Method for producing cermet composite powder and cermet composite powder

By contacting plasma-generated raw material gas with metal raw materials to generate intermediate products and then condensing them, the problems of complex preparation process and insufficient powder density of metal-ceramic composite powders are solved. This results in high-purity metal-ceramic composite powders with controllable particle size, which are suitable for additive manufacturing and metal injection molding technologies.

CN117548681BActive Publication Date: 2026-11-24NANJING TECH UNIV +1
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202210935927.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-08-04
Publication Date
2026-11-24
Estimated Expiration
2042-08-04

AI Technical Summary

Technical Problem

Existing metal-ceramic composite powder preparation processes are complex and lengthy, and the resulting powders have poor density and poor controllability of particle size and particle size distribution.

Method used

Plasma-ionized raw material gas is contacted with metal raw material to generate intermediate products, and metal-ceramic composite powder is obtained by condensation. The ratio of raw material gas and metal raw material and reaction conditions are controlled, and the particle size and particle size distribution are controlled by radio frequency plasma technology.

Benefits of technology

The preparation process was simplified, the purity and density of the powder were improved, the controllability of particle size and particle size distribution was achieved, and the powder's formability and fatigue performance were enhanced.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117548681B_ABST
    Figure CN117548681B_ABST
Patent Text Reader

Abstract

This application relates to a method (10) for preparing a metal-ceramic composite powder and the metal-ceramic composite powder obtained therefrom. The preparation method (10) includes the following steps: (12) providing a raw material gas, the raw material gas including one or more of oxygen, nitrogen, and carbon-containing gases; (14) ionizing the raw material gas to obtain a raw material gas plasma; (16) contacting the raw material gas plasma with a metal raw material to generate an intermediate product; and (18) condensing the intermediate product to obtain the metal-ceramic composite powder. This application embodiment can help to simplify the preparation process of the metal-ceramic composite powder, shorten the process flow, and can benefit the metal-ceramic composite powder with higher purity, better density, and better controllability of particle size and particle size distribution.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of materials and manufacturing technology, and in particular to a method for preparing metal-ceramic composite powder and the metal-ceramic composite powder obtained therefrom. Background Technology

[0002] With the development of additive manufacturing (AM, commonly known as 3D printing) and metal injection molding (MIM) technologies, the design of raw materials, processing methods, and manufacturing equipment all need continuous innovation and optimization. Improving the quality and performance of raw materials has become a crucial foundation for advancing the fields of additive manufacturing and metal injection molding.

[0003] According to research, metal-ceramic composite powders can provide an innovative underlying impetus for additive manufacturing and metal injection molding technologies.

[0004] However, most current preparation processes for metal-ceramic composite powders are complex, lengthy, generate byproducts, and produce powders with poor density, particle size, and particle size distribution.

[0005] Therefore, existing methods for preparing metal-ceramic composite powders need further improvement. Summary of the Invention

[0006] One object of the present invention is to provide an improved method for preparing metal-ceramic composite powder and the metal-ceramic composite powder obtained therefrom.

[0007] To achieve the above objectives, one aspect of the present invention relates to a method for preparing a metal-ceramic composite powder, comprising the following steps: providing a raw material gas, the raw material gas including one or more of oxygen, nitrogen, and carbon-containing gases; ionizing the raw material gas to obtain a raw material gas plasma; contacting the raw material gas plasma with a metal raw material to generate an intermediate product; and condensing the intermediate product to obtain the metal-ceramic composite powder.

[0008] In some embodiments, the amount of the metal raw material is greater than the amount required to react with the raw material gas plasma.

[0009] In some embodiments, the volume of the unreacted feed gas accounts for 5-15% of the total volume of the feed gas.

[0010] In some embodiments, the feed gas includes a silicon-containing gas.

[0011] In some embodiments, the silicon-containing gas includes hexamethylsiloxane, silane, or a mixture of the two.

[0012] In some embodiments, the carbon-containing gas includes methane, acetylene, or a mixture of both.

[0013] In some embodiments, the metal raw material includes one or more of the following: iron-based alloys, titanium-based alloys, nickel-based alloys, tungsten alloys, aluminum alloys, magnesium alloys, copper alloys, and precious metals.

[0014] In some embodiments, the metal raw material includes tungsten.

[0015] In some embodiments, the metal raw material is in a solid or liquid state.

[0016] In some embodiments, the form of the metal raw material includes one or more of the following: powder, wire, rod, and tube.

[0017] In some embodiments, the metal raw material is in the form of droplets when it comes into contact with the raw material gas plasma.

[0018] Another aspect of this invention relates to a metal-ceramic composite powder, which is prepared by the metal-ceramic composite powder preparation method described in this application.

[0019] Where technical conditions permit, the technical solutions of the various embodiments in this application can be combined in any way.

[0020] The present application will be further described below with reference to the accompanying drawings. The same or similar reference numerals may be used in the drawings to refer to the same or similar steps in different embodiments, and descriptions of the same or similar steps, features, and effects in different embodiments, as well as descriptions of steps, features, and effects that are the same or similar to those in the prior art, may be omitted. Attached Figure Description

[0021] Figure 1 This is a schematic flowchart of a method for preparing a metal-ceramic composite powder according to some embodiments of the present invention. Detailed Implementation

[0022] Figure 1 This is a schematic flowchart illustrating a method for preparing a metal-ceramic composite powder according to some embodiments of the present invention. Figure 1 As shown, one aspect of the present invention relates to a method 10 for preparing a metal-ceramic composite powder, which includes the following steps: 12. providing a raw material gas, the raw material gas including one or more of oxygen, nitrogen, and carbon-containing gases; 14. ionizing the raw material gas to obtain a raw material gas plasma; 16. contacting the raw material gas plasma with a metal raw material to generate an intermediate product; and 18. condensing the intermediate product to obtain the metal-ceramic composite powder.

[0023] The embodiments of this application can help to simplify the preparation process of metal-ceramic composite powders, shorten the process, and improve the purity, density, particle size and particle size distribution of the metal-ceramic composite powders.

[0024] For example, the raw material gas plasma can provide the heat required for the chemical reaction to generate ceramics, and can also serve as a raw material for ceramic generation. The controllable atmosphere helps improve the uniformity and purity of the metal-ceramic composite powder product. Contact between the raw material gas plasma and the metal raw material also facilitates the physical composite of the generated ceramic and metal. Therefore, the preparation method of the metal-ceramic composite powder involved in this application has a simple process, a short flow, no by-products, and high purity.

[0025] Furthermore, by contacting the raw material gas plasma with the metal raw material, the metal and the raw material gas undergo a chemical reaction in an ionic state to generate ceramics and / or undergo physical composite formation to prepare metal-ceramic composite powder. This facilitates the formation of coherent and semi-coherent relationships between ceramic molecules and metal atoms. That is, metal ions are both nucleation sites and catalysts for ceramic reactions. At the same time, the atomic interface between the metal and ceramic will form coherent and semi-coherent relationships after the reaction. Compared with traditional physical mixing of metal and ceramic, the metal-ceramic composite powder involved in this application has stronger interfacial bonding force, higher powder particle density, and better forming and fatigue properties of the powder material products.

[0026] Furthermore, the particle size and particle size distribution of the metal-ceramic composite powder can be controlled by adjusting the flow rate of the raw material gas, the flow rate of the metal raw material, the feeding speed, and / or the power of the plasma, offering good controllability. For example, the particle size and ceramic particle mass ratio of the metal-ceramic composite powder can be controlled by adjusting the reaction rates of metal, oxygen, nitrogen, and carbon per unit time. Generally speaking, the higher the plasma power, the faster the metal raw material feeding speed, and the higher the raw material gas flow rate, the faster the reaction rate, which is more conducive to the formation and growth of ceramics, and ultimately results in a larger particle size of the metal-ceramic composite powder.

[0027] Furthermore, the molar ratio between the individual atoms in the metal raw material and the raw material gas can be set to be consistent with the molar ratio between the elements in the target metal-ceramic composite powder, thereby obtaining a target metal-ceramic composite powder with standard stoichiometry, which is beneficial to improving the uniformity of the chemical composition of the metal-ceramic composite powder.

[0028] The preparation method 10 can be implemented using a plasma device (not shown). For example, the raw material gas can be supplied to the plasma generating chamber of the plasma device so that the raw material gas is plasmaized in the plasma generating chamber by an electric field such as direct current (DC), radio frequency (RF), or microwave (MP) to obtain the raw material gas plasma.

[0029] In some embodiments, radio frequency plasma technology is used to ionize the raw material gas to obtain the raw material gas plasma. This can help to effectively control the hollow powder ratio of the metal composite ceramic powder based on the high heat energy input and stable flow atomization characteristics of the raw material gas plasma. The powder has high sphericity and can exhibit "water-like" fluidity.

[0030] The raw material gas is ionized using radio frequency plasma technology to obtain the raw material gas plasma. Wire material can be used as the metal raw material. The raw material gas plasma melts the wire material, which is then impacted, dispersed, and atomized into ultrafine droplets. These droplets exchange heat with condensed gas (argon) and are then cooled and solidified into ultrafine powder. This process ensures high sphericity of the metal-ceramic composite powder while producing finer powder with excellent fine powder yield. It also ensures high fine powder yield, higher powder sphericity, and almost no hollow powder in the fine powder; production efficiency is also high.

[0031] The raw material gas is ionized using radio frequency plasma technology to obtain the raw material gas plasma. When the metal raw material is a wire, the metal raw material will not come into contact with the reactor wall such as ceramic during the melting process, which can reduce the risk of inclusions. At the same time, the prepared metal-ceramic composite powder has almost no hollow powder, ensuring the "high purity and low void ratio" of the metal-ceramic composite powder.

[0032] The raw material gas is plasmaized using radio frequency plasma technology to obtain the raw material gas plasma. Using hot atomizing gas instead of cold atomizing gas can prevent the metal-ceramic composite powder particles from cooling rapidly and agglomerating into irregular shapes. The produced metal-ceramic composite powder has the characteristic of "high sphericity".

[0033] The metal raw material can be supplied to the plasma generating chamber and / or the reaction chamber communicating with the plasma generating chamber, so that the raw material gas plasma comes into contact with the metal raw material in the plasma generating chamber and / or the reaction chamber to generate the intermediate product.

[0034] The metal raw material can be added from outside the plasma generating chamber and / or the reaction chamber via a feeding device (not shown) to the interior of the plasma generating chamber and / or the reaction chamber, such as the top. The conveying speed of the metal raw material can be in the range of 1 kg / h to 15 kg / h or 2 kg / h to 8 kg / h. This helps to strike a balance between feeding efficiency and reaction speed, avoiding low production efficiency due to too slow a feeding speed, or incomplete reaction due to too fast a feeding speed, thus failing to achieve the ideal component ratio.

[0035] Alternatively, the metal raw material can be pre-placed in the plasma generating chamber and / or the reaction chamber. For example, a crucible can be placed at the bottom of the plasma generating chamber and / or the reaction chamber to support the metal raw material and raise it into the raw material gas plasma (plasma torch) to participate in the reaction and undergo recombination.

[0036] The intermediate product can be condensed to obtain the metal-ceramic composite powder by introducing a condensing gas into the plasma generating chamber and / or the reaction chamber, and bringing the condensing gas into contact with the intermediate product. The condensing gas may include argon, nitrogen, or a mixture of both. The temperature of the condensing gas can be room temperature. The flow rate of the condensing gas can be in the range of 3 m³ / s. 3 / h to 8m 3 / h.

[0037] In this embodiment of the invention, unless otherwise specifically indicated, the numerical values ​​may include errors such as measurement error, accuracy error, and measurement error, for example, errors within the range of ±5%. For example, 5% may include numerical values ​​within the range of 5% × (1 ± 5%), that is, numerical values ​​within the range of 4.75% to 5.25%.

[0038] In embodiments of the present invention, unless otherwise specifically indicated, the numerical range may include any sub-range therein, for example, 5%-15% may include 5%-10%, 10%-15%, 6%-12%, etc.

[0039] In some embodiments, when the raw material gas plasma comes into contact with the metal raw material, a portion of the metal raw material can undergo a chemical reaction with the raw material gas to generate a metal ceramic.

[0040] In some embodiments, the amount of the metal raw material is greater than the amount required to react with the raw material gas plasma.

[0041] In this way, the excess metal raw materials that have not participated in the chemical reaction can be physically combined with the metal ceramics generated by the chemical reaction.

[0042] On the other hand, in some embodiments, the raw material gas can undergo a complete chemical reaction, that is, the total amount of the raw material gas is equal to the amount of gas required for the reaction.

[0043] In some embodiments, the total amount of the raw material gas is greater than the amount of gas required for the reaction. The portion exceeding the amount required for the reaction is the portion of the raw material gas that did not participate in the reaction, which can also be referred to as the redundant portion.

[0044] The specific redundancy ratio of the raw material gas can be related to the output power of the power supply that ionizes the raw material gas and the flow rate of the raw material gas. For example, the lower the output power of the power supply that ionizes the raw material gas and the higher the flow rate of the raw material gas, the higher the redundancy ratio. The specific redundancy ratio of the raw material gas can also be related to the movement trajectory of metal ions, the gas turbulence state, etc.

[0045] The power output of the power source for ionizing the raw material gas can range from 30kW to 150kW. The gas pressure range of the plasma generation chamber and / or the reaction chamber can range from 40kPa to 160kPa. The flow rate of the raw material gas can range from 2m³ / h. 3 / h to 6m 3 / h or 3m 3 / h to 5m 3 / h.

[0046] In some embodiments, the volume of the unreacted feed gas accounts for 5-15% of the total volume of the feed gas.

[0047] In this way, it is beneficial to avoid the following: if the total amount of raw material gas is too large, the metal raw material will completely react to form metal ceramics, and there will be no remaining metal for physical composite; or if the total amount of raw material gas is too small, the amount of metal ceramics formed by the reaction will be insufficient and the target requirements cannot be met.

[0048] The unreacted raw material gas may include reactive gases that can participate in the reaction, such as one or more of oxygen, nitrogen, and carbon-containing gases, or non-reactive gases that cannot participate in the reaction, such as argon, or any mixture of the reactive and non-reactive gases.

[0049] The non-reactive gas can be provided and plasma-ionized before the reactive gas. The reactive gas can be provided after the plasma torch generated by the plasmaization of the non-reactive gas has stabilized, for example, the reactive gas can be provided 1 minute after the non-reactive gas is provided.

[0050] The non-reactive gas can generate a protective atmosphere and serve as a carrier gas. During the first ventilation phase, the non-reactive gas, supplied separately and initially, can have a power output range of 20kW to 50kW or 30kW to 50kW, a pressure range of 30kPa to 60kPa or 40kPa to 60kPa, and a flow rate range of 1m³. 3 / h to 15m 3 / h or 7m 3 / h to 8m 3 Plasmating under conditions of / h.

[0051] After the plasma torch generated by the ionization of the non-reactive gas stabilizes, the reactive gas can be introduced. During this second ventilation stage, the flow rate of the non-reactive gas can be reduced, and the flow rate of the non-reactive gas can be within the range of 3 m³ / s. 3 / h to 5m 3 / h or 3m 3 / h to 4m 3 / h, the flow rate of the reactive gas can be in the range of 2m³ / h. 3 / h to 6m 3 / h or 3m 3 / h to 5m 3 The power output range is 30kW to 150kW or 40kW to 100kW, and the gas pressure range is 40kPa to 160kPa or 80kPa to 100kPa. The plasma obtained by ionizing the raw material gas is a plasma mixture of the reactive gas and the non-reactive gas. The plasma mixture can react with each other and / or react and recombine with the metal raw material to generate the intermediate product.

[0052] Through the two aeration stages described above, the obtained plasma mixture exhibits stable performance, which is beneficial for controlling subsequent reactions and thus obtaining a metal-ceramic composite powder product with uniform particle size.

[0053] The reactive gas and the non-reactive gas can be introduced from different inlets. For example, in the first ventilation stage, the non-reactive gas is introduced from the central inlet and the edge inlet; in the second ventilation stage, the flow rate of the non-reactive gas in the central inlet remains unchanged, while the non-reactive gas is introduced from the edge inlet at a set reduced speed, and the reactive gas is introduced from the edge inlet at the same time.

[0054] In some embodiments, the feed gas includes a silicon-containing gas.

[0055] In this way, it can help the silicon-containing gas to react chemically with one or more of oxygen, nitrogen, and carbon-containing gases to generate silicon ceramics, and then the silicon ceramics can be physically combined with the metal raw materials to generate the intermediate product.

[0056] The silicon-containing gas can be a reactive gas that can participate in the reaction.

[0057] The amounts of reactive gases such as oxygen, nitrogen, carbon-containing gases, and silicon-containing gases, as well as the amounts of the metal raw materials, can be set according to the metal-to-ceramic ratio in the final metal-ceramic composite powder. Since no other elements are added in the preparation method 10, the purity of the metal raw materials or reactive gases participating in the reaction is very high, for example, above 99.9%. Therefore, the purity of the metal-ceramic composite powder can be greater than 99%, or even reach above 99.9%.

[0058] The percentage of the total volume of reactive gases such as oxygen, nitrogen, carbon-containing gases, and silicon-containing gases relative to the total volume of the raw material gases can range from 5% to 85%.

[0059] Controlling the amount of oxygen allows for control of the oxygen plasma content, thereby controlling the reaction rate and preventing deviations in the stoichiometry of the generated metal-ceramic composite powder from the target. It also facilitates control over the particle size and distribution of the metal-ceramic composite powder. Unreacted carbon can react with oxygen to form CO2; unreacted hydrogen can react with oxygen to form H2O.

[0060] In some embodiments, the silicon-containing gas includes hexamethylsiloxane (C6H4H2O). 18 OSi2), silane, or a mixture of both.

[0061] This can facilitate the production of higher quality silicon ceramics, such as SiC.

[0062] In some embodiments, the silicon-containing gas is hexamethylsiloxane, and the volume of hexamethylsiloxane accounts for 5% to 85% or 20% to 60% of the total volume of the raw material gas.

[0063] In some embodiments, the carbon-containing gas includes methane, acetylene, or a mixture of both.

[0064] This can help produce ceramics of better quality.

[0065] In some embodiments, the metal raw material includes one or more of the following: iron-based alloys, titanium-based alloys, nickel-based alloys, tungsten alloys, aluminum alloys, magnesium alloys, copper alloys, and precious metals.

[0066] This facilitates the acquisition of one or more metal-ceramic composite powders, including iron-based alloys, titanium-based alloys, nickel-based alloys, tungsten alloys, aluminum alloys, magnesium alloys, copper alloys, and precious metals.

[0067] In some embodiments, the metal raw material includes tungsten.

[0068] This facilitates the preparation of tungsten-containing cermet composite powders, such as tungsten-silicon carbide-tungsten carbide cermet composite powders with the chemical formula Wx(SiC)y(WC)z, where x, y, and z can be proportioned according to product performance requirements. (SiC)y(WC)z can be preferentially generated, with excess W added as needed. In some embodiments, x = 0-99%, y = 0.1-99%, and z = 0.1-99% by mass fraction.

[0069] For example, the temperature of the thermal plasma flame of hexamethylsiloxane can reach up to 10,000°C. At such a high temperature, the metallic raw material tungsten can melt instantly, and some of the tungsten can be oxidized instantly. The excess tungsten will fully and uniformly combine with SiC and WC in atomic form at the atomic level, which is beneficial to improving the production efficiency and product quality of tungsten-silicon carbide-tungsten carbide metal ceramic composite powder products.

[0070] In some embodiments, the metal raw material is in a solid or liquid state.

[0071] This facilitates the sourcing, transportation, and storage of the metal raw materials.

[0072] In some embodiments, the form of the metal raw material includes one or more of the following: powder, wire, rod, and tube.

[0073] This can facilitate the sourcing, transportation, and storage of the metal raw materials.

[0074] In some embodiments, the metal raw material is in the form of droplets when it comes into contact with the raw material gas plasma.

[0075] This can help avoid the formation of nano-metal particle satellite spheres.

[0076] The metal raw material can be controlled to form droplets upon contact with the plasma by controlling the power output of the power source that ionizes the raw material gas. If the power output is too high, the metal raw material will vaporize and condense into nano-metal satellite particles. These nano-metal particles are undesirable components, reducing the flowability of the metal-ceramic composite powder and the density of the sintered product. With appropriate power, such as in the range of 40kW to 100kW, the solid metal raw material can be liquefied into droplets, and the liquid state can be maintained or transformed into droplets. This avoids volatilization or agglomeration in the plasma (plasma torch), reducing or eliminating the possibility of nano-metal satellite particle formation and promoting the formation of coherent and semi-coherent relationships between ceramic molecules and metal atoms.

[0077] Another aspect of the present invention relates to a metal-ceramic composite powder, which is prepared by the metal-ceramic composite powder preparation method 10 as described in this application.

[0078] The metal-ceramic composite powder of this application has a simple preparation process, a short process, high purity, good density, and good controllability of particle size and particle size distribution.

[0079] The metal-ceramic composite powder material products of the present application have better forming and fatigue properties, and can be used as materials for additive manufacturing technology and metal injection molding technology.

[0080] The particle size distribution of the metal-ceramic composite powder can be: D50 ranging from 5 micrometers to 120 micrometers, or 30 micrometers to 100 micrometers, with the ratio of D90 to D50 less than 3, and the ratio of D10 to D50 greater than 0.3. Here, D represents the diameter of the powder particles, D50 represents the diameter of the cumulative 50% of the particles, D10 represents the diameter of the cumulative 10% of the particles, and D90 represents the diameter of the cumulative 90% of the particles. In some embodiments, the obtained metal-ceramic composite powder particle size distribution is: D50 of 50 micrometers, D90 less than 100 micrometers, and D10 greater than 30 micrometers.

[0081] The metal-ceramic composite powder has the characteristics of high purity, small particle size, and narrow particle size distribution. Using the metal-ceramic composite powder, metal-ceramic composite parts can be prepared by 3D printing and heat treatment, which can improve the sintering density, formability and fatigue performance of the parts.

[0082] The various specific embodiments described above and shown in the accompanying drawings are for illustrative purposes only and do not represent the entirety of the invention. Any modifications made by those skilled in the art within the scope of the basic technical concept of this invention are within the protection scope of this invention.

Claims

1. A method for preparing a metal-ceramic composite powder (10), characterized in that, Includes the following steps: (12) Provide raw material gas, the raw material gas including one or more of oxygen, nitrogen, and carbon-containing gas, the raw material gas including silicon-containing gas, the silicon-containing gas including hexamethylsiloxane, silane, or a mixture of the two; (14) Plasmonize the raw material gas to obtain raw material gas plasma; (16) The raw material gas plasma is brought into contact with a metal raw material to generate an intermediate product, wherein the metal raw material is in the form of droplets when in contact with the raw material gas plasma, the amount of the metal raw material is greater than the amount required to react with the raw material gas plasma, and the volume of the raw material gas that does not participate in the reaction accounts for 5-15% of the total volume of the raw material gas; and (18) Condensate the intermediate product to obtain the metal-ceramic composite powder.

2. The method for preparing the metal-ceramic composite powder as described in claim 1 (10), characterized in that, The raw material gas is plasma-ionized using radio frequency plasma technology to obtain the raw material gas plasma.

3. The method for preparing the metal-ceramic composite powder as described in claim 1 (10), characterized in that, The unreacted raw material gas includes non-reactive gases that cannot participate in the reaction, or any mixture of reactive gases and non-reactive gases that can participate in the reaction, wherein the non-reactive gases are provided and plasma-ionized before the reactive gases.

4. The method for preparing the metal-ceramic composite powder as described in claim 1 (10), characterized in that, The carbon-containing gas includes methane, acetylene, or a mixture of both.

5. The method for preparing the metal-ceramic composite powder according to any one of claims 1-4 (10), characterized in that, The metal raw materials include one or more of the following: iron-based alloys, titanium-based alloys, nickel-based alloys, tungsten alloys, aluminum alloys, magnesium alloys, copper alloys, and precious metals.

6. The method for preparing the metal-ceramic composite powder according to any one of claims 1-4 (10), characterized in that, The metallic raw material includes tungsten.

7. The method for preparing the metal-ceramic composite powder according to any one of claims 1-4 (10), characterized in that, The metal raw materials are in solid or liquid states.

8. The method for preparing the metal-ceramic composite powder according to any one of claims 1-4 (10), characterized in that, The metal raw materials may be in the form of one or more of the following: powder, wire, rod, and tube.

9. A metal-ceramic composite powder, characterized in that, It is prepared by the method (10) for preparing metal-ceramic composite powder as described in any one of claims 1-8.

10. The metal-ceramic composite powder as described in claim 9, characterized in that, The particle size distribution is as follows: D50 ranges from 5 micrometers to 120 micrometers or from 30 micrometers to 100 micrometers, the ratio of D90 to D50 is less than 3, and the ratio of D10 to D50 is greater than 0.3.

Citation Information

Patent Citations

  • Process for producing ultrafine particles of ceramics

    US4642207A