High electron mobility transistor epitaxial structure

By designing a first nitride layer and a second nitride layer in the epitaxial structure of a high electron mobility transistor, the problems of cracking and warping caused by the difference in the thermal expansion coefficients of the materials were solved, thereby improving the voltage withstand performance and epitaxial quality of the transistor.

CN117594650BActive Publication Date: 2026-11-20GLOBALWAFERS CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202310483606.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2022-08-18
Filing Date
2023-04-28
Publication Date
2026-11-20
Estimated Expiration
2043-04-28

AI Technical Summary

Technical Problem

Existing high electron mobility transistor structures are prone to defects such as cracks, warping, and breakage under temperature changes due to differences in the thermal expansion coefficients of the materials, which affects their voltage withstand performance.

Method used

A high electron mobility transistor epitaxial structure is adopted, including a substrate, a nucleation layer, a buffer layer, a first nitride layer, a second nitride layer, a channel layer, and a barrier layer. By designing the carbon doping and film thickness ratio of the first nitride layer and the second nitride layer, defects such as warpage and breakage are reduced.

Benefits of technology

It effectively reduces cracks, warpage, and fractures in high electron mobility transistor structures, improving the transistor's voltage withstand performance and epitaxial quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117594650B_ABST
    Figure CN117594650B_ABST
Patent Text Reader

Abstract

A high electron mobility transistor epitaxial structure includes a substrate, a nucleation layer, a buffer layer, a first nitride layer, a second nitride layer, a channel layer, and a barrier layer, the nucleation layer is located above the substrate; the buffer layer is located above the nucleation layer; the first nitride layer is located above and in contact with the buffer layer; the second nitride layer is located above and in contact with the first nitride layer, the film thickness of the first nitride layer is less than the film thickness of the second nitride layer, the second nitride layer has carbon doping, the carbon concentration in the first nitride layer is less than the carbon concentration in the second nitride layer; the channel layer is located above the second nitride layer.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to semiconductor technology; in particular, it relates to a high electron mobility transistor. Background Technology

[0002] A high electron mobility transistor (HEMT) is a transistor with a two-dimensional electron gas (2-DEG). The 2-DEG is adjacent to the heterojunction surface between two materials with different band gaps. Since the HEMT does not use doped regions as the carrier channels of the transistor, but uses a 2-DEG with high electron mobility as the carrier channels, the HEMT has characteristics such as high breakdown voltage, high electron mobility, low on-resistance and low input capacitance, and can be widely used in high-power semiconductor devices.

[0003] However, in existing high electron mobility transistor (HEM) structures, the different materials used in each layer, along with varying coefficients of thermal expansion, can lead to surface cracks, warping, or fractures due to varying temperatures and the resulting dissimilar stresses. This can negatively impact the HEM's voltage withstand capability. Therefore, reducing defects such as cracks, warping, and fractures in HEM structures is a pressing issue that needs to be addressed. Summary of the Invention

[0004] In view of this, the purpose of the present invention is to provide a high electron mobility transistor epitaxial structure that can effectively reduce defects such as cracks, warping and breakage in high electron mobility transistor structures.

[0005] To achieve the above objectives, the present invention provides a high electron mobility transistor epitaxial structure comprising a substrate, a nucleation layer, a buffer layer, a first nitride layer, a second nitride layer, a channel layer, and a barrier layer. The nucleation layer is located above the substrate; the buffer layer is located above the nucleation layer; the first nitride layer is located above and in contact with the buffer layer; the second nitride layer is located above and in contact with the first nitride layer, the thickness of the first nitride layer is less than the thickness of the second nitride layer, the second nitride layer is carbon-doped, and the carbon concentration in the first nitride layer is less than the carbon concentration in the second nitride layer; the channel layer is located above the second nitride layer; and a two-dimensional electron gas is formed in the channel layer along the interface between the channel layer and the barrier layer.

[0006] The present invention also provides a high electron mobility transistor epitaxial structure comprising a substrate, a nucleation layer, a buffer layer, a first nitride layer, a second nitride layer, a channel layer, and a barrier layer. The nucleation layer is located above the substrate; the buffer layer is located above the nucleation layer; the first nitride layer is located above and in contact with the buffer layer; the second nitride layer is located above and in contact with the first nitride layer; the channel layer is located above the second nitride layer; a two-dimensional electron gas is formed in the channel layer along the interface between the channel layer and the barrier layer; wherein the absolute value of the warpage (BOW) of the high electron mobility transistor epitaxial structure is less than 30 μm.

[0007] The advantage of this invention is that, through the structural design of the first nitride layer and the second nitride layer, defects such as cracks, warping and breakage in the high electron mobility transistor structure can be effectively reduced. Attached Figure Description

[0008] Figure 1 This is a schematic diagram of a high electron mobility transistor epitaxial structure according to a preferred embodiment of the present invention.

[0009] Figure 2 This is a flowchart of a preferred embodiment of the high electron mobility transistor epitaxy method of the present invention.

[0010] Figure 3 This is a flowchart of a preferred embodiment of the high electron mobility transistor epitaxy method of the present invention.

[0011] Figure 4 This is a schematic diagram of a high electron mobility transistor epitaxial structure as a comparative example.

[0012] Explanation of reference numerals in the attached figures: 1,2: Epitaxial structure of high electron mobility transistor 10: Substrate 20: Nucleation layer 30: Buffer layer 40: First nitride layer 50: Second nitride layer 52: Third nitride layer 521: Low-doped nitride layer 522: Highly doped nitride layer 60: Channel Layer 70: Barrier Layer 80: Passivation layer S02, S04, S06, S08, S10, S12, S14: Steps Detailed Implementation To more clearly illustrate the present invention, preferred embodiments are described in detail below with reference to the accompanying drawings. Please refer to... Figure 1 As shown, a high electron mobility transistor epitaxial structure 1 according to a preferred embodiment of the present invention includes a substrate 10, a nucleation layer 20, a buffer layer 30, a first nitride layer 40, a second nitride layer 50, a channel layer 60 and a barrier layer 70.

[0013] The substrate 10 may be, for example, a silicon (Si) substrate, a gallium arsenide (GaAs) substrate, a gallium nitride (GaN) substrate, a silicon carbide (SiC) substrate, or a sapphire (Al2O3) substrate; the nucleation layer 20 may be, for example, an aluminum nitride (AlN) or aluminum gallium nitride (AlGaN) layer; in this embodiment, the buffer layer 30 is composed of aluminum gallium nitride (AlGaN), the surface aluminum (Al) concentration of the buffer layer is 25±10%, and the first nitride layer 40 and the second nitride layer 50 are both gallium nitride (GaN) layers; the channel layer 60 may be, for example, an aluminum gallium nitride (AlGaN) or gallium nitride (GaN) channel layer; the barrier layer 70 may be, for example, an aluminum gallium nitride (AlGaN), aluminum nitride (AlN), aluminum indium nitride (AlInN), or aluminum indium gallium nitride (AlInGaN) barrier layer.

[0014] In this embodiment, the high electron mobility transistor epitaxial structure 1 includes a passivation layer 80 and a third nitride layer 52. The passivation layer 80 may be, for example, a silicon nitride (SiN) or gallium nitride (GaN) passivation layer, and the third nitride layer 52 is a gallium nitride (GaN) layer. The ratio of the second nitride layer 50, the third nitride layer 52, and the first nitride layer 40 (V / III) is 1:4:5. Figure 1 As shown, the nucleation layer 20 is located above the substrate 10; the buffer layer 30 is located above the nucleation layer 20; the first nitride layer 40 is located above and in contact with the buffer layer 30; the second nitride layer 50 is located above and in contact with the first nitride layer 40; the channel layer 60 is located above the second nitride layer 50; a two-dimensional electron gas is formed in the channel layer 60 along the interface between the channel layer 60 and the barrier layer 70; the third nitride layer 52 is located above and in contact with the second nitride layer 50; the third nitride layer 52 is located between the second nitride layer 50 and the channel layer 60, and the channel layer 60 is located above the third nitride layer 52; the passivation layer 80 is located above the barrier layer 70. In other embodiments, the third nitride layer 52 may not be provided.

[0015] In this embodiment, the thickness of the first nitride layer 40 is less than the thickness of the second nitride layer 50; the ratio of the thickness of the second nitride layer 50 to the thickness of the first nitride layer 40 satisfies a range greater than or equal to 1 and less than or equal to 6, preferably, the ratio of the thickness of the second nitride layer 50 to the thickness of the first nitride layer 40 is 3; the sum of the thickness of the second nitride layer 50 and the thickness of the first nitride layer 40 is less than or equal to 1 μm, preferably, the sum of the thickness of the second nitride layer 50 and the thickness of the first nitride layer 40 is greater than or equal to 0.5 μm and less than or equal to 1 μm.

[0016] In this embodiment, the second nitride layer 50 is carbon-doped, and the carbon concentration in the first nitride layer 40 is less than the carbon concentration in the second nitride layer 50, wherein the ratio of the carbon concentration in the second nitride layer 50 to the carbon concentration in the first nitride layer 40 is greater than or equal to 10.

[0017] In this embodiment, the thickness of the third nitride layer 52 is 2.5~3.5μm. The third nitride layer 52 comprises a plurality of third nitride films. The third nitride layer 52 is a superlattice layer formed by stacking the plurality of third nitride films. The ratio of the carbon concentration of two adjacent third nitride films with the larger carbon concentration to the carbon concentration with the smaller carbon concentration satisfies a range of greater than or equal to 10. In this embodiment, the third nitride layer 52 is described as comprising a low-doped nitride layer 521 and a high-doped nitride layer 522. In other embodiments, the third nitride layer 52 may also comprise one or more low-doped nitride layers and one or more high-doped nitride layers, and the low-doped nitride layers and high-doped nitride layers may be arranged in an alternating stacked manner.

[0018] In this embodiment, the absolute value of the warpage (BOW) of the high electron mobility transistor epitaxial structure 1 is less than 30 μm. The high electron mobility transistor epitaxial structure 1 is an 8-inch wafer. The warpage value represents the degree of wafer bending, with positive and negative values ​​indicating the bending direction. A positive value indicates upward bending, and a negative value indicates downward bending. The number of defects with a diameter greater than 0.5 μm per square centimeter on the surface of the passivation layer 80 is less than 10. These defects can be, for example, hexagonal defects, stacking defects, pit defects, or other common defects in epitaxial processes, and do not include defects formed by external forces such as dust or scratches. The defects include: the longest crack length extending inward from the outer periphery of the passivation layer 80 in the high electron mobility transistor epitaxial structure 1 is less than or equal to 3 mm. For example, the aforementioned crack can be a crack extending from the outer periphery of the wafer into the wafer; the collapse voltage of the high electron mobility transistor epitaxial structure 1 is greater than or equal to 0.09 V / nm; and by X-ray diffraction analysis, the full width at half maximum (FWHM) of the high electron mobility transistor epitaxial structure (102) is less than 700 arcsec, and the full width at half maximum (FWHM) of the high electron mobility transistor epitaxial structure (002) is less than 600 arcsec.

[0019] Please refer to Figure 3 The diagram shown is a flowchart of a high electron mobility transistor epitaxial method according to a preferred embodiment of the present invention. This high electron mobility transistor epitaxial method is used to form the aforementioned high electron mobility transistor epitaxial structure 1. The high electron mobility transistor epitaxial method includes the following steps: Step S02, a substrate 10 is provided; as described above, the substrate 10 may be a silicon (Si) substrate, a gallium arsenide (GaAs) substrate, a gallium nitride (GaN) substrate, a silicon carbide (SiC) substrate or a sapphire (Al2O3) substrate.

[0020] Step S04: A nucleation layer is formed on the substrate 10. The nucleation layer 20 may be formed on the substrate 10 by metal-organic chemical vapor deposition (MOCVD), and the nucleation layer 20 may be, for example, an aluminum nitride (AlN) or aluminum gallium nitride (AlGaN) layer.

[0021] Step S06: A buffer layer 30 is formed on the nucleation layer 20. The buffer layer may be formed on the nucleation layer 20 by metal-organic chemical vapor deposition (MOCVD). The buffer layer 30 is composed of aluminum gallium nitride (AlGaN) and the surface aluminum (Al) concentration of the buffer layer 30 is 25±10%.

[0022] Step S08: A first nitride layer 40 is formed on the buffer layer 30, and the first nitride layer 40 is in contact with the buffer layer 30; the first nitride layer 40 may be formed on the buffer layer 30 by metal-organic chemical vapor deposition (MOCVD), and the first nitride layer 40 is a gallium nitride (GaN) layer.

[0023] Step S10: A second nitride layer 50 is formed on the first nitride layer 40, and carbon doping is performed on the second nitride layer 50. The second nitride layer 50 is in contact with the first nitride layer 40. The second nitride layer 50 may be formed on the first nitride layer by metal-organic chemical vapor deposition (MOCVD), and the second nitride layer 50 is a gallium nitride (GaN) layer.

[0024] In this embodiment, the growth temperature of the second nitride layer 50 is lower than that of the first nitride layer 40. Specifically, the temperature difference between the growth temperatures of the first nitride layer 40 and the second nitride layer 50 is greater than or equal to 100 degrees Celsius. The V / III ratio of the second nitride layer 50 is less than that of the first nitride layer 40. The ratio of the carbon concentration in the second nitride layer 50 to the carbon concentration in the first nitride layer 40 is greater than or equal to 10. The film thickness of the first nitride layer 40 is less than that of the second nitride layer 50. The ratio of the film thickness of the second nitride layer 50 to that of the first nitride layer 40 is greater than that of the first nitride layer 40. The ratio of the film thicknesses satisfies the range of greater than or equal to 1 and less than or equal to 6. Preferably, the ratio of the film thickness of the second nitride layer 50 to the film thickness of the first nitride layer 40 is 3. The sum of the film thicknesses of the second nitride layer 50 and the first nitride layer 40 is less than or equal to 1 μm. Preferably, the sum of the film thicknesses of the second nitride layer 50 and the first nitride layer 40 is greater than or equal to 0.5 μm and less than or equal to 1 μm. That is to say, the first nitride layer 40 and the second nitride layer 50 are formed under different growth conditions such as temperature, V / III gas flow ratio, thickness, and carbon doping concentration.

[0025] Step S12: A channel layer 60 is formed on the second nitride layer 50. The channel layer 60 may be formed on the second nitride layer 50 by metal-organic chemical vapor deposition (MOCVD), and the channel layer 60 may be, for example, an aluminum gallium nitride (AlGaN) or gallium nitride (GaN) channel layer. In this embodiment, the thickness of the channel layer 60 is between 100 and 500 nm.

[0026] Step S14: A barrier layer 70 is formed on the channel layer 60. A two-dimensional electron gas is formed in the channel layer 60 along the interface between the channel layer 60 and the barrier layer 70. The barrier layer 70 may be formed on the channel layer 60 by metal-organic chemical vapor deposition (MOCVD), and the barrier layer 70 may be, for example, aluminum gallium nitride (AlGaN), aluminum nitride (AlN), aluminum indium nitride (AlInN), or aluminum indium gallium nitride (AlInGaN) barrier layer.

[0027] In this embodiment, the high electron mobility transistor epitaxial method further includes a step S11 between steps S10 and S12, in which a third nitride layer 52 is formed on the second nitride layer 50. The third nitride layer 52 may be formed on the second nitride layer 50 by metal-organic chemical vapor deposition (MOCVD). The third nitride layer 52 is in contact with the second nitride layer 50 and is located between the channel layer 60 and the second nitride layer 50. The third nitride layer 52 is a gallium nitride (GaN) layer. In other embodiments, such as... Figure 2 As shown, step S11 can also be omitted.

[0028] In this embodiment, the growth temperature of the second nitride layer 50 is lower than the growth temperature of the third nitride layer 52. Preferably, the growth temperature of the second nitride layer 50 is lower than the growth temperatures of the first nitride layer 40 and the third nitride layer 52, and the temperature difference between the growth temperatures of the second nitride layer 50 and the first nitride layer 40 and the third nitride layer 52 is greater than 100 degrees Celsius. The V / III ratio of the second nitride layer 50, the third nitride layer 52, and the first nitride layer 40 is 1:4:5. The film thickness of the third nitride layer 52 is 2.5~3.5 μm. The third nitride layer 52 comprises a plurality of third nitride films, and the third nitride layer 52 is a superlattice layer formed by stacking the plurality of third nitride films. The ratio of the carbon concentration of two adjacent third nitride films with a larger carbon concentration to the carbon concentration with a smaller carbon concentration satisfies a range greater than or equal to 10.

[0029] In this embodiment, the high electron mobility transistor epitaxial method further includes a step S16 after step S14, in which a passivation layer 80 is formed on the barrier layer 70. The passivation layer 80 may be formed on the barrier layer 70 by metal-organic chemical vapor deposition (MOCVD), and the barrier layer may be, for example, aluminum gallium nitride (AlGaN), aluminum nitride (AlN), aluminum indium nitride (AlInN), or aluminum indium gallium nitride (AlInGaN) barrier layer.

[0030] In this embodiment, the high electron mobility transistor epitaxial method includes detecting the high electron mobility transistor epitaxial structure 1 formed using the high electron mobility transistor epitaxial method, wherein the absolute value of the warpage (BOW) of the high electron mobility transistor epitaxial structure 1 is less than 30 μm, wherein the detected high electron mobility transistor epitaxial structure 1 is an 8-inch wafer, and the warpage value represents the degree of wafer bending, with positive and negative values ​​indicating the direction of wafer bending, positive values ​​indicating the degree of upward bending and negative values ​​indicating the degree of downward bending; the number of defects with a diameter greater than 0.5 μm per square centimeter on the surface of the passivation layer 80 is less than 10, and the aforementioned defect examples... For example, it can be a common defect in epitaxial processes such as hexagonal defects, stacking defects, pitting defects, etc., and the aforementioned defects do not include defects caused by external forces such as dust or scratches; the longest crack length extending inward from the outer periphery of the passivation layer 80 of the high electron mobility transistor epitaxial structure 1 is less than or equal to 3 mm. For example, the aforementioned crack can be a crack extending from the outer periphery of the 8-inch wafer into the wafer; the collapse voltage of the high electron mobility transistor epitaxial structure 1 is greater than or equal to 0.09 V / nm; by X-ray diffraction analysis, the full width at half maximum (FWHM) of the high electron mobility transistor epitaxial structure (102) is less than 700 arcsec, and the full width at half maximum (FWHM) of the high electron mobility transistor epitaxial structure (002) is less than 600 arcsec.

[0031] The following is a comparative example and an embodiment for illustration.

[0032] [Comparative Example 1] like Figure 4 As shown, the high electron mobility transistor epitaxial structure 2 of Comparative Example 1 has a substantially the same structure as the high electron mobility transistor epitaxial structure 1 of the above embodiment, and also includes a substrate 10, a nucleation layer 20, a buffer layer 30, a channel layer 60, a barrier layer 70 and a passivation layer 80. The difference is that the high electron mobility transistor epitaxial structure 2 of Comparative Example 1 does not have a first nitride layer 40, a second nitride layer 50 and a third nitride layer 52.

[0033] [Example 1] Please cooperate. Figure 1 , is the high electron mobility transistor structure 1 formed using the high electron mobility transistor epitaxial method.

[0034] The growth conditions for the first nitride layer 40 are as follows: The growth temperature is 1050 degrees Celsius, and the nitrogen (N) / hydrogen (H) gas flow ratio is 1:1; the epitaxial thickness of the first nitride layer is 250 nm, and the first nitride layer is not doped with carbon; the background carbon concentration of the first nitride layer is less than 5E17 cm⁻¹.-3 .

[0035] The growth conditions for the second nitride layer 50 are as follows: The growth temperature is 940 degrees Celsius, and the nitrogen (N) / hydrogen (H) gas flow ratio is 6:4; the epitaxial thickness of the second nitride layer is 750 nm, and the second nitride layer is doped with carbon, with a carbon concentration between 5E18 and 5E19 cm⁻¹. -3 .

[0036] The growth conditions for the third nitride layer 52 are as follows: The growth temperature is 1055 degrees Celsius, and the nitrogen (N) / hydrogen (H) gas flow ratio is 1:2. The thickness of the third nitride layer 52 is 2.5~3.5 μm. The third nitride layer 52 comprises a low-doped nitride layer 521 and a high-doped nitride layer 522. The third nitride layer 52 is a superlattice layer formed by the overlapping of the low-doped nitride layer 521 and the high-doped nitride layer 522. The epitaxial thickness of the low-doped nitride layer 521 is 10~100 nm, and the low-doped nitride layer 521 is not doped with carbon. The carbon concentration of the low-doped nitride layer 521 is less than 1E18 cm⁻¹. -3 The highly doped nitride layer 522 has an epitaxial thickness of 100~500 nm and is doped with carbon, with a carbon concentration between 5E18 and 5E19 cm⁻¹. -3 .

[0037] Furthermore, the ratio of the second nitride layer 50, the third nitride layer 52, and the first nitride layer 40 (V / III) is 1:4:5.

[0038] Please refer to Table 1 below for the test results of the high electron mobility transistor epitaxial structures of Comparative Example 1 and Example 1. It can be seen that Comparative Example 1, which does not have the first nitride layer 40 and the second nitride layer 50, performs worse than the test results of the high electron mobility transistor epitaxial structure of Example 1 in terms of longest crack length, warpage (BOW), full width at half maximum (FWHM) of the (102) plane, and defect density. In other words, Example 1, by setting the first nitride layer 40 and the second nitride layer 50, can effectively reduce the generation of cracks, warpage and defects in the high electron mobility transistor structure 1, and can improve the epitaxial quality of the high electron mobility transistor structure.

[0039] In addition, since the high electron mobility transistor structure 2 of Comparative Example 1 does not have the first nitride layer 40, the second nitride layer 50 and the third nitride layer 52, as can be seen from Table 1, the high electron mobility transistor structure 2 of Comparative Example 1 performs significantly worse in terms of breakdown voltage than the high electron mobility transistor structure 1 of Embodiment 1. In other words, this Embodiment 1 can effectively improve the breakdown voltage performance of the high electron mobility transistor structure 1 by setting the first nitride layer 40, the second nitride layer 50 and the third nitride layer 52.

[0040] Table 1:

[0041] The following comparative examples will be used to illustrate this further.

[0042] Furthermore, in this embodiment 1, the thickness of the channel layer 60 is 100~500nm, the thickness of the third nitride layer 52 is 2.5~3.5μm, the thickness of the first nitride layer 40 accounts for 25% of the total thickness of the first nitride layer 40 and the second nitride layer 50, and the thickness of the second nitride layer 50 accounts for 75% of the total thickness of the first nitride layer 40 and the second nitride layer 50, that is, the ratio of the thickness of the second nitride layer 50 to the thickness of the first nitride layer 40 is 3.

[0043] [Comparative Examples 2-5] Comparative Examples 2-5 have a high electron mobility transistor structure substantially the same as that of Example 1, wherein the thickness of the channel layer 60 is 100-500 nm, and the thickness of the third nitride layer 52 is 2.5-3.5 μm. The difference is that in Comparative Example 2, the thickness of the first nitride layer accounts for 0% of the total thickness of the first and second nitride layers, and the thickness of the second nitride layer accounts for 100% of the total thickness of the first and second nitride layers; in Comparative Example 3, the thickness of the first nitride layer accounts for 5% of the total thickness of the first and second nitride layers. In Comparative Example 3, the thickness of the second nitride layer was 50% of the total thickness of the first and second nitride layers; in Comparative Example 4, the thickness of the first nitride layer was 75% of the total thickness of the first and second nitride layers, and the thickness of the second nitride layer was 25% of the total thickness of the first and second nitride layers; in Comparative Example 5, the thickness of the first nitride layer was 100% of the total thickness of the first and second nitride layers, and the thickness of the second nitride layer was 0% of the total thickness of the first and second nitride layers.

[0044] Please refer to Table 2 below for the test results of the high electron mobility transistor epitaxial structures of Example 1 and Comparative Examples 2-5. As can be seen from the table, the high electron mobility transistor epitaxial structure of Example 1 has better breakdown voltage performance and lower defect density compared with the high electron mobility transistor epitaxial structures of Comparative Examples 2-5. Therefore, it can be seen that when the ratio of the thickness of the second nitride layer 50 to the thickness of the first nitride layer 40 is 3, the high electron mobility transistor epitaxial structure 1 has better breakdown voltage performance and lower defect density.

[0045] Table 2:

[0046] In summary, the advantages of this invention are that, through the structural design of the first nitride layer 40 and the second nitride layer 50, defects such as cracks, warping, and breakage in the high electron mobility transistor structure 1 can be effectively reduced. In addition, through the provision of the first nitride layer 40, the second nitride layer 50, and the third nitride layer 52, the voltage withstand performance of the high electron mobility transistor epitaxial structure 1 can be effectively improved.

[0047] The above description is only a preferred embodiment of the present invention. Any equivalent changes made by applying the present invention specification and claims should be included within the scope of the claims of the present invention.

Claims

1. A high electron mobility transistor epitaxial structure, comprising: One substrate; A nucleation layer is located above the substrate; A buffer layer is located above the nucleation layer; A first nitride layer is located above and in contact with the buffer layer; A second nitride layer is located above and in contact with the first nitride layer. The thickness of the first nitride layer is less than the thickness of the second nitride layer. The second nitride layer is carbon-doped. The carbon concentration in the first nitride layer is less than the carbon concentration in the second nitride layer. A channel layer is located above the second nitride layer; A barrier layer is formed in the channel layer along the interface between the channel layer and the barrier layer; A third nitride layer is located above the second nitride layer, and the third nitride layer is located between the second nitride layer and the channel layer. The thickness of the third nitride layer is 2.5 μm to 3.5 μm, and the third nitride layer is a superlattice layer.

2. The high electron mobility transistor epitaxial structure as claimed in claim 1, wherein the ratio of the carbon concentration in the second nitride layer to the carbon concentration in the first nitride layer is greater than or equal to 10.

3. The high electron mobility transistor epitaxial structure as described in claim 1, wherein the ratio of the thickness of the second nitride layer to the thickness of the first nitride layer satisfies a range greater than or equal to 1 and less than or equal to 6.

4. The high electron mobility transistor epitaxial structure as described in claim 1 or 3, wherein the sum of the thickness of the second nitride layer and the thickness of the first nitride layer is less than or equal to 1 μm.

5. The high electron mobility transistor epitaxial structure as claimed in claim 1, wherein the third nitride layer comprises a plurality of third nitride films, the plurality of third nitride films are stacked on top of each other, and the ratio of the carbon concentration of two adjacent third nitride films with a larger carbon concentration to the carbon concentration with a smaller carbon concentration satisfies a range of greater than or equal to 10.

6. The high electron mobility transistor epitaxial structure of claim 5, wherein the first nitride layer, the second nitride layer and the third nitride layer comprise gallium nitride.

7. The high electron mobility transistor epitaxial structure as described in claim 1, wherein the buffer layer is composed of AlGaN and the surface Al concentration of the buffer layer is 25±10%.

8. A high electron mobility transistor epitaxial structure, comprising: One substrate; A nucleation layer is located above the substrate; A buffer layer is located above the nucleation layer; A first nitride layer is located above and in contact with the buffer layer; A second nitride layer is located above and in contact with the first nitride layer; A third nitride layer is located above and in contact with the second nitride layer; A channel layer is located above the second nitride layer and above the third nitride layer; A barrier layer is formed in the channel layer along the interface between the channel layer and the barrier layer; The absolute value of the warpage of the high electron mobility transistor epitaxial structure is less than 30 μm. The first nitride layer, the second nitride layer, and the third nitride layer comprise gallium nitride.

9. The high electron mobility transistor epitaxial structure of claim 8, comprising a passivation layer located above the barrier layer, wherein the number of defects with a diameter greater than 0.5 μm per square centimeter on the surface of the passivation layer is less than 10.

10. The high electron mobility transistor epitaxial structure of claim 8, comprising a passivation layer located above the barrier layer, wherein the longest crack length extending inward from the outer periphery of the passivation layer is less than or equal to 3 mm.

11. The high electron mobility transistor epitaxial structure of claim 8, comprising a passivation layer located above the barrier layer, wherein the breakdown voltage of the high electron mobility transistor epitaxial structure is greater than or equal to 0.09 V / nm.

12. The high electron mobility transistor epitaxial structure of claim 8, wherein the ratio of the second nitride layer, the third nitride layer, and the first nitride layer V / III is 1:4:

5.

13. The high electron mobility transistor epitaxial structure of claim 8, comprising a passivation layer located above the barrier layer, wherein, The full width at half maximum (FWHM) of the high electron mobility transistor epitaxial structure (102) is less than 700 arcsec.

14. The high electron mobility transistor epitaxial structure as described in claim 8, wherein, The full width at half maximum (FWHM) of the (002) plane of the high electron mobility transistor epitaxial structure is less than 600 arcsec.

15. The high electron mobility transistor epitaxial structure of claim 8, wherein the buffer layer is composed of AlGaN and the surface Al concentration of the buffer layer is 25±10%.

Citation Information

Patent Citations

  • Compound semiconductor substrate

    CN113302345A

  • Semiconductor wafer, semiconductor device, and semiconductor wafer manufacturing method

    WO2016152106A1