Packaging structure and packaging method of silicon carbide power device
By optimizing the double-sided heat dissipation structure and the thermally conductive interconnect layer, the problems of poor heat dissipation performance and high thermal resistance of silicon carbide power devices have been solved, achieving high-temperature operation stability and compact packaging, and improving the thermomechanical reliability and electrical connection reliability of the devices.
Patent Information
- Application Number
- CN202311708263.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-13
- Publication Date
- 2026-11-20
- Estimated Expiration
- 2043-12-13
AI Technical Summary
Existing silicon carbide power device packaging structures suffer from poor heat dissipation, high thermal resistance, large parasitic inductance, and single-sided heat dissipation cannot meet the requirements for high-temperature operation.
A double-sided heat dissipation structure is adopted, using a thermally conductive stress buffer layer, a thermally conductive interconnect layer, and a lead frame layer to replace the traditional copper-clad ceramic substrate. Combined with molybdenum sheets, silver pads, and core-shell structured nano-silver-coated copper particle solder paste, the thermal stress distribution and adhesion strength are optimized to achieve double-sided heat dissipation and electrical connection.
It effectively reduces package inductance, improves the thermomechanical reliability and heat dissipation performance of the device, ensures voltage breakdown resistance, and achieves high-temperature operation stability and package compactness.
Smart Images

Figure CN117457595B_ABST
Abstract
Description
Technical Field
[0001] This application relates to the technical field of electrical component packaging, and more specifically, to a packaging structure and packaging method for a silicon carbide power device. Background Technology
[0002] Silicon carbide (SiC) chips are a type of wide-bandgap semiconductor device. Compared to traditional silicon, they possess superior thermal, mechanical, and electrical properties, such as better high-temperature operation, higher power density, higher breakdown voltage, and wider frequency bandwidth. To fully utilize the excellent electrical characteristics of SiC power devices, reliable electrical signal connection and stable control of the device junction temperature are achieved through packaging structures.
[0003] Currently, most silicon carbide power devices still use the planar packaging method of silicon-based devices. In this packaging structure, the silicon carbide power chip and the Schottky diode are soldered to the copper-based surface of the same copper-clad ceramic substrate, and the interface connection between the chip and the copper-clad ceramic substrate is completed through tin-based interconnect technology. The copper-clad ceramic substrate is then connected to a heat sink to complete single-sided heat dissipation.
[0004] However, the aforementioned packaging structure can no longer meet the development and application requirements of silicon carbide devices. First, the existing copper-clad ceramic substrate has a relatively high thermal resistance, and the connection between the copper-clad ceramic substrate and the base plate introduces parasitic inductance. Second, the packaging structure of traditional silicon-based devices is for single-sided heat dissipation. The heat generated by power devices packaged according to traditional silicon-based packaging can only be transferred through the base plate, resulting in limited heat dissipation. The operating junction temperature is generally 150°C, while the operating temperature of silicon carbide power devices needs to reach above 300°C. Therefore, the packaging structure of traditional silicon-based devices is not suitable for silicon carbide chips, and silicon carbide devices cannot fully utilize their high-temperature operating capabilities. Summary of the Invention
[0005] To address the issue of poor heat dissipation performance in silicon carbide power devices, this application provides a packaging structure and packaging method for silicon carbide power devices.
[0006] In a first aspect, this application provides a packaging structure for a silicon carbide power device, employing the following technical solution:
[0007] A packaging structure for a silicon carbide power device includes a chip layer. From the inside out, a thermally conductive stress buffer layer, a lead frame layer, and a heat sink are sequentially disposed on both sides of the chip layer. Thermally conductive interconnect layers are disposed between the chip layer and the thermally conductive stress buffer layer, and between the thermally conductive stress buffer layer and the lead frame layer. A thermally conductive interface layer is disposed between the lead frame layer and the heat sink. An insulating encapsulation layer is filled between the chip layer and the lead frame layer.
[0008] Furthermore, the thickness of the thermally conductive stress buffer layer is 0.1 mm to 1 mm.
[0009] Furthermore, the thermally conductive stress buffer layer is cylindrical.
[0010] Furthermore, the thermal stress buffer layer includes a first thermal stress buffer layer and a second thermal stress buffer layer disposed sequentially, the first thermal stress buffer layer being close to the chip layer, and the chip layer and the first thermal stress buffer layer being connected through a thermally conductive interconnect layer.
[0011] Furthermore, the first thermally conductive stress buffer layer is a molybdenum sheet.
[0012] Furthermore, the second thermally conductive stress buffer layer is a silver pad.
[0013] Furthermore, the thermally conductive interconnect layer is made of solder paste containing silver-coated copper nanoparticles with a core-shell structure.
[0014] Furthermore, the thickness of the thermally conductive interconnect layer is 15μm to 30μm.
[0015] Furthermore, the lead frame layer is made of copper leads.
[0016] Furthermore, the material of the insulating encapsulation layer is any one of epoxy resin, polyimide, and glass-ceramic.
[0017] Secondly, this application provides a packaging method for silicon carbide power devices, employing the following technical solution:
[0018] A packaging method for a silicon carbide power device includes the following steps:
[0019] A thermally conductive stress buffer layer is placed on each side of the chip layer. Solder paste is filled between the thermally conductive stress buffer layer and the chip. The solder paste is sintered and cured to form a thermally conductive interconnect layer, thus completing one interconnection.
[0020] A lead frame layer is placed on the side of the thermal stress buffer layer away from the chip layer. Solder paste is filled between the thermal stress buffer layer and the lead frame layer. The solder paste is sintered and cured to form a thermally conductive interconnect layer, thus completing the secondary interconnect.
[0021] A heat sink is placed on the side of the lead frame layer away from the thermal stress buffer layer. A thermally conductive interface material is filled between the lead frame layer and the heat sink. After the thermally conductive interface material is cured into a thermally conductive interface layer, the thermally conductive interconnection between the lead frame layer and the heat sink is completed.
[0022] The gap between the two heat sinks is filled with a molding compound adhesive, which cures to form an insulating encapsulation layer, thus completing the encapsulation of the silicon carbide power device.
[0023] In summary, the technical solution of this application has at least the following advantages:
[0024] First, this application employs a double-sided heat dissipation packaging structure. Through the cooperation of a thermally conductive stress buffer layer, a thermally conductive interconnect layer, and a lead frame layer, the lead frame layer replaces the traditional copper-clad ceramic substrate and traditional long-loop bonding wires. The lead frame layer serves both as the main carrier of the chip layer and as the electrical connection between the internal circuit leads and external leads. The thickness of the lead frame layer is much smaller than that of the copper-clad ceramic substrate, thus effectively reducing the package size and improving the device's compactness. Simultaneously, since the packaging structure of this application eliminates the traditional copper-clad ceramic substrate and traditional long-loop bonding wires, the package inductance is significantly reduced. The use of an insulating encapsulation layer and a thermally conductive interface layer ensures that the device maintains good voltage breakdown performance even after eliminating the copper-clad ceramic substrate.
[0025] Secondly, due to the large difference in thermal expansion coefficients between the chip layer and the lead frame layer, thermal stress is easily generated due to thermal expansion and contraction. Therefore, this application employs a symmetrical thermal stress buffer layer with a certain deformation capacity to reduce the stress on the chip layer and the thermal interconnect layer, thereby improving the thermomechanical reliability of the device. Simultaneously, this application uses a bimetallic symmetrical buffer structure of a molybdenum sheet and a silver pad. Both the molybdenum sheet and the silver pad possess a certain deformation capacity and extremely low thermal resistance, further optimizing the thermomechanical reliability of the device. Furthermore, the silver pad itself acts as solder, eliminating the need for a thermal interconnect layer between the silver pad and the molybdenum sheet. After melting, the silver pad can form a reliable connection with various metals, alloys, and packaging materials.
[0026] Third, in this application, both the molybdenum sheet and the silver pad are cylindrical pads. The edges of the cylindrical pads are rounded, and the stress distribution is more uniform. In contrast, the edges or sharp corners of the square buffer layer are prone to stress concentration in the chip layer and the thermal interconnect layer, which can easily cause a sharp increase in local thermal stress.
[0027] Fourth, this application uses core-shell structured silver-coated copper nanoparticles instead of traditional tin-based solder. The nanoscale silver-coated copper particles possess good surface activity, resulting in low soldering interconnect temperatures and high packaging reliability. Secondly, nanoscale copper particles are prone to oxidation, but the silver coating overcomes this oxidation defect. Furthermore, copper's good resistance to electron migration overcomes silver's tendency to migrate. Therefore, core-shell structured silver-coated copper nanoparticles, as the main component of the thermally conductive interconnect layer, can achieve interconnect structures with higher electrical conductivity, higher thermal conductivity, higher high-temperature resistance, and higher reliability.
[0028] Fifth, this application optimizes the thickness of the thermal stress buffer layer and the thermally conductive interconnect layer. A thinner thermal stress buffer layer can reduce thermal resistance and improve heat dissipation performance, but may also affect mechanical strength. Conversely, a thicker thermal stress buffer layer can improve mechanical strength and electrical insulation performance, but may increase thermal resistance and affect heat dissipation performance. Therefore, to achieve a balance between heat dissipation performance, mechanical strength, and electrical insulation performance, the thickness of the thermal stress buffer layer is optimally controlled at 0.1 mm. A thinner thermally conductive interconnect layer can reduce thermal resistance and improve heat dissipation performance, but may also affect adhesive strength, thereby affecting device reliability. Within a certain range, the adhesive strength between layers of the thermal stress buffer layer increases with increasing thickness, but the thermal resistance also increases accordingly. Therefore, the thickness of the thermally conductive interconnect layer is optimally controlled between 15 μm and 30 μm. Attached Figure Description
[0029] Figure 1 This is a cross-sectional schematic diagram of the packaging structure of the silicon carbide power device in Embodiment 1.
[0030] Reference numerals: 1. Chip layer; 2. Thermal stress buffer layer; 21. First thermal stress buffer layer; 22. Second thermal stress buffer layer; 3. Lead frame layer; 4. Thermally conductive interconnect layer; 5. Thermally conductive interface layer; 6. Heat sink; 7. Insulating encapsulation layer. Detailed Implementation
[0031] Due to the poor heat dissipation performance of single-sided silicon carbide (SiC) devices, related double-sided packaging structures have been developed in the industry. For example, patent number WO2019071742A1 describes a modular packaging method for SiC MOS devices based on double-sided interconnection using nano-silver solder paste. This packaging structure still uses a copper-clad ceramic substrate. While the large thickness of the copper-clad ceramic substrate provides good insulation properties, allowing it to function as a carrier, it still suffers from the following drawbacks: First, the large thickness and high thermal resistance of the copper-clad ceramic substrate mean that even with a double-sided packaging structure, the overall thermal resistance of the device remains high, offering limited improvement in heat dissipation performance. Second, parasitic inductance is easily generated when the copper-clad ceramic substrate connects to the substrate. Third, nano-silver paste is costly, has poor migration resistance, and is prone to stress cracking, resulting in poor reliability.
[0032] Based on the above, the double-sided structure of this application eliminates the copper-clad ceramic substrate, replacing it with a lead frame layer as the carrier for the chip layer. The lead frame layer is made of bonding material, typically copper leads, and it enables the electrical connection between the internal circuit leads and the external leads. The lead frame layer is thinner than the copper-clad ceramic substrate, effectively reducing the package size and improving device compactness. Furthermore, the lead frame layer has a high thermal conductivity, reducing the thermal resistance of the silicon carbide power device package structure and thus improving the overall thermal performance of the device.
[0033] Simultaneously, the nano-silver-coated copper solder paste sintering technology addresses the issue of insufficient adhesion strength between the leadframe layer and the chip layer. During the sintering process, the silver layer of the nano-silver-coated copper particles de-wets on the surface of the leadframe layer, exposing the internal copper. At this point, the silver layer tends to sinter with itself, forming a network structure, while the exposed copper particles come into contact with the leadframe layer and begin to sinter, continuously crystallizing and growing to form dense copper blocks. Ultimately, this results in dense copper blocks distributed like islands within the silver network. The resulting thermally conductive interconnect layer effectively improves the adhesion strength between the leadframe layer and the chip layer. Furthermore, the copper restricts the migration ability of the silver, thus enhancing device reliability.
[0034] Furthermore, due to the significant difference in thermal expansion coefficients between the chip layer, the thermally conductive interconnect layer, and the lead frame layer, a thermally conductive buffer layer is placed between the chip layer and the lead frame layer. The deformation effect of the thermally conductive buffer layer and the symmetrical distribution of the upper and lower structures enable a uniform distribution of thermal stress within the device. The double-sided packaging structure of this application exhibits low overall thermal resistance and excellent thermal conductivity, allowing for rapid heat dissipation from the chip layer on both sides. Simultaneously, by eliminating the copper-clad ceramic substrate, parasitic inductance introduced by the connection between the copper-clad ceramic substrate and the substrate is avoided; however, thanks to the insulating encapsulation layer and the thermally conductive interface layer, the overall insulation withstand voltage performance of the silicon carbide device is almost unaffected.
[0035] Furthermore, this application adopts a bimetallic thermally conductive buffer layer structure. Through the combination of molybdenum sheet and silver pad, the uniform distribution of thermal stress inside the device is fully improved without affecting the thermal conductivity, thereby improving the reliability of the device.
[0036] To make the objectives, technical solutions, and advantages of this invention clearer, the device proposed by this invention will be further described in detail below with reference to the accompanying drawings and specific embodiments. The advantages and features of this invention will become clearer from the following description. It should be noted that the accompanying drawings are in a very simplified form and use non-precise proportions, only for the purpose of conveniently and clearly illustrating the embodiments of this invention. Please refer to the accompanying drawings to make the objectives, features, and advantages of this invention more apparent and understandable. It should be understood that the structures, proportions, sizes, etc., depicted in the accompanying drawings are only for the purpose of assisting those skilled in the art in understanding and reading the content disclosed in the specification, and are not intended to limit the implementation conditions of this invention. Therefore, they do not have substantial technical significance. Any modifications to the structure, changes in the proportional relationships, or adjustments to the size, without affecting the effects and objectives achieved by this invention, should fall within the scope of the technical content disclosed in this invention.
[0037] Example
[0038] Example 1
[0039] See Figure 1 A packaging structure for a silicon carbide power device is disclosed. From the inside out, a thermally conductive stress buffer layer 2, a lead frame layer 3, and a heat sink 6 are sequentially disposed on both sides of a chip layer 1. Thermally conductive interconnect layers 4 are disposed between the chip layer 1 and the thermally conductive stress buffer layer 2, and between the thermally conductive stress buffer layer 2 and the lead frame layer 3. A thermally conductive interface layer 5 is disposed between the lead frame layer 3 and the heat sink 6. An insulating encapsulation layer 7 fills the space between the chip layer 1 and the lead frame layer 3. In this application, the interaction between the thermally conductive stress buffer layer 2, the thermally conductive interconnect layer 4, and the lead frame layer 3 replaces the traditional copper-clad ceramic substrate and long bonding wires. This reduces the packaging inductance, ensures low overall thermal resistance of the silicon carbide device, and achieves double-sided heat dissipation, resulting in high heat dissipation performance. Furthermore, the device in this application achieves a thin and lightweight package.
[0040] See Figure 1 In this design, lead frame layer 3 replaces the copper-clad ceramic substrate to support chip layer 1. The thickness of lead frame layer 3 is smaller than that of traditional copper-clad ceramic substrates, resulting in a more compact internal structure. Electrodes on both the upper and lower surfaces of chip layer 1 are led out using a customized lead frame layer 3, enabling electrical connections between the internal circuit leads and external leads. Lead frame layer 3 can be customized based on the chip arrangement in chip layer 1. Lead frame layer 3 is typically made of copper; copper lead frames have low packaging inductance, further reducing the overall packaging inductance of the device.
[0041] See Figure 1 Due to the significant difference in thermal expansion coefficients between chip layer 1 and lead frame layer 3, large thermal stresses are generated, which can easily reduce the thermomechanical reliability of the device. Therefore, the deformation capability of the thermally conductive stress buffer layer 2 is used to disperse the stress between chip layer 1 and lead frame layer 3. The thermally conductive stress buffer layer 2 is symmetrically distributed about chip layer 1, and this symmetrical arrangement can also disperse the internal stress of the device to a certain extent.
[0042] See Figure 1 The thickness of the thermal stress buffer layer 2 affects the device's heat dissipation performance, mechanical strength, and electrical insulation performance. A smaller thickness of the thermal stress buffer layer 2 reduces thermal resistance and improves heat dissipation, but it also tends to worsen stress dispersion, affecting the device's mechanical strength. Conversely, a larger thickness of the thermal stress buffer layer 2 improves mechanical strength and electrical insulation performance, but it may increase thermal resistance, also impacting heat dissipation performance. Therefore, the thickness of the thermal stress buffer layer 2 is controlled between 0.1 mm and 1 mm, with 0.1 mm being optimal.
[0043] See Figure 1To further optimize the stress distribution within the device, the thermal stress buffer layer 2 is configured with a double-layer structure, comprising a first thermal stress buffer layer 21 and a second thermal stress buffer layer 22 stacked sequentially. The first thermal stress buffer layer 21 is located close to the chip layer 1 and is made of molybdenum sheet. The second thermal stress buffer layer 22 is made of silver pad. Both the molybdenum sheet and the silver pad possess certain deformation capabilities and extremely low thermal resistance. This dual buffering effect ensures stable operation of the device at high temperatures, further optimizing its thermomechanical reliability. Furthermore, both the molybdenum sheet and the silver pad are cylindrical, with rounded edges for more uniform stress distribution. The silver pad itself can act as solder, generating relatively low stress during melting and solidification, which helps reduce stress damage to components and circuit boards, improving device reliability and lifespan. Therefore, there is no need for a thermally conductive interconnect layer 4 to connect the silver pad and the molybdenum sheet; the melted silver pad can form a reliable connection with various metals, alloys, and packaging materials.
[0044] See Figure 1 Since the chip layer 1, the thermally conductive stress buffer layer 2, and the lead frame layer 3 are all connected by the thermally conductive interconnect layer 4, the device as a whole has good thermal conductivity and low overall thermal resistance, enabling sufficient heat dissipation. However, using conventional Sn-based solder and nano-silver paste for the lead frame layer 3 can easily lead to poor bonding strength. Therefore, in this embodiment, the thermally conductive interconnect layer 4 is selected as a solder paste containing core-shell structured nano-silver-coated copper particles.
[0045] Compared to traditional tin-based solders and nano-silver pastes, nano-silver-coated copper particles exhibit better surface activity and lower welding interconnect temperatures. During the sintering process, the silver layer of the nano-silver-coated copper particles de-wets on the surface of the lead frame layer 3, exposing the internal copper. At this point, the silver layer tends to sinter with the lead frame layer, forming a network structure. Meanwhile, the exposed copper particles come into contact with the lead frame layer 3, begin sintering, and continuously crystallize and grow, forming dense copper blocks. Ultimately, this results in dense copper blocks distributed like islands within the silver network. The resulting thermally conductive interconnect layer 4 effectively enhances the adhesion strength between the lead frame layer 3 and the chip layer 1. Simultaneously, the copper restricts the migration ability of silver, improving device reliability.
[0046] Secondly, nanoscale copper particles are prone to oxidation, but coating them with a silver layer can overcome this oxidation problem. Furthermore, copper possesses good resistance to electron migration, which overcomes the migration-prone nature of silver. Therefore, core-shell structured silver-coated copper nanoparticles, as the main component of the thermally conductive interconnect layer 4, can achieve an interconnect structure with higher electrical conductivity, higher thermal conductivity, better high-temperature resistance, and higher reliability.
[0047] See Figure 1While a thinner thermally conductive interconnect layer 4 can reduce thermal resistance and improve heat dissipation, it may also affect the bonding strength, thus impacting device reliability. Conversely, within a certain range, the bonding strength between layers in the thermally conductive stress buffer layer 2 increases with increasing thickness, but the thermal resistance also increases. Therefore, the optimal thickness of the thermally conductive interconnect layer 4 is controlled between 15 μm and 30 μm.
[0048] See Figure 1 The thermal interface layer 5 is made of thermally conductive silicone and the heat sink 6 is a liquid cooler. The liquid cooler is connected to the lead frame layer 3 through the thermal interface layer 5. The heat generated by the chip layer 1 is transferred to the liquid cooler to achieve efficient heat dissipation.
[0049] See Figure 1 To improve the packaging stability of the device, epoxy resin is filled between the two lead frame layers 3. The epoxy resin cures to form an insulating encapsulation layer 7, allowing the lead frame layer 3 and chip layer 1 to be integrally formed. The insulating encapsulation layer 7 can also be made of materials such as polyimide and microcrystalline glass instead of epoxy resin. The insulating encapsulation layer 7 can replace traditional copper-clad ceramic substrates, giving the device excellent electrical insulation properties. The insulating encapsulation layer 7 also has good waterproofing properties, effectively isolating moisture in the device's operating environment, preventing moisture from affecting the device's electrical performance, and further improving the device's operational stability.
[0050] The preparation process in this embodiment:
[0051] A molybdenum sheet is placed on each side of chip layer 1. The space between the molybdenum sheet and chip layer 1 is filled with nano-silver-coated copper particle solder paste. The nano-silver-coated copper particle solder paste is sintered and cured to complete one interconnection.
[0052] A silver pad is placed on the side of the molybdenum sheet away from chip layer 1. The silver pad is melted and then solidified to complete the secondary interconnection.
[0053] A copper lead frame is placed on the side of the silver pad away from the molybdenum pad. Nano-silver-coated copper particle solder paste is filled between the silver pad and the copper lead frame. The nano-silver-coated copper particle solder paste is sintered and cured to complete the three interconnects.
[0054] Place the heat sink 6 on the side of the copper lead frame away from the silver pad, fill the space between the copper lead frame and the heat sink 6 with thermally conductive silicone, and let the thermally conductive silicone cure to complete the thermally conductive interconnection between the copper lead frame and the heat sink 6.
[0055] Epoxy resin is filled into the gap between the two heat sinks 6, and the epoxy resin is cured to form an insulating encapsulation layer 7, thus completing the encapsulation of the silicon carbide power device.
[0056] The technical features of the above embodiments can be combined in any way. For the sake of brevity, not all possible combinations of the technical features in the above embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.
[0057] Furthermore, the above-described embodiments merely illustrate several implementation methods of the present invention, and while the descriptions are relatively specific and detailed, they should not be construed as limiting the scope of the invention patent. It should be noted that those skilled in the art can make various modifications and improvements without departing from the concept of the present invention, and these all fall within the protection scope of the present invention. Therefore, the protection scope of this invention patent should be determined by the appended claims.
Claims
1. A packaging structure for a silicon carbide power device, comprising a chip layer (1), characterized in that: The chip layer (1) is provided with a thermally conductive stress buffer layer (2), a lead frame layer (3) and a heat sink (6) arranged sequentially from the inside to the outside on both sides. A thermally conductive interconnect layer (4) is provided between the chip layer (1) and the thermally conductive stress buffer layer (2) and between the thermally conductive stress buffer layer (2) and the lead frame layer (3). A thermally conductive interface layer (5) is provided between the lead frame layer (3) and the heat sink (6). An insulating encapsulation layer (7) is filled between the chip layer (1) and the lead frame layer (3). The thermal stress buffer layer (2) includes a first thermal stress buffer layer (21) and a second thermal stress buffer layer (22) arranged sequentially. The first thermal stress buffer layer (21) is close to the chip layer (1). The chip layer (1) and the first thermal stress buffer layer (21) are connected by a thermal interconnect layer (4). The first thermal stress buffer layer (21) is a molybdenum sheet. The second thermal stress buffer layer (22) is a silver pad.
2. The packaging structure of a silicon carbide power device as described in claim 1, characterized in that: The thickness of the thermally conductive stress buffer layer (2) is 0.1 mm to 1 mm.
3. The packaging structure of a silicon carbide power device as described in claim 1, characterized in that: The thermally conductive stress buffer layer (2) is cylindrical.
4. The packaging structure of a silicon carbide power device as described in claim 1, characterized in that: The thermally conductive interconnect layer (4) is made of solder paste containing silver-coated copper nanoparticles with a core-shell structure.
5. The packaging structure of a silicon carbide power device as described in claim 1, characterized in that: The thickness of the thermally conductive interconnect layer (4) is 15μm to 30μm.
6. The packaging structure of a silicon carbide power device as described in claim 1, characterized in that: The lead frame layer (3) is made of copper leads.
7. The packaging method of a silicon carbide power device according to any one of claims 1-6, characterized in that: Includes the following steps: A thermally conductive stress buffer layer (2) is placed on each side of the chip layer (1). Solder paste is filled between the thermally conductive stress buffer layer (2) and the chip. The solder paste is sintered and solidified to form a thermally conductive interconnect layer (4), thus completing one interconnection. A lead frame layer (3) is placed on the side of the thermal stress buffer layer (2) away from the chip layer (1). Solder paste is filled between the thermal stress buffer layer (2) and the lead frame layer (3). The solder paste is sintered and cured to form a thermally conductive interconnect layer (4), thus completing the secondary interconnect. A heat sink (6) is placed on the side of the lead frame layer (3) away from the thermal stress buffer layer (2). A thermal interface material is filled between the lead frame layer (3) and the heat sink (6). After the thermal interface material is cured into a thermal interface layer (5), the thermal interconnection between the lead frame layer (3) and the heat sink (6) is completed. The gap between the two heat sinks (6) is filled with a plastic sealant, which is then cured to form an insulating encapsulation layer (7), thus completing the encapsulation of the silicon carbide power device.
Citation Information
Patent Citations
NANO silver solder paste double-sided interconnected silicon carbide MOS device-based modular encapsulation method
WO2019071742A1