负极组合物、负极浆料、负极极片、二次电池及含有该二次电池的用电装置

By using POSS block copolymers and polyester plasticizers with specific structures in the negative electrode composition of secondary batteries, the cracking problem of the negative electrode film layer as the thickness and speed increase are solved, achieving a balance between high energy density and good cycle performance.

CN117378062BActive Publication Date: 2026-07-17CONTEMPORARY AMPEREX TECHNOLOGY CO LTD

Patent Information

Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
CONTEMPORARY AMPEREX TECHNOLOGY CO LTD
Filing Date
2022-03-04
Publication Date
2026-07-17

AI Technical Summary

Technical Problem

In the process of increasing the thickness of the negative electrode film and the coating speed to improve the energy density, existing secondary batteries are prone to problems such as film cracking, difficulty in electrolyte wetting, and poor kinetics, which affect cycle performance and safety.

Method used

A negative electrode composition is formed by using a block copolymer containing POSS and a polyester containing -[O-CH(CH3)-C(=O)]- structural units as plasticizers, combined with an organic solvent with a boiling point of 160℃~250℃. The plasticizer is uniformly dispersed in the polymer binder and CMC molecular network, reducing strong hydrogen bonding, improving flexibility and electrolyte affinity, and reducing drying stress.

Benefits of technology

It effectively reduces the brittleness of the negative electrode film, reduces cracking, improves electrolyte wetting performance and lithium-ion conductivity, enhances the cycle performance and rate performance of secondary batteries, and maintains stable electrochemical performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117378062B_ABST
    Figure CN117378062B_ABST
Patent Text Reader

Abstract

本申请公开了一种负极组合物、负极浆料、负极极片、二次电池及含有该二次电池的用电装置,该负极组合物包括负极活性材料以及增塑剂,所述增塑剂包括第一增塑剂以及可选的第二增塑剂,所述第一增塑剂包括含有POSS的嵌段共聚物、含有‑[O‑CH(CH3)‑C(=O)]‑结构单元的聚酯中的至少一种,所述第二增塑剂包括沸点Tm为160℃~250℃的有机溶剂。