Vessels and grilling apparatus

By setting a medium layer inside the vessel, the problem of uneven temperature in the vessel is solved, achieving uniform temperature distribution and rapid heating, thus improving the cooking effect and safety of the food.

CN117378938BActive Publication Date: 2026-11-24FOSHAN SHUNDE MIDEA ELECTRICAL HEATING APPLIANCES MFG CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202210794605.7
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-07-05
Publication Date
2026-11-24
Estimated Expiration
2042-07-05

AI Technical Summary

Technical Problem

Existing cookware suffers from uneven temperature during heating, with higher temperatures near the heating element and lower temperatures further away, resulting in poor cooking outcomes.

Method used

A medium layer is placed inside the vessel body. The medium layer is made of heat storage material with a thermal conductivity to thickness ratio greater than or equal to 2. The medium layer absorbs and stores heat energy, and distributes and regulates the temperature evenly.

Benefits of technology

It achieves a uniform temperature distribution within the vessel, reduces the temperature difference between the cooking and heating sides, improves the cooking effect and safety of the food, and reduces the risk of overheating.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117378938B_ABST
    Figure CN117378938B_ABST
Patent Text Reader

Abstract

This application discloses a utensil and a grilling device. The utensil includes: a utensil body; and a medium layer disposed within the utensil body, the medium layer being made of a heat-storing material. Where the thermal conductivity is expressed in W / mK and the thickness in mm, the ratio of the thermal conductivity to the thickness of the medium layer is greater than or equal to 2. The utensil provided in this application, by having a ratio of thermal conductivity to thickness of the medium layer greater than or equal to 2, ensures the thermal conductivity efficiency of the medium layer, guarantees its thermal conductivity effect, and ensures that the utensil body can heat up quickly while maintaining uniform temperature and latent heat, thereby reducing the user's waiting time.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application relates to the field of household appliance technology, and more particularly to a utensil and a grilling device. Background Technology

[0002] In everyday household appliances, utensils can be heated by heat pipes, heating plates, or electromagnetic heating. The temperature of the utensils is generally higher when they are close to the heating element and lower when they are farther away from the heating element, resulting in a large temperature difference on the surface of the utensils. Summary of the Invention

[0003] The present invention aims to solve at least one of the technical problems existing in the prior art or related art.

[0004] Therefore, a first aspect of the present invention provides a vessel.

[0005] A second aspect of the present invention provides a frying and grilling apparatus.

[0006] In view of this, a vessel is provided according to a first aspect of the embodiments of this application, comprising:

[0007] The vessel itself;

[0008] A medium layer is disposed within the vessel body, and the medium layer is made of a heat storage material;

[0009] Where the unit of thermal conductivity is W / mK and the unit of thickness is mm, the ratio of the thermal conductivity of the dielectric layer to the thickness of the dielectric layer is greater than or equal to 2.

[0010] In one feasible implementation, when the thermal conductivity is in W / mK and the thickness is in mm, the ratio of the thermal conductivity of the dielectric layer to the thickness of the dielectric layer is less than or equal to 20.

[0011] In one feasible implementation, the thermal conductivity of the dielectric layer is between 5 W / mK and 30 W / mK.

[0012] In one feasible implementation, the thickness of the dielectric layer is 1 mm to 5 mm.

[0013] In one feasible implementation, the heat storage material is a phase change material.

[0014] In one feasible implementation, the phase change material is a molten salt, and / or

[0015] The phase transition temperature of the phase change material is 180°C to 200°C, and / or

[0016] The phase change material has a compression density of 0.85 g / cm³. 3Up to 1.75 g / cm 3 between.

[0017] In one feasible implementation, the vessel body includes:

[0018] A sealing plate and a cooking plate, wherein the sealing plate is connected to the cooking plate, a gap is formed between the cooking plate and the sealing plate, and the medium layer is disposed within the gap.

[0019] In one feasible implementation, the vessel further includes:

[0020] Side panels are connected to the periphery of the cooking board and together with the cooking board form a cooking space.

[0021] In one possible implementation, the sealing plate and the cooking plate are made of metal.

[0022] According to a second aspect of the embodiments of this application, a grilling apparatus is provided, comprising:

[0023] The vessel as described in any of the above technical solutions.

[0024] In one feasible implementation, the grilling apparatus further includes:

[0025] A heating element is provided, and the dish is disposed on the heating element. When the grilling equipment is in operation, the temperature difference between the side of the dish closest to the heating element and the side furthest from the heating element is less than or equal to 120 degrees Celsius.

[0026] In one feasible implementation, when the grilling equipment is in operation, the temperature of the side of the dish closest to the heating element is less than or equal to 300 degrees Celsius.

[0027] In one feasible implementation, the difference between the phase change temperature of the medium layer and the minimum cooking temperature of the heating element is 0 to 20 degrees Celsius.

[0028] In one feasible implementation, the difference between the maximum cooking temperature of the heating component and the phase transition temperature of the medium layer is 0 to 10 degrees Celsius.

[0029] In one possible implementation, the heating element is attached to the vessel.

[0030] Compared with the prior art, the present invention has at least the following beneficial effects: The utensil provided in the embodiments of this application includes a utensil body and a medium layer disposed within the utensil body. The medium layer is made of a heat storage material. During the cooking process in the utensil, the heating component that provides heat energy to the utensil first transfers the heat energy to one side of the utensil body, and then the heat energy is transferred to the medium layer via a sealing plate. On the one hand, the medium layer can absorb and store the heat energy from the heating component, making the heat energy distribution within the medium layer more uniform. Then, the medium layer exchanges heat with the side of the utensil body closest to the food. This allows for a more even temperature distribution within the vessel, improving the cooking results. Furthermore, the medium layer absorbs heat; when a localized area of ​​the vessel is too cold, the medium layer releases the absorbed latent heat to heat that area. For example, when new food is added to the vessel, a significant temperature difference occurs between the vessel and the food. In this case, the food quickly absorbs heat from the vessel, causing a rapid drop in temperature at the contact point. The medium layer then releases its latent heat to regulate the temperature of the vessel. In the embodiments of this application, the ratio of the thermal conductivity of the medium layer to its thickness is greater than or equal to 2, provided the thermal conductivity is measured in W / mK and the thickness in mm. It is understandable that the thermal conductivity and thickness of the medium layer are related to its temperature uniformity and the heating efficiency of the container body on the side in contact with the food. A higher ratio of thermal conductivity to thickness results in better thermal conductivity but reduced temperature uniformity; conversely, a lower ratio results in lower thermal conductivity but stronger temperature uniformity. A ratio of thermal conductivity to thickness greater than or equal to 2 ensures efficient thermal conductivity, guaranteeing the container body can heat up quickly while maintaining both uniform temperature and latent heat, thus reducing user waiting time. Furthermore, the thermal conductivity and thickness of the medium layer are related to the temperature uniformity and the heating efficiency of the food contact side. The temperature uniformity of the medium layer is related to the heating efficiency of the side of the vessel body in contact with the food. The larger the ratio of thermal conductivity to thickness, the better the thermal conductivity of the medium layer and the lower the temperature uniformity. The smaller the ratio of thermal conductivity to thickness, the lower the thermal conductivity of the medium layer and the stronger the temperature uniformity. By making the ratio greater than or equal to 2, the heating efficiency is controlled, which can reduce the temperature difference between the cooking side and the heating side of the vessel body. It can control the temperature difference between the cooking side and the heating side of the vessel body within 120℃, which is conducive to the transfer of heat to the cooking surface and allows the cooking surface to reach the cooking temperature. On the other hand, it reduces the risk of cooking interruption caused by overheating at the contact surface between the vessel body and the heating element. Attached Figure Description

[0031] Various other advantages and benefits will become apparent to those skilled in the art upon reading the following detailed description of preferred embodiments. The accompanying drawings are for illustrative purposes only and are not intended to limit the scope of this application. Furthermore, the same reference numerals denote the same parts throughout the drawings.

[0032] In the attached diagram:

[0033] Figure 1 A schematic structural diagram of a vessel from one angle, according to one embodiment of this application;

[0034] Figure 2 A schematic structural diagram of a vessel from another angle, representing one embodiment of this application;

[0035] Figure 3 A schematic structural diagram of a vessel from another angle, according to one embodiment of this application;

[0036] Figure 4 A schematic structural diagram of the disassembled state of a vessel according to one embodiment of this application.

[0037] in, Figures 1 to 4 The correspondence between the reference numerals and component names in the attached drawings is as follows:

[0038] 100 vessel body, 200 medium layer;

[0039] 110 sealing plate, 120 cooking plate, 130 side plate. Detailed Implementation

[0040] To better understand the above technical solutions, the technical solutions of the embodiments of this application will be described in detail below with reference to the accompanying drawings and specific embodiments. It should be understood that the embodiments of this application and the specific features in the embodiments are detailed descriptions of the technical solutions of the embodiments of this application, rather than limitations on the technical solutions of this application. In the absence of conflict, the embodiments of this application and the technical features in the embodiments can be combined with each other.

[0041] like Figures 1 to 4 As shown, a vessel is provided according to a first aspect of the embodiments of this application, comprising: a vessel body 100; a medium layer 200 disposed within the vessel body 100, the medium layer 200 being made of a heat storage material; wherein, when the unit of thermal conductivity is W / mK and the unit of thickness is mm, the ratio of the thermal conductivity of the medium layer 200 to the thickness of the medium layer 200 is greater than or equal to 2.

[0042] The utensil provided in this embodiment includes a utensil body 100 and a medium layer 200 disposed within the utensil body 100. The medium layer 200 is made of a heat storage material. During cooking in the utensil, the heating component that provides heat energy to the utensil first transfers heat energy to one side of the utensil body 100, and then the heat energy is transferred to the medium layer 200 via the sealing plate 110. On the one hand, the medium layer 200 can absorb and store the heat energy from the heating component, making the heat energy distribution within the medium layer 200 more uniform. Then, the medium layer 200 exchanges heat with the side of the utensil body 100 closest to the food, enabling the utensil body 100 to... The temperature distribution is more even, which is conducive to improving the cooking effect of the ingredients. On the other hand, the medium layer 200 absorbs heat energy. When the local temperature on the vessel body 100 is too low, the medium layer 200 can release the absorbed latent heat to heat the lower temperature area of ​​the vessel body 100. For example, when new ingredients are put into the vessel body 100, the temperature difference between the vessel body 100 and the ingredients is large. In this case, the ingredients will quickly absorb the heat energy of the vessel body 100, causing the temperature at the contact point between the vessel body 100 and the newly put ingredients to drop rapidly. In this case, the medium layer 200 can release latent heat to regulate the temperature of the vessel body 100.

[0043] In this embodiment, with thermal conductivity measured in W / mK and thickness in mm, the ratio of the thermal conductivity to the thickness of the dielectric layer 200 is greater than or equal to 2. It is understood that the thermal conductivity and thickness of the dielectric layer 200 are related to its temperature uniformity and the heating efficiency of the container body 100 on the side in contact with the food. A higher ratio of thermal conductivity to thickness results in better thermal conductivity and reduced temperature uniformity of the dielectric layer 200; conversely, a lower ratio results in reduced thermal conductivity and stronger temperature uniformity. By ensuring that the ratio of the thermal conductivity to thickness of the dielectric layer 200 is greater than or equal to 2, the thermal conductivity of the dielectric layer 200 can be guaranteed to be good. Thermal efficiency ensures the heat conduction effect of the medium layer 200, ensuring that the vessel body 100 can heat up quickly while having uniform temperature and latent heat effect, so as to reduce the user's waiting time; it can reduce the temperature difference between the cooking side and the heating side of the vessel body 100, and can control the temperature difference between the cooking side and the heating side of the vessel body 100 within 120°C, which is conducive to the transfer of heat to the cooking surface, so that the cooking surface reaches the cooking temperature. On the other hand, it reduces the risk of cooking interruption caused by overheating of the contact surface between the vessel body and the heating element.

[0044] It is understood that the explanation of the units of thermal conductivity and thickness in this application is only to determine the order of magnitude between thermal conductivity and thickness. The proportional relationship defined in this application can be obtained by conversion through other units and is also within the scope of protection of this application.

[0045] Considering that the performance of the heating element is limited when heating the vessel, and that the electrical control devices and components of the heating element may melt, be damaged, or fail when the temperature of the contact side between the heating element and the vessel exceeds 300°C, the temperature of the contact side between the heating element and the vessel is usually kept below 300°C. Furthermore, the cooking process requires a specific temperature for the vessel body 100; the temperature of the side of the vessel body 100 in contact with the food must generally reach above the boiling point of water, typically between 180°C and 200°C, which meets the cooking requirements for most foods. Therefore, to ensure effective cooking, a temperature difference ΔT between the temperature T1 of the vessel body 100 near the heating element and the temperature T2 of the vessel body 100 near the food is required, and ΔT is typically less than or equal to 120°C.

[0046] Based on this, if the thickness of the dielectric layer 200 is greater, it will increase the difficulty of heat transfer within the dielectric layer 200, thus increasing the value of ΔT. The vessel provided in this embodiment of the application...

[0047] In this embodiment, the ratio of the thermal conductivity of the medium layer 200 to the thickness of the medium layer 200 is greater than or equal to 2. This allows for the adjustment of the temperature difference ΔT between the side of the vessel body 100 near the heating element and the side of the vessel body 100 near the food, ensuring that the value of ΔT can be greater than or equal to 120°C. This ensures that when the heating element provides heat energy to the vessel, the contact side between the vessel and the food has sufficient temperature to cook the food.

[0048] In some examples, where the thermal conductivity is measured in W / mK and the thickness is measured in mm, the ratio of the thermal conductivity of the dielectric layer 200 to the thickness of the dielectric layer 200 is less than or equal to 6.

[0049] The vessel provided in this application embodiment has a thermal conductivity of medium layer 200 with a ratio of less than or equal to 6 to its thickness. It can be understood that the heat conduction time of medium layer 200 is related to the thickness of medium layer 200 and its own thermal conductivity. If the thickness of medium layer 200 is greater, the time required for heat energy to be transferred to the side of the vessel body 100 in contact with the food is longer. By having a ratio of the thermal conductivity of the vessel to the thickness of medium layer 200 of less than or equal to 6, it can be ensured that the medium layer 200 can achieve a uniform temperature effect while the vessel body 100 can heat up quickly, thereby improving the heating efficiency of the vessel, especially in the initial stage of heating the vessel by the heating element.

[0050] It is understandable that if the ratio of the thermal conductivity of the medium layer 200 to the thickness of the medium layer 200 is greater than 6, the heat conduction time of the medium layer 200 will be too long when the heating component heats the vessel, resulting in a slow temperature rise on the side of the vessel body 100 that is in contact with the food, which will increase the user's waiting time.

[0051] In some examples, the thermal conductivity of the dielectric layer 200 is between 5 W / mK and 30 W / mK.

[0052] In this technical solution, the thermal conductivity of the medium layer 200 is 5W / mK to 30W / mK. Considering that the heating element is usually located at the bottom of the vessel body 100, the heat energy provided by the heating element will be transferred to the cooking side along the height direction of the vessel body 100. With a thermal conductivity of 5W / mK to 30W / mK, on ​​the one hand, the heating efficiency of the cooking side can be improved, which helps to shorten the user's waiting time; on the other hand, it can ensure that the temperature of the side of the vessel in contact with the food can reach the effective cooking temperature, which can improve the user experience; and on the other hand, it can improve the temperature uniformity of the side of the vessel body 100 in contact with the heating element, which can improve the efficiency of temperature transfer.

[0053] In some examples, to further improve the temperature uniformity, the thermal conductivity of the dielectric layer 200 is preferably between 5 W / mK and 10 W / mK.

[0054] Understandably, the thermal conductivity of metals is typically greater than or equal to 30 W / mK. If the thermal conductivity of the dielectric layer 200 along its height is greater than 30 W / mK, heat conduction is rapid. The temperature of the cooking side of the vessel is significantly affected by the contact between the bottom heating element and the vessel; areas where the heating element is in close contact with the vessel will be too hot, while areas with gaps will be too cold. Conversely, if the thermal conductivity of the dielectric layer 200 along its height is less than 5 W / mK, the thermal resistance is too high, resulting in a longer time for heat to transfer to the cooking side. This increases the user's waiting time and also creates a large temperature difference between the cooking and heating sides of the vessel, affecting the cooking results.

[0055] Understandably, the effective cooking temperature refers to the temperature of the vessel required to effectively cook the food. The effective cooking temperature usually needs to be higher than the boiling point of water, that is, the effective cooking temperature needs to be greater than 100℃. Different foods can have different effective cooking temperatures. For example, the effective cooking temperature of vegetables is usually greater than 150℃, and the effective cooking temperature of meat is usually around 180℃. Such settings can ensure that the cooked food has a better taste and flavor.

[0056] like Figure 1 and Figure 4As shown, in some examples, the thickness of the medium layer 200 is 1 mm to 5 mm. Furthermore, in order to further improve the cooking effect and ensure that the cooking side temperature can reach above the effective cooking temperature, the thickness of the medium layer 200 is preferably 1 mm to 3 mm.

[0057] In this technical solution, the specific thickness of the medium layer 200 is further selected. The thickness of the medium layer 200 is 1mm to 5mm. With this setting, on the one hand, the medium layer 200 has a suitable thickness, which can achieve the effect of uniform temperature; on the other hand, the medium layer 200 has a moderate amount of latent heat storage, which can balance the temperature of the cooking side of the vessel while taking into account the heat conduction efficiency; furthermore, the thickness of the medium layer 200 is between 1mm and 5mm, which can control the temperature difference between the heating side and the cooking side of the vessel to be within a reasonable range, ensuring that the temperature of the cooking side can reach above the effective cooking temperature when the heating component is working normally.

[0058] In some examples, the thermal storage material is a phase change material.

[0059] In this technical solution, the heat storage material can be a phase change material. When the ambient temperature of the medium layer 200 is high, the heat storage material can store heat energy through phase change. When the ambient temperature of the medium layer 200 is low, the phase change material can release heat energy to make the temperature distribution of the vessel more uniform.

[0060] In some examples, the phase change material is a molten salt.

[0061] In this technical solution, the phase change material can be molten salt. Molten salt has a low cost, which helps to reduce the production and processing cost of the dielectric layer 200. At the same time, molten salt has good latent heat of phase change, which can effectively store heat energy. In the event of localized low temperature in the vessel, it is beneficial to quickly adjust the temperature of the vessel so that the lower temperature area can be heated up.

[0062] Understandably, the molten salt can be NaNO3-LiNO3.

[0063] In some examples, the phase transition temperature of the phase change material is between 180°C and 200°C.

[0064] This technical solution further provides the range of phase change temperature values ​​for the phase change material.

[0065] This technical solution further provides a lower limit temperature for the phase change temperature of the medium layer 200, namely, the phase change temperature of the medium layer 200 is greater than or equal to 180℃. This setting ensures that when absorbing heat energy below 180℃, the medium layer 200 will undergo a phase change at or above 180℃, guaranteeing that the medium layer 200 can store sufficient latent heat to make the temperature on the cooking side more even. When the phase change temperature of the medium layer 200 is less than 180℃, considering the actual working conditions of the vessel, the medium layer 200 is in a phase change state in most cases, making it unsuitable for storing latent heat in most situations, thus weakening the temperature regulation effect of the medium layer 200 on the cooking side.

[0066] This technical solution further provides an upper limit for the phase change temperature of the medium layer 200, namely, the phase change temperature of the medium layer 200 is less than or equal to 200℃. This setting ensures that when absorbing heat energy below 200℃, the medium layer 200 will undergo a phase change under operating conditions below 200℃, ensuring that the medium layer 200 can release latent heat in a timely manner to make the temperature on the cooking side more even. When the phase change temperature of the medium layer 200 is greater than 200℃, considering the actual operating conditions of the vessel, the medium layer 200 will not undergo a phase change in most cases, meaning that the medium layer 200 cannot release latent heat in most situations, which will weaken the temperature regulation effect of the medium layer 200 on the cooking side.

[0067] It is understandable that the phase change of the dielectric layer 200 refers to the phase change of the dielectric layer 200 or some of its components when the phase change temperature is reached. For example, when the phase change temperature is reached, the dielectric layer 200 may change from a solid to a liquid and melt to release latent heat. Or, the dielectric layer may change from a liquid to a gas and evaporate to release latent heat.

[0068] In some examples, the compression density of the phase change material is 0.85 g / cm³. 3 Up to 1.75 g / cm 3 between.

[0069] In this technical solution, the compression density of the phase change material is further provided. It can be understood that the selection of the compression density can determine the total volume of the interlayer space within the phase change material, as well as the total volume of the interlayer space between two adjacent layered structures. If the total volume of multiple interlayer spaces and the volume of each interlayer space are too small, the space that the heat storage material can fill will be too small, resulting in a small amount of heat storage material and poor temperature uniformity. On the other hand, if the total volume of multiple interlayer spaces and the volume of each interlayer space are too large, the contact effect between the heat storage material and the skeleton material may be poor, which will affect the thermal conductivity of the phase change material.

[0070] The compression density of the phase change material is 0.85 g / cm³. 3 Up to 1.75 g / cm 3The spacing between the layers ensures that the total volume of the interlayer space and the volume of each interlayer space are within a suitable range. This guarantees that the thermal storage material has sufficient filling capacity, the phase change material can store latent heat, and the thermal storage material and the skeleton material have good contact effect, thus ensuring the heat transfer capacity of the phase change material. When the phase change material is used in a vessel or plate, it can improve the heating efficiency of the vessel or plate and reduce the user's waiting time.

[0071] The compression density of the phase change material is 0.85 g / cm³. 3 Up to 1.75 g / cm 3 On the one hand, with a fixed filling space for the phase change material, the density of the phase change material will directly affect the amount of phase change material used. This is achieved by ensuring the density of the phase change material is greater than or equal to 0.85 g / cm³. 3 This ensures that the phase change material has sufficient effective heat storage capacity, guaranteeing that it can provide enough heat energy to the cooking side during phase change heat release; and the density of the phase change material is less than or equal to 1.75 g / cm³. 3 It can control the maximum heat storage capacity of phase change materials, which can prevent the heat storage capacity of phase change materials from being too strong, resulting in a slow heating rate of the vessel in the early stage of heating, thus reducing the waiting time for users.

[0072] It is understandable that if the density of the phase change material is less than or equal to 0.85 g / cm³, 3 This could lead to weak effective heat storage capacity of the phase change material, resulting in poor temperature uniformity; if the density of the phase change material is greater than or equal to 1.75 g / cm³, it may also result in poor effective heat storage capacity of the phase change material. 3 This could lead to low heating efficiency in vessels equipped with the phase change material during the initial heating phase.

[0073] The density of the phase change material is 0.85 g / cm³. 3 Up to 1.75 g / cm 3 On the other hand, the density of a phase change material (PCM) can reflect its porosity, and porosity determines the deformation coefficient of the PCM. The density of the PCM is 0.85 g / cm³. 3 Up to 1.75 g / cm 3 This allows the coefficient of deformation of the phase change material under heat to be close to that of the vessel body, thus preventing excessive expansion of the phase change material that could cause the vessel containing it to crack, and preventing severe shrinkage of the phase change material that could lead to poor contact between the phase change material and the vessel and reduce heat transfer efficiency.

[0074] It is understandable that if the density of the phase change material is less than or equal to 0.85 g / cm³, 3This could lead to a large deviation in the deformation coefficient between the phase change material and the vessel using it, making it easy for gaps to form between the phase change material and the vessel during heating, which is detrimental to heat transfer; if the density of the phase change material is greater than or equal to 1.75 g / cm³... 3 This could lead to a large deviation between the deformation coefficient of the phase change material and the vessel using it, and could also cause the phase change material to expand rapidly under heat, resulting in cracking of the vessel.

[0075] like Figure 1 and Figure 4 As shown, in some examples, the vessel body 100 includes a sealing plate 110 and a cooking plate 120, the sealing plate 110 being connected to the cooking plate 120, a gap being formed between the cooking plate 120 and the sealing plate 110, and a medium layer 200 being disposed within the gap.

[0076] In this technical solution, the structural composition of the vessel body 100 is further provided. The vessel body 100 may include a sealing plate 110 and a cooking plate 120. During the preparation of the vessel body 100, the filler for preparing the medium layer 200 can be filled onto the cooking plate 120 first, and then the sealing plate 110 is connected to the cooking plate 120. The gap between the sealing plate 110 and the cooking plate 120 can accommodate the medium layer 200, which facilitates the production and processing of the vessel and the filling and preparation of the medium layer 200.

[0077] like Figure 2 and Figure 3 As shown, in some examples, the utensil also includes a side plate 130, which is connected to the periphery of the cooking plate 120 and encloses the cooking plate 120 to form a cooking space.

[0078] In this technical solution, the vessel may also include a side plate 130, which is connected to the cooking plate 120 to form a cooking space. This cooking space can be used to hold ingredients. The side plate 130 can prevent the soup from spilling out of the ingredients, which helps to improve the taste of the cooked ingredients.

[0079] In some examples, the sealing plate 110 and the cooking plate 120 are made of metal.

[0080] In this technical solution, the sealing plate 110 and the cooking plate 120 can be made of metal materials, which on the one hand gives the vessel body 100 good high temperature resistance and can improve the service life of the vessel body 100; on the other hand, it gives the vessel body 100 good wear resistance and mechanical strength, which can further improve the service life of the vessel body 100.

[0081] In some examples, the sealing plate 110 and the cooking plate 120 can be made of the same material so that the thermal conductivity of the sealing plate 110 and the cooking plate 120 is similar, while also facilitating the preparation of the sealing plate 110 and the cooking plate 120.

[0082] In some examples, the cover plate 110 may be made of aluminum or stainless steel, and the cooking plate 120 may also be made of aluminum or stainless steel. It is understood that the aluminum material may be an aluminum alloy.

[0083] In some examples, with the height direction of the vessel body 100 as the first direction and the length or width direction of the vessel body 100 as the second direction, the thermal conductivity of the dielectric layer 200 in the first direction is lower than that in the second direction.

[0084] The utensil provided in this application embodiment has a lower thermal conductivity of the medium layer 200 along its height direction than that along its length or width direction. During use, when food needs to be cooked using the utensil, it can be placed on the heating element. The heat energy emitted by the heating element is first transferred to the utensil body 100, and then transferred through the medium layer 200 inside the utensil body 100 to the surface of the utensil body 100 that contacts the food. The utensil body 100 provided in this application embodiment has an anisotropic thermal conductivity of the medium layer 200, so the heat energy is preferentially transferred along the length or width direction of the medium layer 200, and then transmitted along the height direction, making the temperature of the utensil body 100 and the surface of the food contact more even and improving the cooking effect of the food.

[0085] Understandably, during the heat transfer process through the medium layer 200, since the thermal conductivity of the medium layer 200 in the first direction is lower than that in the second direction, the heat will preferentially be transferred in the length or width direction of the medium layer 200, making the heat distribution in the length or width direction of the medium layer 200 more even. Then, the heat will be transferred to the direction away from the heating element of the medium layer 200. This cycle makes the temperature distribution of the medium layer 200 in the same plane more even. It will not cause the temperature of a certain position on the medium layer 200 to be too low because it is far away from the heating element, nor will it cause the temperature of a certain position on the medium layer 200 to be too high because it is close to the heating element. With this setting, the heat energy is transferred through the medium layer 200 to the surface of the utensil body 100 that is in contact with the food, which can make the temperature distribution on the cooking side of the utensil body 100 more even, which is conducive to improving the cooking effect of the food and at the same time can prevent the utensil body 100 from cracking due to uneven heating.

[0086] It is understood that the medium layer 200 can be plate-shaped or sheet-shaped, and the length or width direction of the medium layer 200 can be the direction of the plane where the medium layer 200 is located; the medium layer 200 is set inside the vessel body 100, and the vessel body 100 can form a cooking space for holding food, and the direction perpendicular to the medium layer 200 through the cooking space is the height direction of the medium layer 200.

[0087] According to a second aspect of the embodiments of this application, a grilling apparatus is provided, comprising: a vessel as described in any of the above technical solutions.

[0088] The grilling equipment provided in this application includes the vessel of the above-mentioned technical solution, and therefore possesses all the beneficial effects of the vessel of the above-mentioned technical solution.

[0089] In some examples, the grilling equipment also includes a heating element, with a dish placed on the heating element, wherein when the grilling equipment is in operation, the temperature difference between the side of the dish closer to the heating element and the side farther from the heating element is less than or equal to 120 degrees Celsius.

[0090] In this technical solution, the grilling equipment may also include a heating element. This heating element provides heat to the cookware, facilitating the cooking of the food. The side of the cookware in contact with the food can be called the cooking side, and the side in contact with the heating element can be called the heating side. The ratio of the thermal conductivity of the medium layer 200 to its thickness is greater than or equal to 2, which reduces the temperature difference between the cooking side and the heating side. This allows heat stored in the heating side through the medium layer to be quickly transferred to the cooking side, ensuring the cooking side reaches the cooking temperature. This reduces heat accumulation on the heating side, minimizing the risk of overheating and shutdown due to heat buildup, thus preventing cooking interruption. Furthermore, the temperature difference between the heating side and the cooking side is set to be less than or equal to 120 degrees Celsius. This limit prevents excessive temperature difference on the heating side, avoiding heat concentration there. This facilitates heat transfer to the cooking surface, ensuring it reaches the cooking temperature, and also reduces the risk of overheating and cooking interruption on the heating side.

[0091] In some examples, when the grilling equipment is in operation, the temperature of the side of the dish closest to the heating element is less than or equal to 300 degrees Celsius.

[0092] In this technical solution, considering the limited operating power of the heating component and the limited heat-bearing capacity of its components, by ensuring that the temperature on the heating side is less than or equal to 300 degrees Celsius, overheating of the heating side of the vessel can be avoided, preventing the food inside from burning and preventing the components of the heating component from melting.

[0093] In some examples, the difference between the phase change temperature of the medium layer and the minimum cooking temperature of the heating element is 0 to 20 degrees Celsius.

[0094] In this technical solution, the relationship between the phase change temperature and the minimum cooking temperature of the heating element is further provided. The difference between the two is between 0 degrees Celsius and 20 degrees Celsius, preferably between 0 degrees Celsius and 15 degrees Celsius. The pre-stored energy phase change material releases its stored energy for cooking, and the heating element continuously charges the phase change element, enabling the phase change material to work continuously. Setting the difference within the aforementioned range ensures that the energy of the heating element can fully charge the phase change material, allowing the stored energy to be continuously released, thus ensuring the cooking process and reducing the risk of food being burned.

[0095] In some examples, the difference between the maximum cooking temperature of the heating element and the phase change temperature of the medium layer is 0 to 10 degrees Celsius.

[0096] In this technical solution, the relationship between the phase change temperature and the maximum cooking temperature of the heating element is further provided. The difference between the two is between 0 degrees Celsius and 10 degrees Celsius. This can control the maximum cooking temperature to not exceed the preset range of the phase change temperature of the phase change material, avoid excessive temperature fluctuations that would prevent the heating element from being able to meet the cooking requirements, and reduce the risk of food being burned.

[0097] The grilling apparatus provided in this application includes a vessel body 100 and a medium layer 200 disposed within the vessel body 100. The medium layer 200 is made of a heat-storing material. During cooking in the vessel, the heating element that provides heat energy to the vessel first transfers heat energy to one side of the vessel body 100, and then the heat energy is transferred to the medium layer 200 via the sealing plate 110. On the one hand, the medium layer 200 can absorb and store the heat energy from the heating element, making the heat energy distribution within the medium layer 200 more uniform. Then, the medium layer 200 exchanges heat with the side of the vessel body 100 closest to the food, enabling the vessel body 100 to... The temperature distribution of the medium layer 200 is more even, which is conducive to improving the cooking effect of the ingredients. On the other hand, the medium layer 200 absorbs heat energy. When the local temperature on the vessel body 100 is too low, the medium layer 200 can release the absorbed latent heat to heat the lower temperature area of ​​the vessel body 100. For example, when new ingredients are put into the vessel body 100, the temperature difference between the vessel body 100 and the ingredients is large. In this case, the ingredients will quickly absorb the heat energy of the vessel body 100, causing the temperature at the contact point between the vessel body 100 and the newly put ingredients to drop rapidly. In this case, the medium layer 200 can release latent heat to regulate the temperature of the vessel body 100.

[0098] The grilling equipment provided in this application embodiment, with thermal conductivity measured in W / mK and thickness in mm, has a thermal conductivity to thickness ratio of the medium layer 200 greater than or equal to 2. It is understood that the thermal conductivity and thickness of the medium layer 200 are related to its temperature uniformity and the heating efficiency of the container body 100 on the side in contact with the food. A larger ratio of thermal conductivity to thickness results in better thermal conductivity of the medium layer 200 but reduced temperature uniformity; conversely, a smaller ratio results in reduced thermal conductivity but stronger temperature uniformity. By ensuring the ratio of thermal conductivity to thickness of the medium layer 200 is greater than or equal to 2, the thermal conductivity of the medium layer 200 is guaranteed, ensuring its thermal conductivity effect and allowing the container body 100 to heat up quickly while maintaining a uniform temperature, thus reducing the user's waiting time.

[0099] In some examples, the heating element is attached to the vessel. This attachment allows for faster heat transfer to the vessel, improving heat utilization efficiency and overall heating efficiency.

[0100] In some examples, the phase change material can be: NaNO3-LiNO3 with a phase transition temperature of 195℃.

[0101]

[0102] The results from Examples 1 to 4 in the table above show that when the ratio of the thermal conductivity to the thickness of the medium layer 200 is greater than or equal to 2, the temperature difference between the cooking side and the heating side of the vessel can be controlled below 75 degrees Celsius, which is beneficial for improving the cooking effect. Comparative Examples 1 and 2 show that when the ratio of the thermal conductivity to the thickness of the medium layer 200 is less than 2, the temperature difference between the cooking side and the heating side of the vessel increases significantly, resulting in a poor cooking effect.

[0103] In this invention, the terms "first," "second," and "third" are used for descriptive purposes only and should not be construed as indicating or implying relative importance; the term "multiple" refers to two or more unless otherwise explicitly defined. The terms "install," "connect," "link," and "fix" should be interpreted broadly. For example, "connect" can be a fixed connection, a detachable connection, or an integral connection; "link" can be a direct connection or an indirect connection through an intermediate medium. Those skilled in the art can understand the specific meaning of the above terms in this invention according to the specific circumstances.

[0104] In the description of this invention, it should be understood that the terms "upper," "lower," "left," "right," "front," "rear," etc., indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings. They are only for the convenience of describing this invention and simplifying the description, and do not indicate or imply that the device or unit referred to must have a specific orientation or be constructed and operated in a specific orientation. Therefore, they should not be construed as limitations on this invention.

[0105] In the description of this specification, the terms "one embodiment," "some embodiments," "specific embodiment," etc., refer to a specific feature, structure, material, or characteristic described in connection with that embodiment or example, which is included in at least one embodiment or example of the present invention. In this specification, the illustrative expressions of the above terms do not necessarily refer to the same embodiment or example. Furthermore, the specific features, structures, materials, or characteristics described may be combined in any suitable manner in one or more embodiments or examples.

[0106] The above are merely preferred embodiments of the present invention and are not intended to limit the present invention. Various modifications and variations can be made to the present invention by those skilled in the art. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of the present invention should be included within the scope of protection of the present invention.

Claims

1. A vessel, characterized in that, include: The vessel itself; A medium layer is disposed within the vessel body, and the medium layer is made of a heat storage material; Where the unit of thermal conductivity is W / mK and the unit of thickness is mm, the ratio of the thermal conductivity of the dielectric layer to the thickness of the dielectric layer is greater than or equal to 2. With the height direction of the vessel body as the first direction and the length or width direction of the vessel body as the second direction, the thermal conductivity of the medium layer in the first direction is lower than that in the second direction, so that the temperature distribution of the medium layer in the same plane is more uniform.

2. The vessel according to claim 1, characterized in that, When the thermal conductivity is expressed in W / mK and the thickness is expressed in mm, the ratio of the thermal conductivity of the dielectric layer to the thickness of the dielectric layer is less than or equal to 20.

3. The vessel according to claim 1, characterized in that, The thermal conductivity of the dielectric layer ranges from 5 W / mK to 30 W / mK.

4. The vessel according to claim 1, characterized in that, The thickness of the dielectric layer is 1 mm to 5 mm.

5. The vessel according to any one of claims 1 to 4, characterized in that, The heat storage material is a phase change material.

6. The vessel according to claim 5, characterized in that, The phase change material is a molten salt; and / or The phase change material has a phase change temperature of 180°C to 200°C; and / or The phase change material has a compression density of 0.85 g / cm³. 3 Up to 1.75 g / cm 3 between.

7. The vessel according to any one of claims 1 to 4, characterized in that, The vessel body includes: A sealing plate and a cooking plate, wherein the sealing plate is connected to the cooking plate, a gap is formed between the cooking plate and the sealing plate, and the medium layer is disposed within the gap.

8. The vessel according to claim 7, characterized in that, Also includes: Side panels are connected to the periphery of the cooking board and together with the cooking board form a cooking space.

9. A grilling / frying device, characterized in that, include: The vessel as described in any one of claims 1 to 8.

10. The grilling equipment according to claim 9, characterized in that, Also includes: A heating element is provided, and the dish is disposed on the heating element. When the grilling equipment is in operation, the temperature difference between the side of the dish closest to the heating element and the side furthest from the heating element is less than or equal to 120 degrees Celsius.

11. The grilling equipment according to claim 10, characterized in that, When the grilling equipment is in operation, the temperature of the side of the dish closest to the heating element is less than or equal to 300 degrees Celsius.

12. The grilling equipment according to claim 10, characterized in that, The difference between the phase transition temperature of the medium layer and the minimum cooking temperature of the heating element is 0 to 20 degrees Celsius.

13. The grilling equipment according to claim 10, characterized in that, The difference between the maximum cooking temperature of the heating element and the phase transition temperature of the medium layer is 0 to 10 degrees Celsius.

14. The grilling equipment according to claim 10, characterized in that, The heating element is attached to the vessel.

Citation Information

Patent Citations

  • Double-walled crockery provided with a pouch filled with phase-change material

    CN109475243A

  • Liquid heater

    CN207355952U