the figure. Figure 5 The image. Figure 8 This is a top view showing the unfolded state of a modified example 3 of the organic EL display device according to the first embodiment of the present invention, which is equivalent to... Figure 2 The image. Figure 9 It shows along Figure 8 The enlarged cross-sectional view of Modified Example 3 of the Organic EL Display Device of the First Embodiment of the present invention, folded into a U-shape, is equivalent to... Figure 5 The image. Figure 10 This is a top view of the display area of ​​the organic EL display device according to the first embodiment of the present invention. Figure 11 This is a cross-sectional view of the display area of ​​an organic EL display device according to the first embodiment of the present invention. Figure 12 This is an equivalent circuit diagram of the TFT layer of the organic EL display device according to the first embodiment of the present invention. Figure 13 This is a cross-sectional view of the organic EL layer constituting the organic EL display device according to the first embodiment of the present invention. Figure 14 This is a cross-sectional view showing the unfolded state of the organic EL display device according to the second embodiment of the present invention, which is equivalent to... Figure 3 The image. Figure 15 This is a cross-sectional view of a modified example of the organic EL display device according to the second embodiment of the present invention in its unfolded state, which is equivalent to... Figure 3 The image. Figure 16 This is a cross-sectional view of the organic EL display device according to the third embodiment of the present invention in its unfolded state, which is equivalent to... Figure 3 The image. Figure 17 This is an enlarged cross-sectional view showing the organic EL display device of the third embodiment of the present invention folded into a U-shape, which is equivalent to Figure 5 The image. Figure 18 This is an enlarged cross-sectional view showing the folded state of the organic EL display device according to the third embodiment of the present invention, folded into a teardrop shape. It is equivalent to... Figure 5 The picture Figure 19 This is a cross-sectional view showing the unfolded state of the organic EL display device according to the fourth embodiment of the present invention, which is equivalent to... Figure 3 The image. Figure 20 This is a top view showing the unfolded state of the support substrate of the organic EL display device constituting the fourth embodiment of the present invention. Detailed Implementation

[0013] Hereinafter, embodiments of the present invention will be described in detail with reference to the accompanying drawings. However, the present invention is not limited to the following embodiments.

[0014] [First Implementation Method] Figures 1 to 13 A first embodiment of the display device and its manufacturing method according to the present invention is shown. Furthermore, in the following embodiments, an organic EL display device including an organic EL element is exemplified as a display device including a light-emitting element. Here, Figure 1 This is a perspective view showing the unfolded state of the organic EL display device 70a. Figure 2 This is a plan view showing the unfolded state of the organic EL display device 70a. Figure 3 It is along Figure 2 A cross-sectional view of the organic EL display device 70a in its unfolded state along line III-III. Figure 4 This is a top view showing the unfolded state of a modified example 1 of the organic EL display device 70a, which is equivalent to... Figure 2 The image. Figure 5 It shows along Figure 4 An enlarged cross-sectional view of a modified example 1 of the organic EL display device 70a with VV lines, folded into a U-shape. Figure 6 This is a top view showing the unfolded state of Modified Example 2 of the organic EL display device 70a, which is equivalent to... Figure 2 The image. Additionally. Figure 7 It is along Figure 6The enlarged cross-sectional view of the modified example 2 of the organic EL display device 70a with lines VII-VII in the image, folded into a U-shape, is equivalent to... Figure 5 The image. Figure 8 This is a top view showing the unfolded state of Modified Example 3 of the organic EL display device 70a, which is equivalent to... Figure 2 The image. Additionally. Figure 9 It is along Figure 8 The enlarged cross-sectional view of the modified example 3 of the organic EL display device 70a with IX-IX lines, folded into a U-shape, is equivalent to... Figure 5 The image. Figure 10 This is a top view of the display area D of the organic EL display device 70a. Figure 11 This is a cross-sectional view of the display area D of the organic EL display device 70a. Figure 12 This is an equivalent circuit diagram showing the TFT layer 20 that constitutes the organic EL display device 70a. Figure 13 This is a cross-sectional view of the organic EL layer 23 constituting the organic EL display device 70a. Furthermore, in the organic EL display device 70a, a direction X parallel to the substrate surface of the organic EL display panel 40 (described later), a direction Y perpendicular to direction X and parallel to the substrate surface of the organic EL display panel 40, and a direction Z perpendicular to both directions X and Y are defined.

[0015] like Figures 1 to 3 As shown, the organic EL display device 70a includes at least an organic EL display panel 40, a support substrate 50, and a housing 60.

[0016] like Figure 1 and Figure 2 As shown, the organic EL display panel 40, for example, has a rectangular display area (active area) D for displaying images and a frame-shaped border area (non-display area) N surrounding the display area D. Furthermore, in this embodiment, a rectangular display area D is exemplified, but this rectangle also includes, for example, shapes with rounded sides, rounded corners, or cutouts on part of the sides, etc., generally rectangular shapes. Furthermore, in the border area N... Figure 1 Figure 3 At one end in the X direction, there is a terminal section (not shown) with multiple terminals arranged thereon.

[0017] like Figures 1 to 3 As shown, the display area D includes a pair of flat portions (the non-curved area R described later) that maintain a flat surface. F Fa and Fb, and a curved portion (the curved region R described later) disposed between a pair of flat portions Fa and Fb and held in a flexible manner. B Part B. In the bend B (bend area R) BIn ) such as Figure 1 and Figure 2 As shown, a pair of flat portions Fa and Fb are positioned opposite each other, and the bending axis (bending axis, bending center) C, which allows bending at 180° (U-shape), extends along the Y direction. Furthermore, when viewed from the side, the bending shape of the organic EL display panel 40 is not limited to a U-shape. Figure 5 , Figure 7 , Figure 9 , refer to Figure 17 For example, it can also be teardrop-shaped (see reference). Figure 18 ).

[0018] In addition, such as Figure 1 and Figure 2 As shown, the organic EL display panel 40 consists of a curved region R along the bending axis C. B and located in the curved region R B A pair of non-curved regions R at both ends of the direction X F R F Composition. Bending region R B like Figure 1 and Figure 2 As shown, this refers to the region that includes the curved portion B (a part of the display area D) and the two ends of the curved portion B in the Y direction (a part of the border area N), extending in a straight line along the bending axis C (direction Y). The non-curved region R... F It is the curved region R B The area outside refers to the rectangular area that, when viewed from above, includes a pair of flat portions Fa and Fb (part of the display area D) and the periphery of each pair of flat portions Fa and Fb (part of the border area N).

[0019] The size of the organic EL display panel 40 is, for example, the width ( Figure 2 The longitudinal and Y-direction lengths are approximately 10cm, and the length is ( Figure 1 Figure 3 The horizontal and vertical (X-length) dimensions are approximately 18cm, and the thickness is ( Figure 1 as well as Figure 3 The length (in the longitudinal direction and Z-axis) is approximately several hundred μm. Furthermore, the specific composition of the organic EL display panel 40 will be explained later.

[0020] like Figure 3 As shown, the support substrate 50 is configured to be disposed on the back side of the organic EL display panel 40. Figure 3The support substrate 50 is located on the lower middle side and flatly supports the organic EL display panel 40. The support substrate 50 includes a flexible metal film and is flexible. Alternatively, the support substrate 50 may be composed (only) of a flexible metal film monomer. The metal film is preferably a component with a high elastic modulus, such as a material containing at least one selected from stainless steel, titanium, aluminum, and copper. The thickness (Z-direction length) of the metal film is, for example, 20 μm or more and 45 μm or less, preferably 25 μm or more and 35 μm or less. The elastic modulus of the metal film layer is, for example, 60 GPa or more and 210 GPa or less.

[0021] Alternatively, the support substrate 50 may also be a laminate (metal film / resin film) comprising a flexible resin film and a resin film and a metal film. Alternatively, it may be a laminate (metal film / adhesive layer / resin film) with an adhesive layer between the metal film and the resin film. The resin film is, for example, composed of ABS (acrylonitrile-butadiene-styrene copolymer) resin, PS (polystyrene) resin, PC (polycarbonate) resin, PMMA (polymethyl methacrylate) resin, etc. The thickness (Z-length) of the resin film is, for example, 25 μm or more and 300 μm or less, preferably 50 μm or more and 150 μm or less. The elastic modulus of the resin film is, for example, 30 MPa or more and 5 GPa or less.

[0022] Alternatively, the support substrate 50 may be a laminate comprising an elastomer layer (e.g., silicone rubber) in addition to a metal film and a resin film, and including the elastomer layer, resin film, and metal film. Alternatively, the support substrate 50 may be composed (only) of an elastomer layer monomer. The thickness (Z-direction length) of the elastomer layer is, for example, 100 μm or more and 500 μm or less. The elastic modulus of the elastomer layer is, for example, 1 MPa or more and 10 MPa or less.

[0023] The thickness of the support substrate 50 (in the case of a laminate, the overall thickness of the laminate) is, for example, 20 μm or more and 500 μm or less, preferably 30 μm or more and 300 μm or less. From the viewpoint of maintaining the shape of the organic EL display panel 40 flat and preventing undulations, the elastic modulus of the support substrate 50 is preferably a relatively large elastic modulus, for example, 1 MPa or more and 210 GPa or less, preferably 30 MPa or more and 200 GPa or less.

[0024] In the organic EL display device 70a, such as Figure 3 As shown, the support substrate 50 is composed of a single substrate spanning the entire area of ​​the organic EL display panel 40. In other words, the support substrate 50 extends across the non-bending region R. F (flat regions Fa, Fb) and curved regions R B(Bend portion B) has the same configuration. That is, the support base plate 50 is also provided (present) in the bend region R. B The lower side (the portion overlapping with the bend B when viewed from above). Therefore, relative to an impact on or near the bend B, the support substrate 50 located on the lower side of the bend B bends, thereby suppressing localized deformation of the organic EL display panel 40. Additionally, in the bend region R... B In addition, it can also reduce problems such as creases or bending when the organic EL display panel 40 is undulating.

[0025] like Figure 1 and Figure 3 As shown, the frame 60 is a housing (casing) that houses the organic EL display panel 40 and the support substrate 50. Figure 3 As shown, the housing 60 is disposed on the lower side of the support base plate 50 to support the support base plate 50. The housing 60 is non-flexible (rigid) and is made of a rigid component such as metal or resin. Figure 3 As shown, the thickness of the portion of the housing 60 overlapping the curved portion B becomes thinner when viewed from above, and a hinge mechanism 61 is provided in this thin-walled portion. Through the hinge mechanism 61, the organic EL display device 70a functions as a foldable display. Furthermore, the hinge mechanism 61 is not particularly limited to any mechanism capable of bending. Additionally, batteries, circuit boards, etc., may also be provided in the housing 60.

[0026] The organic EL display device 70a configured as described above houses, for example, an organic EL display panel 40 and a support substrate 50 within a housing 60 having a hinge mechanism 61, and can be deformed between the following states: an unfolded state in which one flat portion Fa, a curved portion B, and another flat portion Fb are arranged on the same plane (see reference). Figures 1-3 , Figure 4 , Figure 6 , Figure 8 ); and the folded state in which the curved portion B is bent so that a pair of flat portions Fa and Fb are arranged opposite each other. Figure 5 , Figure 7 , Figure 9 ).

[0027] Here, in the organic EL display device 70a, such as Figure 3 As shown, the organic EL display panel 40 and the support substrate 50 are not fixed throughout the entire display area D. Therefore, even with a point impact as large as a pen stroke, the organic EL display panel 40 deforms only slightly. Furthermore, the unfixed area of ​​the organic EL display panel 40 and the support substrate 50 may not be the entire display area D, but may be at least a portion of the display area D; from the viewpoint of impact resistance, it is preferable to provide the area throughout the entire display area D.

[0028] Furthermore, in the display area D (preferably the entire area), the organic EL display panel 40 and the support substrate 50 can be either not fixed or have a gap (air gap, space) between them.

[0029] Additionally, in the organic EL display device 70a, such as Figure 3 As shown, in a top view, the entire area overlapping the display area D (hereinafter also referred to as "display area D") has a gap (air gap) G formed between the support substrate 50 and the housing 60. The gap G is the space divided by the support substrate 50 and the housing 60. That is, as... Figure 3 As shown, the support substrate 50 and the housing 60 are not fixed throughout the entire display area D. Therefore, the support substrate 50 can bend sufficiently downwards (in the direction where the gap G exists), thus mitigating even large point impacts. Furthermore, the gap G may not be the entire display area D, or it may be at least a portion of the display area D; from an impact resistance point of view, it is preferable to provide it throughout the entire display area D.

[0030] The void G can be filled with gases such as air or inert gases, or it can contain gases such as air that may be present in the usual manufacturing process. The void G can be a completely enclosed space (a space where air cannot enter or exit) or a partially enclosed space (a space where air can enter or exit).

[0031] The thickness (length in the Z direction) of the gap G is, for example, about 300 μm. From the viewpoint that the support substrate 50 can be fully bent so that even large point impacts are mitigated, it is preferably 200 μm or more and 750 μm or less, and more preferably 300 μm or more and 450 μm or less.

[0032] As a method for forming void G, such as Figure 3 As shown, examples include the area overlapping the border area N when viewed from above (hereinafter also referred to as "border area N"), for instance, a method of fixing the support base plate 50 and the frame 60 via a fixing member 55, etc. That is, as... Figure 3 As shown, in the border region N, the support base plate 50 and the frame 60 are fixed. Specifically, the support base plate 50 and the frame 60 are fixed only in the portions that overlap with the border region N when viewed from above.

[0033] Examples of fixing components 55 include a resin or metal frame that overlaps with the bezel region N when viewed from above, arranged in a frame shape around the display area D; and resin or metal blocks that are rectangular, circular, or elliptical when viewed from above. For example, the frame-shaped fixing component 55 can be arranged along the entire circumference of the organic EL display panel 40 along the bezel region N. In this case, the gap G formed by the frame-shaped fixing component 55, the support substrate 50, and the frame 60 is formed in the aforementioned completely enclosed space. Alternatively, the block-shaped fixing component 55 can be arranged in an island-like configuration along the bezel region N. In this case, the gap G formed by the block-shaped fixing component 55, the support substrate 50, and the frame 60 is formed in the aforementioned partially enclosed space.

[0034] The thickness (Z-direction length) of the fixing component 55 is not particularly limited, and can be appropriately determined according to the thickness of the aforementioned gap G. The support base plate 50 and frame 60 can be fixed to the fixing component 55 by applying an adhesive layer (OCA (optical clear adhesive), adhesive tape, sponge pad, etc.) or by using screws or other threaded connections. Furthermore, if a gap G is formed between the support base plate 50 and frame 60 by using adhesive bonding or screwing with thick adhesive tape, sponge pads, etc., the fixing component 55 may not be necessary.

[0035] Similarly, as mentioned above, Figure 3 As shown, the organic EL display panel 40 and the support substrate 50 are fixed in the bezel region N. Specifically, the organic EL display panel 40 and the support substrate 50 are fixed only in the bezel region N.

[0036] The organic EL display panel 40 and the support substrate 50 can be fixed by adhesive layer (OCA, adhesive tape, foam pad, etc.) or by screws. When using adhesive fixing, such as... Figure 3 As shown, a frame-shaped adhesive layer 48 may also be provided between the organic EL display panel 40 and the support substrate 50, extending around the display area D, so that it overlaps with the bezel area N when viewed from above. In this case, the adhesive layer 48 is provided along the entire circumference of the organic EL display panel 40 along the bezel area N. In other words, an opening is provided on the adhesive layer 48 at the portion that overlaps with the display area D when viewed from above. That is, the adhesive layer 48 has an opening (hereinafter also referred to as "display area opening") 48a formed in the portion that overlaps with the display area D when viewed from above (refer to...). Figure 4 , 6 8). The thickness (Z-direction length) of the adhesive layer 48 can be relatively thick, preferably 15 μm or more and 100 μm or less. The elastic modulus of the adhesive layer 48 is preferably 2.0 × 10⁻⁶. 4[Pa] or higher and 1.0 × 10 6 [Pa] or less, more preferably 3.0 × 10 4 [Pa] or higher and 1.5 × 10 5 [Pa] below.

[0037] Thus, in the organic EL display device 70a, such as Figure 3 As shown, in the portion overlapping with the bezel region N when viewed from above (the portion corresponding to the bezel region N), the upper surface of the support substrate 50 is fixed to the lower surface of the organic EL display panel 40, and the lower surface of the support substrate 50 is fixed to the upper surface of the frame 60. On the other hand, in the entire portion overlapping with the display region D when viewed from above (the portion corresponding to the display region D), the support substrate 50 is not fixed to either the organic EL display panel 40 or the frame 60, and a gap G exists on the lower side of the support substrate 50. Therefore, in the organic EL display device 70a, while maintaining excellent flexibility, the impact resistance to large point impacts is improved.

[0038] Variation 1 of the First Embodiment like Figure 4 and Figure 5 As shown, an opening may also be provided on the adhesive layer 48 in the portion overlapping with the border area N when viewed from above. That is, the adhesive layer 48 may also have a pair of openings (hereinafter also referred to as "border area openings") 48b, 48b, which, together with the display area opening 48a, are formed in the curved area R extending along the curved portion B. B The portion that overlaps with the border region N when viewed from above. In this case, as... Figure 4 As shown, the adhesive layer 48 is cut (separated) into two separate parts through a pair of frame area openings 48b, 48b, and configured separately. Additionally, in Figure 4 The organic EL display panel 40 is omitted from the text. Figure 6 The frame 60 is omitted.

[0039] In variation example 1, such as Figure 4 As shown, a pair of frame region openings 48b, 48b are formed in the frame region N and the curved portion B (curved region R). B The overlapping portion when viewed from above is set as a rectangle. That is to say, as... Figure 4 and Figure 5 As shown, when viewed from above, the curved region R containing the curved portion B... BIn the overlapping area, the organic EL display panel 40 and the support substrate 50 are not fixed. Therefore, even if there are differences in the amount of bending caused by the difference in the elastic modulus of the organic EL display panel 40 and the support substrate 50, they are unlikely to affect each other. In this case, the adhesive layer 48 can be thinned, for example, to a thickness of 2 μm or more but less than 50 μm.

[0040] Variation 2 of the First Embodiment like Figure 6 and Figure 7 As shown, the adhesive layer 48 may also have a pair of border area openings 48c, 48c, which, together with the display area opening 48a, are formed in the curved region R extending along the curved portion B. B The portion that overlaps with the border region N when viewed from above. In this case, as... Figure 6 As shown, the adhesive layer 48 is cut (separated) into two separate parts through a pair of frame area openings 48c, 48c, and configured separately. Additionally, in Figure 6 The organic EL display panel 40 is omitted from the text. Figure 7 The frame 60 is omitted.

[0041] In variation example 2, such as Figure 6 as well as Figure 7 As shown, the shape and size of the pair of border area openings 48c, 48c are different from those of the pair of border area openings 48b, 48b in Modified Example 1. Specifically, as... Figure 6 As shown, a pair of frame area openings 48c, 48c are formed along the curved portion B (curved region R). B A slit-like shape extending along the bending axis C (direction Y). That is, as... Figure 6 as well as Figure 7 As shown, in the bending region R containing the bending portion B B In the region near the bending axis C, where the area overlaps when viewed from above, the organic EL display panel 40 and the support substrate 50 are not fixed. Therefore, even if there are differences in the amount of bending caused by the difference in the elastic modulus of the organic EL display panel 40 and the support substrate 50, they are unlikely to affect each other. In this case, the adhesive layer 48 can be thinned, for example, to a thickness of 2 μm or more but less than 50 μm.

[0042] Variation 3 of the First Embodiment like Figure 8 and Figure 9 As shown, the adhesive layer 48 may also have, together with the display area opening 48a, a pair of border area openings 48d, 48d that, when viewed from above, overlap with a pair of border areas N, N respectively disposed around a pair of flat portions Fa, Fb. In this case, as Figure 8As shown, the adhesive layer 48 is cut (separated) into four separate portions through a pair of border area openings 48d, 48d, and is configured separately. Additionally, in Figure 8 The organic EL display panel 40 is omitted from the text. Figure 9 The frame 60 is omitted.

[0043] In variation example 3, such as Figure 8 as well as Figure 9 As shown, the positions and numbers of the pair of border area openings 48d, 48d differ from those of the pair of border area openings 48c, 48c in Variation Example 2. Specifically, as... Figure 8 As shown, in the adhesive layer 48, near the curved portion B, in a pair of border regions N, N respectively disposed around a pair of flat portions Fa, Fb, two sets (a total of four) of a pair of border region openings 48d, 48d are formed. More specifically, the pair of border region openings 48d, 48d are non-curved regions R F The portion that overlaps with the border area N when viewed from above, in the curved area R B Near (bend B), the terrain, similar to that in variation 2, forms a slit-like shape extending along the bending axis C (direction Y) of bend B. That is, as... Figure 8 as well as Figure 9 As shown, in the non-curved region R containing a pair of flat portions Fa and Fb F The curved region R, including the curved portion B. B In the region near both ends of direction X, where the two overlap when viewed from above, the organic EL display panel 40 and the support substrate 50 are not fixed. Therefore, even if there is a difference in the amount of bending caused by the difference in the elastic modulus of the organic EL display panel 40 and the support substrate 50, they are unlikely to affect each other. In this case, the adhesive layer 48 can be thinned, for example, to a thickness of 2 μm or more but less than 50 μm.

[0044] like Figure 3 As shown, the organic EL display panel 40 includes a flexible display layer 41, a functional layer 42, and a cover 43, which are stacked in this order.

[0045] like Figure 10 As shown, multiple sub-pixels P are arranged in a matrix in the display area D of the flexible display layer 41 (organic EL display panel 40). Furthermore, in the display area D, as... Figure 10 As shown, for example, a sub-pixel P having a red emitting area Lr for displaying red, a sub-pixel P having a green emitting area Lg for displaying green, and a sub-pixel P having a blue emitting area Lb for displaying blue are arranged adjacent to each other. Furthermore, in the display area D, a pixel is formed by three adjacent sub-pixels P having the red emitting area Lr, the green emitting area Lg, and the blue emitting area Lb.

[0046] like Figure 11 As shown, the organic EL display device 70a includes the following in the flexible display layer 41 (organic EL display panel 40): a resin substrate layer 10 serving as a base substrate; a TFT layer 20 disposed on the resin substrate layer 10; an organic EL element layer 30 disposed on the TFT layer 20 as a light-emitting element layer; and a sealing film 35 configured to cover the organic EL element layer 30.

[0047] The resin substrate layer 10 is made of, for example, polyimide resin.

[0048] like Figure 11 As shown, the TFT layer 20 includes: a base coating film 11 disposed on the resin substrate layer 10; a plurality of first TFTs 9a, a plurality of second TFTs 9b, and a plurality of capacitors 9c disposed on the base coating film 11; and a planarization film 19 disposed on each of the first TFTs 9a, each of the second TFTs 9b, and each of the capacitors 9c. Here, in the TFT layer 20, as... Figure 11 As shown, the base coating 11, semiconductor layers 12a and 12b, gate insulating film 13, and gate line 14 (see reference) Figure 10 ), gate electrodes 14a and 14b, and lower conductive layer 14c, etc., first wiring layer, first interlayer insulating film 15, upper conductive layer 16, second interlayer insulating film 17, source line 18f (refer to Figure 10 The second wiring layer, including source electrodes 18a and 18c, drain electrodes 18b and 18d, and power lines 18g, and the planarization film 19 are sequentially stacked on the resin substrate layer 10. Furthermore, as... Figure 10 as well as Figure 12 As shown, in the TFT layer 20, a plurality of gate lines 14 are arranged in a manner that extends parallel to each other in the lateral direction shown in the figure. Furthermore, as... Figure 10 as well as Figure 12 As shown, in the TFT layer 20, multiple source lines 18f are arranged in a manner that extends parallel to each other in the vertical direction shown in the figure. Additionally, as... Figure 10 as well as Figure 12 As shown, in the TFT layer 20, multiple power lines 18g are arranged in a manner that extends parallel to each other in the longitudinal direction shown in the figure. Furthermore, as... Figure 10 As shown, each power line 18g is positioned adjacent to each source line 18f. Furthermore, in the TFT layer 20, as... Figure 12 As shown, each sub-pixel P is provided with a first TFT9a, a second TFT9b, and a capacitor 9c.

[0049] The base coating film 11, the gate insulating film 13, the first interlayer insulating film 15, and the second interlayer insulating film 17 are, for example, composed of a single layer or a stack of inorganic insulating films such as silicon nitride, silicon oxide, and silicon oxynitride.

[0050] The first TFT 9a and the second TFT 9b are, for example, p-type TFTs in which impurities such as boron are doped in semiconductor layers 12a and 12b, which will be described later.

[0051] like Figure 12 As shown, in each sub-pixel P, the first TFT 9a is electrically connected to the corresponding gate line 14 and source line 18f. Figure 11 As shown, the first TFT 9a includes a semiconductor layer 12a, a gate insulating film 13, a gate electrode 14a, a first interlayer insulating film 15, a second interlayer insulating film 17, a source electrode 18a, and a drain electrode 18b sequentially disposed on the base coating film 11. Here, as... Figure 11 As shown, the semiconductor layer 12a is disposed on the base coating film 11 in an island-like manner and has a channel region, a source region, and a drain region. Furthermore, as... Figure 11 As shown, the gate insulating film 13 is provided in a manner that covers the semiconductor layer 12a. Furthermore, as... Figure 11 As shown, the gate electrode 14a is disposed on the gate insulating film 13 in a manner that overlaps with the channel region of the semiconductor layer 12a. Furthermore, as... Figure 11 As shown, the first interlayer insulating film 15 and the second interlayer insulating film 17 are sequentially disposed such that they cover the gate electrode 14a. Furthermore, as... Figure 11 As shown, the source electrode 18a and the drain electrode 18b are disposed on the second interlayer insulating film 17 in a manner separate from each other. Furthermore, as... Figure 11 As shown, the source electrode 18a and the drain electrode 18b are connected to the source region and the drain region of the semiconductor layer 12a respectively via contact holes formed in the stacked film of the gate insulating film 13, the first interlayer insulating film 15 and the second interlayer insulating film 17.

[0052] like Figure 12 As shown, in each sub-pixel P, the second TFT9b is electrically connected to the corresponding first TFT9a and power line 18g. Additionally, as... Figure 11 As shown, the second TFT 9b includes a semiconductor layer 12b, a gate insulating film 13, a gate electrode 14b, a first interlayer insulating film 15, a second interlayer insulating film 17, a source electrode 18c, and a drain electrode 18d sequentially disposed on the base coating film 11. Here, as... Figure 11 As shown, the semiconductor layer 12b is disposed on the base coating film 11 in an island-like manner and has a channel region, a source region, and a drain region. Additionally, as... Figure 11 As shown, the gate insulating film 13 is provided in a manner that covers the semiconductor layer 12a. Additionally, as... Figure 11 As shown, the gate electrode 14b is disposed on the gate insulating film 13 in a manner that overlaps with the channel region of the semiconductor layer 12b. Furthermore, as... Figure 11As shown, the first interlayer insulating film 15 and the second interlayer insulating film 17 are sequentially disposed to cover the gate electrode 14b. Additionally, as... Figure 11 As shown, the source electrode 18a and the drain electrode 18d are disposed on the second interlayer insulating film 17 in a manner separate from each other. Furthermore, as... Figure 2 As shown, the source electrode 18c and the drain electrode 18d are electrically connected to the source region and drain region of the semiconductor layer 12b, respectively, via contact holes formed in the stacked film of the gate insulating film 13, the first interlayer insulating film 15 and the second interlayer insulating film 17.

[0053] Furthermore, in this embodiment, a top-gate type first TFT 9a and a second TFT 9b are exemplified, but the first TFT 9a and the second TFT 9b can also be bottom-gate type TFTs.

[0054] like Figure 12 As shown, in each sub-pixel P, capacitor 9c is electrically connected to the corresponding first TFT 9a and power line 18g. Here, as... Figure 11 As shown, capacitor 9c includes: a lower conductive layer 14c; a first interlayer insulating film 15 disposed to cover the lower conductive layer 14c; and an upper conductive layer 16 disposed on the first interlayer insulating film 15 to overlap with the lower conductive layer 14c. Furthermore, as... Figure 11 As shown, the upper conductive layer 16 is electrically connected to the power line 18g via a contact hole formed on the second interlayer insulating film 17.

[0055] In the display area D, the planarization film 19 has a flat surface and is made of an organic resin material such as polyimide resin.

[0056] like Figure 11 As shown, the organic EL element layer 30 has a plurality of organic EL elements 25, which are multiple light-emitting elements arranged in a matrix corresponding to a plurality of sub-pixels P.

[0057] like Figure 11 As shown, the organic EL element 25 includes: a first electrode 21 disposed on each sub-pixel P on a planarization film 19, an organic EL layer 23 disposed on the first electrode 21 on each sub-pixel P, and a second electrode 24 disposed on the organic EL layer 23 on a plurality of sub-pixels P.

[0058] Here, as Figure 11As shown, the first electrode 21 is electrically connected to the drain electrode 18d of the second TFT 9b of each sub-pixel P via a contact hole formed in the planarization film 19. Furthermore, the first electrode 21 has the function of injecting holes into the organic EL layer 23. In order to improve the hole injection efficiency into the organic EL layer 23, the first electrode 21 is more preferably formed of a material with a high work function. Examples of materials that can be used to form the first electrode 21 include, for example, metallic materials such as silver (Ag), aluminum (Al), vanadium (V), cobalt (Co), nickel (Ni), tungsten (W), gold (Au), titanium (Ti), ruthenium (Ru), manganese (Mn), indium (In), ybium (Yb), lithium fluoride (LiF), platinum (Pt), palladium (Pd), molybdenum (Mo), iridium (Ir), and tin (Sn). In addition, the material constituting the first electrode 21 can also be, for example, an alloy of astatine (At) / astatine oxide (AtO2). Furthermore, the material constituting the first electrode 21 can be, for example, a conductive oxide such as tin oxide (SnO), zinc oxide (ZnO), indium tin oxide (ITO), or indium zinc oxide (IZO). Additionally, the first electrode 21 can be formed by stacking multiple layers of the above-mentioned materials. Furthermore, compound materials with high work functions are, for example, indium tin oxide (ITO) and indium zinc oxide (IZO). Moreover, the peripheral end of the first electrode 21 is provided to cover a grid-like edge mask 22 shared by multiple sub-pixels P. Here, the material constituting the edge mask 22 can be, for example, a positive photosensitive resin such as polyimide resin, acrylic resin, polysiloxane resin, or phenolic varnish resin.

[0059] Here, as Figure 13 As shown, the organic EL layer 23 includes a hole injection layer 1, a hole transport layer 2, a light emission layer 3, an electron transport layer 4, and an electron injection layer 5 sequentially disposed on the first electrode 21.

[0060] Hole injection layer 1, also known as the anolyte buffer layer, brings the energy levels of the first electrode 21 and the organic EL layer 23 closer together, thereby improving the hole injection efficiency from the first electrode 21 to the organic EL layer 23. Materials constituting hole injection layer 1 may include, for example, triazole derivatives, oxadiazole derivatives, imidazole derivatives, polyaryl alkyl derivatives, pyrazoline derivatives, phenylenediamine derivatives, oxazole derivatives, styrene-anthracene derivatives, fluorenone derivatives, hydrazone derivatives, and stilbene derivatives.

[0061] The hole transport layer 2 functions to improve the transport efficiency of holes from the first electrode 21 to the organic EL layer 23. Examples of materials constituting the hole transport layer 2 include porphyrin derivatives, aromatic tertiary amine compounds, phenylethylamine derivatives, polyvinylcarbazole, poly-p-phenylacetylene, polysilanes, triazole derivatives, oxadiazole derivatives, imidazole derivatives, polyarylalkyl derivatives, pyrazoline derivatives, pyrazolone derivatives, phenylenediamine derivatives, aromatic amine derivatives, amine-substituted chalcone derivatives, oxazole derivatives, styrene-anthracene derivatives, fluorenone derivatives, hydrazone derivatives, stilbene derivatives, hydrogenated amorphous silicon, hydrogenated amorphous silicon carbide, zinc sulfide, and zinc selenide.

[0062] The light-emitting layer 3 is the region in which holes and electrons are injected from the first electrode 21 and the second electrode 24 respectively and recombine when a voltage is applied to the first electrode 21 and the second electrode 24. Here, the light-emitting layer 3 is formed of a material with high luminous efficiency. Furthermore, materials constituting the light-emitting layer 3 may include, for example, metal hydroxyquinoline compounds [8-hydroxyquinoline metal complexes], naphthalene derivatives, anthracene derivatives, stilbene derivatives, vinyl acetone derivatives, triphenylamine derivatives, butadiene derivatives, coumarin derivatives, benzoxazole derivatives, oxadiazole derivatives, oxazole derivatives, benzimidazole derivatives, thiadiazole derivatives, benzothiazazole derivatives, styryl derivatives, styreneamine derivatives, stilbeneylbenzene derivatives, tristyrylbenzene derivatives, perylene derivatives, pyrene derivatives, aminopyrene derivatives, pyridine derivatives, rhodamine derivatives, acridine derivatives, phenoxazinone, quinacridone derivatives, rubrene, poly(p-phenylenevinylene), polysilane, etc.

[0063] The electron transport layer 4 has the function of enabling electrons to migrate efficiently to the light-emitting layer 3. Here, the materials constituting the electron transport layer 4 can be, for example, organic compounds such as diazole derivatives, triazole derivatives, benzoquinone derivatives, naphthoquinone derivatives, anthraquinone derivatives, tetracyanoanthraquinone dimethane derivatives, biphenylquinone derivatives, fluorenone derivatives, thiophene derivatives, and metal hydroxyquinoline compounds.

[0064] The electron injection layer 5 is close to the energy levels of the second electrode 24 and the organic EL layer 23, and has the function of improving the efficiency of electron injection from the second electrode 24 to the organic EL layer 23. Through this function, the driving voltage of the organic EL element 25 can be reduced. In addition, the electron injection layer 5 is also referred to as the cathode buffer layer. Here, the materials constituting the electron injection layer 5 include, for example, inorganic alkali compounds such as lithium fluoride (LiF), magnesium fluoride (MgF2), calcium fluoride (CaF2), strontium fluoride (SrF2), and barium fluoride (BaF2), as well as aluminum oxide (Al2O3) and strontium oxide (SrO).

[0065] like Figure 11As shown, the second electrode 24 serves as a common electrode and is provided in a manner that covers the organic EL layer 23 and the edge mask 22 of each sub-pixel P. Furthermore, the second electrode 24 has the function of injecting electrons into the organic EL layer 23. In addition, to improve the electron injection efficiency into the organic EL layer 23, the second electrode 24 is more preferably made of a material with a low work function. Examples of materials constituting the second electrode 24 include, for example, silver (Ag), aluminum (Al), vanadium (V), cobalt (Co), nickel (Ni), tungsten (W), gold (Au), calcium (Ca), titanium (Ti), yttrium (Y), sodium (Na), ruthenium (Ru), manganese (Mn), indium (In), magnesium (Mg), lithium (Li), ytterbium (Yb), and lithium fluoride (LiF). Furthermore, the second electrode 24 may also be formed of alloys such as magnesium (Mg) / copper (Cu), magnesium (Mg) / silver (Ag), sodium (Na) / potassium (K), astatine (At) / astatine oxide (AtO2), lithium (Li) / aluminum (Al), lithium (Li) / calcium (Ca) / aluminum (Al), and lithium fluoride (LiF) / calcium (Ca) / aluminum (Al). Additionally, the second electrode 24 may also be formed of conductive oxides such as tin oxide (SnO), zinc oxide (ZnO), indium tin oxide (ITO), and indium zinc oxide (IZO). Furthermore, the second electrode 24 may also be formed by stacking multiple layers composed of the above-mentioned materials. In addition, materials with low work functions include, for example, magnesium (Mg), lithium (Li), lithium fluoride (LiF), magnesium (Mg) / copper (Cu), magnesium (Mg) / silver (Ag), sodium (Na) / potassium (K), lithium (Li) / aluminum (Al), lithium (Li) / calcium (Ca) / aluminum (Al), lithium fluoride (LiF) / calcium (Ca) / aluminum (Al), etc.

[0066] like Figure 11 As shown, the sealing film 35 is arranged as a cathode to cover each organic EL layer 25 and the edge shield 32. Here, as... Figure 11 As shown, the sealing film 35 includes: a first inorganic sealing film 31 disposed to cover the second electrode 24; an organic sealing film 32 disposed on the first inorganic sealing film 31; and a second inorganic sealing film 33 disposed to cover the organic sealing film 32. This sealing film 35 also functions to protect the organic EL layer 23 from moisture, oxygen, and other influences. Here, materials constituting the first inorganic film 31 and the second inorganic film 33 include, for example, silicon oxide (SiO2), aluminum oxide (Al2O3), and silicon nitride (SiN2O3) such as silicon tetranitride (Si3N4). x (x is a positive number)) and inorganic materials such as silicon carbonitride (SiCN). In addition, the organic sealing film 32 is composed of organic materials such as acrylic resin, polyurea resin, parylene resin, polyimide resin, and polyamide resin.

[0067] like Figure 3 As shown, the functional layer 42 is disposed on the flexible display layer 41 in a manner that covers the flexible display layer 41. Examples of functional layers 42 include functional films with various functions such as optical compensation, touch panel sensor functions, and protective functions. The functional layer 42 is flexible to ensure the flexibility of the organic EL display panel. Furthermore, an adhesive layer (OCA) may be disposed between the flexible display layer 41 and the functional layer 42 as needed.

[0068] like Figure 3 As shown, the cover 43 is provided on the functional layer 42 in a manner that covers the functional layer 42. The cover 43 is used to protect the flexible display layer 41 (and the functional layer 42), and the cover 43 is flexible in order to ensure the flexibility of the organic EL display panel. As a flexible cover 43, it is made of, for example, a UV-curable silicone resin. As a specific example of the cover 43, known window films that have undergone hard coating processing can be cited. It should be noted that an adhesive layer (OCA) may also be provided between the functional layer 42 and the cover 43 as needed.

[0069] The aforementioned organic EL display device 70a is configured such that, in each sub-pixel P, a gate signal is input to the first TFT 9a via gate line 14, thereby turning the first TFT 9a on. A predetermined voltage corresponding to the source signal is written to the gate electrode 14b and capacitor 9c of the second TFT 9b via source line 18f. Current from the power line 18g, which is defined based on the gate voltage boundary of the second TFT 9b, is supplied to the organic EL layer 23, thereby causing the light-emitting layer 3 of the organic EL layer 23 to emit light, thus displaying an image. Furthermore, in the organic EL display device 70a, even if the first TFT 9a is in the off state, the light emission of the light-emitting layer 3 is maintained because the gate voltage of the second TFT 9b is held by capacitor 9c, until the gate signal of the next frame is input. [Example]

[0070] The embodiments of this disclosure are described below based on the accompanying drawings. Furthermore, this disclosure is not limited to the following embodiments, and variations and modifications can be made to the following embodiments based on the spirit of the invention; these modifications are not intended to exclude them from the scope of the invention.

[0071] (Comparative Example 1) A flexible organic EL display panel, consisting of a flexible display layer, a functional layer, and a cover layer stacked sequentially, was manufactured. An organic EL display device (folding display) composed solely of the flexible organic EL display panel was subjected to drop impact and bending tests using the methods described below. As a result, the organic EL display device according to Comparative Example 1 passed the bending test, but failed the drop impact test due to point defects caused by damage to the TFT layer.

[0072] [Drop Impact Test] A flexible organic EL display panel is placed on a plastic substrate (50mm thick). In this state, a ballpoint pen tip is dropped onto the panel surface from a height of 10cm.

[0073] [Bending Test] (Experiment Preparation) • Non-flexible area R of flexible organic EL panel F (Refer to Figure 1 , Figure 2 It is fixed to a plastic mounting plate. Double-sided tape is used to secure it to the mounting plate. Alternatively, the mounting plate can be made of metal or fixed to the panel using adhesive; in this case, it is unlikely to affect the test results. Next, the organic EL panel fixed to the fixing plate is mounted onto the bending test apparatus (manufactured by YuasaSystem Machinery Co., Ltd., model: DMLHP) via the fixing plate, so that the bending area R F The bending radius R is 2.0–3.0 mm. At this time, the cover 43 of the organic EL display panel (refer to...) Figure 3 It is set to be located on the inside of the bend. (Testing order) • Alternately repeat the unbent state (0°) and the bent state (180°) of the organic EL panel at room temperature (around 25°C) and a bending speed of 30 rpm for 200,000 bends.

[0074] (Comparative Example 2) A 50 μm thick adhesive layer is provided on the back side (back side of the flexible display layer) of the flexible organic EL display panel obtained from Comparative Example 1, and a support substrate (stainless steel plate, thickness: 30 μm, elastic modulus: approximately 193 GPa) is bonded and fixed through this adhesive layer. The bonding and fixing of the support substrate and the organic EL display panel includes the display area D and the bezel area N (bending area R). B and non-curved region R FThe entire area of ​​the organic EL display panel (the whole organic EL display panel) was subjected to drop impact and bending tests in the same manner as described above. Using an organic EL display device (foldable display) composed of a laminate in which a support substrate is bonded and fixed to the entire back of the organic EL display panel, the bending test was passed. However, the drop impact test failed due to point defects caused by damage to the TFT layer. Furthermore, as a reason for passing the bending test, in Comparative Example 2, because a relatively thick adhesive layer was provided, the adhesive layer slipped (deformed in the thickness direction), thus preventing damage caused by bending of the organic EL display panel.

[0075] (Comparative Example 3) Except for using an adhesive layer with a thickness of 5 μm or less, an organic EL display device (folding display) consisting of a laminate in which a support substrate is bonded and fixed to the entire back side of the organic EL display panel was manufactured in the same manner as Comparative Example 2, and drop impact test and bending test were performed in the same manner as described above. As a result, the organic EL display device according to Comparative Example 3 passed the drop impact test, but failed the bending test due to display defects caused by damage to the TFT layer.

[0076] (Comparative Example 4) On the back side of the flexible organic EL display panel obtained in Comparative Example 1 (the back side of the flexible display layer), an adhesive layer with a thickness of 50 μm is provided, which is formed in a frame shape and overlaps with the frame area N of the organic EL display panel when viewed from above. A support substrate identical to that in Comparative Example 2 is bonded and fixed through this adhesive layer. Next, an adhesive layer with a thickness of 50 μm is provided entirely on the back side of the support substrate, and a similar frame (made of metal, hereinafter referred to as "frame") having a hinge-like mechanism is bonded and fixed through this adhesive layer. The frame and the support substrate are connected in the display area D and the frame area N (bending area R). B and non-curved region R F The entire area (the entire organic EL display panel) is bonded and fixed.

[0077] In Comparative Example 4, the support substrate and the organic EL display panel are bonded and fixed only in the bezel region N (the entire area of ​​the bezel region N, along the entire perimeter of the bezel region N), while the display region D is not bonded and fixed. Furthermore, a gap of approximately 50 μm in thickness is formed between the two (hereinafter referred to as the "upper gap" in the embodiment).

[0078] Using the organic EL display device (folding display, a laminate in which the support substrate is not bonded to the back of the organic EL display panel in display area D) obtained above, drop impact test and bending test were performed in the same manner as described above. As a result, the organic EL display device according to Comparative Example 4 passed the bending test, but failed the drop impact test due to point defects caused by damage to the TFT layer. Furthermore, even when the thickness of the upper gap was set to 1200 μm, no improvement in impact resistance was observed.

[0079] (Example 1) Similar to Comparative Example 4, a support substrate identical to that in Comparative Example 2 was bonded to the back of the flexible organic EL display panel via a frame-shaped adhesive layer around the display area D, such that the thickness of the upper gap was approximately 50 μm. Next, a frame-shaped fixing member (a resin frame with a thickness of 300 μm) was formed on the back of the support substrate, overlapping the border area N of the organic EL display panel when viewed from above, and the same frame-shaped adhesive as in Comparative Example 4 was bonded and fixed via this fixing member. Furthermore, double-sided adhesive tape was used to fix the support substrate, frame, and fixing member.

[0080] In this embodiment, in display area D, not only are the support substrate and the organic EL display panel not bonded together, but the support substrate and the housing are also not bonded together, and a gap of approximately 300 μm in thickness (hereinafter referred to as the "lower gap" in this embodiment) is formed between them. Thus, in embodiment 1, in display area D, a lower gap and an upper gap are formed on the back side (lower surface) and the surface (upper surface) of the support substrate, respectively, and the total thickness of the two gaps is approximately 350 μm.

[0081] Using the organic EL display device obtained above (in the folding display, display area D, the display panel and support substrate are not fixed, and a laminate with a gap is formed between the support substrate and the housing), drop impact tests and bending tests were performed in the same manner as described above. As a result, the organic EL display device according to Example 1 passed both the drop impact test and the bending test. Therefore, in the organic EL display device of Example 1, both impact resistance to large point impacts and the bending resistance of the display panel can be balanced. Specifically, by further providing a gap of approximately 300 μm thickness (lower gap) between the support substrate and the frame, even when the total thickness of the gaps is less than 400 μm, an improvement in impact resistance is visible for the entire device.

[0082] <Effect> As explained above, the organic EL display device 70a according to this embodiment can achieve the following effects.

[0083] As mentioned above, in OLED display devices such as foldable displays, flexibility needs to be maintained. Therefore, OLED display panels are composed only of flexible components, and the following improvements are needed in this regard. (A) Poor impact resistance. (B) Due to the undulations and warping, it is relatively difficult to maintain the organic EL display panel in a flat shape. (C) The methods and means used to solve (A) and (B) above sometimes cannot maintain the flexibility of organic EL display panels.

[0084] (1) Regarding the above aspects, in the organic EL display device 70a, a support substrate 50 is provided on the underside of the flexible organic EL display panel 40. The support substrate 50 is made of a single plate in a manner that covers the entire organic EL display panel 40. Although it is flexible, by using a component with a high elastic modulus (for example, about 193 GPa), the shape of the organic EL display panel 40 can be kept flat, and undulations can be prevented (which can improve the point (B) above).

[0085] (2) In the organic EL display device 70a, in the display area D, the organic EL display panel 40 and the support substrate 50 are not fixed, and a gap G is formed by the support substrate 50 and the frame 60. Specifically, in the display area D, there is no adhesive layer or the like between the organic EL display panel 40 and the support substrate 50, and the organic EL display panel 40 and the support substrate 50 can bend independently of each other. That is, even if there is a difference in the amount of deflection due to the difference in elastic modulus, the organic EL display panel 40 and the support substrate 50 are not likely to affect each other. Moreover, there is a sufficient gap G on the underside of the support substrate 50 that can serve as an air buffer. As a result, even if the surface of the organic EL display panel 40 is subjected to a point impact of a size such as a pen stroke, since the support substrate 50 can bend smoothly and sufficiently, it is difficult to become a local impact, and the impact can be dispersed and mitigated (improving the point mentioned in (A) above). As a result, the inorganic film of the TFT layer 20 constituting the organic EL display panel 40 is less likely to crack, and the occurrence of display defects can be reduced.

[0086] (3) In the organic EL display device 70a, the flexibility of the organic EL display panel 40 is also maintained (which can improve the point mentioned in (C) above).

[0087] Therefore, in the organic EL display device 70a, both impact resistance against large point impacts and flexibility of the organic EL display panel 40 can be achieved simultaneously (solving the issues of (A), (B) and (C) mentioned above at the same time).

[0088] (5) In addition, the above-described modified example 1 is applied to the organic EL display device 70a. In any of the three cases, the curved region R on the adhesive layer 48 disposed between the organic EL display panel 40 and the support substrate 50, which overlaps with the bezel region N when viewed from above and includes the curved portion B. B Nearby, a pair of bezel area openings 48b, 48c, and 48d are formed. Since the organic EL display panel 40 and the support substrate 50 are not bonded together in the bezel area openings 48b, 48c, and 48d, even if there are differences in the amount of bending caused by the difference in their elastic moduli, they are unlikely to affect each other. Therefore, the flexibility of the organic EL display panel 40 can be further improved. In this case, the adhesive layer 48 can be made relatively thin (e.g., about 2 μm or more and about 50 μm less).

[0089] Second Implementation Method Next, the second embodiment of the present invention will be described. Figure 14 and Figure 15 A second embodiment of the display device according to the present invention is shown. Figure 14 This is a cross-sectional view showing the unfolded state of the organic EL display device 70b according to the second embodiment, which is equivalent to... Figure 3 The image. Figure 15 This is a cross-sectional view showing a modified example of the organic EL display device 70b in its unfolded state, which is equivalent to... Figure 3 The image.

[0090] The overall structure of the organic EL display device 70b is the same as that of the first embodiment described above, except for the structure between the organic EL display panel 40 and the support substrate 50; therefore, a detailed description is omitted here. Furthermore, the same reference numerals are used for components identical to those in the first embodiment, and their descriptions are omitted.

[0091] In the organic EL display device 70b, such as Figure 14 As shown, a metal thin film layer 45 is disposed between the organic EL display panel 40 and the support substrate 50. By disposing the metal thin film layer 45 on the back side of the organic EL display panel 40, point impacts on the surface of the organic EL display panel 40 are converted into surface impacts. The metal thin film layer 45 is preferably a component with a high elastic modulus (e.g., about 193 GPa), such as a material comprising at least one selected from stainless steel, titanium, aluminum, and copper. The thickness of the metal film layer 45 is, for example, 20 μm or more and 45 μm or less, preferably 25 μm or more and 35 μm or less. The elastic modulus of the metal film layer 45 is, for example, 100 GPa or more and 210 GPa or less, preferably 120 GPa or more and 200 GPa or less.

[0092] In the organic EL display device 70b, such as Figure 14As shown, the organic EL display panel 40 and the support substrate 50 are fixed on the frame area N of the organic EL display panel 40 through a metal thin film layer 45.

[0093] Specifically, such as Figure 14 As shown, an adhesive layer 44 is provided between the organic EL display panel 40 and the metal thin film layer 45, and the two are bonded and fixed by the adhesive layer 44. Examples of adhesive layers 44 include OCA, adhesive tape, and sponge pads. From the viewpoint of flexibility, it is preferable that the adhesive layer 44 is relatively thick and flexible, for example, with a thickness of 15 μm or more and 100 μm or less, and a shear modulus of elasticity of 500 kPa or less at 25°C. It should be noted that the adhesive layer 44 can be provided on the entire surface of the organic EL display panel 40 or the metal thin film layer 45 (full-surface bonding), or it can be provided on at least a portion of them (partial bonding). Alternatively, the adhesive layer 44 may not be provided (non-adhesive).

[0094] The metal thin film layer 45 and the support substrate 50 can be fixed using the same method as that used in the organic EL display device 70a (including the above-described variations 1 to 3) according to the first embodiment, where the organic EL display panel 40 and the support substrate 50 are fixed. Specifically, as... Figure 14 As shown, in the area (preferably the entire area) overlapping with the display area D when viewed from above, the metal thin film layer 45 and the support substrate 50 are not fixed. Furthermore, in the area (preferably the entire area) overlapping with the display area D when viewed from above, the metal thin film layer 45 and the support substrate 50 can simply be unfixed, and a gap may or may not be formed between them.

[0095] Variations of the Second Embodiment In the organic EL display device 70b, such as Figure 15 As shown, a buffer layer (impact absorption layer) 47 can be provided between the metal thin film layer 45 and the support substrate 50. By providing the buffer layer 47 on the lower layer of the metal thin film layer 45 (the back side of the organic EL display panel 40), the impacts received on the surface of the organic EL display panel 40 are absorbed by the buffer layer 47.

[0096] The buffer layer 47 is composed of a single layer or multiple layers comprising at least one layer selected from a flexible resin film layer, a graphite sheet layer, and a foam layer (foam). A preferred embodiment of the buffer layer 47 is a flexible resin film layer. Examples of flexible resin film layers include polyurethane resin films, etc., and the Young's modulus is preferably 1 GPa or less, more preferably 100 MPa or less. The buffer layer 47 may also be a laminate comprising a graphite sheet layer and / or a foam layer together with the flexible resin film layer. The presence of a graphite sheet layer provides a better heat dissipation effect for the organic EL display panel 40. The thickness of the buffer layer 47 is, for example, 25 μm or more and 500 μm or less, preferably 50 μm or more and 200 μm or less.

[0097] In this variation, such as Figure 15 As shown, in the frame area N of the organic EL display panel 40, the organic EL display panel 40 and the support substrate 50 are fixed by the metal film layer 45 and the buffer layer 47.

[0098] Specifically, such as Figure 15 As shown, an adhesive layer 46 is provided between the metal film layer 45 and the buffer layer 47, and the two are bonded and fixed together through the adhesive layer 46. Examples of adhesive layer 46 include OCA, adhesive tape, and sponge padding. From the viewpoint of flexibility, it is preferable that the adhesive layer 46 is relatively thick and flexible, for example, with a thickness of 15 μm or more and 50 μm or less, and a shear modulus of elasticity of 100 kPa or less at 25°C. It should be noted that the adhesive layer 46 may be provided on the entire surface of the metal film layer 45 or the buffer layer 47 (full-surface bonding), or it may be provided on at least a portion of them (partial bonding). Alternatively, the adhesive layer 46 may not be provided, and the buffer layer 47 may be constructed as a laminate that also includes the adhesive layer 46. Alternatively, the metal film layer 45 and the buffer layer 47 may not be bonded together.

[0099] The buffer layer 47 and the support substrate 50 can be fixed using the same method as that used in the organic EL display device 70a (including variations 1 to 3) according to the first embodiment described above, where the organic EL display panel 40 and the support substrate 50 are fixed. That is, as... Figure 15 As shown, in the area (preferably the entire area) overlapping with the display area D when viewed from above, the buffer layer 47 and the support substrate 50 are not fixed. Furthermore, in the area (preferably the entire area) overlapping with the display area D when viewed from above, the buffer layer 47 and the support substrate 50 need only be unfixed; a gap may or may not be formed between them.

[0100] As explained above, the organic EL display device 70b of this embodiment can achieve the following effects based on the effects described in (1) to (5).

[0101] (6) In the organic EL display device 70b, a metal thin film layer 45 is provided on the underside of the organic EL display panel 40. In the area overlapping with the display area D when viewed from above, the metal thin film layer 45 and the support substrate 50 are not fixed. As a result, point impacts can be transformed into surface impacts. Consequently, since the metal thin film layer 45 and the support substrate 50 bend gently, the impact resistance to large point impacts can be further improved.

[0102] (7) In the organic EL display device 70b, since there is a metal thin film layer 45 with high elastic modulus on the underside of the organic EL display panel 40, it is possible to further prevent the organic EL display panel 40 from wavy or warped.

[0103] (8) In the organic EL display device 70b, even when the thickness of the gap G between the support substrate 50 and the frame 60 is small, the impact resistance is as excellent as that of an organic EL display device without a metal thin film layer 45 (such as the organic EL display device 70a described above). That is, in the organic EL display device 70b, the thickness of the gap G can be reduced.

[0104] Furthermore, in the case of the modified example applied in the organic EL display device 70b, a buffer layer 47 serving as an impact-absorbing layer is provided below the metal thin film layer 45. In the area overlapping with the display area D when viewed from above, the buffer layer 47 and the support substrate 50 are not fixed. Therefore, even in the event of a large impact, the impact on the support substrate 50 disposed below the buffer layer 47 is mitigated. Thus, impact resistance can be further improved. In this case, the thickness of the void G can be further reduced.

[0105] Third Implementation Method Next, the third embodiment of the present invention will be described. Figures 16 to 18 A third embodiment of the display device involved in the present invention is shown. Figure 16 This is a cross-sectional view showing the unfolded state of the organic EL display device 70c according to the second embodiment, which is equivalent to... Figure 3 The image. Figure 17 This is an enlarged cross-sectional view showing the organic EL display device 70c folded into a U-shape, which is equivalent to... Figure 5 The image. Figure 18 This is an enlarged cross-sectional view showing the organic EL display device 70c folded into a teardrop shape, which is equivalent to... Figure 5 The picture

[0106] The overall structure of the organic EL display device 70c is the same as that of the second embodiment described above, except for the structure of the metal film layer 45; therefore, detailed descriptions are omitted here. Furthermore, the same reference numerals are used to denote components identical to those in the first and second embodiments, and their descriptions are omitted.

[0107] like Figures 16-18 As shown, in the organic EL display device 70c, similar to the organic EL display device 70b of the second embodiment described above, a metal thin film layer 45 is provided between the organic EL display panel 40 and the support substrate 50, but the difference lies in the fact that an opening is formed in the metal thin film layer 45. Furthermore, Figure 17 and Figure 18 The adhesive layers 44 and 46 and the frame 60 are omitted.

[0108] Specifically, such as Figure 16 Figure 18 As shown, the metal thin film layer 45 has a pair of openings (hereinafter also referred to as "metal openings") 45a, 45a, which are formed in the portion near the curved portion B in the frame regions N, N surrounding the pair of flat portions Fa, Fb, respectively. The pair of metal openings 45a, 45a are formed as slits extending along the bending axis C (direction Y) of the curved portion B. Furthermore, the slit-shaped metal openings 45a can be formed to both ends of the direction Y, or to near both ends of the direction Y. In addition, the metal openings 45a are not limited to slits extending in a straight line along the direction Y, and can also be formed as islands (dashed lines) along the direction Y.

[0109] like Figure 17 As shown, when the curved shape of the organic EL display panel 40 is U-shaped, a pair of metal openings 45a, 45a are arranged in a pair of flat portions Fa, Fb (non-curved regions RF) at portions corresponding to the curved portion B (curved region RB). Figure 18 As shown, when the curved shape of the organic EL display panel 40 is teardrop-shaped, a pair of metal openings 45a, 45a are disposed in a pair of flat portions Fa, Fb at portions corresponding to the inflection points of the outer and inner curved regions. For example... Figure 16 As shown, the metal thin film layer 45 is divided (separated) into multiple parts through a pair of metal openings 45a, 45a. Figure 16 There are three of them in the middle), arranged separately. As a result, the decrease in the flexibility of the organic EL display panel 40 caused by the metal thin film layer 45 can be suppressed.

[0110] Additionally, in the organic EL display device 70c, such as Figure 16 Figure 18 As shown, the buffer layer 47 (and adhesive layer 46) is provided on the lower layer of the metal thin film layer 45, but the buffer layer 47 (and adhesive layer 46) may not be provided.

[0111] As explained above, the organic EL display device 70c of this embodiment can achieve the following effects based on the effects described in (1) to (9) above.

[0112] (10) In the organic EL display device 70c, the metal thin film layer 45 disposed on the underside of the organic EL display panel 40 has a non-bending region R F In the middle and curved region R B A pair of metal openings 45a, 45a are formed in the corresponding portions nearby. As a result, the flexibility of the organic EL display panel 40 is further improved. In this case, even if the adhesive layer 44 disposed between the organic EL display panel 40 and the metal thin film layer 45 is relatively thin (for example, more than 5 μm and less than 45 μm), flexibility can still be ensured.

[0113] [Fourth Implementation Method] Next, the fourth embodiment of the present invention will be described. Figure 19 and Figure 20 A fourth embodiment of the display device according to the present invention is shown. Figure 19 This is a cross-sectional view showing the unfolded state of the organic EL display device 70d according to the second embodiment, which is equivalent to... Figure 3 The image. Figure 20 This is a top view showing the unfolded state of the support substrate 50 of the organic EL display device 70d.

[0114] The overall structure of the organic EL display device 70d is the same as that of the first to third embodiments described above, except for the structure of the support substrate 50; therefore, detailed descriptions are omitted here. Furthermore, the same reference numerals are used for components identical to those in the first to third embodiments, and their descriptions are omitted.

[0115] In the organic EL display device 70d, such as Figure 19 and Figure 20 As shown, an opening is formed on the support substrate 50. Specifically, the support substrate 50 has a portion that overlaps with the curved portion B when viewed from above (including the curved region R of the curved portion B). B at least one of the following: Figure 19 as well as Figure 20 There are 5 openings (hereinafter also referred to as "substrate openings") 50a. The substrate openings 50a are connected to the gaps G that are divided into the lower side of the support substrate 50.

[0116] When the support substrate 50 is relatively thin (e.g., less than about 100 μm (preferably 20 or more and less than 45 μm)) and the support substrate 50 is made of the same material as the metal film layer 45, such as Figure 20 As shown, the substrate opening 50a can also be formed in multiple ways. Figure 20 The five slits extend along the bending axis C (direction Y) of the curved portion B to near both ends in the direction of bending axis C. Furthermore, the substrate opening 50a is not limited to a slit extending linearly along direction Y; it can also be formed as an island (dashed line) along direction Y. In this case, as... Figure 20 As shown, in the buckling portion B, the outer sides of the support base plate 50 at both ends of the opening portion 50a of each base plate in the direction Y are connected to a direction (direction X) that is approximately orthogonal to the buckling axis C direction (without being separated).

[0117] In addition, the portion of the support substrate 50 with substrate opening 50a that overlaps with the curved portion B when viewed from above can also be formed in, for example, a curtain shape, a grid shape, a chain shape, a movable hinge shape (a ghost foot shape), etc.

[0118] On the other hand, when the support substrate 50 is thick (for example, about 100 μm or more and 200 μm or less), the substrate opening 50a can also be formed on the opening that overlaps with the curved portion B when viewed from above. In this case, the support substrate 50 can also be divided (separated) into two by the substrate opening 50a and arranged separately. In other words, the support substrates 50, 50 can be arranged on the portions corresponding to the flat portions Fa, Fb of the organic EL display panel 40.

[0119] Furthermore, in the organic EL display device 70d, such as Figure 19 As shown, a metal thin film layer 45 and a padding layer 47 (re-adhesive layers 44, 46) are provided between the organic EL display panel 40 and the support substrate 50. However, only the metal thin film layer 45 (and the adhesive layer 44) may be provided, or neither the metal thin film layer 45 nor the padding layer 47 (re-adhesive layers 44, 46) may be provided. In addition, a buffer layer with the same structure as the buffer layer 47 may be provided on the underside of the support substrate 50 where the substrate opening 50a is formed.

[0120] As explained above, the organic EL display device 70d of this embodiment can achieve the following effects based on the effects described in (1) to (10).

[0121] (11) In the organic EL display device 70d, at least one substrate opening 50a is formed on the support substrate 50 in the portion overlapping with the curved portion B when viewed from above. Therefore, even if the support substrate 50 is relatively thick (for example, it may be about 100 μm or more and about 200 μm or less), it can be slightly bent through the gap G that exists between the substrate opening 50a and the lower side of the support substrate 50. In addition, when the support substrate 50 is thick, it is possible to prevent undulation of the organic EL display panel 40.

[0122] Other Implementation Methods The configurations in the above embodiments can be appropriately combined and applied.

[0123] In the above embodiments, an organic EL layer with a five-layer stacked structure of hole injection layer, hole transport layer, light emission layer, electron transport layer and electron injection layer is illustrated. However, the organic EL layer may also be a three-layer stacked structure of hole injection layer as hole transport layer, light emission layer and electron transport layer as electron injection layer.

[0124] Furthermore, in the above embodiments, an organic EL display device is illustrated in which the first electrode is set as the anode and the second electrode is set as the cathode. However, the present invention can also be applied to an organic EL display device in which the stacked structure of the organic EL layer is reversed and the first electrode is set as the cathode and the second electrode is set as the anode.

[0125] In the above embodiments, an organic EL display device is illustrated in which the electrode of the TFT connected to the first electrode is designated as the drain electrode. However, the present invention can also be applied to organic EL display devices in which the electrode of the TFT connected to the first electrode is designated as the source electrode.

[0126] In the above embodiments, an organic EL display device was described as an example of a display device, but the present invention can be applied to display devices that include multiple light-emitting elements driven by current. For example, it can be applied to display devices that include QLED (quantum-dot light-emitting diode) light-emitting elements using a quantum dot layer. Industrial practicality

[0127] As explained above, the present invention can be used in flexible display devices, especially foldable displays. Explanation of reference numerals in the attached figures

[0128] B. Bend C Bending shaft D Display Area Fa, Fb flat parts G gap N border area P sub-pixel RB bending area RF non-bending region 40 Organic EL display panel (display panel) 41 Flexible Display Layer 42 Functional Layer 43 Cover 44 Adhesive layer 45 Metal thin film layer 45a Metal opening (opening) 46 Adhesive layer 47 Buffer Layer 48 Adhesive layer 48a Display area opening (opening) 48b, 48c, 48d: Openings in the border area (openings) 50 Support base plate 50a Substrate Opening (Opening) 55 Fixed components 60 frame Organic EL display devices 70a, 70b, 70c, 70d

Claims

1. A display device, characterized in that, include: The display panel is flexible and includes a display area and a bezel area. The display area is composed of a pair of flat portions that remain flat and a curved portion disposed between the pair of flat portions and remaining flexible. The bezel area is disposed around the display area. A support substrate that flatly supports the display panel; and The frame, which supports the supporting base plate, In the display area, the display panel and the supporting substrate are not fixed, and a gap is formed between the supporting substrate and the frame. A metal thin film layer is disposed between the display panel and the supporting substrate. The metal thin film layer and the supporting substrate are fixed only in the frame area. In the area that overlaps with the display area when viewed from above, the metal thin film layer and the supporting substrate are not fixed.

2. The display device according to claim 1, characterized in that, Throughout the entire display area, the display panel and the supporting substrate are not fixed, and a gap is formed between the supporting substrate and the frame.

3. The display device according to claim 1 or 2, characterized in that, An adhesive layer is disposed around the entire circumference of the frame region between the display panel and the supporting substrate. The display panel and the supporting substrate are bonded and fixed together by the adhesive layer.

4. The display device according to claim 3, characterized in that, The adhesive layer has a pair of openings formed in the portion of the curved region extending along the curved portion that overlaps with the border region when viewed from above.

5. The display device according to claim 4, characterized in that, The pair of openings are formed as slits extending along the bending axis of the curved region.

6. The display device according to claim 3, characterized in that, The adhesive layer has a pair of openings, which are respectively formed in the border region near the curved portion, and the border region is respectively disposed around the pair of flat portions. The pair of openings are formed as slits extending along the bending axis of the curved region.

7. The display device according to claim 1, characterized in that, The metal film has a pair of openings, which are respectively formed in the border region near the curved portion, and the border region is respectively disposed around the pair of flat portions. The pair of openings are formed as slits extending along the bending axis of the curved region.

8. The display device according to claim 1 or 7, characterized in that, An adhesive layer is provided between the display panel and the metal thin film layer. The display panel and the metal thin film layer are bonded and fixed together by the adhesive layer.

9. The display device according to any one of claims 1, 7, and 8, characterized in that, The metal thin film layer is composed of a material selected from stainless steel, titanium, aluminum and copper.

10. The display device according to any one of claims 1, 7 to 9, characterized in that, A buffer layer is provided between the metal thin film layer and the supporting substrate. In the area that overlaps with the display area when viewed from above, the buffer layer is not fixed to the supporting substrate.

11. The display device according to claim 10, characterized in that, An adhesive layer is provided between the metal thin film layer and the buffer layer. The metal thin film layer and the buffer layer are bonded and fixed together by the adhesive layer.

12. The display device according to claim 10 or 11, characterized in that, The buffer layer comprises at least one layer selected from flexible resin film layers, graphite sheet layers, and foam layers.

13. The display device according to any one of claims 10 to 12, characterized in that, The Young's modulus of the buffer layer is below 1 GPa.

14. The display device according to any one of claims 1 to 13, characterized in that, The portion of the support substrate that overlaps with the curved portion when viewed from above is formed in the shape of a curtain, a grid, a chain, or a movable hinge.

15. The display device according to any one of claims 1 to 13, characterized in that, The support substrate has at least one opening formed in the portion that overlaps with the curved portion when viewed from above.

16. The display device according to claim 15, characterized in that, The at least one opening is formed in the form of a slit, extending along the bending axis of the bend to near both ends of the bending axis direction of the support substrate.

17. The display device according to any one of claims 1 to 16, characterized in that, The support substrate comprises a flexible metal film.

18. The display device according to claim 17, characterized in that, The metal film is made of a material comprising at least one selected from stainless steel, titanium, aluminum and copper.

19. The display device according to claim 17 or 18, characterized in that, The support substrate is composed of a laminate, which further includes a flexible resin film.

Citation Information

Patent Citations

  • Foldable display

    WO2020203584A1

  • Foldable display

    WO2021111619A1