A building anti-microseismic system and construction method
By employing a micro-vibration prevention system in soft soil areas and utilizing grouting reinforcement and layered, compartmentalized pouring techniques, the problems of poor vibration control and uneven construction of pile-raft vibration reduction foundations were solved, achieving efficient vibration control and concrete crack resistance.
Patent Information
- Application Number
- CN202311593589.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-11-27
- Publication Date
- 2026-11-24
- Estimated Expiration
- 2043-11-27
AI Technical Summary
Existing pile-raft vibration reduction foundations have poor vibration control in soft soil areas, poor construction uniformity, and are prone to cracking during concrete pouring and curing.
The system employs a micro-vibration prevention system, including a frame, anti-settlement foundation, and vibration-damping foundation. The soil is reinforced by grouting, and the bearing capacity of the foundation is improved by using bored cast-in-place piles and CFG piles. Plain concrete and buffer layers are used to isolate vibration. The replacement layer is poured using a layered and compartmentalized method to avoid cracking, and springs are used to disperse the vibration of the power pipeline.
It significantly improves the bearing capacity of the foundation and the vibration control effect, reduces the cost of concrete construction, ensures the overall strength and crack resistance of the building structure, and achieves a vibration reduction effect of over 90%.
Smart Images

Figure CN117627064B_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of civil engineering technology, and in particular relates to a building anti-micro-vibration system and its construction method. Background Technology
[0002] To ensure the normal operation of equipment, large scientific facilities have extremely high requirements for vibration levels and uneven settlement. Taking the synchrotron radiation source facility as an example, the vibration standard for its storage ring tunnel is that the vertical vibration is within the range of 1-100Hz, and the effective displacement value per second is no greater than 25nm. This is far higher than the vibration standards of general industrial buildings and high-tech electronic factories, and is currently the highest standard among all synchrotron radiation facilities in the world. The micro-vibration environment requirements reach the nanometer level, and the uneven settlement requirements reach the micrometer level, far exceeding the standards of general building construction projects.
[0003] Medium-soft soil consists of slightly dense gravel, coarse and medium sand, fine and silty sand (excluding loose sand), cohesive soil and silt with a foundation bearing capacity characteristic value ≤150kPa, fill with a foundation bearing capacity characteristic value >130kPa, and plastic new loess, with a soil shear wave velocity range of 150 m / s-250 m / s. Currently, pile-raft foundations are generally used for micro-vibration environmental control in medium-soft soil areas. However, this type of foundation structure has poor vibration control effect, poor construction uniformity, and is prone to cracking during concrete pouring and curing.
[0004] Therefore, there is an urgent need for a building anti-micro-vibration system and construction method to change the existing technology of pile-raft vibration reduction foundation for micro-vibration environment control, which has poor vibration control effect, poor construction uniformity, and easy cracking during concrete pouring and curing. Summary of the Invention
[0005] Based on the above analysis, the present invention aims to provide a building anti-micro-vibration system and construction method to solve the problems of poor vibration control effect, poor construction uniformity, and easy cracking during concrete pouring and curing in the prior art of pile-raft vibration reduction foundations.
[0006] The objective of this invention is mainly achieved through the following technical solutions: A building vibration damping system includes a frame, an anti-settlement foundation, a vibration damping foundation, and a power pipe gallery. The frame, the anti-settlement foundation, and the vibration damping foundation are all set on the soil, and the power pipe gallery passes through the vibration damping foundation. The anti-settlement foundation includes a solidification layer and pile foundations. The solidification layer is placed on the soil, one end of the pile foundation is connected to the solidification layer, and the other end of the pile foundation is connected to the vibration damping foundation.
[0007] A method for constructing a building vibration damping system, comprising the following steps: A. Design dimensions; B. Grouting reinforcement and evaluation; C. Pile foundation construction; D. Excavation of the foundation pit; E. Construct the replacement layer and power pipe gallery; F. Construct the first and second structural base plates; G. Project acceptance and completion of construction.
[0008] Further, step A, design dimensions, includes: designing and calculating the dimensions of the first structural base plate, solidification layer, pile foundation, replacement layer, and second structural base plate based on the micro-vibration control requirements and uneven settlement requirements of the ring-shaped large scientific equipment.
[0009] Furthermore, step A, design dimensions, also includes: designing the reinforcement layout of the first and second structural base plates according to the load-bearing capacity requirements.
[0010] Furthermore, step B, grouting reinforcement and evaluation, includes grouting reinforcement of the weak soil layer.
[0011] Furthermore, step B, grouting reinforcement and evaluation, also includes evaluating the grouting effect after the grouting curing is completed.
[0012] Furthermore, step B, grouting reinforcement and evaluation, also includes: if the grouting effect is not satisfactory, grouting is performed again.
[0013] Further, step C, pile foundation construction, includes: drilling pile foundation holes in the soil and solidified layer, and pouring pile foundations into the pile foundation holes.
[0014] Furthermore, step C, pile foundation construction, also includes: testing the vibration response of the pile foundation after the pile foundation is poured.
[0015] Compared with the prior art, the present invention can achieve at least one of the following beneficial effects: (1) The solidification layer of the anti-micro-vibration system of the present invention is a filling grouting layer, which strengthens the soft soil layer in the soil and improves the bearing capacity of the foundation; the pile foundation is a bored cast-in-place pile or CFG pile; the anti-settlement foundation fills the voids in the soft soil layer during solidification, improves the bearing capacity of the foundation, and thus provides anti-settlement support for the vibration reduction foundation; the frame and vibration reduction foundation can isolate the ring-shaped large scientific equipment from the soil and the power pipe gallery, and reduce the vibration transmitted from the soil and the power pipe gallery to the ring-shaped large scientific equipment while meeting the settlement and bearing capacity requirements of the soil. (2) The first buffer layer of the anti-micro-vibration system of the present invention is not connected to the vibration reduction foundation. The first buffer layer is used to isolate the soil and prevent the soil from transmitting the vibration to the first structural base plate, and then to the first column and the ring-shaped large scientific equipment. The first buffer layer is also used to isolate the first structural base plate and prevent the power equipment room and the power machine room from transmitting the vibration to the soil through the second column and the third column, and then to the vibration reduction foundation. (3) The material of the replacement layer of the anti-micro-vibration system of the present invention is plain concrete, 3:7 lime-soil, roller-compacted concrete or cement stone powder slag; the concrete grade of plain concrete is C15 or C20, which reduces the concrete construction cost while meeting the requirements of concrete replacement soil; the filling material is injected into the third section joint so that the third pouring layer no longer has cracks, and the overall strength of the replacement layer is improved. (4) The suspension component of the anti-micro-vibration system of the present invention consists of multiple springs. The multiple springs are evenly distributed around the power pipeline. The multiple springs can disperse the gravity and vibration of the power pipeline and prevent the power pipeline from transmitting vibration to the pipeline body. The third buffer layer is used to isolate the pipeline body and the backfill layer and prevent the pipeline body from transmitting vibration to the backfill layer. (5) The construction method of this invention adopts a layered and compartmentalized method for pouring the replacement layer. During the pouring process of the second compartment, the first compartment joint is filled, which can repair the first pouring layer. During the pouring process of the third compartment, the second compartment joint is filled, which can repair the second pouring layer and improve the overall strength of the replacement layer. Filling material is injected into the third compartment joint so that the third pouring layer is free of cracks, thus improving the overall strength of the replacement layer. No steel reinforcement is added to the entire replacement layer, and there are no cracks, yet the overall strength is still guaranteed. During construction, the dynamic parameters of the compartment joints are detected by shear wave velocity testing, which can quantitatively analyze and evaluate the effect of the grouting reinforcement treatment of the compartment joints, ensuring the quality of the project.
[0016] In this invention, the above-described technical solutions can be combined with each other to achieve more preferred combinations. Other features and advantages of this invention will be set forth in the following description, and some advantages may become apparent from the specification or be learned by practicing the invention. The objectives and other advantages of this invention can be realized and obtained from the content specifically pointed out in the text and drawings. Attached Figure Description
[0017] The accompanying drawings are for illustrative purposes only and are not intended to limit the invention. Throughout the drawings, the same reference numerals denote the same parts.
[0018] Figure 1 A schematic diagram of the longitudinal section of the anti-micro-vibration system; Figure 2 This is a top-down structural diagram of the building complex; Figure 3 This is a schematic diagram of the longitudinal section of the replacement layer; Figure 4 This is a schematic diagram of the longitudinal section structure of the power utility tunnel; Figure 5 To prevent the vibration frequency and vibration displacement curves of the micro-vibration system; Figure 6 This is a flowchart illustrating the construction method.
[0019] Attached reference numerals: 1-Column; 2-First structural base plate; 3-Consolidation layer; 4-Pile foundation; 5-Replacement layer; 6-Second structural base plate; 7-First buffer layer; 8-Second buffer layer; 9-Power pipe gallery; 51-First pouring layer; 52-Second pouring layer; 53-Third pouring layer; 54-Third compartment joint; 91-Pipe gallery body; 92-Power pipeline; 93-Suspension assembly; 94-Third buffer layer; 100-Soil; 101-Main building; 102-Power equipment room; 103-Power machine room; 110-Circular large scientific equipment; 120-Power equipment; 130-Power machine. Detailed Implementation
[0020] The preferred embodiments of the present invention will now be described in detail with reference to the accompanying drawings, which constitute a part of the present invention and are used together with the embodiments of the present invention to illustrate the principles of the present invention, but are not intended to limit the scope of the present invention.
[0021] Example 1 A specific embodiment of the present invention, such as Figure 1 As shown, a building vibration damping system (hereinafter referred to as the vibration damping system) is disclosed, including a frame, a vibration damping foundation, an anti-settlement foundation, and a dynamic pipe gallery 9. The frame, vibration damping foundation, and anti-settlement foundation are all set on the soil 100, and the dynamic pipe gallery 9 passes through the vibration damping foundation. The frame and vibration damping foundation can isolate the annular large scientific equipment 110 from the soil 100 and the dynamic pipe gallery 9, and reduce the vibration transmitted from the soil 100 and the dynamic pipe gallery 9 to the annular large scientific equipment 110 while meeting the settlement and bearing capacity requirements of the soil 100.
[0022] like Figure 2 As shown, the anti-vibration system of this embodiment is used to reduce vibration of the ring-shaped large scientific equipment 110. A complex of buildings is provided to support the ring-shaped large scientific equipment 110. The complex includes a main building 101, a power equipment room 102, a power generator room 103, and a power pipe corridor 9. The main building 101 is in a closed ring shape. The power equipment room 102 is located inside the ring of the main building 101, and the power generator room 103 is located outside the ring of the main building 101. The ring-shaped large scientific equipment 110 is housed inside the main building 101. The power equipment room 102 contains a power device 120, which drives the ring-shaped large scientific equipment. The power generator room 103 contains a power generator 130, which generates power and drives the power device 120. To reduce electromagnetic interference, the power pipe corridor 9 needs to pass through the vibration-damping foundation and transmit the power generated from the power generator room 103 to the power equipment room 102 via a power medium for use by the ring-shaped large scientific equipment. The power medium can be gas or liquid. The perimeter of the main building 101 is 400-2000m.
[0023] Preferably, such as Figure 1As shown, the frame of the anti-micro-vibration system in this embodiment includes a first column 1, a second column, a third column, and a first structural base plate 2, which is set on a vibration-damping foundation. The first column 1, second column, and third column are all connected to the first structural base plate 2, and they respectively support the main building 101, the power equipment room 102, and the power machine room 103. The power equipment 120 and the power machine 130 are fixedly connected to the first structural base plate 2.
[0024] Preferably, the first structural base plate 2 is a reinforced concrete structural base plate with a thickness of 0.8-1.5m, which ensures that the power equipment 120 and the power machine 130 are provided with a solid and flat foundation, and the self-weight and rigidity of the first structural base plate 2 prevent the power equipment 120 and the power machine 130 from vibrating.
[0025] Spaces exist within the medium-soft soil layer, such as karst caves and surface karst development zones, resulting in poor foundation bearing capacity and susceptibility to vibration. Preferably, the anti-settlement foundation includes a solidification layer 3 and pile foundations 4. The solidification layer 3 is placed on the soil mass 100, and one end of the pile foundation 4 penetrates the solidification layer 3 to reach the moderately weathered rock layer within the soil mass. The other end of the pile foundation 4 is placed on the vibration-damping foundation. The solidification layer 3 is a grouting layer. By filling the underground space with grouting material, the voids in the weak soil layer are filled, improving the foundation's bearing capacity and overall rigidity. The grouting material is concrete or cement grout. The pile foundation 4 is a bored cast-in-place pile or a CFG pile. The pile foundation 4 provides a rigid connection between the vibration-damping foundation and the moderately weathered rock layer. The anti-settlement foundation fills and solidifies the spaces existing in the medium-soft soil layer, improving the foundation's bearing capacity and thus providing anti-settlement support for the vibration-damping foundation.
[0026] Preferably, the vibration-damping foundation includes a replacement layer 5 and a second structural base plate 6. The replacement layer 5 is disposed on the pile foundation 4, and the second structural base plate 6 is disposed on the replacement layer 5. Both the replacement layer 5 and the second structural base plate 6 are annular. The replacement layer 5 is used to isolate the first structural base plate 2 and the second structural base plate 6 from the soil 100, preventing the vibration of the soil 100 from being transmitted to the first structural base plate 2 and the second structural base plate 6. The second structural base plate 6 is used to support the annular large scientific equipment 110, providing a solid foundation for the annular large scientific equipment 110. The area where the annular large scientific equipment 110 is located is a micro-vibration control zone. The width of the micro-vibration control zone is B, which is 10-50m. The width of the replacement layer 5 is B+0.0-B+3.0m, and the thickness of the replacement layer 5 is 2.0-3.0m. The width of the second structural base plate 6 is B+0.0-B+3.0m, and the thickness of the second structural base plate 6 is 0.8-1.5m.
[0027] Preferably, the material of the replacement layer 5 is plain concrete, 3:7 lime-soil mixture, roller-compacted concrete, or cement-stone powder slag. Preferably, the plain concrete has a concrete grade of C15 or C20, which reduces the concrete construction cost while meeting the requirement of 100mm for concrete replacement soil.
[0028] Large-volume concrete has a high heat of hydration, making it prone to cracking during construction. To avoid cracking, methods such as increasing the concrete grade and adding crack-resistant steel reinforcement are often used. However, due to the large amount of replacement material, additional steel reinforcement is required to meet crack resistance requirements, significantly increasing costs. Preferably, such as... Figure 3 As shown, the replacement layer 5 includes a first pouring layer 51, a second pouring layer 52, and a third pouring layer 53. The second pouring layer 52 is placed on the first pouring layer 51, and the third pouring layer 53 is placed on the second pouring layer 52. The first pouring layer 51 is a cushion layer, serving as a transition layer between the soil 100 and the replacement layer 5, isolating the second pouring layer 52 from the soil 100, and leveling the first pouring layer 51. The first pouring layer 51 includes multiple first compartments, with first compartment joints provided between them. The width of the first joint is 1000mm to facilitate subsequent construction.
[0029] Preferably, the second pouring layer 52 includes multiple second compartments. During the pouring process, the second compartments fill the first compartment joints, which can repair the first pouring layer 51 and improve the overall strength of the replacement layer 5. Second compartment joints are provided between the second compartments, and these second compartment joints are not connected to the first compartment joints. The third pouring layer 53 includes multiple third compartments. During the pouring process, the third compartments fill the second compartment joints, which can repair the second pouring layer 52 and improve the overall strength of the replacement layer 5. Third compartment joints 54 are provided between the third compartments, and these third compartment joints are not connected to the second compartment joints.
[0030] Preferably, to fill the third compartment joint 54, filler material can be injected into the third compartment joint 54, so that the third pouring layer 53 is free of cracks, thereby improving the overall strength of the replacement layer 5. Preferably, the filler material is epoxy resin or a mixture of epoxy resin and cement, wherein the mixture is prepared by mixing epoxy resin and cement at a mass ratio of 3:1 to 2:1. The replacement layer 5 does not require reinforcement and is free of cracks, improving the integrity and crack resistance of the replacement foundation and ensuring the rigidity of the replacement foundation.
[0031] Preferably, such as Figure 1 As shown, the ring-shaped large scientific equipment 110 is large in volume and has a high load. The second structural base plate 6 is a reinforced concrete structural base plate, with steel bars or prestressed steel bars, ensuring a solid and flat foundation for the ring-shaped large scientific equipment 110. The prestressed steel bars can reduce cracking in the second structural base plate 6.
[0032] Preferably, the anti-micro-vibration system of this embodiment further includes a first buffer layer 7 and a second buffer layer 8. Both the first buffer layer 7 and the second buffer layer 8 are connected to the second structural base plate 6, and the second buffer layer 8 is disposed on the first buffer layer 7. The first buffer layer 7 is used to isolate the second structural base plate 6 from the first structural base plate 2, preventing the first structural base plate 2 from transmitting vibration to the second structural base plate 6, and then to the ring-shaped large scientific equipment 110.
[0033] Preferably, the first buffer layer 7 is a polystyrene board buffer layer with a thickness of 50-100mm. The polystyrene board buffer layer has low surface hardness. The second buffer layer 8 is used to isolate the second structural base plate 6 from the first structural base plate 2, preventing the first structural base plate 2 from transmitting vibrations to the second structural base plate 6. As a floor layer for personnel activity, it needs to have a surface hardness that will not be damaged by foot traffic. Preferably, the second buffer layer 8 is an epoxy putty buffer layer, which enhances the surface hardness of the first buffer layer 7.
[0034] Preferably, such as Figure 1 and Figure 4 As shown, the power utility tunnel 9 passes through the backfill layer 5. The power utility tunnel 9 includes a tunnel body 91, a power pipeline 92, and a suspension assembly 93. The power pipeline 92 is connected to the tunnel body 91 via the suspension assembly 93. The power pipeline 92 is used to transmit power media. The suspension assembly 93 is used to reduce the vibration transmitted from the power pipeline 92 to the tunnel body 91.
[0035] Preferably, the suspension assembly 93 is a spring, which can disperse the weight and vibration of the power pipeline 92 and prevent the power pipeline 92 from transmitting vibration to the pipe rack body 91. Preferably, a third buffer layer 94 is provided between the pipe rack body 91 and the replacement layer 5. The third buffer layer 94 is used to isolate the pipe rack body 91 and the replacement layer 5 and prevent the pipe rack body 91 from transmitting vibration to the replacement layer 5. Preferably, the third buffer layer 94 is a polystyrene board buffer layer with a thickness of 50-150 mm.
[0036] Compared to existing technologies, in this embodiment, the solidification layer 3 of the anti-micro-vibration system is a grouting layer. By filling the underground space with grouting material, the space is filled and the bearing capacity of the foundation is improved. The pile foundation 4 is a bored cast-in-place pile or a CFG pile. The anti-settlement foundation fills the space in the solidified soft soil layer, improving the bearing capacity of the foundation, thereby providing anti-settlement support for the vibration-damping foundation. The frame and vibration-damping foundation can isolate the annular large scientific equipment 110 from the soil 100 and the power pipe gallery 9, reducing the settlement and bearing capacity requirements of the soil 100 while meeting them. The vibrations transmitted from the soil 100 and the power pipe gallery 9 to the circular large scientific equipment 110 are transmitted. The material of the replacement layer 5 is plain concrete, 3:7 lime-soil mixture, roller-compacted concrete, or cement-stone powder slag. The concrete grade of the plain concrete is C15 or C20, which reduces the concrete construction cost while meeting the requirements of the concrete replacement soil 100. Filling material is poured into the third section joint 54 to prevent cracks in the third pouring layer 53 and improve the overall strength of the replacement layer 5. The replacement layer 5 does not require steel reinforcement and does not have cracks, yet it can still guarantee the overall strength.
[0037] The first buffer layer 7 is used to isolate the second structural base plate 6 from the first structural base plate 2, preventing the first structural base plate 2 from transmitting vibrations to the second structural base plate 6, and then to the circular large scientific equipment 110; the second buffer layer 8 is an epoxy mortar buffer layer, which strengthens the surface hardness of the first buffer layer 7, allowing personnel to move on it; the third buffer layer 94 is used to isolate the pipe gallery body 91 from the replacement layer 5, preventing the pipe gallery body 91 from transmitting vibrations to the replacement layer 5.
[0038] The vibration reduction structure of this invention has been tested in practice, such as... Figure 5 As shown, the vibration reduction structure can achieve vibration reduction effect in the entire frequency band from 1 to 100 Hz, with a maximum vibration reduction of over 90%. The vibration on the second structure base plate 6 is a vertical vibration displacement effective value within 20 nm within 1 second.
[0039] The replacement layer 5 is 3m thick and 30m wide C15 plain concrete. The second structural base slab 6 is 1m thick and 30m wide C30 prestressed reinforced concrete. The pile foundation is cast-in-place concrete piles.
[0040] A vibrator was used for excitation during the experiment, with the vibrator positioned 60m away from the center of the second structural base plate 6. A measuring point was placed at the center of the second structural base plate 6. As a control, a measuring point was placed on the soil 100 at a distance of 60m from the vibrator. The load frequency range of the vibrator output was 1-100Hz. The differences in vibration response between the soil and the structural base plate under the same excitation were analyzed.
[0041] Example 2 Another specific embodiment of the present invention, such as Figure 6As shown, a method for constructing a building anti-micro-vibration system (hereinafter referred to as the construction method) is disclosed to construct the anti-micro-vibration system of Example 1.
[0042] The construction method in this embodiment includes the following steps: Step 1: Design Dimensions Based on the micro-vibration control requirements and uneven settlement requirements of the circular large scientific equipment 110, the dimensions of the solidification layer 3, pile foundation 4, replacement layer 5, and second structural base slab 6 are designed and calculated. The reinforcement layout or prestressed reinforcement layout of the second structural base slab 6 is designed according to the bearing capacity requirements.
[0043] Step 2: Grouting reinforcement and assessment Grouting is performed on the weak soil layer. After curing, the grouting effect is evaluated using geological survey methods. If the effect is satisfactory, the next step is carried out. If it is unsatisfactory, grouting is performed again.
[0044] Step 3: Pile Foundation Construction Drill pile foundation holes in the soil 100 and the solidification layer 3, and pour pile foundation 4 into the pile foundation holes.
[0045] Step 4: Excavate the foundation pit Excavate 100mm of soil for a 5mm replacement layer in the foundation pit.
[0046] Preferably, if the soil layer whose design elevation has not yet reached the bearing capacity design requirements is excavated, it should be over-excavated by 0.6m, and the over-excavated part should be replaced with plain concrete, 3:7 lime-soil mixture, roller-compacted concrete or cement-stone powder slag to the design elevation.
[0047] Preferably, the replacement section needs to be compacted in layers, with each layer having a thickness of no more than 300 mm, a compaction coefficient of no less than 0.96, and a foundation bearing capacity of no less than the bearing capacity of the bearing layer.
[0048] Step 5: Construct the replacement layer 5 and the power pipe gallery 9, including the following sub-steps: Preferably, the replacement layer 5 is poured using a layered, compartmentalized method.
[0049] Step 51: Pour the first layer of the silo and leave the first compartment joint, which is 1000mm wide, and cure for 2 days.
[0050] Step 52: Pour the second layer of the silo and fill the first compartment joint, leaving space for the second compartment joint and the pipe gallery trench, and cure for 4 days. The thickness of the second layer of the silo shall not exceed 1m, and its length and width shall not exceed 15m.
[0051] Step 53: Lay a third buffer layer 94 on the inner wall of the pipe gallery trench; lay the pipe gallery body 91; lay the third buffer layer 94 on the pipe gallery body 91.
[0052] Step 54: Pour the third layer of the silo and fill the second compartment joint, leaving the third compartment joint 54. Cure for 7-10 days. The thickness of the third layer of the silo should not exceed 1m, and its length and width should not exceed 15m.
[0053] The replacement layer 5 is poured using a layered, compartmentalized method. The second compartment fills the first compartmentalized joint during the pouring process, which can repair the first poured layer 51. The third compartment fills the second compartmentalized joint during the pouring process, which can repair the second poured layer 52 and improve the overall strength of the replacement layer 5.
[0054] Step 6: Grouting to reinforce the third compartment joint 54 Filler material is injected into the third compartment joint 54 for pressureless grouting, and the surface of the third compartment joint 54 is not sealed. Preferably, the filler is epoxy resin or a mixture of epoxy resin and cement, wherein the mixture is prepared by mixing cement and epoxy resin in a mass ratio of 1:3 to 1:2.
[0055] Preferably, during construction in winter or rainy season, the epoxy resin or epoxy resin and cement mixture is heated to 40℃-60℃ on site, left to stand for 15-20 minutes, and then the grouting is performed.
[0056] Filling material is injected into the third compartment joint 54 to eliminate cracks in the third pouring layer 53 and improve the overall strength of the replacement layer 5; the entire replacement layer 5 does not contain steel reinforcement and does not have cracks, yet it still maintains its overall strength.
[0057] Step 7: Quality Inspection The dynamic parameters and vibration response of each compartment and compartment joint inside the replacement layer 5 are tested; if the design requirements are met, proceed to step 8; if the design requirements are not met, proceed to step 6 again.
[0058] Preferably, after the crack filling is completed, a full-depth core sample is taken from the middle position of the third compartment joint 54 to check the filling material filling condition and test the density, elastic modulus and damping of the core sample; after the crack filling is completed, the shear wave velocity dynamic parameters of the third compartment joint 54 are sampled and tested.
[0059] Preferably, a sampling rate of 90% or higher and a shear wave velocity greater than 2000 m / s are considered sufficient for grouting reinforcement to be considered qualified.
[0060] Preferably, the shear wave velocity dynamic parameter is detected using ultrasonic testing technology, wherein the transmitter is placed on one side of the compartment joint and the receiver is placed on the other side, and both the transmitter and receiver need to be firmly bonded to the surface of the replacement layer 5. First, the distance L between the transmitter and the receiver is measured. Then, the transmitter emits a signal and it is received by the receiver. The time t when the receiver receives the signal is recorded. The shear wave velocity is obtained by dividing L by t.
[0061] The dynamic parameters of the compartment joints can be detected by using shear wave velocity testing, which allows for quantitative analysis and evaluation of the effectiveness of grouting reinforcement treatment for the compartment joints.
[0062] Step 8: Construct the first structural base plate 2 and the second structural base plate 6 The first structural base slab 2 and the second structural base slab 6 are poured using a compartmentalized and post-pouring method. The length and width of each compartment are no more than 15m. The first column 1, the second column and the third column are constructed on the first structural base slab 2.
[0063] Step 9: Construct the first buffer layer 7 and the second buffer layer 8 A first buffer layer 7 is constructed on both sides of the second structural base plate 6, and a second buffer layer 8 is constructed on the first buffer layer 7.
[0064] Step 10: Project acceptance and completion of construction. Compared with existing technologies, the construction method of this embodiment adopts a layered, compartmentalized method for pouring the replacement layer 5. During the pouring process, the second compartment fills the first compartmentalized joint, which repairs the first poured layer 51. Similarly, during the pouring process, the third compartment fills the second compartmentalized joint, which repairs the second poured layer 52, thus improving the overall strength of the replacement layer 5. Filler material is injected into the third compartmentalized joint 54, ensuring that the third poured layer 53 is crack-free, further improving the overall strength of the replacement layer 5. The entire replacement layer 5 does not contain reinforcing steel and is free of cracks, yet it still maintains its overall strength.
[0065] During construction, the dynamic parameters of the compartment joints are detected by shear wave velocity testing, which can quantitatively analyze and evaluate the effect of the grouting reinforcement treatment of the compartment joints and ensure the quality of the project.
[0066] The above description is only a preferred embodiment of the present invention, but the scope of protection of the present invention is not limited thereto. Any changes or substitutions that can be easily conceived by those skilled in the art within the scope of the technology disclosed in the present invention should be included within the scope of protection of the present invention.
Claims
1. A method for constructing a building vibration damping system, characterized in that, The building anti-micro-vibration system is constructed, which includes a frame, an anti-settlement foundation, a vibration reduction foundation and a power pipe gallery (9). The frame, the anti-settlement foundation and the vibration reduction foundation are all set on the soil (100), and the power pipe gallery (9) passes through the vibration reduction foundation. The anti-settlement foundation includes a solidification layer (3) and a pile foundation (4). The solidification layer (3) is placed on the soil (100) and connected to the pile foundation (4). One end of the pile foundation (4) is connected to the vibration damping foundation. The vibration-damping foundation includes a replacement layer (5) and a second structural base plate (6). The second structural base plate (6) is set on the replacement layer (5), and the replacement layer (5) is set on the pile foundation (4). The replacement layer (5) is used to isolate the first structural base plate (2) of the frame from the soil (100). The replacement layer (5) includes a first pouring layer (51). The second pouring layer (52) and the third pouring layer (53) are provided. The second pouring layer (52) is set on the first pouring layer (51), and the third pouring layer (53) is set on the second pouring layer (52). The first pouring layer (51) includes multiple first-level compartments, and a first compartment joint is provided between the first-level compartments. The second pouring layer (52) includes multiple second-level compartments, and a second compartment joint is provided between the second-level compartments. The second compartment joint is not connected to the first compartment joint. The third pouring layer (53) includes multiple third-level compartments, and a third compartment joint (54) is provided between the third-level compartments. The third compartment joint (54) is not connected to the second compartment joint. The replacement layer (5) has no steel reinforcement and no cracks. The power pipe gallery (9) is used to transmit the power generated by the power machine room (103) to the power equipment room (102) via a power medium. The power pipe gallery (9) includes the gallery body (91), the power pipe (92) and the suspension assembly (93). The power pipe (92) is connected to the gallery body (91) via the suspension assembly (93). The power pipe (92) is used to transmit the power medium. The suspension assembly (93) is a spring. The spring can disperse the gravity and vibration of the power pipe (92) and prevent the power pipe (92) from transmitting vibration to the gallery body (91). A third buffer layer (94) is provided between the gallery body (91) and the backfill layer (5). The third buffer layer (94) is used to isolate the gallery body (91) and the backfill layer (5) and prevent the gallery body (91) from transmitting vibration to the backfill layer (5). The construction method includes the following steps: A. Design dimensions; B. Grouting reinforcement and evaluation; C. Pile foundation construction; D. Excavation of the foundation pit; E. Construct the replacement layer (5) and the power pipe gallery (9); The second layer fills the first compartment joint during the pouring process, which can repair the first pouring layer (51). The third layer fills the second compartment joint during the pouring process, which can repair the second pouring layer (52) and improve the overall strength of the replacement layer (5). Filling material is injected into the third compartment joint (54) for pressureless grouting. The surface of the third compartment joint (54) is not sealed, so that the third pouring layer (53) no longer has cracks. F. Construct the first structural base plate (2) and the second structural base plate (6); G. Project acceptance and completion of construction.
2. The construction method of the building anti-micro-vibration system according to claim 1, characterized in that, Step A, design dimensions, includes: designing and calculating the dimensions of the first structural base plate (2), solidification layer (3), pile foundation (4), replacement layer (5), and second structural base plate (6) according to the micro-vibration control requirements and uneven settlement requirements of the ring-shaped large scientific equipment (110).
3. The construction method of the building anti-micro-vibration system according to claim 2, characterized in that, Step A, design dimensions, also includes: designing the reinforcement arrangement of the first structural base plate (2) and the second structural base plate (6) according to the bearing capacity requirements.
4. The construction method of the building anti-micro-vibration system according to claim 1, characterized in that, Step B, grouting reinforcement and evaluation, includes: grouting reinforcement of the weak soil layer.
5. The construction method of the building anti-micro-vibration system according to claim 4, characterized in that, Step B, grouting reinforcement and evaluation, also includes: evaluating the grouting effect after the grouting curing is completed.
6. The construction method of the building anti-micro-vibration system according to claim 5, characterized in that, Geological exploration methods were used to evaluate the grouting effect.
7. The construction method of the building anti-micro-vibration system according to claim 6, characterized in that, Step B, grouting reinforcement and evaluation, also includes: if the grouting effect is not satisfactory, grouting is performed again.
8. The construction method of the building anti-micro-vibration system according to claim 1, characterized in that, Step C, pile foundation construction, includes: drilling pile foundation holes in the soil (100) and the solidified layer (3), and pouring pile foundations (4) into the pile foundation holes.
9. The construction method of the building anti-micro-vibration system according to claim 8, characterized in that, Step C, pile foundation construction, also includes: after the pile foundation (4) is poured, the vibration response of the pile foundation (4) is detected.
Citation Information
Patent Citations
Composite treatment for foundation and piles