An integrated stir welding apparatus and method
By designing an integrated stir welding device, the clamping system is simplified, solving the problems of clamping system complexity and welding accuracy, and realizing high-precision stir friction welding.
Patent Information
- Application Number
- CN202311558591.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-11-21
- Publication Date
- 2026-11-24
- Estimated Expiration
- 2043-11-21
AI Technical Summary
In existing friction stir welding technology, the clamping system is complex, which affects the welding quality, especially in structures with multiple weld seams, and the welding accuracy is difficult to guarantee.
An integrated stirring welding device is adopted, which integrates the clamping system through components such as the transfer flange, bidirectional pressure device, and grooved pressure plate. By combining multiple forces such as friction, adhesion, and spring compression, the clamping system is simplified and the welding quality is improved.
This simplifies the clamping system for friction stir welding and improves welding quality control, thereby enhancing welding accuracy and consistency.
Smart Images

Figure CN117464158B_ABST
Abstract
Description
Technical Field
[0001] This application relates to the field of friction stir welding technology, and in particular to an integrated friction stir welding apparatus and welding method. Background Technology
[0002] Friction stir welding is a method that utilizes the heat generated by the mutual movement and friction of the workpiece end faces to bring the ends to a thermoplastic state, followed by rapid upsetting to complete the weld. Friction stir welding can conveniently join similar or dissimilar materials, including metals, some metal matrix composites, ceramics, and plastics. Friction stir welding has advantages such as minimal post-weld microstructure changes, minimal heat-affected zone, low residual stress, no need for welding additives, resistance to deformation, and good weld strength. However, it also has disadvantages such as requiring rigid positioning, difficulty in repair, low welding speed, rapid wear of the stirring head, and the need for a welding backing plate.
[0003] In friction stir welding, significant upward, forward, and lateral forces are present on the welding head. Poor clamping of the welded parts can easily lead to displacement, affecting welding accuracy. Therefore, the design of the spindle head and clamping system is crucial. Currently, domestic friction stir welding spindle head machining and clamping are designed separately, with some areas using anti-deformation rollers for the weld seams. However, this method places extremely high demands on the clamping system, especially for structures with multiple weld seams. The clamping system is extremely complex, and a poorly designed clamping system directly affects welding quality, with deformation of the welded structure having a significant impact at the sub-millimeter level.
[0004] To reduce the complexity of the clamping system and improve the consistency of welding quality provided by friction stir welding equipment, there is an urgent need to study an integrated welding device and method with local bidirectional clamping positioning and shape correction. Summary of the Invention
[0005] The purpose of this application is to provide a buffer structure and manufacturing method for short- to medium-duration high-temperature impact conditions, which is suitable for temperature buffering under short- to medium-duration high-temperature or short-duration extremely high-temperature impact conditions.
[0006] To achieve the above objectives, this application adopts the following technical solution:
[0007] An integrated stir welding device includes a transfer flange, a bidirectional pressing device, and a grooved pressure plate. The upper surface of the transfer flange, after passing through the stirring head, is fixed to the lower end face of the machine tool spindle. The bidirectional pressing device is fixed to the lower surface of the transfer flange. The part to be welded is placed on the welding platform. Two sets of grooved pressure plates are respectively pressed against both sides of the weld seam of the part to be welded. The machine tool spindle moves downward, and the bidirectional pressing device applies a pressing force inward and downward to the two sets of grooved pressure plates to compact the weld seam of the part to be welded. The bidirectional pressing device includes a pressing body, two sets of symmetrical actuators, four sets of slide rails, two sets of rollers, eight compression springs, and eight matching spring shafts. The pressing body is a T-shaped partition structure with a tool hole in the middle that passes through the machine tool spindle and is mounted on the lower surface of the adapter flange. The two sets of rollers are mounted on the front and rear sides of the partition. The two sets of symmetrical actuators are mounted on both sides of the partition on the lower surface of the pressing body via slide rails. The slide rail tracks are mounted on the lower surface of the pressing body and perpendicular to the partition. The slide rail pairs are mounted on the upper surface of the actuators. Four sets of compression springs are evenly distributed on each side of the partition on the lower surface of the pressing body. The spring shafts pass through the compression springs and are perpendicular to the partition. The pressing body and actuators limit the ends of the compression springs. The actuators include a base plate and a vertical plate fixed to the base plate. Two rows of ball bearings are arranged parallel to each other on the lower surface of the base plate, and a row of ball bearings is arranged on the inner side of the vertical plate, parallel to the two rows of ball bearings on the base plate. The upper and outer surfaces of the grooved pressure plate are provided with semi-circular grooves that mate with the balls on the action body. The radius of the semi-circular grooves is larger than the radius of the balls. The longitudinal ends of the grooved pressure plate are provided with a ramp guide structure.
[0008] Welding using this welding equipment includes the following steps:
[0009] 1. The slotted pressure plate presses the part to be welded: When the part to be welded is a slotted part, the slotted pressure plate crosses the two vertical ribs of the slotted part before welding and presses it on the upper surface of the part that actually contacts the welding platform; when the part to be welded is a flat part or a slotted part but the distance between the vertical ribs exceeds the pressing range of the slotted pressure plate, a transition plate is set between the slotted pressure plate and the upper surface of the part to be welded. The transition plate has a convex plate structure. The upper protrusion fits with the inner cavity of the slotted pressure plate to restrict the lateral sliding of the slotted pressure plate. The lower part of the plane that contacts the upper surface of the part to be welded is roughened, and the roughness should be greater than 3.2μm; when the material of the part to be welded is a soft material that is prone to indentation, a nylon plate is set under the slotted pressure plate or the transition plate; when the roughness of the upper surface of the part to be welded is greater than 1.6μm, double-sided easy-tear adhesive is bonded between the lower surface of the transition plate and the upper surface of the part to be welded.
[0010] 2. The machine tool spindle drives the bidirectional pressing device to be introduced from the inclined guide structure at the longitudinal end of the slotted pressure plate. The compression spring contracts, and the two sets of action bodies expand outward on both sides of the machine tool spindle. The action bodies press the slotted pressure plate inward through the ball bearings.
[0011] 3. The machine tool spindle drives the bidirectional pressing device to apply downward pressure, pressing the parts to be welded vertically, and the two sets of rollers simultaneously press the weld seam surface at the front and rear ends of the machine tool spindle.
[0012] 4. The stirring head rotates to start welding. The machine tool spindle moves forward along the weld seam. During the movement, the machine tool spindle adjusts the axial feed to keep the axial downward pressure transmitted to the welded parts by the bidirectional downward pressure device constant.
[0013] The advantage of this application lies in the integration of multiple forces, such as friction, adhesion, spring compression, and spindle force, to integrate the machine tool spindle machining system and the clamping system. This simplifies the friction stir welding clamping system, integrates the welding head, and controls the welding quality, making it universally applicable to the research and development of friction stir welding equipment and processing technology.
[0014] The present application will be further described in detail below with reference to the accompanying drawings and embodiments. Attached Figure Description
[0015] Figure 1 Axonometric schematic diagram of an integrated stirring welding device and method;
[0016] Figure 2 A schematic diagram of the structure of an integrated stirring welding device and method;
[0017] Figure 3 Axial view of the bidirectional pressing device structure;
[0018] Figure 4 Cross-sectional schematic diagram of the bidirectional downward pressing device;
[0019] Figure 5 Top view of the bidirectional downward pressing device structure;
[0020] Figure 6 Schematic diagram of the functional part.
[0021] The numbers in the diagram are explained as follows: 1. Machine tool spindle; 2. Stirring head; 3. Welding platform; 4. Part to be welded; 5. Adapter flange; 6. Bidirectional pressing device; 7. Channel-shaped pressure plate; 8. Pressing body; 9. Actuating body; 10. Slide rail; 11. Roller; 12. Compression spring; 13. Spring shaft; 14. Partition plate; 15. Base plate; 16. Vertical plate; 17. Ball bearing. Detailed Implementation
[0022] See Figures 1-6An integrated stirring welding device includes a transfer flange 5, a bidirectional pressing device 6, and a grooved pressure plate 7. The upper surface of the transfer flange 5 is fixed to the lower end face of the machine tool spindle 1 after passing through the stirring head 2. The bidirectional pressing device 6 is fixed to the lower surface of the transfer flange 5. The part to be welded 4 is placed on the welding platform 3. The two sets of grooved pressure plates 7 are respectively pressed on both sides of the weld seam of the part to be welded 4. The machine tool spindle 1 moves downward, and the two sets of grooved pressure plates 7 are pressed inward and downward by the bidirectional pressing device 6 to compact the weld seam of the part to be welded 4.
[0023] The bidirectional pressing device 6 includes a pressing body 8, two sets of symmetrical action bodies 9, four sets of slide rails 10, two sets of rollers 11, eight compression springs 12, and eight matching spring shafts 13. The pressing body 8 is a T-shaped partition structure with a tool hole in the middle that passes through the machine tool spindle 1 and is mounted on the lower surface of the adapter flange 5. The two sets of rollers 11 are mounted on the front and rear sides of the partition 14. The two sets of symmetrical action bodies 9 are mounted on both sides of the partition 14 on the lower surface of the pressing body 8 via slide rails 10. The track of the slide rail 10 is mounted on the lower surface of the pressing body 8 and is perpendicular to the partition 14. The slide rail pair of the slide rail 10 is mounted on the upper surface of the action body 9. Four sets of compression springs 12 are evenly distributed on each side of the partition 14 on the lower surface of the pressing body 8. The spring shafts 13 pass through the compression springs 12 and are perpendicular to the partition 14. The pressing body 8 and the action bodies 9 limit the two ends of the compression springs 13.
[0024] The action body 9 includes a base plate 15 and a vertical plate 16 fixed to the base plate. Two rows of balls 17 are arranged parallel to each other on the lower surface of the base plate 15, and a row of balls 17 is arranged on the inner side of the vertical plate 16 and is parallel to the two rows of balls 17 on the base plate 15.
[0025] The upper surface and outer side of the grooved pressure plate 7 are provided with semi-circular grooves that cooperate with the balls 17 on the action body 9. The radius of the semi-circular grooves is larger than the radius of the balls 17. The longitudinal end of the grooved pressure plate 7 is provided with a ramp guide structure.
[0026] Welding using this integrated stir welding apparatus includes the following steps:
[0027] 1. Select the appropriate combination method between the slotted pressure plate 7 and the part 4 to be welded, based on the different structures;
[0028] 2. The machine tool spindle 1 drives the bidirectional pressing device 6 to be introduced from the inclined guide structure at the longitudinal end of the grooved pressure plate 7. The compression spring 12 contracts, and the two sets of action bodies 9 expand outward on both sides of the machine tool spindle 1. The action bodies press the grooved pressure plate 7 inward through the ball bearings 17.
[0029] 3 The machine tool spindle 1 drives the bidirectional pressing device 6 to apply downward pressure, pressing the part 4 to be welded vertically, and the two sets of rollers 11 simultaneously press on the weld surface at the front and rear ends of the machine tool spindle 1.
[0030] 4. The stirring head 2 rotates to start welding. The machine tool spindle 1 moves forward along the weld seam. During the movement, the machine tool spindle 1 adjusts the axial feed to keep the axial downward pressure transmitted to the welded parts by the bidirectional downward pressure device constant.
[0031] When the parts to be welded 4 are different, the method of using the grooved pressure plate 7 is also different. The specific method of use is as follows:
[0032] When the part to be welded 4 is a groove-shaped part, the groove-shaped pressure plate 7 crosses over the two vertical ribs of the part to be welded 4 before welding 4 is formed and presses it on the upper surface of the part that actually contacts the welding platform.
[0033] The part to be welded 4 is a flat part or a grooved part, but the spacing between the vertical ribs exceeds the clamping range of the grooved pressure plate. The grooved pressure plate 7 and the upper surface of the part to be welded 4 are provided with a transition plate. The transition plate is a convex plate structure. The upper protrusion is matched with the inner cavity of the grooved pressure plate to restrict the lateral sliding of the grooved pressure plate. The lower part of the plane that contacts the upper surface of the part to be welded is roughened, and the roughness should be greater than 3.2μm.
[0034] When the material of the part 4 to be welded is a soft material that is prone to indentation, a nylon plate is placed under the grooved pressure plate 7 or the transition plate.
[0035] When the surface roughness of the part to be welded 4 is greater than 1.6μm, double-sided easy-tear adhesive is applied between the lower surface of the adapter plate and the upper surface of the part to be welded.
[0036] Although embodiments of the invention have been shown and described, it will be understood by those skilled in the art that various changes, modifications, substitutions and alterations can be made to these embodiments without departing from the principles and spirit of the invention, the scope of which is defined by the appended claims and their equivalents.
Claims
1. An integrated stir welding method, characterized in that... Welding is performed using an integrated stir welding device, which includes a transition flange, a bidirectional pressing device, and grooved pressure plates. The upper surface of the transition flange, after passing through the stirring head, is fixed to the lower end face of the machine tool spindle. The bidirectional pressing device is fixed to the lower surface of the transition flange. The workpiece to be welded is placed on the welding platform, and two sets of grooved pressure plates press against both sides of the weld seam of the workpiece. The machine tool spindle moves downward, and the bidirectional pressing device applies a pressing force inward and downward to the two sets of grooved pressure plates, compacting the weld seam of the workpiece. The bidirectional pressing device includes a pressing body, two sets of symmetrical action bodies, four sets of slide rails, two sets of rollers, eight compression springs, and eight matching spring shafts. The pressing body is a T-shaped partition structure with a tool hole in the middle that passes through the machine tool spindle and is installed on the lower surface of the transition flange. The two sets of rollers... Wheels are installed on the front and rear sides of the partition. Two sets of symmetrical action bodies are installed on both sides of the partition on the lower surface of the pressing body via slide rails. The slide rail tracks are installed on the lower surface of the pressing body and perpendicular to the partition. The slide rail pairs are installed on the upper surface of the action bodies. Four sets of compression springs are evenly distributed on each side of the partition on the lower surface of the pressing body. The spring shafts pass through the compression springs and are perpendicular to the partition. The pressing body and the action bodies limit the ends of the compression springs. The action body includes a base plate and a vertical plate fixed to the base plate. Two rows of balls are arranged parallel to each other on the lower surface of the base plate. One row of balls is arranged on the inner side of the vertical plate and is parallel to the two rows of balls on the base plate. The upper and outer sides of the grooved pressure plate are provided with semi-circular grooves that mate with the balls on the action body. The radius of the semi-circular grooves is larger than the radius of the balls. The longitudinal ends of the grooved pressure plate are provided with a ramp guide structure. The specific steps include the following: 1-1 The grooved pressure plate presses the parts to be welded; 1-2 The machine tool spindle drives the bidirectional pressing device to be introduced from the inclined guide structure at the longitudinal end of the slotted pressure plate. The compression spring contracts, and the two sets of action bodies expand outward on both sides of the machine tool spindle. The action bodies press the slotted pressure plate inward through the ball bearings. 1-3 The machine tool spindle drives the bidirectional pressing device to apply downward pressure, pressing the parts to be welded vertically, and the two sets of rollers simultaneously press the weld seam surface at the front and rear ends of the machine tool spindle; 1-4 The stirring head rotates to start welding. The machine tool spindle moves forward along the weld seam. During the movement, the machine tool spindle adjusts the axial feed to keep the axial downward pressure transmitted to the welded parts by the bidirectional downward pressure device constant.
2. The integrated stir welding method according to claim 1, characterized in that... When the part to be welded is a groove-shaped part, the groove-shaped pressure plate passes over the two vertical ribs of the groove-shaped part before welding and is pressed against the upper surface of the part that actually contacts the welding platform.
3. The integrated stir welding method according to claim 1, characterized in that... The part to be welded is a flat part or a grooved part, but the distance between the vertical ribs exceeds the clamping range of the grooved pressure plate. A transition plate is provided between the grooved pressure plate and the upper surface of the part to be welded. The transition plate has a convex plate structure. The upper protrusion cooperates with the inner cavity of the grooved pressure plate to restrict the lateral sliding of the grooved pressure plate. The lower part of the plane that contacts the upper surface of the part to be welded is roughened, and the roughness should be greater than 3.2μm.
4. The integrated stir welding method according to claim 1, characterized in that... When the material of the part to be welded is a soft material that is prone to indentation, a nylon plate is provided under the grooved pressure plate or the transition plate.
5. The integrated stir welding method according to claim 1, characterized in that... When the surface roughness of the part to be welded is greater than 1.6μm, double-sided easy-tear adhesive is bonded between the lower surface of the adapter plate and the upper surface of the part to be welded.