A high avalanche tolerance fast recovery diode and its manufacturing method
By injecting an N-region into the cell region on the back side of the fast recovery diode and adjusting the breakdown voltage, the avalanche breakdown point is transferred to the cell region, solving the problems of insufficient avalanche tolerance and uneven electric field in traditional diodes, and achieving higher avalanche tolerance and uniformity.
Patent Information
- Application Number
- CN202311663590.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-06
- Publication Date
- 2026-11-20
- Estimated Expiration
- 2043-12-06
Smart Images

Figure CN117637472B_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of semiconductor fabrication technology, and in particular to a fast recovery diode with high avalanche tolerance and its manufacturing method. Background Technology
[0002] Fast recovery diodes are widely used in electronic circuits as one of the most commonly used basic components. Short reverse recovery time, high breakdown voltage, low reverse cutoff current, soft recovery characteristics, and low forward voltage drop are important requirements for fast recovery diodes. Especially in recent years, the reverse breakdown voltage and switching speed of semiconductor power devices have rapidly increased, placing increasingly higher demands on the voltage withstand capability and reverse recovery speed of diodes connected in parallel.
[0003] The structure of a PIN diode is as follows Figure 1 As shown, it consists of three parts: the anode P-region, the base N-region, and the cathode N+ region. During forward conduction, the N-region stores a large number of charge carriers from the P+ and N+ regions. The injected charge carriers form excess charge carriers, resulting in a high conductivity modulation effect, reducing the resistance of the N-region and thus lowering the forward voltage drop of the fast recovery diode. When a reverse bias is applied, under the influence of an external electric field, the charge carriers in the N-region are extracted, forming a depletion region, and the diode switches to a reverse blocking state. The reverse extraction of charge carriers from the N-region takes a certain amount of time; this process, which affects the diode's turn-off speed, is called the reverse recovery of the diode, and the time required is called the reverse recovery time. The shorter the reverse recovery time, the higher the diode's operating frequency and the lower its energy consumption.
[0004] Because the cell region of a diode is a planar PN junction, it has the strongest breakdown voltage. However, the termination region, which includes cylindrical and spherical PN junctions, has a lower breakdown voltage than the cell region under the same structure and doping concentration. Traditionally, the avalanche breakdown point of a diode is at the termination. Figure 2 As shown. The avalanche tolerance depends on the size of the avalanche area and the uniformity of the avalanche current; the larger the avalanche area, the higher the avalanche tolerance. The more uniform the avalanche current, the less likely current filament buildup will occur, and the higher the reliability of the device.
[0005] Based on the above analysis, traditional fast recovery diodes that place the avalanche breakdown point in the terminal region have the following disadvantages: 1. Traditional high-voltage, high-current fast recovery diodes typically have a cell area larger than the terminal area. Therefore, ensuring that the breakdown point of the device is in the cell area is more conducive to improving the avalanche tolerance of the device. Conversely, placing the avalanche breakdown point in the smaller terminal area can easily lead to insufficient avalanche area and reduced avalanche tolerance.
[0006] 2. The electric field distribution in the terminal region is less uniform than that in the cell region. A well-designed terminal structure requires a uniform electric field distribution, but this distribution is significantly affected by the manufacturing process. A uniform surface electric field distribution places high demands on the design of the terminal structure. When the electric field distribution is uneven, dynamically unstable current filaments are easily generated in areas with strong electric fields. If these current filaments are too large and cannot dissipate quickly, heat will accumulate in a small area, causing localized overheating and damage to the device. In contrast, the cell region is a single planar PN junction with a uniform electric field distribution. Therefore, in the event of avalanche breakdown, the avalanche current distribution is uniform. Summary of the Invention
[0007] The technical problem to be solved by this invention is to overcome the defects of the existing technology. This invention proposes a fast recovery diode with high avalanche tolerance and its manufacturing method. A certain concentration and depth of N-region is injected into the cell region on the back side. By adjusting the energy and dosage injected on the back side, the reverse breakdown voltage of the cell region is controlled to be lower than the terminal breakdown voltage. The avalanche breakdown point is designed in the cell region to increase the avalanche area and improve the uniformity of the avalanche breakdown current, thereby increasing the avalanche tolerance of the device.
[0008] To solve the above-mentioned technical problems, the technical solution adopted by the present invention is: a method for manufacturing a fast recovery diode with high avalanche tolerance, characterized in that the manufacturing method includes the following steps: S1. Substrate preparation: An N-Sub substrate with a resistivity of 70-90 ohm-cm is selected. Arsenic is doped into the N-Sub substrate to an impurity concentration of 4.8e13-6.8e13cm. -3 ; S2, A 14k-20k thick oxide layer is grown on the front side of the wafer; S3. Photolithography and wet etching of the anode P region and terminal Ring region of the wafer, followed by B ion implantation with an ion concentration range of 1E13-2E15, and then annealing. S4. Mark the ion implantation area on the back side of the wafer, implant the first concentration of impurity phosphorus into the marked area, and then perform an annealing process and push-in to form an N-doped region. The N-doped region and the cell region are coaxially distributed on both sides of the wafer. The amount of impurity phosphorus injected at the first concentration is 1E12-1E13, and the injection energy is 1000-2500 keV; S5. Implant a second concentration of impurity phosphorus onto the back side of the wafer, followed by annealing and push-in to form an N+ doped region; the second concentration is higher than the first concentration. S6, Wafer back electrode growth.
[0009] Furthermore, in the annealing process, the annealing temperature is 1000-1200℃ and the annealing time is 200-400min.
[0010] Furthermore, in S5, the amount of impurity phosphorus injected at the second concentration is 1E15-5E15, and the injection energy is 50-100keV.
[0011] Furthermore, in the annealing process, the annealing temperature is 400-600℃ and the annealing time is 30-60min.
[0012] Furthermore, in S3, the implantation stoichiometry of B ions is 1E13-2E15, and the implantation energy is 70-90 keV.
[0013] Furthermore, during the annealing process, the annealing temperature is 1000-1200℃ and the annealing time is 200-400min.
[0014] Furthermore, in S4, the ion implantation region is marked on the back side of the wafer using photoresist or by fabricating a hard film layer on the back side of the wafer using PETEOS.
[0015] Furthermore, the calibration of the ion implantation region by fabricating a hard film layer on the back side of the wafer using PETEOS specifically includes the following steps: S41. Coat the back of the wafer with a 5000A thick PETEOS film; S42. Apply photoresist to the front side of the wafer, and then define the desired pattern on the photoresist as a template for subsequent etching of PETEOS. S43. Etch PETEOS to match the pattern defined by the photoresist; S44. Photoresist removal and ion implantation: Ion implantation is performed after photoresist removal; S45. Remove the remaining PETEOS layer on the back side of the wafer. S46, Annealing Activation: Annealing the wafer to activate the ion implantation region.
[0016] Furthermore, a high avalanche tolerance fast recovery diode includes: an anode P-region, a cathode N-region, and a PN junction located between the anode P-region and the cathode N-region, wherein the PN junction is fabricated according to the above-described manufacturing method, and the PN junction includes: The cell region close to the anode P region, The N-doped region close to the cathode N-region An N+ doped region is provided close to the outer edge of the N-doped region; The N-doped region and the N+ doped region are coaxially distributed on opposite sides of the PN junction.
[0017] Compared with the prior art, the beneficial effects of the present invention include: by using N-injection on the back side of the cell region, the breakdown voltage of the cell region is reduced to be lower than the breakdown voltage of the terminal structure, the avalanche breakdown point is controlled in the cell region, the avalanche area is increased while ensuring good uniformity of the avalanche current, thereby improving the avalanche tolerance of the device. Attached Figure Description
[0018] The disclosure of this invention is illustrated with reference to the accompanying drawings. It should be understood that the drawings are for illustrative purposes only and are not intended to limit the scope of protection of this invention. In the drawings, the same reference numerals are used to refer to the same parts. Wherein: Figure 1 The schematic diagram illustrates the structure of a traditional PIN diode; Figure 2 This schematic illustrates the structure of a traditional PIN+ fast recovery diode. Figure 3 The N-Sub substrate structure in S1 is schematically shown; Figure 4 The diode structure in S2 is schematically shown; Figure 5 The diode structure in S3 is schematically shown; Figure 6-7 The diode structure in S4 is schematically shown; Figure 8 The diode structure in S5 is illustrated schematically. Detailed Implementation
[0019] It is readily understood that, based on the technical solution of this invention, those skilled in the art can propose various interchangeable structural methods and implementations without altering the essential spirit of the invention. Therefore, the following detailed embodiments and accompanying drawings are merely illustrative examples of the technical solution of this invention and should not be considered as the entirety of the invention or as limitations or restrictions on the technical solution of this invention.
[0020] Example 1
[0021] A method for manufacturing a fast recovery diode with high avalanche tolerance includes the following steps: S1, such as Figure 3 As shown, the substrate was prepared by selecting an N-Sub substrate with a resistivity of 70-90 ohm-cm and doping it with arsenic at an impurity concentration of 4.8e13-6.8e13cm. -3 ; S2, such as Figure 4 As shown, a 14k-20k thick oxide layer is grown on the front side of the wafer; S3, such as Figure 5As shown, the anode P region and terminal Ring region of the wafer are photolithographically and wet-etched, and then B ion implanted with a dose of 1E13-2E15 and an implantation energy of 70-90keV. After that, annealing is performed at a temperature of 1000-1200℃ and an annealing time of 200-400min. S4, such as Figure 6-7 As shown, the ion implantation region is marked on the back of the wafer using photoresist. A first concentration of impurity phosphorus is implanted into the marked region. The first concentration of impurity phosphorus implantation dose is 1E12-1E13, and the implantation energy is 1000-2500keV. After annealing and push-in, an N-doped region is formed. In the annealing process, the annealing temperature is 1000℃ and the annealing time is 200min. The aforementioned N-doped region and cell region are coaxially distributed on both sides of the wafer. S5, such as Figure 8 As shown, a second concentration of impurity phosphorus is implanted onto the back side of the wafer. The implantation dose of the second concentration of impurity phosphorus is 1E15-5E15, and the implantation energy is 50-100keV. After that, an annealing process is performed and an N+ doped region is formed after push-in. In the annealing process, the annealing temperature is 400℃ and the annealing time is 30min. The aforementioned second concentration is higher than the first concentration. S6, Wafer back electrode growth.
[0022] Example 2
[0023] The difference from Example 1 is as follows: S4. The ion implantation region is marked on the back of the wafer using photoresist. The marked region is implanted with the first concentration of impurity phosphorus, the first concentration of impurity phosphorus implantation amount is 1E12-1E13, and the implantation energy is 1000-2500keV. After that, the N-doped region is formed by annealing. In the annealing process, the annealing temperature is 1080℃ and the annealing time is 290min. The aforementioned N-doped region and cell region are coaxially distributed on both sides of the wafer. S5. Implant a second concentration of impurity phosphorus onto the back side of the wafer. The second concentration of impurity phosphorus implantation dose is 1E15-5E15, and the implantation energy is 50-100keV. After that, an annealing process is performed and an N+ doped region is formed after push-in. In the annealing process, the annealing temperature is 530℃ and the annealing time is 42min. The aforementioned second concentration is higher than the first concentration.
[0024] Example 3
[0025] The difference from Example 1 is as follows: S4. The ion implantation region is marked on the back of the wafer using photoresist. The marked region is implanted with the first concentration of impurity phosphorus, the first concentration of impurity phosphorus implantation amount is 1E12-1E13, and the implantation energy is 1000-2500keV. After that, the N-doped region is formed by annealing process to push the trap. In the annealing process, the annealing temperature is 1200℃ and the annealing time is 400min. The aforementioned N-doped region and cell region are coaxially distributed on both sides of the wafer. S5. Implant a second concentration of impurity phosphorus onto the back side of the wafer. The second concentration of impurity phosphorus implantation dose is 1E15-5E15, and the implantation energy is 50-100keV. After that, an annealing process is performed and an N+ doped region is formed after push-in. In the annealing process, the annealing temperature is 600℃ and the annealing time is 60min. The aforementioned second concentration is higher than the first concentration.
[0026] Example 4
[0027] The difference from Example 1 is as follows: In S4, a hard film layer is fabricated on the back side of the wafer using PETEOS to complete the calibration of the ion implantation region. The specific steps include the following: S41. Coat the back of the wafer with a 5000A thick PETEOS film; S42. Apply photoresist to the front side of the wafer, and then define the desired pattern on the photoresist as a template for subsequent etching of PETEOS. S43. Etch PETEOS to match the pattern defined by the photoresist; S44. Photoresist removal and ion implantation: Ion implantation is performed after photoresist removal; S45. Remove the remaining PETEOS layer on the back side of the wafer. S46, Annealing Activation: Annealing the wafer to activate the ion implantation region.
[0028] By adding a back-injected cell region to a traditional PIN diode, and controlling the reverse breakdown voltage of the cell region by adjusting the back-injection energy and dosage to keep it below the termination breakdown voltage, the avalanche breakdown point is shifted to the cell region. Because the cell region is a planar PN junction, it has the strongest withstand voltage. Furthermore, the cell region has a larger area and more uniform structure compared to the termination regions on both sides, resulting in a more uniform electric field and current distribution during breakdown. Shifting the avalanche breakdown point to the cell region increases the avalanche area and avalanche uniformity, reducing the likelihood of uneven current filament accumulation causing chip aging and improving the device's avalanche withstand capability. For example, using a 1200V platform, the termination voltage can be designed to be 1400V, while the cell region voltage can be adjusted to 1350V. This controls the avalanche breakdown point within the cell region, increasing the avalanche area and thus improving the uniformity of the avalanche breakdown current, thereby increasing the device's avalanche withstand capability.
[0029] The technical scope of this invention is not limited to the content described above. Those skilled in the art can make various modifications and variations to the above embodiments without departing from the technical concept of this invention, and all such modifications and variations should fall within the protection scope of this invention.
Claims
1. A method for manufacturing a fast recovery diode with high avalanche tolerance, characterized in that, The manufacturing method includes the following steps: S1. Substrate preparation: An N-Sub substrate with a resistivity of 70-90 ohm-cm is selected. Arsenic is doped into the N-Sub substrate to an impurity concentration of 4.8e13-6.8e13cm. -3 ; S2, A 14k-20k thick oxide layer is grown on the front side of the wafer; S3. Photolithography and wet etching of the anode P region and terminal Ring region of the wafer, followed by B ion implantation with an ion concentration range of 1E13-2E15, and then annealing. S4. Mark the ion implantation area on the back side of the wafer, implant the first concentration of impurity phosphorus into the marked area, and then perform an annealing process and push-in to form an N-doped region. The N-doped region and the cell region are coaxially distributed on both sides of the wafer. The first concentration of impurity phosphorus was injected at a dose of 1E12-1E13, and the injection energy was 1000-2500 keV; S5. Implant a second concentration of impurity phosphorus onto the back side of the wafer, followed by annealing and push-in to form an N+ doped region; the second concentration is higher than the first concentration. S6, Wafer back electrode growth.
2. The method for manufacturing a high avalanche tolerance fast recovery diode according to claim 1, characterized in that, In the annealing process, the annealing temperature is 1000-1200℃ and the annealing time is 200-400min.
3. The method for manufacturing a high avalanche tolerance fast recovery diode according to claim 1, characterized in that, In S5, the second concentration of impurity phosphorus is injected at a dose of 1E15-5E15 and the injection energy is 50-100keV.
4. The method for manufacturing a high avalanche tolerance fast recovery diode according to claim 3, characterized in that, In the annealing process, the annealing temperature is 400-600℃ and the annealing time is 30-60min.
5. The method for manufacturing a high avalanche tolerance fast recovery diode according to claim 1, characterized in that, In S3, the B ion implantation dose is 1E13-2E15, and the implantation energy is 70-90 keV.
6. The method for manufacturing a high avalanche tolerance fast recovery diode according to claim 5, characterized in that, During the annealing process, the annealing temperature is 1000-1200℃ and the annealing time is 200-400min.
7. The method for manufacturing a high avalanche tolerance fast recovery diode according to claim 1, characterized in that, In S4, the ion implantation region is marked on the back side of the wafer using photoresist or by fabricating a hard film layer on the back side of the wafer using PETEOS.
8. The method for manufacturing a high avalanche tolerance fast recovery diode according to claim 7, characterized in that, The specific steps for completing the calibration of the ion implantation region by fabricating a hard film layer on the back side of the wafer using PETEOS include the following: S41. Coat the back of the wafer with a 5000A thick PETEOS film; S42. Apply photoresist to the front side of the wafer, and then define the desired pattern on the photoresist as a template for subsequent etching of PETEOS. S43. Etch PETEOS to match the pattern defined by the photoresist; S44. Photoresist removal and ion implantation: Ion implantation is performed after photoresist removal; S45. Remove the remaining PETEOS layer on the back side of the wafer. S46, Annealing Activation: Annealing the wafer to activate the ion implantation region.
9. A fast recovery diode with high avalanche tolerance, comprising: An anode P-region, a cathode N-region, and a PN junction located between the anode P-region and the cathode N-region, characterized in that the PN junction is manufactured according to the manufacturing method of a high avalanche tolerance fast recovery diode according to any one of claims 1-8, and the PN junction comprises: The cell region close to the anode P region, The N-doped region close to the cathode N-region An N+ doped region is disposed close to the outer edge of the N-doped region; the N-doped region and the N+ doped region are coaxially distributed on opposite sides of the PN junction.
Citation Information
Patent Citations
Fast recovery diode (FRD) chip and manufacturing method for FRD chip
CN103208531A
Preparation method of fast recovery diode
CN103531465A