Long straight weld reciprocating filling friction stir welding method and welding device

By employing a reciprocating filling friction stir wire welding method for long straight welds, and utilizing the reciprocating motion of the upper and lower stirring pins and a split design, problems such as incomplete penetration and incomplete fusion in the welding of long straight welds are solved, thereby improving welding efficiency and stirring head life, and forming high-quality welds without keyholes.

CN117564435BActive Publication Date: 2026-11-20SHANDONG UNIV
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202311280973.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-09-28
Publication Date
2026-11-20
Estimated Expiration
2043-09-28

AI Technical Summary

Technical Problem

Existing friction stir welding methods have problems such as incomplete penetration, incomplete fusion, and weak connection in long straight welds. In addition, the stirring pin has a large insertion depth, high forward resistance, slow welding speed, low efficiency, and short stirring head life.

Method used

The long straight weld seam reciprocating filling friction stir wire welding method is adopted. Through the reciprocating motion and synergistic effect of the upper and lower stirring pins, the old material enters and the new material exits in a cyclical disturbance, reducing the insertion depth of the stirring pins and improving the material flowability. The split stirring tool design is adopted to adapt to workpieces of different thicknesses.

Benefits of technology

It achieves high-quality long straight weld seam connections, reduces forward resistance, improves welding speed and efficiency, extends the life of the stirring head, and results in a smooth weld seam surface without keyholes and good weld performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117564435B_ABST
    Figure CN117564435B_ABST
Patent Text Reader

Abstract

The present application relates to the technical field of friction stir welding, and particularly relates to a long straight weld reciprocating filling type friction stir line welding method and a welding device. The line welding method comprises the following steps: moving an upper stirring tool and a lower stirring tool to the upper and lower sides of a welding starting point of a workpiece to be welded respectively, and pressing the workpiece to be welded at a predetermined pressure and rotating; moving the upper stirring needle and the lower stirring needle at the same speed simultaneously and reciprocating, until the temperature field and the plastic flow field of the welding starting point reach a quasi-steady state, wherein the maximum distance of the movement is half of the total thickness of the workpiece to be welded; moving the upper stirring needle and the lower stirring needle at the same speed along the horizontal direction while moving upward and downward, and the upper stirring sleeve and the lower stirring sleeve keep the position unchanged in the vertical direction and follow the translation, until reaching a welding ending point. The present application solves the problems of incomplete penetration, incomplete fusion and weak connection in the line welding process of long straight weld, and reduces the forward resistance in the transverse movement process of the stirring needle.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of friction stir welding technology, and in particular to a method and apparatus for reciprocating filling friction stir wire welding of long straight weld seams. Background Technology

[0002] The information disclosed in this background section is intended only to enhance understanding of the overall background of the invention and is not necessarily to be construed as an admission or in any way implying that such information constitutes prior art known to those skilled in the art.

[0003] Friction stir welding (FSW) is a solid-state welding method invented by the Welding Institute in the UK in 1991. Its main advantages include low heat input, high weld quality, minimal deformation, and an environmentally friendly welding process. It is particularly suitable for welding lightweight non-ferrous metals such as aluminum alloys and has significant application potential in aerospace, rail transportation, and new energy vehicles.

[0004] Subsequently, researchers proposed several improved friction stir welding methods, including static shoulder friction stir welding, double shoulder friction stir welding, hot / cold source assisted friction stir welding, and ultrasonic energy field assisted friction stir welding. However, after the stirring head leaves the workpiece after welding, these methods leave an exit hole (usually called a keyhole) on the workpiece, which not only affects the aesthetics and smoothness of the weld but also weakens the overall performance of the weld.

[0005] The prior art discloses a backfill spot welding method, which can produce spot welded joints without keyholes. However, it is only for spot welding of lap joints. In the process of wire welding of long straight welds, it still faces problems such as incomplete penetration / incomplete welding / weak connection at the bottom of the workpiece. In addition, the stirring pin / rod has a large insertion depth, which causes it to bear a large forward resistance. The welding speed should not be too fast, the welding efficiency is low, and the life of the stirring head is short. Summary of the Invention

[0006] To address the shortcomings of existing technologies, the purpose of this invention is to provide a reciprocating filling friction stir wire welding method for long straight welds. During the lateral movement, old material continuously enters and new material is discharged from the cavities of the upper / lower stirring pins, which greatly improves the plastic flow of material in the horizontal and vertical directions. This solves problems such as incomplete penetration / incomplete welding / weak connection in the wire welding process of long straight welds and reduces the forward resistance of the stirring pins during the lateral movement.

[0007] To achieve the above objectives, the embodiments of the present invention provide the following technical solutions:

[0008] A method for reciprocating filling friction stir wire welding of long straight weld seams includes:

[0009] The upper stirring tool and the lower stirring tool are moved to the upper and lower sides of the starting point of the workpiece to be welded, respectively, and are pressed against the sides of the workpiece to be welded with a predetermined pressure and rotated. The upper stirring tool includes an upper stirring sleeve and an upper stirring needle, and the lower stirring tool includes a lower stirring sleeve and a lower stirring needle.

[0010] The upper and lower stirring pins move up and down simultaneously at the same speed until the temperature field and plastic flow field at the starting point of the weld reach a quasi-steady state. The maximum distance moved is half the total thickness of the workpiece material being welded.

[0011] The upper and lower stirring pins move horizontally at the same speed as they move up and down, while the upper and lower stirring sleeves remain in their vertical positions and follow the horizontal movement until the final welding point is reached.

[0012] Optionally, the workpieces to be welded may be pretreated between welding operations, including: grinding the mating surfaces of the workpieces to be welded to a smooth surface, removing the oxide film, cleaning with anhydrous ethanol, and drying.

[0013] Optionally, before the upper and lower stirring tools come into contact with the workpiece to be welded, the ends of the upper stirring pin and the upper stirring sleeve are flush, and the ends of the lower stirring pin and the lower stirring sleeve are flush.

[0014] Optionally, during the reciprocating motion of the upper and lower stirring needles, the upper and lower stirring needles move at the same speed in the vertical direction, and the distance between the lower end of the upper stirring needle and the upper end of the lower stirring needle remains unchanged.

[0015] Optionally, when the upper and lower stirring pins move upward, the lower stirring pin squeezes the plastic material of the workpiece to be welded into the upper stirring sleeve; when the upper and lower stirring pins move downward, the upper stirring pin squeezes the plastic material of the workpiece to be welded into the lower stirring sleeve.

[0016] Optionally, the upper stirring sleeve, upper stirring pin, lower stirring sleeve, and lower stirring pin have the same translation speed during the welding stage; the upper stirring sleeve, upper stirring pin, lower stirring sleeve, and lower stirring pin may have the same or different rotation speeds.

[0017] Optionally, after reaching the final weld point, the upper stirring pin moves to a position flush with the end of the upper stirring sleeve, and the lower stirring pin moves to a position flush with the end of the lower stirring sleeve; the upper and lower stirring tools stop rotating and move upward and downward respectively to complete the welding.

[0018] This invention also provides a welding apparatus for the reciprocating filling friction stir wire welding method for long straight welds as described above, comprising an upper stirring tool and a lower stirring tool, the upper stirring tool and the lower stirring tool being located on opposite sides of the workpiece to be welded; the upper stirring tool comprises an upper stirring sleeve and an upper stirring pin, the upper stirring sleeve having a through hole, the upper stirring pin being disposed within the through hole of the upper stirring sleeve and movable along the axis of the upper stirring sleeve; the lower stirring tool comprises a lower stirring sleeve and a lower stirring pin, the lower stirring sleeve having a through hole, the lower stirring pin being disposed within the through hole of the lower stirring sleeve and movable along the axis of the lower stirring sleeve.

[0019] Optionally, the outer diameters of the upper and lower stirring sleeves are equal, and they are kept aligned vertically during welding. The diameters of the upper and lower stirring pins are also equal.

[0020] Optionally, the ends of the upper and lower stirring sleeves facing the workpiece to be welded are smooth planes or rough surfaces; the ends of the upper and lower stirring pins facing the workpiece to be welded are smooth planes or rough surfaces, and the circumferential side surfaces are smooth or rough surfaces.

[0021] One or more technical solutions provided in the embodiments of the present invention have at least the following technical effects or advantages:

[0022] 1. The reciprocating filling friction stir wire welding method for long straight welds of the present invention can achieve high-quality connection of long straight welds in thick plates with butt joints, lap joints, or other possible joint forms. While the upper / lower stirring tools move laterally, old material continuously enters and new material is discharged from the cavity of the upper / lower stirring pins. The upper / lower stirring pins are repeatedly inserted into the workpiece, cyclically disturbing the butt / lap joint interface, which greatly improves the plastic flow of material in the horizontal and vertical directions. It solves the problems of incomplete penetration / incomplete welding / weak connection in the wire welding process of long straight welds, reduces the forward resistance of the stirring pins during the lateral movement, thus increasing the welding speed and thus the welding efficiency, and also extending the service life of the stirring head.

[0023] 2. The size of the stirring tool is highly flexible. Since the upper / lower stirring pins can move independently of the upper / lower stirring sleeve, their insertion depth into the workpiece can be adjusted arbitrarily. Therefore, when the thickness of the workpiece changes, only the insertion depth of the upper / lower stirring pins needs to be changed, and there is no need to replace the stirring tool.

[0024] 3. The maximum insertion depth of the upper / lower stirring pins is only half the total thickness of the workpiece material to complete high-quality welding, which greatly reduces the stress on the stirring tool and improves welding efficiency.

[0025] 4. There is almost no material loss during the welding process, no keyhole after welding, the weld surface is smooth, and the overall performance of the weld is good.

[0026] Advantages of additional aspects of the invention will be set forth in the description which follows, and in part will be obvious from the description, or may be learned by practice of the invention.

[0027] To make the above-mentioned objects, features and advantages of the present invention more apparent and understandable, preferred embodiments are described below in detail with reference to the accompanying drawings. Attached Figure Description

[0028] To more clearly illustrate the technical solutions in the embodiments of this application or the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments recorded in this application. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.

[0029] Figure 1 This is a schematic diagram of a long straight weld seam reciprocating filling friction stir wire welding method using the welding device of the present invention;

[0030] In the diagram: 1. Upper stirring sleeve; 2. Upper stirring pin; 3. Lower stirring sleeve; 4. Lower stirring pin; 5. Workpiece to be welded;

[0031] The distances or dimensions between parts have been exaggerated to show their positions; the diagram is for illustrative purposes only. Detailed Implementation

[0032] It should be noted that the following detailed description is illustrative and intended to provide further explanation of the invention. Unless otherwise specified, all technical and scientific terms used in this invention have the same meaning as commonly understood by one of ordinary skill in the art to which this invention pertains.

[0033] It should be noted that the terminology used herein is for the purpose of describing particular embodiments only and is not intended to limit the scope of exemplary embodiments according to the invention. As used herein, unless otherwise expressly indicated by the invention, the singular form is intended to include the plural form as well. Furthermore, it should be understood that when the terms "comprising" and / or "including" are used in this specification, they indicate the presence of features, steps, operations, devices, components, and / or combinations thereof.

[0034] Conventional friction stir welding (FSW) is designed for wire welding of long, straight weld seams. As mentioned in the background section, it was invented by the Welding Institute in the UK in 1991. Conventional friction stir spot welding, on the other hand, was invented by Mazda in Japan around 1993. Existing spot welding techniques designed for lap joints, if directly applied to wire welding of butt or lap joints of long, straight weld seams, require the stirring pin / rod to have an insertion depth equal to or slightly less than the plate thickness. Therefore, problems such as incomplete penetration / incomplete fusion / weak connection at the bottom of the workpiece still exist. Furthermore, a large insertion depth of the stirring pin / rod results in significant forward resistance, limiting welding speed, shortening the stirring head's lifespan, and reducing welding efficiency.

[0035] For ease of understanding, this embodiment first introduces the welding apparatus of the present invention, such as... Figure 1 As shown, it includes an upper stirring tool and a lower stirring tool, which are located on both sides of the workpiece to be welded. The workpiece to be welded can adopt a butt joint, lap joint, or other possible joint forms.

[0036] The upper stirring tool includes an upper stirring sleeve and an upper stirring needle. The upper stirring sleeve has a through hole, and the upper stirring needle is disposed within the through hole of the upper stirring sleeve and can move along the axis of the upper stirring sleeve. The lower stirring tool includes a lower stirring sleeve and a lower stirring needle. The lower stirring sleeve has a through hole, and the lower stirring needle is disposed within the through hole of the lower stirring sleeve and can move along the axis of the lower stirring sleeve. The terms "upper" and "lower" only indicate the upward and downward directions as shown in the drawings themselves and do not limit the structure. They are merely for the convenience of describing the invention and simplifying the description, and do not indicate or imply that the device or component referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limitations on the invention.

[0037] The upper and lower stirring tools are respectively placed on the upper and lower sides of the workpiece to be welded, and are driven by different servo motors to realize rotation, upward movement, downward movement, translation and other actions to complete the welding.

[0038] Both the upper and lower stirring sleeves are cylindrical, with their ends being smooth flat surfaces or rough surfaces with certain textured features. Both the upper and lower stirring pins are cylindrical / conical, and their sides may have features such as threads, flat surfaces, or grooves. Their ends may be flat surfaces or rough surfaces with certain textured features.

[0039] The outer diameters of the upper and lower stirring sleeves are 1mm to 500mm and should be equal, and they should be kept aligned vertically during welding. The inner diameters of the upper stirring pin (upper stirring sleeve) and the lower stirring pin (lower stirring sleeve) are 1mm to 200mm and should be equal or slightly different.

[0040] During the welding process, when the upper stirring tool (upper stirring sleeve 1 and upper stirring needle 2) and the lower stirring tool (lower stirring sleeve 3 and lower stirring needle 4) move along the welding direction, the angle deviating from the vertical direction is 0° to 15°.

[0041] During welding, the upper and lower sets of stirring tools work together, pressing the workpiece against the workpiece from both above and below, rotating at high speed and moving along a predetermined trajectory. Under the influence of frictional heat, the workpiece material reaches a plastic state. Then, the upper and lower stirring pins reciprocate up and down at the same speed, driving the material to flow in both horizontal and vertical directions and disturbing the bonding interface of the workpiece. Finally, the upper and lower stirring pins return to their flush positions with the upper and lower stirring sleeves, completing the welding and forming a high-quality, keyhole-free, long, straight weld seam in a thick plate.

[0042] The welding device of this invention features a split design for both the upper and lower stirring tools. Both the upper and lower stirring sleeves and the upper and lower stirring pins can move independently up and down vertically, enabling precise control of welding heat input and material plastic flow. The upper and lower stirring pins act on the upper and lower surfaces of the workpiece, effectively avoiding welding defects such as incomplete penetration, incomplete fusion, and weak connections, thus enhancing the metallurgical bonding strength of the workpiece. The maximum insertion depth of both the upper and lower stirring pins is only half the total thickness of the workpiece, reducing welding resistance and improving welding efficiency. Throughout the welding process, there is almost no loss of workpiece material, resulting in a smooth weld seam without keyholes.

[0043] A method for reciprocating filling wire welding of long straight weld seams of lapped or butt joints of thick plates using the aforementioned welding equipment includes:

[0044] Step 1: Corresponding Figure 1 (a) The mating surfaces of the workpiece 5 to be welded are ground flat, the oxide film is cleaned, and the workpiece 5 is cleaned and dried with anhydrous ethanol. Then the workpiece 5 to be welded is fixed with a specific clamp. The upper stirring tool (upper stirring sleeve 1 and upper stirring needle 2) and the lower stirring tool (lower stirring sleeve 3 and lower stirring needle 4) are moved to the upper and lower sides of the starting point of the workpiece 5 to be welded and aligned. The ends of the upper stirring needle 2 and the upper stirring sleeve 1 are flush, and the ends of the lower stirring needle 4 and the lower stirring sleeve 3 are flush.

[0045] Step 2: Corresponding Figure 1 (b) Start the automatic program to begin the welding process. The upper stirring tool (upper stirring sleeve 1 and upper stirring needle 2) and the lower stirring tool (lower stirring sleeve 3 and lower stirring needle 4) press on both sides of the starting point of the workpiece 5 under a certain pressure and start to rotate respectively.

[0046] Step 3: Corresponding Figure 1(c) When the temperature at the starting point of the weld reaches the plastic state of the material, the upper stirring sleeve 1 and the lower stirring sleeve 3 remain stationary, while the upper stirring pin 2 and the lower stirring pin 4 move up or down at the same speed. The maximum distance of the upward or downward movement is half of the total thickness of the material of the workpiece 5 to be welded.

[0047] Step 4: Corresponding Figure 1 (d) Repeat step 3, with the upper stirring needle 2 and the lower stirring needle 4 moving up or down at the same speed, reciprocating until the temperature field and plastic flow field around the stirring tool reach a quasi-steady state.

[0048] Step 5: Corresponding Figure 1 (e) The upper stirring tool (upper stirring sleeve 1 and upper stirring needle 2) and the lower stirring tool (lower stirring sleeve 3 and lower stirring needle 4) move horizontally at the same speed to begin welding. During this process, the upper stirring sleeve 1 and the lower stirring sleeve 3 maintain their vertical positions, while the upper stirring needle 2 and the lower stirring needle 4 move upward or downward simultaneously at the same speed. The maximum upward or downward distance is half the total thickness of the material of the workpiece 5 to be welded.

[0049] Step 6: Corresponding Figure 1 (f) Repeat step 5, with the upper stirring needle 2 and the lower stirring needle 4 moving up or down at the same speed, reciprocating until the upper stirring tool (upper stirring sleeve 1 and upper stirring needle 2) and the lower stirring tool (lower stirring sleeve 3 and lower stirring needle 4) reach the final welding point.

[0050] Step 7: Corresponding Figure 1 (g) Upon reaching the final welding point, the upper stirring pin 2 moves to a position flush with the end of the upper stirring sleeve 1, and the lower stirring pin 4 moves to a position flush with the end of the lower stirring sleeve 3.

[0051] Step 8: Corresponding Figure 1 (h) The upper stirring tool (upper stirring sleeve 1 and upper stirring needle 2) and the lower stirring tool (lower stirring sleeve 3 and lower stirring needle 4) stop rotating and move upward and downward respectively, leaving the workpiece 5 to be welded, thus completing the welding.

[0052] The rotation speeds of the four tool components—upper stirring sleeve 1, upper stirring needle 2, lower stirring sleeve 3, and lower stirring needle 4—can be the same or different to adjust and optimize the heat generation and material flow during the welding process. The rotation speed can be 0–20,000 rpm.

[0053] The four tool components, namely the upper stirring sleeve 1, the upper stirring needle 2, the lower stirring sleeve 3, and the lower stirring needle 4, have the same translation speed during the welding stage, which is 0 to 10 m / min.

[0054] The speed / distance of the upper stirring needle 2 and the lower stirring needle 4 moving in the vertical direction are always kept consistent. The purpose is to ensure that the material in the stirring area does not overflow or form cavities, thus ensuring the quality of the weld formation.

[0055] The above steps are applicable for welding long straight welds in thick plates using butt joints, lap joints, and other possible joint forms on aluminum alloys, magnesium alloys, copper alloys, titanium alloys, high-entropy alloys, steel, and any two or more dissimilar metals mentioned above. Furthermore, they offer significant improvements and advantages over conventional methods.

[0056] First, both the upper and lower stirring tools are designed as separate units, and the components work together to adapt to workpieces of different thicknesses. When the thickness of the workpiece changes, welding can be achieved simply by modifying the insertion depth of the upper and lower stirring pins in the welding program.

[0057] Secondly, the stirring tool works synergistically from the upper and lower surfaces of the workpiece being welded. Old material continuously enters and new material is discharged from the cavities of the upper and lower stirring pins, which greatly improves the plastic flow of the material in the horizontal and vertical directions. Furthermore, the heat input and material flow behavior at different parts of the workpiece being welded can be easily optimized by adjusting the rotation speed of the stirring tool, effectively avoiding welding defects such as incomplete penetration, incomplete fusion, and weak connection, and improving the weld bonding strength.

[0058] Furthermore, the maximum insertion depth of the upper and lower stirring pins is only half the total thickness of the workpiece material being welded, thus significantly reducing the rotational torque and forward resistance of the stirring pins, reducing the wear tendency of the stirring tool, ensuring the service life of the stirring tool, reducing production costs, and improving welding efficiency.

[0059] Finally, the synergistic effect of the various parts of the stirring tool ensures that the material in the plastic deformation area is always contained within a region of constant volume. Therefore, there is almost no loss of the workpiece material during the entire welding process. There is no keyhole at the final weld point after welding, the weld surface is smooth, and the overall performance of the weld is good.

[0060] While the specific embodiments of the present invention have been described above in conjunction with the accompanying drawings, this is not intended to limit the scope of protection of the present invention. Those skilled in the art should understand that various modifications or variations that can be made by those skilled in the art without creative effort based on the technical solutions of the present invention are still within the scope of protection of the present invention.

[0061] Finally, it should be noted that, unless otherwise specified, the embodiments of the present invention and the various features thereof can be combined with each other, all of which are within the protection scope of the present invention. Furthermore, all or part of the steps in the above methods can be executed in a computer system such as a set of computer-executable instructions, and although the steps are listed in the order 1, 2, 3…, in some cases, the steps shown or described may be performed in a different order than that shown here.

Claims

1. A method for reciprocating filling friction stir wire welding of long straight weld seams, characterized in that, include: The upper stirring tool and the lower stirring tool are moved to the upper and lower sides of the starting point of the workpiece to be welded, respectively, and are pressed against the sides of the workpiece to be welded with a predetermined pressure and rotated. The upper stirring tool includes an upper stirring sleeve and an upper stirring needle, and the lower stirring tool includes a lower stirring sleeve and a lower stirring needle. The upper and lower stirring pins move up and down simultaneously at the same speed until the temperature field and plastic flow field at the starting point of the weld reach a quasi-steady state. The maximum distance moved is half the total thickness of the workpiece material being welded. The upper and lower stirring pins move horizontally at the same speed as they move up and down, while the upper and lower stirring sleeves remain in their vertical positions and follow the horizontal movement until the final welding point is reached.

2. The long straight weld seam reciprocating filling friction stir wire welding method as described in claim 1, characterized in that, Pre-treatment of the workpieces to be welded between welding operations includes: grinding the joint surfaces of the workpieces to be welded smooth, removing the oxide film, cleaning with anhydrous ethanol, and drying.

3. The reciprocating filling friction stir wire welding method for long straight weld seams as described in claim 1, characterized in that, Before the upper and lower stirring tools come into contact with the workpiece to be welded, the ends of the upper stirring pin and the upper stirring sleeve are flush, and the ends of the lower stirring pin and the lower stirring sleeve are flush.

4. The reciprocating filling friction stir wire welding method for long straight welds as described in claim 1, characterized in that, During the reciprocating motion of the upper and lower stirring needles, the upper and lower stirring needles move at the same speed in the vertical direction, and the distance between the lower end of the upper stirring needle and the upper end of the lower stirring needle remains unchanged.

5. The reciprocating filling friction stir wire welding method for long straight welds as described in claim 4, characterized in that, When the upper and lower stirring pins move upward, the lower stirring pin squeezes the plastic material of the workpiece to be welded into the upper stirring sleeve; when the upper and lower stirring pins move downward, the upper stirring pin squeezes the plastic material of the workpiece to be welded into the lower stirring sleeve.

6. The reciprocating filling friction stir wire welding method for long straight welds as described in claim 1, characterized in that, The upper stirring sleeve, upper stirring pin, lower stirring sleeve, and lower stirring pin have the same translation speed during the welding stage; the upper stirring sleeve, upper stirring pin, lower stirring sleeve, and lower stirring pin may have the same or different rotation speeds.

7. The reciprocating filling friction stir wire welding method for long straight welds as described in claim 1, characterized in that, After reaching the final welding point, the upper stirring pin moves to a position flush with the end of the upper stirring sleeve, and the lower stirring pin moves to a position flush with the end of the lower stirring sleeve. The upper and lower stirring tools stop rotating and move upward and downward respectively to complete the welding.

8. A welding apparatus for use in the reciprocating filling friction stir wire welding method for long straight welds as described in any one of claims 1-7, characterized in that, It includes an upper stirring tool and a lower stirring tool, which are located on both sides of the workpiece to be welded; The upper stirring tool includes an upper stirring sleeve and an upper stirring needle. The upper stirring sleeve has a through hole, and the upper stirring needle is disposed in the through hole of the upper stirring sleeve and can move along the axis of the upper stirring sleeve. The lower stirring tool includes a lower stirring sleeve and a lower stirring needle. The lower stirring sleeve has a through hole, and the lower stirring needle is disposed in the through hole of the lower stirring sleeve and can move along the axis of the lower stirring sleeve.

9. The welding apparatus as described in claim 8, characterized in that, The outer diameters of the upper and lower stirring sleeves are equal, and they remain aligned vertically during welding. The diameters of the upper and lower stirring pins are also equal.

10. The welding apparatus as claimed in claim 8, characterized in that, The ends of the upper and lower stirring sleeves facing the workpiece to be welded are smooth or rough surfaces; the ends of the upper and lower stirring pins facing the workpiece to be welded are smooth or rough surfaces, and the circumferential side surfaces are smooth or rough surfaces.

Citation Information

Patent Citations

  • Double-sided friction stir welding method for metal plate and double-sided friction stir welding device

    CN111050973A

  • Key-hole-free friction stir spot welding method

    WO2021212650A1