Display panel and display device

By adopting a single-layer wiring structure within the display area of ​​the OLED display panel, combined with a grid design of fan-out wiring and auxiliary wiring, the uneven display problem of high-resolution, narrow-bezel OLED display panels when the screen is off is solved, achieving a better display effect.

CN117479701BActive Publication Date: 2026-11-24WUHAN CHINA STAR OPTOELECTRONICS SEMICONDUCTOR DISPLAY TECHNOLOGY CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202311091993.3
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-08-28
Publication Date
2026-11-24
Estimated Expiration
2043-08-28

AI Technical Summary

Technical Problem

High-resolution, narrow-bezel, small-sized OLED display panels are prone to display unevenness mura defects when the screen is off, especially when using a combination of LTPO and FIAA technologies, which are caused by uneven metal trace density.

Method used

A single-layer routing structure is adopted in the display area. By setting the fan-out routing and auxiliary routing at intersections and setting the breaks on the auxiliary routing, the auxiliary routing is only used to adjust the routing density, avoid the projection area of ​​the anode layer, form a grid structure, and control the uniformity of the routing density.

Benefits of technology

It improves the display unevenness issue when the screen is off by using uniform wiring density and avoiding uneven reflection caused by uneven surface of the anodized layer, thus improving the display effect.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117479701B_ABST
    Figure CN117479701B_ABST
Patent Text Reader

Abstract

This application discloses a display panel and a display device. The display area of ​​the display panel includes a first routing area and a second routing area. The display area includes a first planarization layer, a first metal layer, and an anode layer. The first metal layer is located on the first planarization layer and includes fan-out routing lines and auxiliary routing lines. The auxiliary routing lines have breaks. The first routing area includes intersecting fan-out routing lines and auxiliary routing lines. The second routing area includes auxiliary routing lines. The anode layer is located on the side of the first metal layer away from the first planarization layer. In the plane where the first planarization layer is located, the breaks all avoid the projection area of ​​the anode layer. This application can achieve FIAA (Fixed-Area Surface Adjustment) single-layer routing in the display area. The density uniformity of the routing lines in the display area can be controlled by the auxiliary routing lines. It can also avoid uneven reflection under screen-off conditions caused by unevenness of the anode layer surface due to routing breaks, as well as the reflection of differences in routing metal reflection through pixel openings, thereby improving the defects of screen-off mura.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application relates to the field of display technology, specifically to a display panel and display device. Background Technology

[0002] With the continuous advancement of display technology, small-to-medium-sized OLED (Organic Light-Emitting Diode) flexible foldable displays are rapidly developing towards higher resolution, better display effects, and narrower bezels. For OLED display panels using LTPO (Low Temperature Polycrystalline Oxide) technology, FIAA (Fanout in AA) technology is typically used to achieve narrower bezels, which involves placing some fanout lines within the display area. However, when the display panel design needs to achieve WQ (Wide Quad) resolution, the dense pixel density makes it very difficult to route the fanout metal traces within the AA (display area). Furthermore, the uneven metal density of the traces can easily cause display unevenness (mura) when the OLED display panel is off. Summary of the Invention

[0003] Embodiments of this application provide a display panel and display device to improve the problem of uneven display mura that occurs when a small-sized OLED display panel with high resolution and narrow bezels is off.

[0004] To address the aforementioned technical problems, embodiments of this application disclose the following technical solutions:

[0005] In a first aspect, a display panel is provided, including a display area, the display area including a first wiring area and a second wiring area, the display area including:

[0006] First planarization layer;

[0007] A first metal layer is located on the first planarization layer. The first metal layer includes fan-out traces and auxiliary traces. The auxiliary traces are provided with breaks. The first trace area includes the fan-out traces and auxiliary traces that are arranged in a cross pattern. The second trace area includes the auxiliary traces.

[0008] An anode layer, wherein the anode layer is located on the side of the first metal layer opposite to the first planarization layer;

[0009] The first planarization layer has multiple fracture regions on the side facing the first metal layer, each fracture region being located on the fracture region, and each fracture region being located outside the orthogonal projection of the anode layer onto the first planarization layer.

[0010] In conjunction with the first aspect, the fan-out routing includes a first fan-out routing extending along a first direction X and a second fan-out routing extending along a second direction Y, wherein the first direction X and the second direction Y intersect.

[0011] In conjunction with the first aspect, the auxiliary routing includes a first auxiliary routing extending along the first direction X and a second auxiliary routing extending along the second direction Y. Within the first routing area, the fan-out routing and the auxiliary routing form a mesh structure, and within the second routing area, the first auxiliary routing and the second auxiliary routing form a mesh structure.

[0012] In conjunction with the first aspect, the fracture surface includes a first fracture surface and a second fracture surface;

[0013] The first break is located at the intersection of the first auxiliary route and the first fan-out route; and / or, the first break is located on the first auxiliary route between any two adjacent second fan-out routes;

[0014] The second break is located at the intersection of the second auxiliary route and the second fan-out route; and / or, the second break is located on the second auxiliary route between any two adjacent first fan-out routes.

[0015] In conjunction with the first aspect, the orthographic projection of the anode layer on the first planarization layer and the adjacent first fracture surface have a first distance d1 along the first direction X, and the orthographic projection of the anode layer on the first planarization layer and the adjacent second fracture surface have a second distance d2 along the second direction Y. The first distance d1 and the second distance d2 satisfy the following: the first distance d1 corresponding to each anode layer is the same; and / or, the second distance d2 corresponding to each anode layer is the same.

[0016] In conjunction with the first aspect, both the first fan-out routing line and the second fan-out routing line are straight lines; and / or, both the first auxiliary routing line and the second auxiliary routing line are straight lines.

[0017] In conjunction with the first aspect, the density of the fracture in the first metal layer is less than or equal to .%.

[0018] In conjunction with the first aspect, the display area further includes:

[0019] A second planarization layer is located on the side of the first planarization layer that is opposite to the first metal layer;

[0020] A second metal layer, located on the second planarization layer, includes data signal lines configured to transmit display data.

[0021] In conjunction with the first aspect, vias are formed on the first planarization layer, and each of the fan-out traces and each of the data signal lines are electrically connected through the corresponding vias.

[0022] In conjunction with the first aspect, the display area further includes:

[0023] A third planarization layer is located on the side of the second planarization layer that is opposite to the second metal layer;

[0024] A third metal layer, the third metal layer being located on the third planarization layer;

[0025] A gate layer, which is located on the side of the third planarization layer opposite to the third metal layer.

[0026] In a second aspect, a display device is provided, comprising a display panel as described in any of the first aspects.

[0027] One of the above technical solutions has the following advantages or beneficial effects:

[0028] Compared with the prior art, the present application provides a display panel including a display area, which includes a first wiring area and a second wiring area. The display area includes a first planarization layer, a first metal layer and an anode layer. The first metal layer is located on the first planarization layer and includes fan-out wirings and auxiliary wirings. The auxiliary wirings have breaks. The first wiring area includes fan-out wirings and auxiliary wirings arranged in a cross pattern. The second wiring area only includes auxiliary wirings. The anode layer is located on the side of the first metal layer away from the first planarization layer. The first planarization layer has multiple break regions, each break corresponding to a break region, and each break region is located outside the orthographic projection of the anode layer. The display panel provided in this application can achieve FIAA single-layer routing within the display area, which can better adapt to scenarios with dense pixels. By using auxiliary routing to control the density uniformity of the routing within the display area, the defect of mura when the screen is off can be improved. By avoiding the projection area of ​​the anode layer with the routing breaks, the unevenness of the anode layer surface caused by the routing breaks can be avoided, as well as the difference in metal reflection caused by the routing breaks being reflected through the pixel openings. This further improves the problem of uneven display mura when the high-resolution, narrow-bezel small-sized OLED display panel is off. Attached Figure Description

[0029] To more clearly illustrate the technical solutions in the embodiments of this application, the accompanying drawings used in the description of the embodiments will be briefly introduced below. Obviously, the accompanying drawings described below are only some embodiments of this application. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.

[0030] Figure 1 This is a partial cross-sectional structural diagram of the display panel according to an embodiment of this application;

[0031] Figure 2 for Figure 1 Diagram of FIAA wiring configuration in the middle section;

[0032] Figure 3 for Figure 1 A schematic diagram of the routing method for the first metal layer in the middle;

[0033] Figure 4 This is a schematic diagram showing the relative positional relationship between the first and second fracture surfaces and the anode layer in an embodiment of this application;

[0034] Figure 5 This is a schematic diagram showing the distribution of vias on the first planarization layer in an embodiment of this application;

[0035] Figure 6 This is a schematic diagram showing the distribution of vias on the second planarization layer in an embodiment of this application;

[0036] Figure 7 This is a schematic flowchart illustrating the method for manufacturing a display panel according to an embodiment of this application.

[0037] Figure label:

[0038] 10-Display area; 101-First routing area; 102-Second routing area; 11-First planarization layer; 111-Via; 12-First metal layer; 121-Fan-out routing; 1211-First fan-out routing; 1212-Second fan-out routing; 122-Auxiliary routing; 1221-First auxiliary routing; 1222-Second auxiliary routing; 123-Break; 1231-First break; 1232-Second break; 13-Anode layer; 14-Second planarization layer; 15-Second metal layer; 151-Data signal line; 16-Fourth planarization layer; 17-Third planarization layer; 18-Third metal layer; 20-Non-display area. Detailed Implementation

[0039] The technical solutions of the embodiments of this application will be clearly and completely described below with reference to the accompanying drawings. In the description of this application, it should be understood that the terms "center," "longitudinal," "lateral," "length," "width," "thickness," "upper," "lower," "front," "rear," "left," "right," "vertical," "horizontal," "top," "bottom," "inner," "outer," "clockwise," and "counterclockwise," etc., indicating the orientation or positional relationship, are based on the orientation or positional relationship shown in the accompanying drawings and are only for the convenience of describing this application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limitations on this application. Furthermore, the terms "first" and "second" are used for descriptive purposes only and should not be construed as indicating or implying relative importance or implicitly specifying the number of indicated technical features. Thus, features defined with "first" and "second" may explicitly or implicitly include one or more of the stated features. In the description of this application, "multiple" means two or more, unless otherwise explicitly specified.

[0040] The applicant noted that small-to-medium-sized OLED (Organic Light-Emitting Diode) flexible foldable displays are rapidly developing towards higher resolution, better display effects, and narrower bezels. WQ resolution (2560×1440) is currently the highest resolution for small-sized displays. LTPO technology can achieve better display effects, and FIAA technology is the best technical route for achieving narrow bezels. However, there is currently no way to combine these three technologies because the extremely small pixel size makes metal wiring within the display area very difficult. Furthermore, uneven metal density in the wiring can easily cause display unevenness (mura) when the OLED display panel is off.

[0041] In view of this, the present application provides a display panel that adapts to scenarios with dense pixels by performing single-layer wiring within the display area, controls the density uniformity of the wiring within the display area by using auxiliary wiring, and improves the defect of screen-off mura by avoiding the projection area of ​​the anode layer by avoiding the wiring breaks. It also meets the technical requirement of combining WQ resolution, LTPO technology and FIAA technology.

[0042] Please see Figure 1 , Figure 1The illustration shows a partial cross-sectional structure of a display panel according to an embodiment of this application. The display panel includes a display area 10 and a non-display area that at least partially surrounds the display area 10. The display area 10 includes a first planarization layer 11, a first metal layer 12, and an anode layer 13. The first metal layer 12 is disposed on the first planarization layer 11, and the anode layer 13 is located on the side of the first metal layer 12 opposite to the first planarization layer 11.

[0043] In some embodiments, the display area 10 may further include a second planarization layer 14 and a second metal layer 15. The second planarization layer 14 is located on the side of the first planarization layer 11 opposite to the first metal layer 12. The second metal layer 15 is disposed on the second planarization layer 14, and on a plane parallel to the second planarization layer 14, the second metal layer 15 may include a data signal line 151 extending along a second direction Y, the data signal line 151 being configured to transmit display data. Exemplarily, the second direction Y may be parallel to the height direction of the display panel.

[0044] In addition, the display area 10 may also include a fourth planarization layer 16, which is disposed between the first metal layer 12 and the anode layer 13 to separate the first metal layer 12 and the anode layer 13.

[0045] Furthermore, the display area 10 may also include a third planarization layer 17, a third metal layer 18, and a gate layer (not shown in the figure). The third planarization layer 17 is located on the side of the second planarization layer 14 opposite to the second metal layer 15, the third metal layer 18 is located on the third planarization layer 17, and the gate layer is located on the side of the third planarization layer 17 opposite to the third metal layer 18. It is understood that in this embodiment, the first metal layer 12 is an SD3 layer, and the second metal layer 15 is an SD2 layer.

[0046] Please refer to the following: Figure 1 , Figure 2 and Figure 3 , Figure 2 It indicated Figure 1 The FIAA wiring method in the middle section Figure 3 It indicated Figure 1The routing method of the first metal layer. In this embodiment, the display area 10 includes a first routing area 101 and a second routing area 102. The first metal layer 12 includes a fan-out routing line 121 and an auxiliary routing line 122. The auxiliary routing line 122 has a break 123. The fan-out routing line 121 is used to connect the data signal line 151 in the display area 10 to the source driver chip to transmit display data. The auxiliary routing line 122 does not transmit signals and is only used to adjust the routing density. The first routing area 101 includes the fan-out routing line 121 and the auxiliary routing line 122 arranged in a cross pattern. The second routing area 102 includes the auxiliary routing line 122. That is to say, the first routing area 101 has both the fan-out routing line 121 and the auxiliary routing line 122. The second routing area 102 does not have the fan-out routing line 121, only the auxiliary routing line 122. In this way, it can be ensured that the routing in each area of ​​the display area 10 is uniform, thereby reducing screen-off mura.

[0047] The first planarization layer 11 has multiple fracture regions A on the side facing the first metal layer 12, with each fracture 123 located on a corresponding fracture region A, and each fracture region A located outside the orthogonal projection of the anode layer 13 onto the first planarization layer 11. Thus, since the fracture 123 below the anode layer 13 reflects light through pixel openings, and the light difference caused by the fracture 123 also leads to unevenness below the anode layer 13, exacerbating the screen-off mura, setting the fracture 123 to avoid the orthogonal projection of the anode layer 13 can effectively improve the screen-off mura.

[0048] In some embodiments, the fan-out trace 121 includes a first fan-out trace 1211 extending along a first direction X and a second fan-out trace 1212 extending along a second direction Y, wherein the first direction X and the second direction Y intersect. In some examples, the first direction X is parallel to the width direction of the display panel, the second direction Y is parallel to the height direction of the display panel, and the first direction X is perpendicular to the second direction Y.

[0049] In some embodiments, the auxiliary routing 122 includes a first auxiliary routing 1221 extending along a first direction X and a second auxiliary routing 1222 extending along a second direction Y. Within the first routing area 101, the fan-out routing 121 and the auxiliary routing 122 form a mesh structure. Within the second routing area 102, the first auxiliary routing 1221 and the second auxiliary routing 1222 form a mesh structure. It should be noted that... Figure 2 The bold dashed lines are used to represent data signal lines 151 of different layers.

[0050] In some embodiments, the first fan-out trace 1211 and the second fan-out trace 1212 are both straight lines; and / or, the first auxiliary trace 1221 and the second auxiliary trace 1222 are both straight lines. Thus, by adjusting both the fan-out trace 121 and the auxiliary trace 122 to be straight lines, the total length of the traces can be reduced, thereby reducing the overall reflection of a single-layer trace and reducing the non-uniformity of the metal within the display area 10, improving the mutagenesis when the screen is off.

[0051] In some embodiments, the fan-out trace 121 has a first linewidth L1 along the first direction X or the second direction Y, satisfying: L1 ≤ 2.2 micrometers; and / or, the auxiliary trace 122 has a second linewidth L2 along the first direction X or the second direction Y, satisfying: L2 ≤ 2.2 micrometers. This reduces the trace size, lowers the overall reflection of a single-layer trace, and reduces the non-uniformity of the metal within the display area 10, improving the mura when the screen is off. It should be noted that the linewidths of the fan-out trace 121 and the auxiliary trace 122 can be made as small as possible, depending on the capabilities of the manufacturing process.

[0052] In some embodiments, the density of the breaks 123 in the first metal layer 12 is less than or equal to 0.2%. This reduces the degree of metal density non-uniformity and glare, thereby preventing screen mutagenesis and improving the display effect.

[0053] The density of the break 123 in the first metal layer 12 can be determined in the following way:

[0054] First, determine the first trace density of the first metal layer 12 of the display area 10. The first trace density is the designed trace density without the break 123. Then, determine the second trace density of the first metal layer 12 of the display area 10. The second trace density is the actual trace density after the break 123 is present. Finally, determine the difference between the first trace density and the second trace density as the density of the break 123 in the first metal layer 12.

[0055] Based on the design of fan-out traces 121 and auxiliary traces 122, a trace area can be defined on the first planarization layer 11. The quotient of the total area of ​​the trace area and the area of ​​the display area 10 is determined as the first trace density of the first metal layer 12. The quotient of the actual total area of ​​the fan-out traces 121 and auxiliary traces 122 and the area of ​​the display area 10 is determined as the second trace density of the first metal layer 12. It can be understood that the area of ​​the break 123 is removed from the total area of ​​the trace area. The total area of ​​the fan-out traces 121 and auxiliary traces 122 refers to the sum of the areas of the fan-out traces 121 and the auxiliary traces 122. The area of ​​the fan-out trace 121 is the product of the length of the fan-out trace 121 and the first line width L1, and the area of ​​the auxiliary trace 122 is the product of the length of the auxiliary trace 122 and the second line width L2.

[0056] If the density of the fracture 123 is greater than 0.2%, the density of the fracture 123 can be controlled within 0.2% by adjusting the number of auxiliary traces 122 in the first trace area 101 and / or the second trace area 102, adjusting the line width of the metal traces in the first trace area 101 and / or the second trace area 102, or adjusting the size of the fracture 123.

[0057] Please continue reading. Figure 1 , Figure 2 and Figure 3 In some embodiments, the break 123 includes a first break 1231 and a second break 1232. The first break 1231 is located at the intersection of the first auxiliary route 1221 and the first fan-out route 1211; and / or, the first break 1231 is located on the first auxiliary route 1221 between any two adjacent second fan-out routes 1212. The second break 1232 is located at the intersection of the second auxiliary route 1222 and the second fan-out route 1212; and / or, the second break 1232 is located on the second auxiliary route 1222 between any two adjacent first fan-out routes 1211.

[0058] In some embodiments, the first break 1231 has a first dimension D1 along the first direction X, and the second break 1232 has a second dimension D2 along the second direction Y. While maintaining the signal truncation effect, the first dimension D1 and the second dimension D2 can be made as small as possible according to the manufacturing process capabilities. In this way, the impact of the break 123 on the overall reflection of the trace can be reduced, and the difference in metallic reflection caused by the break 123 can be reduced.

[0059] Please refer to the following: Figure 1 and Figure 4 , Figure 4The diagram illustrates the relative positional relationship between the first fracture and the second fracture and the anode layer in an embodiment of this application. In this embodiment, on the plane where the first planarization layer 11 is located, both the first fracture 123 and the second fracture 1232 are located outside the projection area of ​​the anode layer 13.

[0060] In some embodiments, the orthographic projection of the anode layer 13 on the first planarization layer 11 has a first distance d1 with the adjacent first fracture 1231 along the first direction X, and the orthographic projection of the anode layer 13 on the first planarization layer 11 has a second distance d2 with the adjacent second fracture 1232 along the second direction Y. The first distance d1 and the second distance d2 satisfy the following: the first distance d1 corresponding to each anode layer 13 is the same; and / or, the second distance d2 corresponding to each anode layer 13 is the same. That is, for each anode layer 13 and the adjacent first fracture 1231 and second fracture 1232 around the anode layer 13, the projection area of ​​each anode layer 13 has the same distance d1 with the corresponding first fracture 1231 at the same end along the first direction X, and the projection area of ​​each anode layer 13 has the same distance d2 with the corresponding second fracture 1232 at the same end along the second direction Y. This ensures that the relative positional relationship between the anode layer 13 and the fracture 123 remains uniform, thereby better avoiding uneven reflection under screen-off caused by the unevenness of the surface of the anode layer 13 due to the presence of the fracture 123 in the metal traces below the anode layer 13, and ensuring that the difference in metal reflection caused by the fracture reflected through the pixel opening remains uniform.

[0061] Please refer to the following: Figure 5 and Figure 6 , Figure 5 This illustration shows the distribution of vias on the first planarization layer in an embodiment of this application. Figure 6 This diagram illustrates the distribution of vias on the second planarization layer in an embodiment of this application. In some embodiments, vias 111 are also formed on the first planarization layer 11, and each fan-out trace 121 is electrically connected to each data signal line 151 through the corresponding via 111. For example, the first fan-out trace 1211 is electrically connected to the corresponding data signal line 151 through the via 111. In this way, the data signal line 151 is set on a different layer from the traces in the first metal layer 12, thereby avoiding the influence of the dense arrangement of data signals on the fan-out trace 121 and facilitating the arrangement of the fan-out trace 121. In addition, since each fan-out trace 121 and each data signal line 151 are connected through the vias 111 formed on the first planarization layer 11, the vias on the second planarization layer 14 can maintain the original uniform density distribution.

[0062] In this way, the vias 111 on the first planarization layer 11 and the vias on the second planarization layer 14 can maintain a uniform density distribution within the display area 10, thereby further improving the mura defect when the screen is off.

[0063] It is understood that the display panel provided in this application embodiment is different from the traditional double-layer wiring. It can achieve FIAA single-layer wiring in the display area 10, which can better adapt to the dense pixel scene. The density uniformity of the wiring in the display area 10 is controlled by the auxiliary wiring 122, thereby improving the defect of mura when the screen is off. By avoiding the projection area of ​​the anode layer 13 by the wiring break, the uneven surface of the anode layer 13 caused by the wiring break can be avoided, as well as the difference in the metal reflection of the wiring caused by the wiring break can be reflected through the pixel opening, thereby further improving the problem of uneven display mura when the high-resolution, narrow-bezel small-size OLED display panel is off.

[0064] Accordingly, please refer to Figure 7 , Figure 7 This is a schematic flowchart illustrating a method for fabricating a display panel according to an embodiment of this application. The method for fabricating a display panel according to an embodiment of this application includes providing a display area, which includes a first wiring area and a second wiring area. Specifically, providing the display area includes the following steps:

[0065] 701: Provides the first planarization layer.

[0066] 702: A first metal layer is formed on the first planarization layer. Specifically, fan-out traces and auxiliary traces are formed in a first routing area, and auxiliary traces are formed in a second routing area. Breaks are formed on the auxiliary traces, with each break corresponding to multiple break regions on the side of the first planarization layer facing the first metal layer.

[0067] 703: An anode layer is formed on the side of the first metal layer opposite to the first planarization layer. Each fracture region is located outside the orthogonal projection of the anode layer onto the first planarization layer.

[0068] In some embodiments, fan-out traces are formed on the first planarization layer, including:

[0069] A first fan-shaped outgoing trace extending along a first direction X and a second fan-shaped outgoing trace extending along a second direction Y are formed on the first planarization layer, wherein the first direction X and the second direction Y intersect.

[0070] In some embodiments, auxiliary traces are formed on the first planarization layer, including:

[0071] A first auxiliary trace extending along a first direction X and a second auxiliary trace extending along a second direction Y are formed on a first planarization layer. Within the first trace area, the fan-out trace and the auxiliary trace form a mesh structure. Within the second trace area, the first auxiliary trace and the second auxiliary trace form a mesh structure.

[0072] In some embodiments, the fracture includes a first fracture and a second fracture; forming a fracture on an auxiliary trace includes:

[0073] A first break is formed at the intersection of the first auxiliary route and the first outgoing route; and / or, on the first auxiliary route between any two adjacent second outgoing routes.

[0074] A second break is formed at the intersection of the second auxiliary route and the second outgoing route; and / or, on the second auxiliary route located between any two adjacent first outgoing routes.

[0075] In some embodiments, the orthographic projection of the anode layer on the first planarization layer has a first distance d1 with the adjacent first fracture along a first direction, and the orthographic projection of the anode layer on the first planarization layer has a second distance d2 with the adjacent second fracture along a second direction. The first distance d1 and the second distance d2 satisfy the following: the first distance d1 corresponding to each anode layer is the same; and / or, the second distance d2 corresponding to each anode layer is the same.

[0076] In some embodiments, forming a first fan-shaped outgoing trace extending along a first direction X and forming a second fan-shaped outgoing trace extending along a second direction Y on a first planarization layer includes:

[0077] A first fan-shaped trace extending in a straight line along a first direction X is formed on the first planarization layer, and / or a second fan-shaped trace extending in a straight line along a second direction Y is formed on the first planarization layer.

[0078] Forming a first auxiliary trace extending along a first direction X and forming a second auxiliary trace extending along a second direction Y on a first planarization layer, including:

[0079] A first auxiliary trace extending in a straight line along a first direction X is formed on the first planarization layer, and / or a second auxiliary trace extending in a straight line along a second direction Y is formed on the first planarization layer.

[0080] In some embodiments, the density of the first metal layer interruption is less than or equal to 0.2%.

[0081] In some embodiments, providing the display area before providing the first planarization layer further includes the following steps:

[0082] A second planarization layer is provided on the side of the first planarization layer that is opposite to the first metal layer.

[0083] A second metal layer is formed on the second planarization layer. The second metal layer includes data signal lines configured to transmit display data.

[0084] In some embodiments, after performing step 702, providing the display area further includes the following steps:

[0085] Vias are formed on the first planarization layer to allow each fan-out trace to be electrically connected to each data signal line through the corresponding via.

[0086] In some embodiments, providing the display area before providing the second planarization layer further includes the following steps:

[0087] A gate layer is provided on the side of the second planarization layer opposite to the second metal layer.

[0088] A third planarization layer is fabricated on the gate layer;

[0089] A third metal layer is prepared on the side of the third planarization layer facing the second planarization layer.

[0090] It is understood that the display panel manufacturing method provided in this application embodiment can achieve single-layer FIAA wiring within the display area, which can better adapt to scenarios with dense pixels. By using auxiliary wiring to control the density uniformity of wiring within the display area, the defect of mura when the screen is off can be improved. By avoiding the projection area of ​​the anode layer by avoiding the wiring break, the unevenness of the anode layer surface caused by the wiring break can be avoided, as well as the difference in metal reflection caused by the wiring break, which is reflected through the pixel opening. This further improves the problem of uneven display mura when the high-resolution, narrow-bezel small-sized OLED display panel is off.

[0091] Accordingly, the display device provided in this application includes the display panel as described in any of the above embodiments. The display device can be a mobile phone, a computer, a television, a smart wearable device, etc., and this embodiment does not impose any special limitations on it.

[0092] It is understood that the display device of this application embodiment can adapt well to scenarios with dense pixels by using FIAA to route a single layer of traces in the display area. By using auxiliary traces to control the density uniformity of traces in the display area, the defect of mura when the screen is off can be improved. By avoiding the projection area of ​​the anode layer by avoiding the trace break, the unevenness of the anode layer surface caused by the trace break can be avoided, as well as the difference in trace metal reflection caused by the trace break can be reflected through the pixel opening, thereby further improving the problem of uneven display mura when the high-resolution, narrow-bezel small-sized OLED display panel is off.

[0093] The foregoing has provided a detailed description of a display panel and display device according to embodiments of this application. Specific examples have been used to illustrate the principles and implementation methods of this application. The descriptions of the embodiments above are merely for the purpose of helping to understand the technical solutions and core ideas of this application. Those skilled in the art should understand that modifications can still be made to the technical solutions described in the foregoing embodiments, or equivalent substitutions can be made to some of the technical features. These modifications or substitutions do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions in the embodiments of this application.

Claims

1. A display panel comprising a display area (10), characterized in that The display area (10) comprises a first wiring area (101) and a second wiring area (102), the display area (10) comprises: a first planarization layer (11); a first metal layer (12), the first metal layer (12) is located on the first planarization layer (11), the first metal layer (12) comprises fan-out wires (121) and auxiliary wires (122), the auxiliary wires (122) are provided with a break (123), the first wiring area (101) comprises the fan-out wires (121) and the auxiliary wires (122) arranged in cross, and the second wiring area (102) comprises the auxiliary wires (122); an anode layer (13), the anode layer (13) is located on the side of the first metal layer (12) away from the first planarization layer (11); wherein, the first planarization layer (11) has a plurality of break areas on the side facing the first metal layer (12), each break (123) is located on the break area, and each break area is located outside the orthographic projection of the anode layer (13) on the first planarization layer (11).

2. The display panel of claim 1, wherein, The fan-out wires (121) comprise first fan-out wires (1211) extending along a first direction (X) and second fan-out wires (1212) extending along a second direction (Y), and the first direction (X) and the second direction (Y) intersect.

3. The display panel of claim 2, wherein, The auxiliary wires (122) comprise first auxiliary wires (1221) extending along the first direction (X) and second auxiliary wires (1222) extending along the second direction (Y), and the fan-out wires (121) and the auxiliary wires (122) form a grid structure in the first wiring area (101), and the first auxiliary wires (1221) and the second auxiliary wires (1222) form a grid structure in the second wiring area (102).

4. The display panel of claim 3, wherein, The break (123) comprises a first break (1231) and a second break (1232); The first break (1231) is located at the intersection of the first auxiliary wire (1221) and the first fan-out wire (1211); and / or, the first break (1231) is located on the first auxiliary wire (1221) between any two adjacent second fan-out wires (1212); The second break (1232) is located at the intersection of the second auxiliary wire (1222) and the second fan-out wire (1212); and / or, the second break (1232) is located on the second auxiliary wire (1222) between any two adjacent first fan-out wires (1211).

5. The display panel of claim 4, wherein, The orthographic projection of the anode layer (13) on the first planarization layer (11) and the adjacent first fracture (1231) have a first distance d1 along the first direction (X), and the orthographic projection of the anode layer (13) on the first planarization layer (11) and the adjacent second fracture (1232) have a second distance d2 along the second direction (Y). The first distance d1 and the second distance d2 satisfy the following: the first distance d1 corresponding to each anode layer (13) is the same; and / or, the second distance d2 corresponding to each anode layer (13) is the same.

6. The display panel of claim 3, wherein, The first outgoing route (1211) and the second outgoing route (1212) are both straight lines; and / or, the first auxiliary route (1221) and the second auxiliary route (1222) are both straight lines.

7. The display panel of claim 1, wherein, The density of the fracture (123) in the first metal layer (12) is less than or equal to 0.2%.

8. The display panel of claim 1, wherein, The display area (10) also includes: The second planarization layer (14) is located on the side of the first planarization layer (11) away from the first metal layer (12); A second metal layer (15) is located on the second planarization layer (14) and includes a data signal line (151) configured to transmit display data.

9. The display panel of claim 8, wherein, A via (111) is formed on the first planarization layer (11), and each of the fan-out traces (121) and each of the data signal lines (151) are electrically connected through the corresponding via (111).

10. The display panel of claim 8, wherein, The display area (10) also includes: A third planarization layer (17) is located on the side of the second planarization layer (14) away from the second metal layer (15); A third metal layer (18) is located on the third planarization layer (17); A gate layer, which is located on the side of the third planarization layer (17) opposite to the third metal layer (18).

11. A display device, characterized by comprising: Includes the display panel as described in any one of claims 1 to 10.

Citation Information

Patent Citations

  • Display panel and display device

    CN116096172A

  • Display panel and display device

    CN116322187A