A method for detecting the after-arc withstand voltage of a C4F7N / CO2 mixed gas electrical circuit after deterioration.
By detecting the decomposition products of C₄F₇N/CO₂ mixed gas using gas chromatography-mass spectrometry, a linear relationship between the peak area ratio and the after-arc withstand voltage was established. This solved the problem of detecting the after-arc withstand voltage of C₄F₇N/CO₂ mixed gas after electrical disconnection degradation, and improved the accuracy of judging the degree of gas degradation and the assessment of equipment lifespan.
Patent Information
- Application Number
- CN202311275045.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-09-28
- Publication Date
- 2026-11-24
- Estimated Expiration
- 2043-09-28
AI Technical Summary
There are few existing technologies for research and testing methods on the post-arc withstand voltage of C₄F₇N and its mixed gases after electrical interruption degradation, making it difficult to accurately determine the degree of gas degradation, which affects electrical performance and arc extinguishing capability.
The decomposition products of the C₄F₇N/CO₂ mixed gas were detected by gas chromatography-mass spectrometry. A linear relationship between the peak area ratio of the decomposition products and the post-arc withstand voltage was established. The degree of gas degradation was determined by a fitting formula based on the peak area ratio of CF₄ and C₃F₅N.
It enables accurate detection of the post-arc withstand voltage of C₄F₇N/CO₂ mixed gas, improves the accuracy of judging the degree of gas degradation, and can reflect the degradation rate of the mixed gas, guiding equipment service life and power grid safety.
Smart Images

Figure CN117368662B_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the fields of high-voltage insulation technology and gas composition detection, and particularly to a method for detecting the after-arc withstand voltage of a C4F7N / CO2 mixed gas after electrical interruption degradation. Background Technology
[0002] Perfluoroisobutyronitrile (C4F7N) gas is a promising alternative to SF6. The first 220 kV C4F7N environmentally friendly gas insulation system is already in operation. Under high temperature and an electric field, C4F7N gas undergoes a decomposition reaction, generating various decomposition products. Some of these products negatively impact the electrical properties of C4F7N and its mixtures.
[0003] C4F7N / CO2 mixed gas is a new type of environmentally friendly insulating and arc-quenching gas used in electrical engineering power switches. During arc breaking, this gas deteriorates with the increase in the number of arc breaks, exhibiting phenomena such as decomposition and decreased breaking capacity. With the accumulation of usage factors such as the number of breaks and arcing time, the insulation performance and arc-quenching capacity of C4F7N and its mixed gas will also decrease accordingly, indicating that the gas will experience electrical performance degradation after prolonged operation in equipment.
[0004] C4F7N gas is characterized by its complex molecular structure, diverse decomposition products, and limited practical applications. Therefore, research on the electrical performance degradation of C4F7N and its mixtures is still in its initial stages, with few studies and methods available to assess the degree of degradation. Accurately determining the degree of degradation of C4F7N and its mixtures is crucial for engineering applications where C4F7N replaces SF6, for extending the service life of environmentally friendly gas insulation equipment, and for ensuring the safe operation of the power grid. The electrical breaking performance of a gas mixture is directly related to its degree of degradation. However, under different experimental conditions, the number of discharge cycles cannot directly indicate the degree of degradation. The post-arc withstand voltage of a gas mixture is a key parameter reflecting its breaking capacity; therefore, detecting the post-arc withstand voltage of the decomposition products of C4F7N / CO2 gas mixtures is essential. How to achieve this detection is currently a problem to be solved. Summary of the Invention
[0005] To address the limited research and methods available in existing technologies regarding the post-arc withstand voltage of C4F7N and its mixed gases after electrical interruption degradation, this invention aims to provide a method for detecting the post-arc withstand voltage of C4F7N / CO2 mixed gases after electrical interruption degradation. This method utilizes the types and peak areas of the decomposition products of the C4F7N / CO2 mixed gas after use to establish a linear relationship between the peak area ratio of the decomposition products and the highest post-arc withstand voltage of the mixed gas, thereby obtaining its post-arc withstand voltage after degradation.
[0006] To achieve the above objectives, the technical solution of the present invention is: a method for detecting the post-arc withstand voltage after electrical interruption degradation of a C4F7N / CO2 mixed gas, comprising the following steps:
[0007] S1: C4F7N and CO2 are filled into the gas ring network cabinet in a certain volume ratio to simulate an electrical breaking experiment, thereby obtaining the decomposition gas mixture of C4F7N / CO2 mixed gas.
[0008] S2: The decomposition gas mixture of the C4F7N / CO2 mixed gas obtained in step S1 is detected using gas chromatography-mass spectrometry (GC-MS). The obtained mass spectrum is compared with the mass spectrum in the mass spectrometry database. The retention times of each product are compared to determine the types of products produced after decomposition. The ratio of the peak area of CF4 to the peak area of C3F5N is calculated and denoted as R. The after-arc withstand voltage of the C4F7N and CO2 mixed gas is measured using a high-pressure probe based on the ratio. A fitting equation is established for each ratio and the after-arc withstand voltage of the C4F7N and CO2 mixed gas.
[0009] S3: Detect the mixed gas to be tested in the gas ring network cabinet using gas chromatography-mass spectrometry (GC-MS). Compare the mass spectra in the mass spectrometry database with the obtained mass spectra, and determine the types of products produced after decomposition by comparing the retention times of each product. Calculate the ratio of the peak area of CF4 to the peak area of C3F5N. Calculate the post-arc withstand voltage based on the ratio and the fitting equation obtained in step S2.
[0010] Furthermore, the molar ratio of perfluoroisobutyronitrile to carbon dioxide in the C4F7N / CO2 mixed gas is 15%:85% or 20%:80%;
[0011] For a 15% C4F7N-85% CO2 mixed gas, the ratio R of the peak area of CF4 to the peak area of C3F5N is between 4.7 and 8.1. The ratio of CF4 to C3F5N has a negative linear relationship with the highest withstand voltage after arcing of the 15% C4F7N-85% CO2 mixed gas.
[0012] For a 20% C4F7N-80% CO2 mixed gas, the ratio R of the peak area of CF4 to the peak area of C3F5N is between 7.22 and 9.02. The ratio of CF4 to C3F5N has a negative linear relationship with the highest withstand voltage after arcing of the 20% C4F7N-80% CO2 mixed gas.
[0013] Furthermore, the fitting formula for the peak area ratio of CF4 and C3F5N and the maximum withstand voltage after arc is established as follows:
[0014] For a 15% C4F7N-85% CO2 mixture, the fitting formula is:
[0015] U=-181.64R+3436.10, 7.22≤R≤9.02;
[0016] For a 20% C4F7N-80% CO2 mixed gas, the fitting formula is:
[0017] U=-128.02R+3154.67, 4.7≤R≤8.1;
[0018] In the fitting formula, U is the highest voltage withstand after the arc, V; R is the ratio of the peak area of CF4 to the peak area of C3F5N.
[0019] Furthermore, based on the synthetic circuit test system simulating the breaking process of a 12kV arc-extinguishing grid ring main unit under actual working conditions, the synthetic circuit test system includes a current source circuit simulating the large current during the arcing stage, a voltage source circuit simulating the high voltage during the recovery voltage stage, measuring components, and the ring main unit under test. The current source circuit and the voltage source circuit are connected in parallel and then connected in series with the ring main unit under test.
[0020] The current source circuit includes capacitor C1, inductor L1, switch K1, and auxiliary switch K2;
[0021] The voltage source circuit includes capacitor C2, inductor L2, trigger gap K3, frequency modulation resistor R1, and frequency modulation capacitor C3; capacitor C2, inductor L2, and trigger gap K3 are connected in series and then connected in parallel with frequency modulation resistor R1 and frequency modulation capacitor C3;
[0022] The measuring components include a resistive voltage divider RVDT, a high-voltage probe V, and a Rogowski coil Rog. There are two RVDTs, one of which, RVDT1, is used to measure the charging voltage of capacitor C2, and the other, RVDT2, is used to measure the charging voltage of capacitor C1. The high-voltage probe V is used to measure the break voltage of the ring main unit, and the Rogowski coil Rog is used to measure the branch current of the ring main unit.
[0023] Furthermore, in the gas chromatography-mass spectrometry (GC-MS) instrument, the chromatographic column model is GS-GASPRO (30m×0μm×0.32mm), and the splitless mode is adopted; the set detection conditions are: detector is gas chromatograph 6890N-mass spectrometer 5975, injector temperature is 100℃, injection needle capacity is 150μL, carrier gas is H2, hold at 40℃ for 1 min, increase the temperature to 160℃ at 20℃ / min, hold for 1 min, increase the temperature to 240℃ at 40℃ / min, hold for 10 min, and the total detection process lasts for 20 min.
[0024] In summary, the present invention has the following beneficial effects:
[0025] First, this application uses gas chromatography-mass spectrometry to detect the decomposition products of a mixture of perfluoroisobutyronitrile and carbon dioxide in a certain ratio after arc combustion. First, the types of decomposition products are determined by the mass-charge ratio of each gas. Then, the peak area of each product ion peak is obtained according to the mass spectrum. Then, the ratio of the chromatographic peak area of CF4 to C3F5N in the decomposition products is used to establish a fitting formula for the highest voltage withstand capability after arc of the perfluoroisobutyronitrile and carbon dioxide mixture. Based on the fitting formula, the highest voltage withstand capability after arc of the perfluoroisobutyronitrile and carbon dioxide mixture is determined. The breaking capacity of the mixture is inferred from the composition of the decomposition products of the perfluoroisobutyronitrile and carbon dioxide mixture.
[0026] Second, this application utilizes gas chromatography-mass spectrometry to detect the decomposition components of the mixed gas and establishes a fitting relationship between the peak area ratio of the decomposition products and the highest voltage that the perfluoroisobutyronitrile and carbon dioxide mixed gas can withstand after arc. The slope of the fitting formula can be used to predict the degradation rate of the mixed gas. Attached Figure Description
[0027] To more clearly illustrate the technical solutions in the embodiments of the present invention or the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.
[0028] Figure 1 This invention discloses a synthetic circuit testing system.
[0029] Figure 2 This invention discloses the chromatogram and a partial magnified image of the decomposition gas mixture to be tested after 140 breaking tests of a 15% C4F7N-85% CO2 mixed gas;
[0030] Figure 3 This invention discloses a graph showing the relationship between the maximum withstand voltage after arc of a 15% C4F7N-85% CO2 mixed gas and the peak area ratio of CF4 and several types of decomposition products.
[0031] Figure 4 This invention discloses a graph showing the relationship between the peak area ratio R of CF4 to C3F5N in a 15% C4F7N-85% CO2 mixed gas and the maximum withstand voltage U after arc.
[0032] Figure 5 This invention discloses the chromatogram and a partial magnified image of the decomposition gas mixture to be tested after 140 breaking tests of a 20% C4F7N-80% CO2 mixed gas mixture.
[0033] Figure 6 This invention discloses a graph showing the relationship between the highest withstand voltage after arc of a 20% C4F7N-80% CO2 mixed gas and the peak area ratio of CF4 and several types of decomposition products.
[0034] Figure 7 This invention discloses a graph showing the relationship between the peak area ratio R of CF4 and C3F5N in a 20% C4F7N-80% CO2 mixed gas and the maximum withstand voltage U after arc. Detailed Implementation
[0035] To make the objectives, technical solutions, and advantages of the embodiments of the present invention clearer, the following will be described in conjunction with the appendices in the embodiments of the present invention. Figure 1-7 The technical solutions in the embodiments of the present invention are clearly and completely described herein. Obviously, the described embodiments are only some, not all, of the embodiments of the present invention. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.
[0036] Example 1
[0037] A method for detecting the post-arc withstand voltage after electrical interruption degradation of a 15% C4F7N-85% CO2 mixed gas, comprising the following steps:
[0038] S1: Constructing a synthetic loop test system
[0039] Reference Figure 1 The synthetic loop test system includes a current source circuit simulating the high current during the arcing stage, a voltage source circuit simulating the high voltage during the recovery stage, measuring components, and the tested ring main unit. The measuring components include a resistor voltage divider RVDT1, a resistor voltage divider RVDT2, a high-voltage probe V, and a Rogowski coil Rog. The current source circuit includes a capacitor C1, an inductor L1, a switching switch K1, and an auxiliary switch K2. The voltage source circuit includes a capacitor C2, an inductor L2, a trigger gap SG, a frequency modulation resistor R1, and a frequency modulation capacitor C3. The voltage source circuit and the current source circuit are connected in parallel and then in series with the branch containing the ring main unit. In the voltage source circuit, the frequency modulation capacitor C3 is connected in parallel with the capacitor C2. The resistor voltage divider RVDT1 is used to measure the charging voltage of capacitor C2, and the resistor voltage divider RVDT2 is used to measure the charging voltage of capacitor C1. The high-voltage probe V is used to measure the break voltage of the ring main unit, and the Rogowski coil Rog is used to measure the branch current of the ring main unit.
[0040] S2: Simulated switching experiment
[0041] First, a C4F7N with a molar ratio of 15% and CO2 with 85% is charged into the ring main unit. Using the laboratory synthetic circuit test system constructed in step S1, the large current and high voltage generated in actual working conditions are simulated by the sequential operation of the current source circuit and voltage source circuit. First, the switching switch K1 is closed, controlling the working current of the current source circuit to pass sequentially through capacitor C1, switching switch K1, auxiliary switch K2, ring main unit, Rog coil Rog, inductor L1 and back to capacitor C1, to ignite the arc of the 12kV arc-extinguishing grid ring main unit. Before the arc of the ring main unit crosses zero, the auxiliary switch K2 is opened, and the trigger gap K3 is opened. The current of the voltage source circuit passes sequentially through capacitor C2, inductor L2, and returns to capacitor C2 through the tested ring main unit. At this time, there is a superposition of the currents of the current source circuit and the voltage source circuit on the branch of the ring main unit. When the arc of the ring main unit is extinguished, the auxiliary switch K2 has been opened, and the voltage source circuit has completed the circuit switching. At this time, the current passes sequentially through capacitor C2, inductor L2 and back to capacitor C2. L2, frequency modulation resistor R1, and frequency modulation capacitor C3 return to capacitor C2; since the frequency modulation resistor R1 and frequency modulation capacitor C3 are connected in parallel with the ring main unit, when the voltage applied to the frequency modulation resistor R1 and frequency modulation capacitor C3 reaches a certain value, the ring main unit's break point is broken down, causing the current to flow back through capacitor C2, inductor L2, and then through the tested ring main unit back to capacitor C2. The breakdown voltage at this point is recorded as the highest withstand voltage of the mixed gas. Although the recovery voltage applied to the frequency modulation resistor R1 and frequency modulation capacitor C3 will cause the ring main unit's break point to break down and the arc to reignite after the large current arc generated by the current source circuit, the arc current generated by the voltage source circuit has a small amplitude and high frequency. The energy generated by its arc is far less than the energy generated by the current source circuit's single arc. Therefore, in the experiment, only the arc of the ring main unit mainly involved by the current source circuit is counted as one effective arc. The above steps complete one breaking test, and the mixed gas in the ring main unit achieves one effective arc.
[0042] The test system simulates the interruption process of a 12kV arc-extinguishing grid ring main unit under actual operating conditions. Initially, the presence of current causes an arc to ignite in a C4F7N / CO2 mixed gas, releasing a large amount of energy. Under high temperature and electric field, the C4F7N / CO2 mixed gas decomposes into a gaseous mixture. During the zero-current region, the system's voltage recovery and the dielectric insulation recovery compete. When the voltage recovery exceeds the dielectric insulation recovery, the gaseous mixture breaks down, obtaining the post-arc withstand voltage. This process is repeated to achieve multiple arc ignitions. Samples of the decomposed gaseous mixtures obtained after different arc ignition cycles are analyzed, and the highest post-arc withstand voltage for each arc ignition cycle is recorded.
[0043] S3: Qualitative Analysis of Decomposition Products
[0044] The decomposition gas mixture obtained in step S2 was introduced into a gas chromatograph-mass spectrometer (GC-MS). The GC-MS was performed using an Agilent Technologies 6890N-5975 GC-MS instrument. Mass spectra of the decomposition gas mixture were obtained after each interruption test. The analytical conditions for the decomposition gas mixture were as follows: column parameters: GS-GASPRO (30m×0μm×0.32mm); splitless mode was used; the detection conditions were as follows: detector: GC-6890N-5975; injector temperature: 100℃; injection needle capacity: 150μL; carrier gas: H2; temperature: 40℃ for 1 min; temperature: increased to 160℃ at 20℃ / min; temperature: held for 1 min; temperature: increased to 240℃ at 40℃ / min; temperature: held for 10 min; total detection time: 20 min.
[0045] Figure 2 The chromatogram and partial magnified image of the decomposition gas mixture after 140 on / off tests of the 15% C4F7N-85% CO2 mixed gas are shown in Table 1. By comparing the mass spectra in the mass spectrometry database with the obtained mass spectra and comparing the retention times of each product, the types of products produced after discharge decomposition can be determined.
[0046] Table 1 Retention time of decomposition products
[0047] Decomposition products Retention time (min) <![CDATA[CF4]]> 1.157 <![CDATA[C3F8]]> 3.023 <![CDATA[C2F3N]]> 3.512 <![CDATA[C3F6]]> 3.890 <![CDATA[C4F 10 ]]> 4.665 <![CDATA[C3F5N]]> 4.845 <![CDATA[C2N2]]> 5.276
[0048] S4: Data Processing
[0049] Using the peak area of CF4 as a benchmark, the ratio of the peak area of CF4 to the peak areas of other decomposition products was calculated, and the highest arc withstand voltage U of the gas after the breaking test was recorded, as shown in Table 2.
[0050] Table 2140 shows the highest withstand voltage after arcing.
[0051]
[0052] Using the above table, a correspondence was established between the ratio R of the peak area of CF4 to several other types of decomposition products and the highest voltage U that the gas could withstand after the arc test. In order to intuitively obtain the correspondence between the ratio R of the peak area of CF4 to several other types of decomposition products and the highest voltage U that the gas could withstand after the arc test, the controlled variable method was used to statistically analyze the ratio between the peak areas of decomposition products and the highest voltage that could withstand after the arc under different arcing times, in order to obtain a linear ratio relationship between the ratio R of the peak area of CF4 to a certain decomposition product and the highest voltage U, as shown in Table 3.
[0053] Table 3
[0054]
[0055] Based on the data in Table 3, the following was obtained: Figure 3 and Figure 4 , Figure 3 The graph shows the relationship between the peak area of CF4 at different arcing times, the ratio of the peak areas of other decomposition products, and the maximum voltage withstandd after arcing.
[0056] Depend on Figure 3 It can be seen that only the peak area ratio of CF4 to C3F5N decreases monotonically with the increase of the maximum withstand voltage after the arc; based on the linear relationship between the peak area ratio of CF4 and different decomposition products and the maximum voltage, it can be determined that the peak area ratio R of CF4 to C3F5N and the maximum withstand voltage after the arc satisfy a good linear ratio relationship.
[0057] Figure 4 The graph shows the relationship between the peak area ratio R of CF4 and C3F5N and the maximum withstand voltage U after arcing; Figure 4 It can be seen that the fitting formula for the peak area ratio R of CF4 and C3F5N and the maximum withstand voltage U after arc is:
[0058] U = -181.64R + 3436.10, 7.22 ≤ R ≤ 9.02, where U is the highest withstand voltage after arc, in V; and R is the ratio of the peak area of CF4 to the peak area of C3F5N.
[0059] S5: Using the gas chromatography-mass spectrometry (GC-MS) instrument described in the above steps, and under the analytical conditions of step S3, detect the analyte mixture in the gas ring filter. Compare the mass spectra in the mass spectrometry database with the obtained mass spectra, and determine the types of products produced after decomposition by comparing the retention times of each product. Based on the ratio of the peak area of CF4 to the peak area of C3F5N, use... Figure 4 By fitting the equation to the standard curve shown in step S4, the highest voltage that the gas can withstand after the arc is obtained, which is used to determine the degree of degradation of the gas's electrical breaking capability.
[0060] Example 2
[0061] A method for detecting the after-arc withstand voltage of an electrical circuit breaker after degradation due to a 20% C4F7N-80% CO2 mixed gas, comprising the following steps:
[0062] S1: Same as Example 1;
[0063] S2: Simulated switching experiment
[0064] First, a ring main unit with a molar ratio of 20% C4F7N and 80% CO2 is charged into the ring main unit. Using the laboratory synthetic circuit test system constructed in step S1, the large current and high voltage generated in actual working conditions are simulated by the sequential operation of the current source circuit and voltage source circuit. First, the switching switch K1 is closed, and the operating current of the current source circuit is controlled to pass sequentially through capacitor C1, switching switch K1, auxiliary switch K2, ring main unit, Rog coil Rog, inductor L1 and back to capacitor C1 to ignite the arc of the 12kV arc-extinguishing grid ring main unit. Before the arc of the ring main unit crosses zero, the auxiliary switch K2 is opened, and the trigger gap K3 is opened. The current of the voltage source circuit passes sequentially through capacitor C2, inductor L2, and returns to capacitor C2 through the tested ring main unit. At this time, there are current source circuit and voltage source circuit on the branch of the ring main unit. The currents of the two circuits are superimposed. When the arc of the ring main unit is extinguished, the auxiliary switch K2 is opened, and the voltage source circuit completes the circuit switching. At this time, the current flows sequentially through capacitor C2, inductor L2, frequency modulation resistor R1, and frequency modulation capacitor C3 back to capacitor C2. Since the frequency modulation resistor R1 and frequency modulation capacitor C3 are connected in parallel with the ring main unit, when the voltage applied to the frequency modulation resistor R1 and frequency modulation capacitor C3 reaches a certain value, the ring main unit is broken down, causing the current to flow through capacitor C2 and inductor L2 again, and then through the tested ring main unit back to capacitor C2. The breakdown voltage at this time is recorded as the highest withstand voltage of the mixed gas. The above operation is repeated to achieve multiple arcing. The decomposed gas mixture obtained under different arcing times is sampled and analyzed, and the highest withstand voltage after the arc is recorded for the corresponding number of arcing times.
[0065] S3: Same as Example 1
[0066] Figure 5 The chromatogram and partial magnified image of the decomposition gas mixture after 140 on / off tests of the 20% C4F7N-80% CO2 mixed gas are shown in Table 1. By comparing the mass spectra in the mass spectrometry database with the obtained mass spectra and comparing the retention times of each product, the types of products produced after discharge decomposition can be determined.
[0067] S4: Same as Example 1
[0068] Table 4 shows the linear relationship between the peak area ratio R of CF4 and a certain decomposition product and the maximum voltage U.
[0069] Table 4
[0070]
[0071] Based on the data in Table 4, the following was obtained: Figure 6 and Figure 7 , Figure 6 The graph shows the relationship between the peak area of CF4 at different arcing times, the ratio of the peak areas of other decomposition products, and the maximum voltage withstandd after arcing.
[0072] Depend on Figure 6 It can be seen that the peak area ratios of CF4 and C3F5N, and CF4 and C3F8 decrease monotonically with the increase of the maximum withstand voltage after the arc. Based on the linear relationship between the peak area ratios of CF4 and different decomposition products and the maximum voltage, it can be determined that the peak area ratio R of CF4 and C3F5N satisfies a good linear relationship with the maximum withstand voltage after the arc.
[0073] Figure 7 The graph shows the relationship between the peak area ratio R of CF4 and C3F5N and the maximum withstand voltage U after arcing; Figure 7 It can be seen that the fitting formula for the peak area ratio R of CF4 and C3F5N and the maximum withstand voltage U after arc is:
[0074] U = -128.02R + 3154.67, 4.7 ≤ R ≤ 8.1, where U is the highest withstand voltage after arc, in V; and R is the ratio of the peak area of CF4 to the peak area of C3F5N.
[0075] S5: Same as Example 1.
[0076] In summary, combining Figure 6 and Figure 7 It can be seen that the change in the peak area ratio between decomposition products shows a good correlation with the maximum withstand voltage after arc, providing a reliable basis for judging gas degradation. Furthermore, based on the slope of the peak area ratio of CF4 and C3F5N and the maximum withstand voltage after arc of the mixed gas, it can be determined that the degradation rate of the 20% C4F7N-80% CO2 mixed gas is slower than that of the 15% C4F7N-85% CO2 mixed gas. This indicates that the correlation between the mixed gas ratio R and the maximum withstand voltage U can be used to compare the gas degradation rate.
[0077] This invention utilizes gas chromatography-mass spectrometry (GC-MS) to detect the decomposition components of a gas mixture and establishes a linear relationship between the types of decomposition products, their peak area ratios, and the maximum withstand voltage after arcing of the gas mixture. This allows for the determination of the degradation of the breaking capacity of the C4F7N / CO2 gas mixture. The electrical breaking performance of a gas mixture is directly related to its degree of degradation. However, under different experimental conditions, the number of discharges does not directly indicate the degree of gas degradation. This invention uses the ratio of decomposition products to inversely deduce the maximum withstand voltage after arcing, thus improving the accuracy of degradation assessment. Furthermore, the slope of the fitting formula between the peak area ratio and the maximum withstand voltage after arcing reflects the degradation rate of the gas mixture itself, allowing for comparison of degradation rates for gas mixtures with different proportions. This conclusion provides product optimization solutions for the practical application and service life of C4F7N / CO2 gas mixtures in 12kV arc-extinguishing grid ring main units, solving the problem of difficulty in assessing the degree of degradation of the electrical breaking capacity of C4F7N / CO2 gas mixtures in 12kV arc-extinguishing grid ring main units.
[0078] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, and not to limit them; although the present invention has been described in detail with reference to the foregoing embodiments, those skilled in the art should understand that modifications can still be made to the technical solutions described in the foregoing embodiments, or equivalent substitutions can be made to some or all of the technical features; and these modifications or substitutions do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present invention.
Claims
1. A method of detecting the post-arc resistance voltage after degradation of an electrical break of a C4F7N / CO2 gas mixture, characterized in that, Includes the following steps: S1: C4F7N and CO2 are filled into the gas ring network cabinet in a certain volume ratio to simulate an electrical breaking experiment, thereby obtaining the decomposition gas mixture of C4F7N / CO2 mixed gas. S2: The decomposition gas mixture of the C4F7N / CO2 mixed gas obtained in step S1 is detected using gas chromatography-mass spectrometry (GC-MS). The obtained mass spectrum is compared with the mass spectrum in the mass spectrometry database. The retention times of each product are compared to determine the types of products produced after decomposition. The ratio of the peak area of CF4 to the peak area of C3F5N is calculated and denoted as R. The after-arc withstand voltage of the C4F7N and CO2 mixed gas at the given ratio is measured using a high-pressure probe and denoted as U. A fitting equation is established based on different ratios and the after-arc withstand voltage of the C4F7N and CO2 mixed gas. S3: Detect the mixed gas to be tested in the gas ring network cabinet using gas chromatography-mass spectrometry (GC-MS). Compare the mass spectra in the mass spectrometry database with the obtained mass spectra, and determine the types of products produced after decomposition by comparing the retention times of each product. Calculate the ratio of the peak area of CF4 to the peak area of C3F5N. Calculate the post-arc withstand voltage based on the ratio and the fitting equation obtained in step S2.
2. The method for detecting the after-arc withstand voltage of a C4F7N / CO2 mixed gas after electrical disconnection degradation according to claim 1, characterized in that, The molar ratio of perfluoroisobutyronitrile to carbon dioxide in the C4F7N / CO2 mixed gas is 15%:85% or 20%:80%. For a 15% C4F7N-85% CO2 mixed gas, the ratio R of the peak area of CF4 to the peak area of C3F5N is between 4.7 and 8.
1. The ratio of CF4 to C3F5N has a negative linear relationship with the withstand voltage after arcing of the 15% C4F7N-85% CO2 mixed gas. For a 20% C4F7N-80% CO2 mixed gas, the ratio R of the peak area of CF4 to the peak area of C3F5N is between 7.22 and 9.
02. The ratio of CF4 to C3F5N has a negative linear relationship with the withstand voltage after arcing of the 20% C4F7N-80% CO2 mixed gas.
3. The method for detecting the after-arc withstand voltage of a C4F7N / CO2 mixed gas after electrical disconnection degradation according to claim 2, characterized in that, The fitting formula for the peak area ratio of CF4 and C3F5N and the post-arc withstand voltage is as follows: For a 15% C4F7N-85% CO2 mixture, the fitting formula is: U=-181.64R+3436.10, 7.22≤R≤9.02; For a 20% C4F7N-80% CO2 mixed gas, the fitting formula is: U=-128.02R+3154.67, 4.7≤R≤8.1; In the fitting formula, U is the post-arc withstand voltage, V; R is the ratio of the peak area of CF4 to the peak area of C3F5N.
4. The method for detecting the after-arc withstand voltage of a C4F7N / CO2 mixed gas after electrical disconnection degradation according to claim 1, characterized in that, A synthetic circuit test system was used to simulate the breaking process of a 12kV arc-extinguishing grid ring main unit under actual working conditions. The synthetic circuit test system includes a current source circuit simulating the large current during the arcing stage, a voltage source circuit simulating the high voltage during the recovery stage, measuring components, and the ring main unit under test. The current source circuit and the voltage source circuit are connected in parallel and then connected in series with the ring main unit under test. The current source circuit includes capacitor C1, inductor L1, switch K1, and auxiliary switch K2; The voltage source circuit includes capacitor C2, inductor L2, trigger gap K3, frequency modulation resistor R1, and frequency modulation capacitor C3; capacitor C2, inductor L2, and trigger gap K3 are connected in series and then connected in parallel with frequency modulation resistor R1 and frequency modulation capacitor C3; The measuring components include a resistive voltage divider RVDT, a high-voltage probe V, and a Rogowski coil Rog. There are two RVDTs, one of which is used to measure the charging voltage of capacitor C2, and the other is used to measure the charging voltage of capacitor C1. The high-voltage probe V is used to measure the voltage at the break point of the ring main unit, and the Rogowski coil Rog is used to measure the current of the ring main unit.
5. The method for detecting the after-arc withstand voltage of a C4F7N / CO2 mixed gas after electrical disconnection degradation according to claim 1, characterized in that, In the gas chromatography-mass spectrometry (GC-MS) system, the chromatographic column model is GS-GASPRO, 30m×0μm×0.32mm, and the splitless mode is used. The detection conditions are set as follows: detector is gas chromatograph 6890N-mass spectrometer 5975, injector temperature is 100℃, injection needle capacity is 150μL, carrier gas is H2, temperature is maintained at 40℃ for 1 min, temperature is increased to 160℃ at 20℃ / min, held for 1 min, temperature is increased to 240℃ at 40℃ / min, held for 10 min, and the total detection process lasts for 20 min.
Citation Information
Patent Citations
Ring main unit C4F7N mixed gas detection method and device
CN114527081A
Overheat fault analysis method based on insulating gas fault simulation detection platform
CN116008712A