Semiconductor structure and method of fabrication
HKMG, which forms NMOS and PMOS devices through multiple etching and wet etching processes, solves the foot defect problem of PMOS devices and improves process efficiency and product competitiveness.
Patent Information
- Application Number
- CN202210970495.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-08-12
- Publication Date
- 2026-11-24
- Estimated Expiration
- 2042-08-12
AI Technical Summary
When HKMG, an NMOS device, and HKGM, a PMOS device are formed simultaneously, the PMOS device is prone to foot defects, which affect device performance and process reliability.
By simultaneously etching the initial first gate structure and the initial second gate structure multiple times, the top surface of the first insulating layer is not exposed after the first etching. A wet etching process is then used to form the first work function layer and the barrier layer to avoid foot defects.
This effectively avoids foot defects in PMOS devices, reduces the number of photomasks required, lowers process costs, and improves production speed and product competitiveness.
Smart Images

Figure CN117637614B_ABST
Abstract
Description
Technical Field
[0001] This disclosure relates to the field of semiconductors, and in particular to a semiconductor structure and its fabrication method. Background Technology
[0002] With the development of CMOS technology, traditional silicon dioxide gate dielectrics and polycrystalline silicon gate transistors have reached their physical limits. For example, excessive leakage current due to quantum tunneling and depletion issues of polycrystalline silicon gates severely affect the performance of semiconductor devices. Starting from the 45nm technology node, the thickness of the silicon dioxide gate dielectric layer has been reduced to below 2nm. To improve gate leakage current, the semiconductor industry has used high-k dielectric materials HfO2 and HfSiON to replace silicon dioxide as the gate dielectric. The process of using high-k dielectric materials to replace conventional silicon dioxide gate dielectrics and metal gates to replace polycrystalline silicon gates is called the HKMG process technology, where HK is an abbreviation for High K and MG is an abbreviation for Metal Gate.
[0003] The gate structure of a high-dielectric-constant metal-gate MOS transistor uses an HKMG (High-Dielectric-Constant Metal-Gate MOS transistor). The HKMG consists of a high-dielectric-constant layer (HK) and a metal gate (MG). The metal gate includes a metal work function layer and a metal conductive material layer. The metal work function layer is used to adjust the threshold voltage of the device. When the work function of the metal work function layer is different, the flat-band voltage of the device will also be different, ultimately resulting in different threshold voltages. Generally, when forming the gate structure of the peripheral region, to simplify the process, both the HKMG of NMOS devices and the HKGM of PMOS devices are formed simultaneously. Because the initial gate structure of a PMOS device has more film layers than that of an NMOS device, a series of technical problems arise during the etching process, such as footing defects or necking. Summary of the Invention
[0004] This disclosure provides a semiconductor structure and fabrication method that at least helps to improve the situation where the HKMG of an NMOS device and the HKGM of a PMOS device are formed simultaneously, thus avoiding the foot defect problem of the HKMG of the PMOS device.
[0005] According to some embodiments of this disclosure, one aspect of this disclosure provides a method for fabricating a semiconductor structure, comprising: providing a substrate, the substrate including a first type region and a second type region; the substrate of the first type region having a first insulating layer and an initial first gate structure, and the substrate of the second type region having a second insulating layer and an initial second gate structure; simultaneously etching the initial first gate structure and the initial second gate structure multiple times to form a first gate structure and a second gate structure, wherein the bottom of the first gate structure is projected onto the substrate and the top of the first gate structure is projected onto the substrate; wherein, after the first etching process, the top surface of the first insulating layer located in the first type region is not exposed to the outside.
[0006] In some embodiments, the initial first gate structure includes a stacked first work function film, a second work function film, and a conductive film, and the initial second gate structure includes a second work function film and a conductive film. The process step of simultaneously etching the initial first gate structure and the initial second gate structure multiple times includes: etching the conductive film and the second work function film on the substrate of the first type region to form a first conductive layer arranged at intervals, and simultaneously etching the conductive film and the second work function film on the substrate of the second type region to form a second conductive layer arranged at intervals; etching the first work function film using a first wet etching process to form a first work function layer, wherein the orthographic projection of the first work function layer on the substrate is located within the orthographic projection of the first conductive layer on the substrate, the first work function layer and the first conductive layer together constitute the first gate structure, and the second conductive layer serves as the second gate structure.
[0007] In some embodiments, a dry etching process is used to form a first conductive layer and a second conductive layer; the etching solution for the first wet etching process is a hydrochloric acid solution.
[0008] In some embodiments, the concentration of the hydrochloric acid solution is 200:1.
[0009] In some embodiments, the etching time of the first wet etching process is 50s-70s.
[0010] In some embodiments, before forming the second work function film, the method further includes: forming a barrier film on the first work function film; and before etching the first work function film, the method further includes: etching the barrier film to form a barrier layer, wherein the orthographic projection of the barrier layer onto the substrate is located within the orthographic projection of the first conductive layer onto the substrate, and the barrier layer, the first work function layer, and the first conductive layer together constitute the first gate structure.
[0011] In some embodiments, a second wet etching process is used to etch the barrier film, and the etching solution for the second wet etching process is a mixed solution of sulfuric acid and hydrogen peroxide.
[0012] In some embodiments, the mass ratio of sulfuric acid to hydrogen peroxide is 33:1.
[0013] In some embodiments, the etching time of the second wet etching process is 5s-20s.
[0014] In some embodiments, etching of the barrier film and etching of the first work function film are performed alternately until the orthographic projection of the first work function layer on the substrate and the orthographic projection of the barrier layer on the substrate are both located within the orthographic projection of the first conductive layer on the substrate.
[0015] In some embodiments, forming the first insulating layer and the second insulating layer includes: forming a dielectric film on the surface of a substrate, wherein the dielectric film located in a first type region serves as the first insulating layer and the dielectric film located in a second type region serves as the second insulating layer; after etching the initial first gate structure, the method further includes: etching the first insulating layer to form the first gate dielectric layer while simultaneously etching the second insulating layer to form the second gate dielectric layer.
[0016] In some embodiments, the spacing between the side surface of the first work function layer and the side surface of the first conductive layer is less than or equal to 1.5 nm.
[0017] According to some embodiments of the present disclosure, another aspect of the present disclosure also provides a semiconductor structure, including: a substrate, the substrate including a first type region and a second type region; a first insulating layer and a second insulating layer, the first insulating layer being located on the substrate of the first type region and the second insulating layer being located on the substrate of the second type region; a first gate structure, the first gate structure being located on the first insulating layer of the first type region; and a second gate structure, the second gate structure being located on the second insulating layer of the second type region.
[0018] In some embodiments, the first gate structure includes a first work function layer and a first conductive layer stacked together, wherein the orthographic projection of the first work function layer onto the substrate is located within the orthographic projection of the first conductive layer onto the substrate; the second gate structure includes a second conductive layer.
[0019] In some embodiments, the first gate structure further includes a barrier layer located between the first work function layer and the first conductive layer.
[0020] The technical solutions provided in this disclosure have at least the following advantages:
[0021] In the technical solution provided by this disclosure, during the process of simultaneously etching the initial first gate structure and the initial second gate structure multiple times, the top surface of the first insulating layer is not exposed after the first etching, and the orthographic projection of the bottom of the first gate structure onto the substrate is located within the orthographic projection of the top of the first gate structure onto the substrate. That is, there is no foot defect problem at the bottom of the first gate structure. Therefore, when the first and second insulating layers are subsequently etched to form the high-dielectric gate dielectric, the first gate dielectric layer at the bottom of the first gate structure will not have a foot defect problem. Furthermore, simultaneously forming the first and second gate structures can reduce the number of photomasks required to fabricate the first and second gate structures separately, saving process costs and increasing production speed, thereby improving the product's competitiveness. Attached Figure Description
[0022] One or more embodiments are illustrated by way of example with corresponding pictures in the accompanying drawings. These illustrations do not constitute a limitation on the embodiments. Unless otherwise stated, the pictures in the accompanying drawings do not constitute a limitation on scale. In order to more clearly illustrate the technical solutions in the embodiments of this disclosure or the conventional technology, the drawings used in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of this disclosure. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.
[0023] Figure 1 A schematic diagram of a semiconductor structure;
[0024] Figures 2-6 This is a schematic diagram of the steps in the preparation method of a semiconductor structure provided in an embodiment of the present disclosure. Detailed Implementation
[0025] As is known from the background art, when the existing technology simultaneously forms the HKMG of the NMOS device and the HKGM of the PMOS device, the HKMG of the PMOS device may have foot defects.
[0026] Analysis revealed that one of the reasons for the foot defect problem in the HKMG of PMOS devices is that... Figure 1 This is a schematic diagram of a semiconductor structure, for reference. Figure 1The semiconductor structure includes: a substrate 100, which includes a first type region A and a second type region B; a first gate dielectric layer 128 and a second gate dielectric layer 129, wherein the first gate dielectric layer 128 is located on the substrate 100 of the first type region A and the second gate dielectric layer 129 is located on the substrate 100 of the second type region B; a first gate structure 131, which is located on the first gate dielectric layer 128 of the first type region A; and a second gate structure 132, which is located on the second gate dielectric layer 129 of the second type region B. In this design, region A (type 1) is used to form a PMOS device, and region B (type 2) is used to form an NMOS device. Since the first gate structure 131 in region A has a first work function layer 126 and a second work function layer 115, and the second gate structure 132 has a second work function layer 115, during the simultaneous etching of the film layers to form both the first gate structure 131 and the second gate structure 132, the sides of the first work function layer 126 exhibit a footing effect. Furthermore, during the continued formation of the first gate dielectric layer 128 and the second gate dielectric layer 129, the first gate dielectric layer 128 also exhibits a footing effect. Generally, the footing effect can be eliminated by increasing the etching time or the bias voltage. However, increasing the etching time and bias voltage may damage the second gate structure 132, causing the sides of the second gate structure 132 to be etched, thus affecting the performance of the second gate structure 132.
[0027] This disclosure provides a method for fabricating a semiconductor structure. During the simultaneous etching of an initial first gate structure and an initial second gate structure multiple times, the top surface of the first insulating layer is not exposed after the first etching. The orthographic projection of the bottom of the first gate structure onto the substrate lies within the orthographic projection of the top of the first gate structure onto the substrate. This means there are no foot defects at the bottom of the first gate structure. Therefore, when the first and second insulating layers are subsequently etched to form a high-dielectric gate dielectric, the first gate dielectric layer at the bottom of the first gate structure will not have foot defects. Furthermore, simultaneously forming the first and second gate structures reduces the number of photomasks required to fabricate them separately, saving process costs and increasing production speed, thereby improving product competitiveness.
[0028] By using a wet etching process to solve the footing effect of the first work function layer, it will not affect the sidewalls of the second gate structure. The orthographic projection of the first work function layer on the substrate is located within the orthographic projection of the first conductive layer on the substrate, so that the side of the first gate dielectric layer formed subsequently is flush with the side of the first gate structure, that is, there is no foot defect problem. This avoids the risk of short circuits and leakage current problems in adjacent gate structures caused by foot defects.
[0029] The embodiments of this disclosure will now be described in detail with reference to the accompanying drawings. However, those skilled in the art will understand that many technical details have been provided in the embodiments of this disclosure to facilitate a better understanding of the disclosure. However, the technical solutions claimed in this disclosure can be implemented even without these technical details and various variations and modifications based on the following embodiments.
[0030] Figures 2-6 This is a schematic diagram of the steps in the preparation method of a semiconductor structure provided in an embodiment of the present disclosure.
[0031] According to some embodiments of this disclosure, reference is made to Figures 2-6 This disclosure provides a method for fabricating a semiconductor structure, comprising: providing a substrate 200, the substrate 200 including a first type region A and a second type region B; the substrate 200 of the first type region A has a first insulating layer and an initial first gate structure, and the substrate 200 of the second type region B has a second insulating layer and an initial second gate structure; simultaneously etching the initial first gate structure and the initial second gate structure multiple times to form a first gate structure 231 and a second gate structure 232, wherein the bottom of the first gate structure 231 is located within the orthographic projection of the substrate 200, and the top of the first gate structure 231 is located within the orthographic projection of the substrate 200; wherein, after the first etching process, the top surface of the first insulating layer located in the first type region A is not exposed to the outside.
[0032] The formation process of metal gates in semiconductor structures includes Gate-First (MIPS) technology and Gate-Last (RMG) technology. MIPS technology involves embedding a high-melting-point TiN layer and layers with different work functions between a high-k dielectric material and the polysilicon gate. The work function layer is called the "cap layer." The purpose of embedding the high-melting-point metal is to address polysilicon gate depletion in MIPS processes, and embedding the work function cap layer can resolve Fermi level pinning. In some embodiments, MIPS is used to form the metal gate. In other embodiments, a gate-Last (RMG) technology is used. In back-gate technology, a dummy polysilicon gate (DPS) is used to define the gate structure formation region. After self-alignment, sidewalls and source / drain regions are formed. Following the formation of the first interlayer film, the first interlayer film is typically planarized to expose the DPS surface. The DPS is then removed, and trenches are formed in the removed area. HKMG is then formed within the trenches. If a front-gate dielectric layer deposition process is used, the gate dielectric layer is formed before the DPS. Thus, after trench formation, the gate dielectric layer is already present at the bottom of the trench, so only the metal gate needs to be filled. If a back-gate dielectric layer deposition process is used, a dummy gate dielectric layer (typically a gate oxide layer) is used instead of the DPS before the DPS. In this case, after trench formation, the dummy gate dielectric layer at the bottom of the trench needs to be removed before forming the gate dielectric layer and the metal gate within the trench.
[0033] In some embodiments, reference Figure 2 The substrate 200 is a semiconductor substrate, and the material of the semiconductor substrate can be any one of silicon, germanium, silicon carbide, or germanium-silicon. Type I region A is a P-type substrate with P-type dopant elements, and Type II region B is an N-type substrate with N-type dopant elements. A shallow trench isolation structure (not shown) exists between Type I region A and Type II region B. Specifically, the N-type dopant elements can be group V elements such as phosphorus (P), bismuth (Bi), antimony (Sb), or arsenic (As), and the P-type dopant elements can be group III elements such as boron (B), aluminum (Al), gallium (Ga), or indium (In).
[0034] refer to Figure 2The substrate 200 of the first type region A has a channel layer 201, which can serve as the channel region of a semiconductor structure. The material of the channel layer 201 is germanium-silicon, as germanium has a higher carrier mobility. Furthermore, the lattice constant of germanium-silicon is greater than that of silicon. Due to this difference in lattice constant, the substrate 200 generates compressive stress towards the channel layer 201, thereby increasing the mobility of carriers (electrons or holes) within the channel layer 201 and improving the driving current and the speed of the transistor composed of the active region, the channel layer 201, and the first gate structure. The increase in mobility can offset the decrease in mobility caused by the vertical electric field generated when multiple transistors are formed perpendicular to the surface of the substrate 200. In other words, the semiconductor structure can be transformed from 2D to 3D, which is beneficial for increasing the storage density of the semiconductor structure. In some other embodiments, the material of the channel layer can be silicon, and the electron mobility can be improved by implanting germanium ions into the channel layer. In still other embodiments, the material of the channel layer can be germanium, which has a higher carrier mobility.
[0035] refer to Figure 2 An interface layer 202 is formed on the surface of the substrate 200. This interface layer 202 serves as a transition layer between the substrate 200 and the gate dielectric layer of the high-k dielectric material, thereby achieving an ideal silicon dioxide-silicon interface. This effectively improves the interface states between the high-k dielectric material and the substrate 200, and also mitigates the influence of dipole vibrations within the high-k dielectric material on carrier mobility (e.g., carrier phonon scattering), thus increasing carrier mobility. The interface layer 202 is formed using an ISSG (In Situ Steam Generation) process, and the material of the interface layer 202 can be silicon dioxide or silicon oxynitride.
[0036] In some embodiments, a dielectric film 203 is formed on the surface of the interface layer 202. The dielectric film 203 located in the first type region A serves as a first insulating layer, and the dielectric film 203 located in the second type region B serves as a second insulating layer. The dielectric film 203 is formed by MOCVD (Metal Organic Chemical Vapor Deposition) process, and the material of the dielectric film 203 can be hafnium silicate (HfSiO). xHafnium silicate's high dielectric constant can reduce the impact of gate voltage on the active region and decrease gate-induced leakage current. In other embodiments, the formed hafnium silicate is subjected to high-temperature nitriding to form hafnium oxysilicon (HfSiON), which exhibits good high-temperature stability. In still other embodiments, the dielectric film material can be silicon dioxide (SiO2), silicon nitride (Si3N4), aluminum oxide (Al2O3), tantalum pentoxide (Ta2O5), yttrium oxide (Y2O3), hafnium silicate oxide (HfSiO4), hafnium dioxide (HfO2), lanthanum oxide (La2O3), zirconium dioxide (ZrO2), strontium titanate (SrTiO3), or zirconium silicate oxide (ZrSiO4), etc.
[0037] In some embodiments, a protective film 212, a first work function film 213, and a barrier film 214 are stacked on the surface of the dielectric film 203. The protective film 212 is used to protect the dielectric film 203, and the material of the protective film 212 is titanium nitride or other metal nitrides. The thickness of the barrier film 214 is 5nm to 10nm, and the material of the barrier film 214 is titanium nitride or other metal nitrides. It is used to improve the depletion problem of the gate polysilicon. A barrier film is formed between the first work function film and the second work function film to prevent the material of the top metal gate or the material of the second work function film from penetrating down into the first work function film and affecting the first work function layer, thereby stabilizing the performance of the PMOS device. The first work function film 213 is the work function layer of the PMOS device, and the material of the first work function film 213 is aluminum oxide (AlOy). The work function of the P-type metal work function layer usually depletes the top of the valence band of the semiconductor substrate, such as a silicon substrate, thereby reducing the absolute value of the threshold voltage of the PMOS device, which is beneficial to improving the device speed and reducing power consumption. The protective film 212 (titanium nitride film) prevents Al from penetrating downwards.
[0038] In some embodiments, the protective film 212, the first work function film 213, and the barrier film 214 of the second type region B are removed to expose the second insulating layer. A second work function film 204, a second barrier film 205, a semiconductor film 206, a conductive film 207, and a dielectric film 208 are formed on the surface of the barrier film 214 and the second insulating layer of the first type region A. The second work function film 204 is an N-type metal work function layer. The work function of the N-type metal work function layer typically depletes the bottom of the conduction band of the semiconductor substrate, such as a silicon substrate, thereby reducing the threshold voltage of the NMOS device, which is beneficial for improving device speed and reducing power consumption. The material of the second work function film 204 is lanthanum oxide (LaO). The material of the second barrier film 205 is titanium nitride or other metal nitrides. The second barrier film 205 is used to prevent metal in the conductive film 207 from diffusing into the second work function film 204. The second barrier film 205 can be made of amorphous titanium nitride. By setting the second barrier film 205 to an amorphous structure, compared to a polycrystalline structure, the amorphous structure lacks the grain boundaries that penetrate the entire thickness of the polycrystalline structure. This avoids the formation of oxygen diffusion paths caused by grain boundaries, thus reducing or eliminating these paths. This reduces or completely prevents oxygen diffusion to the surface of the metal work function layer, preventing its oxidation. By reducing or eliminating the oxidation structure on the surface of the metal work function layer—making it a low-oxygen or non-oxidized structure—it prevents the shift in the work function caused by oxidation, thereby preventing threshold voltage drift in the device. The semiconductor film 206 is made of polycrystalline silicon. The conductive film 207 can be made of tungsten. By replacing polycrystalline silicon with a metal gate as the device gate material, the pinning phenomenon of the Fermi level can be improved. Simultaneously, the metal gate has extremely high electron density, effectively solving the depletion problem of polycrystalline gates. A third barrier film may be present between the semiconductor film 206 and the conductive film 207. The third barrier film is used to prevent the metal of the conductive film 207 from diffusing into the semiconductor film 206. The material of the third barrier film may be silicon nitride or silicon titanium nitride. The dielectric film 208 is the top capping layer, and the material of the dielectric film 208 may be silicon nitride, silicon oxide, or silicon oxynitride.
[0039] In some embodiments, the initial first gate structure includes a first work function film 213, a second work function film 204, and a conductive film 207 stacked together, and the initial second gate structure includes a second work function film 204 and a conductive film 207. A first mask 209 and a second mask 210 are formed on the top surface 208 of the dielectric film 208; a photoresist layer 211 is formed on the top surface of the second mask 210.
[0040] In some embodiments, the first mask 209 is a spin-coated hard mask layer. Figure 2The top surface of the first mask 209 shown is flush, which can be achieved through chemical polishing (CMP). The second mask 210 is made of silicon oxynitride or amorphous silicon. The material of the second mask 210 has high strength and can be used to protect the dielectric film 208, preventing damage to the top surface of the dielectric film 208 during the etching process. The second mask 210 can also control the patterning accuracy of the first and second gate structures. In some embodiments, the top surface of the first mask in the first type region A is higher than the top surface of the first mask in the second type region B, meaning the thickness of the first mask in the first type region A is the same as the thickness of the first mask in the second type region B.
[0041] refer to Figure 3 While etching the conductive film 207 and the second work function film 204 on the substrate 100 of the first type region A to form a first conductive layer 221 arranged at intervals, the conductive film 207 and the second work function film 204 on the substrate 100 of the second type region B are etched to form a second conductive layer 222 arranged at intervals.
[0042] In some embodiments, a first conductive layer 221 and a second conductive layer 222 are formed using a dry etching process. An initial first gate structure and an initial second gate structure are exposed through a photoresist layer 211, and then each layer of the exposed initial first gate structure and initial second gate structure is etched. The first mask 209 is etched to form a first mask layer 223, and the second mask 210 is etched to form a second mask layer 224.
[0043] refer to Figures 3-4 The barrier film 214 is etched to form a barrier layer 225, and the orthographic projection of the barrier layer 225 onto the substrate 200 is located within the orthographic projection of the first conductive layer 221 onto the substrate 200.
[0044] In some embodiments, a second wet etching process is used to etch the barrier film 214. Based on the selective etching capability of the wet etching process, only the material of the barrier layer 225 can be etched without damaging other film layers, thus maximizing the structural stability of the film layers of the first gate structure and the second gate structure. The second wet etching process can solve the footing effect of the barrier layer 225 and will not affect the sidewalls of the second gate structure. The orthographic projection of the formed barrier layer 225 on the substrate 220 is located within the orthographic projection of the first conductive layer 221 on the substrate 200, so that the side of the first gate dielectric layer subsequently formed is flush with the side of the first gate structure, i.e., there is no footing defect problem. This avoids the risk of short circuits and leakage current problems in adjacent gate structures caused by footing defects.
[0045] In some embodiments, the etching solution for the second wet etching process is a mixed solution of sulfuric acid and hydrogen peroxide (SPM solution). The mass ratio of sulfuric acid to hydrogen peroxide is 33:1. The etching rate of nitrogen is controlled by changing the ratio of sulfuric acid to hydrogen peroxide in the mixed solution. By increasing the content of hydrogen peroxide, the oxidation reaction on the nitrogen surface can be activated, thereby increasing the etching rate of silicon nitride.
[0046] In some embodiments, the etching time of the second wet etching process is 5s-20s. Optionally, the etching time of the second wet etching process is 5s-15s. Specifically, the etching time of the second wet etching process can be 5.3s, 6.8s, 9.1s, or 14.8s. If the second wet etching time is too long, too much of the barrier film 214 will be removed, which may lead to necking, resulting in insufficient support for the bottom support layer of the first gate structure, causing it to tilt or even break. If the etching time is too short, the protruding footing at the end of the barrier layer 225 will not be resolved, resulting in footing in the subsequently formed first gate dielectric layer.
[0047] refer to Figures 4-6 A first work function film 213 is etched using a first wet etching process to form a first work function layer 226. The orthographic projection of the first work function layer 226 onto the substrate 200 lies within the orthographic projection of the first conductive layer 221 onto the substrate 200. The barrier layer 225, the first work function layer 226, and the first conductive layer 221 together constitute the first gate structure 231, and the second conductive layer 222 serves as the second gate structure 232. The first wet etching process can solve the footing effect of the first work function layer 226, without affecting the sidewalls of the second gate structure. The orthographic projection of the formed first work function layer 226 onto the substrate 200 lies within the orthographic projection of the first conductive layer 221 onto the substrate 200, thus making the side of the subsequently formed first gate dielectric layer flush with the side of the first gate structure 231, i.e., eliminating the footing defect problem. This avoids the risk of short circuits and leakage current problems in adjacent gate structures caused by footing defects.
[0048] In some embodiments, the etching solution in the first wet etching process is a hydrochloric acid solution. The concentration of the hydrochloric acid solution is 200:1.
[0049] In some embodiments, the etching time of the first wet etching process is 50s-70s. Optionally, the etching time of the first wet etching process is 50s-60s, and specifically, it can be 52s, 54s, 56s, or 59s. If the first wet etching time is too long, too much of the first work function film 213 will be etched away, which may lead to necking, resulting in insufficient support for the bottom support layer of the first gate structure, causing it to tilt or even break. If the etching time is too short, the protruding footing at the end of the first work function layer 226 will not be resolved, resulting in footing in the subsequently formed first gate dielectric layer.
[0050] In some embodiments, the spacing between the side of the first work function layer 226 and the side of the first conductive layer 221 is less than or equal to 1.5 nm. The degree of necking is controlled by etching process parameters to prevent the first gate structure from tilting or even breaking.
[0051] In some embodiments, reference Figure 5 The protective film 212 is etched to form a protective layer 227. The protective layer 227 is formed by a wet etching process, and the etching solution for the wet etching process is a mixed solution of sulfuric acid and hydrogen peroxide (SPM solution).
[0052] In some embodiments, the etching of the barrier film 214 and the etching of the first work function film 213 are performed alternately until the orthographic projection of the first work function layer 226 onto the substrate 200 and the orthographic projection of the barrier layer 225 onto the substrate 200 are both located within the orthographic projection of the first conductive layer 221 onto the substrate 200. By repeatedly etching the barrier film 214 and the first work function film 213, the morphology of the barrier layer 225 and the first work function layer 226 can be more precisely controlled, thereby avoiding waste of etching solution and reducing costs; at the same time, the footing effect and necking phenomenon can be avoided.
[0053] refer to Figure 6 After etching the initial first gate structure, the process further includes: etching the first insulating layer to form the first gate dielectric layer 228, and simultaneously etching the second insulating layer to form the second gate dielectric layer 229. The first gate dielectric layer 228 and the second gate dielectric layer 229 are formed by a dry etching process; and the first mask layer 223 and the second mask layer 224 are removed.
[0054] In the technical solution provided by this disclosure, during the process of simultaneously etching the initial first gate structure and the initial second gate structure multiple times, the top surface of the first insulating layer is not exposed after the first etching. The orthographic projection of the bottom of the first gate structure 231 onto the substrate 200 is located within the orthographic projection of the top of the first gate structure 231 onto the substrate 200. That is, there is no foot defect problem at the bottom of the first gate structure 231. When the first insulating layer and the second insulating layer are subsequently etched to form a high-dielectric gate dielectric, there will be no foot defect problem in the first gate dielectric layer at the bottom of the first gate structure 231. In addition, simultaneously forming the first gate structure 231 and the second gate structure 232 can reduce the number of photomasks required to separately fabricate the first gate structure 231 and the second gate structure 232, saving process costs and increasing production speed, thereby improving the competitiveness of the product.
[0055] Accordingly, according to some embodiments of this disclosure, another aspect of this disclosure also provides a semiconductor structure prepared using the semiconductor structure preparation method provided in the above embodiments, with the same or corresponding elements as in the above embodiments, which will not be described in detail here.
[0056] refer to Figure 5 The semiconductor structure includes: a substrate 200, which includes a first type region A and a second type region B; a first insulating layer and a second insulating layer, wherein the first insulating layer is located on the substrate 200 of the first type region A and the second insulating layer is located on the substrate 200 of the second type region B; a first gate structure 231, which is located on the first insulating layer of the first type region A; and a second gate structure 232, which is located on the second insulating layer of the second type region B.
[0057] In some embodiments, the first insulating layer and the second insulating layer constitute a continuous dielectric film 203, the first insulating layer being used to subsequently form the first gate dielectric layer, and the second insulating inner layer being used to subsequently form the second gate dielectric layer. In other embodiments, the first insulating layer is the first gate dielectric layer, and the second insulating layer is the second gate dielectric layer. The orthographic projection of the first gate structure onto the surface of the first insulating layer lies within the first insulating layer, and the orthographic projection of the second gate structure onto the surface of the second insulating layer lies within the second insulating layer.
[0058] In some embodiments, the first gate structure 231 includes a first work function layer 226 and a first conductive layer 221 stacked together, wherein the orthographic projection of the first work function layer 226 onto the substrate 200 lies within the orthographic projection of the first conductive layer 221 onto the substrate 220; the second gate structure 232 includes a second conductive layer. The spacing between the side surface of the first work function layer 226 and the side surface of the first conductive layer 221 is less than or equal to 1.5 nm, and the necking degree is controlled by etching process parameters to prevent the first gate structure from tilting or even breaking.
[0059] In some embodiments, the first gate structure 231 further includes: a barrier layer 225 located between the first work function layer 226 and the first conductive layer 221; and a protective layer 227 located between the first work function layer 226 and the first insulating layer.
[0060] Those skilled in the art will understand that the above embodiments are specific examples of implementing this disclosure, and in practical applications, various changes in form and detail may be made without departing from the spirit and scope of this disclosure. Any person skilled in the art can make their own modifications and alterations without departing from the spirit and scope of this disclosure; therefore, the scope of protection of this disclosure should be determined by the scope defined in the claims.
Claims
1. A method for fabricating a semiconductor structure, characterized in that, include: A substrate is provided, the substrate comprising a first type region and a second type region; The first type region has a first insulating layer and an initial first gate structure on its substrate. The initial first gate structure includes a stacked first work function film, a blocking film, a second work function film, and a conductive film. The second type region has a second insulating layer and an initial second gate structure on its substrate. The initial second gate structure includes the second work function film and the conductive film. While etching the conductive film and the second work function film on the substrate of the first type region to form a first conductive layer arranged at intervals, the conductive film and the second work function film on the substrate of the second type region are also etched to form a second conductive layer arranged at intervals. The barrier film is etched to form a barrier layer, and the first work function film is etched using a first wet etching process to form a first work function layer. The etching of the barrier film and the etching of the first work function film are performed alternately until the orthographic projection of the first work function layer on the substrate and the orthographic projection of the barrier layer on the substrate are both located within the orthographic projection of the first conductive layer on the substrate. The first work function layer, the barrier layer, and the first conductive layer together constitute a first gate structure, and the second conductive layer constitutes a second gate structure. In this process, after the first etching process, the top surface of the first insulating layer located in the first type region is not exposed to the outside.
2. The method for preparing a semiconductor structure according to claim 1, characterized in that, The first conductive layer and the second conductive layer are formed using a dry etching process; the etching solution for the first wet etching process is a hydrochloric acid solution.
3. The method for preparing a semiconductor structure according to claim 2, characterized in that, The concentration of the hydrochloric acid solution is 200:
1.
4. The method for preparing a semiconductor structure according to claim 2, characterized in that, The etching time for the first wet etching process is 50s-70s.
5. The method for preparing a semiconductor structure according to claim 1, characterized in that, The barrier film is etched using a second wet etching process, wherein the etching solution for the second wet etching process is a mixed solution of sulfuric acid and hydrogen peroxide.
6. The method for preparing a semiconductor structure according to claim 5, characterized in that, The mass ratio of sulfuric acid to hydrogen peroxide is 33:
1.
7. The method for preparing a semiconductor structure according to claim 5, characterized in that, The etching time for the second wet etching process is 5s-20s.
8. The method for preparing a semiconductor structure according to claim 1, characterized in that, Forming the first insulating layer and the second insulating layer includes: forming a dielectric film on the surface of the substrate, wherein the dielectric film located in the first type region serves as the first insulating layer and the dielectric film located in the second type region serves as the second insulating layer; after etching the initial first gate structure, the method further includes: etching the first insulating layer to form the first gate dielectric layer while simultaneously etching the second insulating layer to form the second gate dielectric layer.
9. The method for preparing a semiconductor structure according to claim 1, characterized in that, The distance between the side surface of the first work function layer and the side surface of the first conductive layer is less than or equal to 1.5 nm.
10. A semiconductor structure prepared by the method of preparing a semiconductor structure according to any one of claims 1 to 9, characterized in that, include: A substrate, the substrate comprising a first type region and a second type region; A first insulating layer and a second insulating layer, wherein the first insulating layer is located on the substrate of the first type region and the second insulating layer is located on the substrate of the second type region; A first gate structure is located on a first insulating layer of the first type region; The second gate structure is located on the second insulating layer of the second type region.
11. The semiconductor structure according to claim 10, characterized in that, The first gate structure includes a first work function layer and a first conductive layer stacked together, wherein the orthographic projection of the first work function layer on the substrate is located within the orthographic projection of the first conductive layer on the substrate; the second gate structure includes a second conductive layer.
12. The semiconductor structure according to claim 11, characterized in that, The first gate structure further includes a barrier layer located between the first work function layer and the first conductive layer.
Citation Information
Patent Citations
Method for making a semiconductor device having a metal gate electrode
CN1902735A
CMOS semiconductor devices having dual work function metal gate stacks
US20070178634A1
