A device and method for purifying ferroferric oxide
By improving the purification device and method, utilizing the premixed structure, the triangular obstacles and toothed grooves in the reactor to form vortices, combined with nitrogen protection and temperature control, the problem of uneven particle size of ferric oxide was solved, and its magnetic properties and application effects were improved.
Patent Information
- Application Number
- CN202210947212.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-08-09
- Publication Date
- 2026-11-20
- Estimated Expiration
- 2042-08-09
AI Technical Summary
In existing technologies, the particle size of ferric oxide after purification is uneven, which affects its magnetic properties and surface properties.
An improved purification apparatus and method is employed, comprising a premixing structure, a reactor, a heating structure, and a stirring element. A vortex is formed by triangular barriers and toothed grooves within the mixing track, combined with nitrogen protection and temperature control, to ensure thorough mixing of raw materials and uniform reaction.
This achieved uniformity in the particle size of ferric oxide, thereby improving its magnetic properties and application effects.
Smart Images

Figure CN117619217B_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of ferric oxide purification technology, and in particular to a ferric oxide purification apparatus and method. Background Technology
[0002] Iron(III) oxide (Fe3O4) is a magnetic black crystal that can be approximated as a combination of ferrous oxide and ferric oxide, thus requiring high purity.
[0003] In the past, co-precipitation was often used to purify iron(III) oxide. However, the co-precipitation method can lead to agglomeration of iron(III) oxide particles and uneven particle size distribution. Particle size often has a significant impact on the magnetic properties and surface properties of iron(III) oxide, which can negatively affect its application. Summary of the Invention
[0004] The purpose of this invention is to provide a ferric oxide purification apparatus and method to solve the problem of uneven particle size after ferric oxide purification in the prior art.
[0005] A ferric oxide purification device includes a premixing structure, a reactor, a heating structure, and a stirring element. The premixing structure is connected to the reactor and is disposed on one side of the reactor. The heating structure is disposed on the lower side of the reactor. The stirring element is disposed on the inner side of the heating structure and is externally connected to an air pump.
[0006] The premixing structure includes two mixing pipes, two storage compartments, and a mixing rail. The two mixing pipes are each located at one end of the mixing rail and are connected to the mixing rail after being connected. The two storage compartments are arranged one-to-one with the two mixing pipes and are connected to the corresponding mixing pipes.
[0007] The premixing structure is used to initially mix the raw materials to prepare a mixed solution. The reactor is used to cooperate with the mixed solution to ensure that the mixed solution can react fully. The heating structure controls the reaction temperature. The stirring element stirs the reacting raw materials inside the reactor to ensure that the raw materials can be fully mixed. The two mixing pipes are used to transport ferric sulfate pentahydrate and ferrous sulfate heptahydrate, respectively. The corresponding storage chambers store ferric sulfate pentahydrate and ferrous sulfate heptahydrate, respectively. The mixing rail premixes the two raw materials and then sends the raw materials to the reactor via the mixing rail.
[0008] The mixing track has several triangular obstacles and a conveying pipe. The triangular obstacles are evenly arranged inside the conveying pipe, and the two ends of the conveying pipe are respectively connected to two mixing pipes and the reactor.
[0009] Several triangular obstacles are used to impede the transport of the mixture. Through the triangular obstacles, the mixture collides with the triangular obstacles during the transport process to form a vortex, thereby improving the uniformity of the mixing of the two raw materials in the transport pipe, and the transport pipe is used to transport the mixture.
[0010] Each of the triangular obstacles has a number of grooves, which are arranged at equal intervals and are located on the side of the triangular obstacle closest to the mixing tube.
[0011] The arrangement of the aforementioned grooves allows the movement path of the mixture to be disrupted when it passes through the triangular obstacle, thereby forming a vortex. This enables the two raw materials in the mixture to be fully mixed, thus completing the premixing of the raw materials.
[0012] The reactor includes a reaction chamber and a cooling water tank. The reaction chamber is connected to the delivery pipe, and the cooling water tank is located outside the delivery pipe and is fixedly connected to the delivery pipe.
[0013] The cooling water tank is used to lower the temperature of the mixture to prevent it from getting too hot, while the reaction chamber is used for subsequent reactions to purify ferric oxide with a more uniform particle size.
[0014] The stirring component includes a gas guide pipe, a nitrogen chamber, and a control valve. The gas guide pipe is located at the bottom of the reaction chamber and is connected to the nitrogen chamber. The control valve is located on one side of the gas guide pipe to control the opening and closing of the gas guide pipe.
[0015] The gas delivery pipe is used to supply nitrogen from the nitrogen chamber to the reaction chamber, thereby ensuring a nitrogen-protected atmosphere during the reaction in the reaction chamber. The control valve is used to control the opening of the gas delivery pipe, allowing nitrogen to be supplied to the reaction chamber when needed. The bottom of the gas delivery pipe is positioned below the liquid surface in the reaction chamber. When nitrogen is being supplied, it allows the nitrogen to rise from below the liquid surface in the reaction chamber, thus agitating the liquid in the reaction chamber and further improving the uniformity of mixing of the raw materials in the reaction chamber.
[0016] This invention also proposes a method for purifying ferric oxide, applied to the aforementioned ferric oxide purification apparatus, comprising the following steps:
[0017] The reaction solution is obtained by mixing ferric sulfate pentahydrate, ferrous sulfate heptahydrate, and concentrated sulfuric acid, adding deionized water, and storing the mixture in any storage chamber.
[0018] Prepare a NaOH solution in another storage compartment;
[0019] After opening the two storage chambers, the reaction solution and NaOH solution are passed through two mixing tubes to prepare a mixture;
[0020] The mixture is sent to the delivery pipe and cooled by the cooling water tank before being sent to the reaction chamber. The heating structure is activated to maintain the temperature and PVP is added. The nitrogen chamber is turned on, and after the reaction is fully carried out under nitrogen conditions, the purification of ferric oxide particles can be completed.
[0021] The reaction solution has a molar ratio of H + Fe 2+ Fe 3+ The solution is in a 2:1:2 ratio.
[0022] The corresponding improvements to the purification equipment and methods are achieved by changing the ratio of raw materials and using Fe... 2 and Fe 3+ Using these as raw materials and by improving the reaction conditions, the particle size of ferric oxide is made uniform, thus achieving the purification of ferric oxide with a more uniform particle size.
[0023] The present invention provides a ferric oxide purification apparatus and method. Based on the prior art, the purification apparatus is improved so that the raw materials can be fully mixed before the reaction, thereby effectively reducing the agglomeration of ferric oxide and controlling the particle size of ferric oxide. This allows the application of ferric oxide to be unrestricted by particle size. At the same time, the purification method is improved in accordance with the improvement of the equipment, so that the particle size of ferric oxide can be more uniform. Attached Figure Description
[0024] Figure 1 This is an isometric structural diagram of a ferric oxide purification device proposed in this invention.
[0025] Figure 2 This is a side view of a ferric oxide purification device proposed in this invention.
[0026] Figure 3 This is a top cross-sectional view of a ferric oxide purification device proposed in this invention.
[0027] Figure 4 This is a schematic diagram of the triangular obstacle structure of the ferric oxide purification device proposed in this invention.
[0028] Figure 5 This is a cross-sectional structural diagram of the reaction chamber of a ferric oxide purification device proposed in this invention.
[0029] Figure 6 This is a schematic diagram of the steps in the purification method of iron tetroxide proposed in this invention.
[0030] 101-Premixing structure, 102-Reactor, 103-Heating structure, 104-Stirring element, 105-Mixing pipe, 106-Storage chamber, 107-Mixing rail, 108-Triangular obstacle, 109-Transport pipe, 110-Groove, 111-Reaction chamber, 112-Cooling water tank, 113-Gas delivery pipe, 114-Nitrogen chamber, 115-Control valve, 116-Water bath, 117-Heating wire, 118-Temperature sensor. Detailed Implementation
[0031] Embodiments of the present invention are described in detail below, examples of which are illustrated in the accompanying drawings, wherein the same or similar reference numerals denote the same or similar elements or elements having the same or similar functions throughout. The embodiments described below with reference to the accompanying drawings are exemplary and intended to explain the present invention, and should not be construed as limiting the present invention.
[0032] Please see Figures 1 to 5 , Figure 1 This is an isometric structural diagram of a magnetite purification device. Figure 2 This is a side view schematic diagram of a magnetite purification device. Figure 3 This is a top-down cross-sectional view of a magnetite purification device. Figure 4 This is a schematic diagram of the triangular obstacle in a magnetite purification device. Figure 5 This is a cross-sectional schematic diagram of the reaction chamber of a magnetite purification device.
[0033] A ferric oxide purification device includes a premixing structure 101, a reactor 102, a heating structure 103, and a stirring element 104. The premixing structure 101 is connected to the reactor 102 and is disposed on one side of the reactor 102. The heating structure 103 is disposed on the lower side of the reactor 102. The stirring element 104 is disposed on the inner side of the heating structure 103 and is externally connected to an air pump.
[0034] The premixing structure 101 includes two mixing pipes 105, two storage compartments 106, and a mixing rail 107. The two mixing pipes 105 are each disposed at one end of the mixing rail 107, and the two mixing pipes 105 are connected to the mixing rail 107 after being connected. The two storage compartments 106 are disposed one-to-one with the two mixing pipes 105, and each is connected to the corresponding mixing pipe 105.
[0035] In this embodiment, the premixing structure 101 is used to initially mix the raw materials to prepare a mixture, and the reactor 102 is used to cooperate with the mixture to ensure that the mixture can react fully. The heating structure 103 controls the reaction temperature, and the stirring element 104 stirs the reacting raw materials inside the reactor 102 to ensure that the raw materials are fully mixed. The two mixing pipes 105 are used to transport ferric sulfate pentahydrate and ferrous sulfate heptahydrate, respectively. The corresponding storage chambers 106 store ferric sulfate pentahydrate and ferrous sulfate heptahydrate, respectively. The mixing rail 107 premixes the two raw materials and then sends the raw materials to the reactor 102 via the mixing rail 107.
[0036] Furthermore, the mixing track 107 has a plurality of triangular obstacles 108 and a conveying pipe 109. The plurality of triangular obstacles 108 are evenly arranged on the inner side of the conveying pipe 109, and the two ends of the conveying pipe 109 are respectively connected to the two mixing pipes 105 and the reactor 102.
[0037] In this embodiment, a plurality of the triangular obstacles 108 are used to obstruct the transport of the mixture. Through the triangular obstacles 108, the mixture forms a vortex after colliding with the triangular obstacles 108 during the transport process, thereby improving the uniformity of the mixing of the two raw materials in the transport pipe 109, which in turn transports the mixture.
[0038] Furthermore, each of the triangular obstacles 108 has a plurality of grooves 110, the plurality of grooves 110 are arranged at equal intervals, and the plurality of grooves 110 are all located on the side of the triangular obstacle 108 near the mixing tube 105.
[0039] In this embodiment, the arrangement of several grooves 110 allows the movement path of the mixture to be disrupted by the grooves 110 when it passes through the triangular obstacle 108, thereby forming a vortex. This allows the two raw materials in the mixture to be fully mixed, thus completing the premixing of the raw materials.
[0040] Furthermore, the reactor 102 includes a reaction chamber 111 and a cooling water tank 112. The reaction chamber 111 is connected to the delivery pipe 109, and the cooling water tank 112 is disposed on the outside of the delivery pipe 109 and is fixedly connected to the delivery pipe 109.
[0041] In this embodiment, the cooling water tank 112 is used to reduce the temperature of the mixture to prevent it from becoming too hot, while the reaction chamber 111 is used for subsequent reactions to purify iron oxide with a more uniform particle size.
[0042] Furthermore, the stirring component 104 includes a gas guide pipe 113, a nitrogen chamber 114, and a control valve 115. The gas guide pipe 113 is located at the bottom of the reaction chamber 111 and is connected to the nitrogen chamber 114. The control valve 115 is located on one side of the gas guide pipe 113 to control the opening and closing of the gas guide pipe 113.
[0043] In this embodiment, the gas guide pipe 113 is used to supply nitrogen from the nitrogen chamber 114 to the reaction chamber 111, so that the reaction chamber 111 is in a nitrogen-protected atmosphere during the reaction. The control valve 115 is used to control the opening of the gas guide pipe 113, so that the gas guide pipe 113 can supply nitrogen to the reaction chamber 111 when needed. The bottom of the gas guide pipe 113 is located below the liquid surface of the reaction chamber 111. When nitrogen is filled, the nitrogen can rise from below the liquid surface of the reaction chamber 111 to agitate the liquid in the reaction chamber 111, thereby further improving the mixing uniformity of the raw materials in the reaction chamber 111.
[0044] Furthermore, the heating structure 103 includes a water bath 116, a heating wire 117, and a temperature sensor 118. The water bath 116 is disposed on the lower side of the reaction chamber 111, the heating wire 117 is disposed at the bottom of the water bath 116, and the temperature sensor 118 is used to sense the temperature of the water bath 116.
[0045] In this embodiment, the water bath 116, in conjunction with the heating wire 117, enables control of the heating temperature. The temperature sensor 118 controls the water temperature, thereby ensuring that the temperature of the water bath 116 remains relatively stable. This facilitates the purification of ferric oxide and prevents significant changes in the particle size of ferric oxide.
[0046] This invention also proposes a method for purifying ferric oxide, applied to the aforementioned ferric oxide purification apparatus, comprising the following steps:
[0047] S101: Mix ferric sulfate pentahydrate, ferrous sulfate heptahydrate and concentrated sulfuric acid, add deionized water and store in any storage chamber 106 to obtain the reaction solution;
[0048] S102: Prepare a NaOH solution in another storage compartment 106;
[0049] S103: After opening the two storage chambers 106, the reaction solution and NaOH solution are mixed by passing through two mixing tubes 105;
[0050] S104: The mixture is sent to the delivery pipe 109 and cooled by the cooling water tank 112 before being sent to the reaction chamber 111. The heating structure 103 is started to heat at a constant temperature and PVP is added. The nitrogen chamber 114 is turned on. After the reaction is fully carried out under nitrogen conditions, the purification of the iron oxide particle size can be completed.
[0051] Furthermore, the reaction solution has a molar ratio of H... + Fe 2+ Fe 3+ The solution is in a 2:1:2 ratio.
[0052] In this embodiment, the purification device is improved, and the purification method is improved by changing the ratio of raw materials and using Fe. 2+ and Fe 3+ Using these as raw materials and by improving the reaction conditions, the particle size of ferric oxide is made uniform, thus achieving the purification of ferric oxide with a more uniform particle size.
[0053] The present invention provides a ferric oxide purification apparatus and method. Based on the prior art, the purification apparatus is improved so that the raw materials can be fully mixed before the reaction, thereby effectively reducing the agglomeration of ferric oxide and controlling the particle size of ferric oxide. This allows the application of ferric oxide to be unrestricted by particle size. At the same time, the purification method is improved in accordance with the improvement of the equipment, so that the particle size of ferric oxide can be more uniform.
Claims
1. A method for purifying ferric oxide, applied to a ferric oxide purification apparatus, characterized in that, The device includes a premixing structure, a reactor, a heating structure, and a stirring element. The premixing structure is connected to the reactor and is disposed on one side of the reactor. The heating structure is disposed on the lower side of the reactor. The stirring element is disposed on the inner side of the heating structure and is externally connected to an air pump. The premixing structure includes two mixing pipes, two storage compartments, and a mixing rail. The two mixing pipes are each located at one end of the mixing rail and are connected to the mixing rail after being connected. The two storage compartments are arranged one-to-one with the two mixing pipes and are connected to the corresponding mixing pipes. The mixing track has several triangular obstacles and a conveying pipe. The triangular obstacles are evenly arranged inside the conveying pipe, and the two ends of the conveying pipe are respectively connected to two mixing pipes and the reactor. Each of the triangular obstacles has a plurality of grooves, the plurality of grooves are arranged at equal intervals, and the plurality of grooves are all located on the side of the triangular obstacle close to the mixing tube; The reactor includes a reaction chamber and a cooling water tank. The reaction chamber is connected to the delivery pipe, and the cooling water tank is located outside the delivery pipe and is fixedly connected to the delivery pipe. The purification method includes the following steps: Ferrous sulfate pentahydrate, ferrous sulfate heptahydrate, and concentrated sulfuric acid were mixed and then added to deionized water and stored in any storage chamber to obtain a reaction solution. The reaction solution had a molar ratio of H₂O / H₂O. + Fe 2+ Fe 3+ A solution with a ratio of 2:1:2; Prepare a NaOH solution in another storage compartment; After opening the two storage chambers, the reaction solution and NaOH solution are passed through two mixing tubes to prepare a mixture; The mixture is sent to the delivery pipe and cooled by the cooling water tank before being sent to the reaction chamber. The heating structure is activated to maintain the temperature and PVP is added. The nitrogen chamber is turned on, and after the reaction is fully carried out under nitrogen conditions, the purification of ferric oxide particles can be completed.
2. The method for purifying iron(III) oxide as described in claim 1, characterized in that, The stirring component includes a gas guide pipe, a nitrogen chamber, and a control valve. The gas guide pipe is located at the bottom of the reaction chamber and is connected to the nitrogen chamber. The control valve is located on one side of the gas guide pipe to control the opening and closing of the gas guide pipe. The bottom of the gas guide pipe is located below the liquid level in the reaction chamber.
3. The method for purifying iron(III) oxide as described in claim 2, characterized in that, The heating structure includes a water bath, a heating wire, and a temperature sensor. The water bath is located on the lower side of the reaction chamber, the heating wire is located at the bottom of the water bath, and the temperature sensor is used to sense the temperature of the water bath.
Citation Information
Patent Citations
Ferrum oxidate nano magnetic material and method for preparing the same
CN101117241A
Pipe reactor with static mixing device
CN102553512A
Nitrogen stirring method for anaerobic treatment
CN103304028A
Preparation method of water-based nano magnetic fluid
CN112309669A
High -efficient line mixer