A method for lightweight design of a semi-finished product of an inner liner of a vehicle tire
By optimizing the thickness design of the inner liner semi-finished product, the problems of redundant inner liner design and high cost were solved, the heat dissipation and air retention performance of the tire were improved, and the service life was extended.
Patent Information
- Application Number
- CN202311626701.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-11-30
- Publication Date
- 2026-11-20
- Estimated Expiration
- 2043-11-30
AI Technical Summary
Existing inner liner design methods fail to effectively reduce material production costs and are redundant, resulting in high production costs for semi-finished components. Furthermore, during use, issues such as inner liner cracks in the tire shoulder and bead areas and insufficient tire air and pressure retention performance may arise.
By optimizing the thickness of the center area of the tire crown, the tire shoulder area, and the area near the inner end of the bead reinforcement layer, and by calculating the elongation rate using material distribution diagrams and equivalent deformation points, the thickness of the inner liner semi-finished product is adjusted to reduce the weight of the transition layer.
Without altering existing equipment, the design cost of the inner liner was reduced, the tire's heat dissipation and air/pressure retention performance were improved, cracks in the inner liner at the tire shoulder and bead areas were reduced, and the tire's service life was extended.
Smart Images

Figure CN117648758B_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of tire semi-finished product design and relates to a method for lightweight design of automotive tire inner liner semi-finished products. Background Technology
[0002] The inner liner is one of the most important components of a tire, composed of a transition layer and an airtight layer. The airtight layer acts as an inner tube, preventing air leakage, maintaining air pressure, and isolating moisture, making it crucial for ensuring tire airtightness. The transition layer primarily covers and isolates the tire carcass steel cords, preventing the airtight layer's adhesive from seeping into the tire carcass and shortening its lifespan. It also maintains a certain level of adhesion with both the tire carcass and the airtight layer, preventing delamination during use and reducing tire lifespan.
[0003] The industry's design methods for semi-finished inner liner components are mainly based on the original multi-layer flat roller design of bias-ply tires. Although this solves the problem of inconsistent thickness between the tire crown and sidewall bead areas, it is based on theoretical calculations demanded by new tires. It primarily addresses the design and pressure-holding performance of the tire's inner liner components, failing to achieve the optimal match between practical use and cost control. Later, an irradiation pre-vulcanization process was developed to treat the semi-finished inner liner components designed using traditional methods. This process ensures airtightness while reducing inner liner thickness and lowering costs. However, this method requires specific equipment with high costs, resulting in limited industry adoption. Summary of the Invention
[0004] To address the aforementioned issues, this invention provides a method for lightweight design of semi-finished automotive tire inner liner layers, which reduces the weight of the transition layer, thereby lowering material production costs and resolving the problems of redundant existing inner liner designs and high production costs for semi-finished components.
[0005] The objective of this invention is achieved in the following manner: a method for lightweight design of semi-finished automotive tire inner liner, specifically by optimizing the thickness of the center region of the tire crown, the tire shoulder region, and the region near the inner end of the bead reinforcement layer; (1) Based on the material distribution location on the material distribution map, The center area of the tire crown, located at the center of the finished tire crown, with the center of the tire crown as the center line, its width is the distance between the inner end of the pad rubber and the center line of the tire crown; it is called the T area; The tire shoulder area, located at the shoulder of the finished tire, has a total width equal to the inner liner arc length between the two ends of the rubber pad bottom width; this is called the S-zone. The area near the inner end of the bead reinforcement layer, whose width is the distance between 10mm and 20mm above and below the inner end of the bead wrapping of the finished tire section, is called Zone B. (2) Based on safety considerations, the point with the maximum deformation is taken as the equivalent deformation point of the region; and it is assumed that the deformation of the inner liner rubber material in contact with the tire carcass is bound to the same following deformation point as the skeleton material, which can be ignored compared with the deformation of the rubber material in this region. The equivalent deformation points of the tire crown center region, tire shoulder region, and region near the inner end point of the bead reinforcement layer are determined respectively. In the T region, the symmetrical center point A of the fetal body in the crown is taken as the equivalent deformation point; In area S, point B, corresponding to the thickest part of the inner liner at the bottom of the belt layer, is taken as the equivalent deformation point. The specific method for taking point B is the intersection of the line connecting the outer end of the tire tread width and the end of the widest belt layer with the tire body. In area B, take the inner end point C of the finished cross-section of the fabric wrapping as the equivalent deformation point; The elongation at point A is represented by T. A The elongation at point B is represented by S. B The elongation at point C is represented by B. C This indicates that the maximum tensile strengths of the central area of the tire crown, the tire shoulder area, and the area near the inner end of the bead reinforcement layer are respectively T A S B B C Determine T A S B B C There are two methods, and either of the following two methods can be used; The first type: T A S B B C It can be calculated using the following formula: in: AD is the diameter of the auxiliary drum; MD is the diameter of the forming drum; W is the width of the padding rubber; D is the width of the forming machine; S1 is the inner positioning of the steel wire wrapped fabric; B1 is the inner circumference of the steel wire ring. The second type: T is measured using a material distribution map method. A S B B C The specific steps to obtain it are as follows: (a) Prepare a material distribution diagram for the finished tire; (b) Determine the nominal diameter of the wheel rim; (c) Measure the distances L from the equivalent deformation points A, B, and C in the center region of the tire crown, the tire shoulder region, and the region near the inner end of the bead reinforcement layer to the central axis of the standard rim, respectively, from the material distribution diagram. A L B L C .
[0006] (4) T A S B B C The calculation formula is as follows: T A =L A / (forming drum radius * μ) S B = L B / (forming drum radius * μ) B C =L C / (forming drum radius * μ) Wherein, the radius of the forming drum is the circumference of the forming drum / 2π, and μ is the coefficient of thermal expansion of the carcass material; (3) The formulas for calculating the thickness of the T, S, and B zones of the semi-finished inner lining layer are derived from the formula: Design thickness of the inner lining layer = Minimum thickness of the zone × Maximum tensile strength of the zone. G T =H Tmin ×T A G S =H Smin ×S B G B =H Bmin ×B C Wherein: H Tmin H Smin H Bmin These are the minimum standard theoretical thicknesses of the inner linings in zones T, S, and B, respectively, after being stretched from semi-finished to finished product dimensions on the finished tire.
[0007] In step (3), the standard theoretical thickness H of the inner lining layer in the crown T area, shoulder S area, and bead B area of the finished tire is determined based on whether the product has an inner tube or not and the position of the inner end of the bead wrapping. This thickness is calculated from the semi-finished product to the finished product size after stretching. T H S H B The minimum value.
[0008] In step (2), the equivalent deformation point B in area S is determined as follows: since the angle between the edge of the padding layer under the finished product cross section is usually no greater than 15°, and the angle between the edge of the upper contour of the finished padding layer and the bottom edge is usually no greater than 30°, considering the safety margin design, the padding layer can be simplified into an isosceles triangle of 60°, 60°, and 60°, and the angle between the padding layer and the belt layer is simplified to 30°. Point B is located at the center point of the base of the equilateral triangle. The stretching of point B is bound to the carcass material at the corresponding position. Then the stretching rate of the center point of the bottom edge of the padding layer is the stretching rate of point B.
[0009] Compared to existing technologies, the purpose of this invention is to adjust the original inner liner design method without changing the existing equipment. Designing and outputting the specific construction dimensions of the semi-finished components according to the method of this invention effectively reduces the design cost of semi-finished products, reduces the weight of the transition layer, and thus reduces material production costs. This solves the problems of redundant inner liner designs and high production costs of semi-finished components in existing systems. Compared to previous inner liner designs, designing and outputting the specific construction dimensions of the semi-finished components according to the method of this invention effectively reduces the design cost of semi-finished products. The reduced thickness of the inner liner in the crown area improves the heat dissipation performance of the tire crown. The increased thickness of the inner liner in the shoulder area and the bead area reduces problems encountered in traditional designs during use, such as cracks in the inner liner at the shoulder and bead areas, and reduces defects such as shoulder gaps caused by leaking threads in the shoulder. It also improves tire air and pressure retention performance and extends tire life. Attached Figure Description
[0010] Figure 1 This is a theoretical functional zone division diagram.
[0011] Figure 2 This is a schematic diagram of the main reference area for the design.
[0012] Figure 3 This is a schematic diagram of the equivalent deformation points.
[0013] Figure 4 This is the outline drawing of the semi-finished component of the inner liner transition layer of a 12R22.5 tubeless tire, drawn using the first method.
[0014] Figure 5 This is the outline drawing of the semi-finished component of the inner liner transition layer of a 12.00R20 specification inner tube tire, drawn using the first method.
[0015] Figure 6 This is the outline drawing of the semi-finished component of the inner liner transition layer of a 12R22.5 tubeless tire, drawn using the second method.
[0016] Figure 7 This is a outline drawing of a semi-finished component of an inner liner transition layer for a 12.00R20 specification inner tube tire, drawn using the second method. Detailed Implementation
[0017] The present invention will now be described in detail with reference to specific embodiments. It should be noted that these embodiments are only used to further illustrate the present invention and should not be construed as limiting the scope of protection of the present invention. Those skilled in the art can make some non-essential improvements and adjustments based on the above description of the present invention.
[0018] A method for lightweight design of semi-finished inner liner of automobile tires, specifically, involves optimizing the thickness of the center area of the tire crown, the tire shoulder area, and the area near the inner end of the bead reinforcement layer, while keeping the thickness of other areas consistent with the existing design; (1) Based on the material distribution location in the material distribution diagram and the different functions and design requirements of each functional area during actual tire use, the inner liner of the tire is divided into 7 theoretical functional areas: 1, 2, 3, 4, 5, 6, and 7. The width of each of the 7 areas is determined, as shown in the attached diagram. Figure 1 and 2 As shown, the details are as follows: Area 1 is the center area of the tire crown, located at the position corresponding to the center of the finished tire crown. With the center of the tire crown as the center line, its width is the distance between the inner end of the pad rubber and the center line of the tire crown; Area 1 is called the T area; Area 2 is the tire shoulder area, located at the shoulder of the finished tire. The total width of the area is the inner liner arc length corresponding to the two ends of the rubber pad bottom width; Area 2 is called Area S. Area 4 is the widest part of the tire cross section, and its width is the distance between 10mm and 20mm above and below the center axis of the widest part of the finished tire cross section.
[0019] Zone 3 is the transition zone between Zone 2 and Zone 4. It is located on the upper side of the finished tire section, and its width is the distance from the end of Zone 2 to the beginning of Zone 4. Zone 6 is the area near the inner end of the bead reinforcement layer. Its width is the distance between 10mm and 20mm above and below the inner end of the bead wrapping of the finished tire section; Zone 6 is called Zone B. Zone 5 is the transition zone between Zone 4 and Zone 6. It is located on the lower tire side of the finished section and its width is the distance from the end of Zone 4 to the beginning of Zone 6.
[0020] Region 7 is the end area of the transition layer, and its width is the distance between the end point of region 6 and the end of the total width of the transition layer.
[0021] (2) Determine the maximum tensile strength of the central area of the tire crown, the tire shoulder area, and the area near the inner end of the bead reinforcement layer, respectively, as T A S B B C ; Determine T A S B B C There are two methods, and either of the following two methods can be used; The first type: The crown elongation T is calculated by using the equivalent deformation points of the region. A Shoulder stretch ratio S B , Sub-mouth elongation B CThe calculation model for determining the elongation of the product's inner lining layer in zones T, S, and B is as follows: For safety reasons, the point of maximum deformation is taken as the equivalent deformation point of this region. Furthermore, it is assumed that the deformation of the inner liner rubber compound in contact with the carcass is bound to the same deformation point as the skeleton material, and can be ignored compared to the deformation of the rubber compound in this region.
[0022] like Figure 3 As shown, point A, the center of symmetry of the fetal body in the crown, is taken as the equivalent deformation point in region T; In area S, point B, corresponding to the thickest part of the inner liner at the bottom of the belt layer, is taken as the equivalent deformation point. Specifically, point B is the intersection of the line connecting the outer end of the tire tread width and the end of the widest belt layer with the tire carcass. Since the included angle of the edge of the belt layer under the rubber pad on the finished cross-section is usually no greater than 15°, and the angle between the upper contour edge and the bottom edge of the finished rubber pad is usually no greater than 30°, considering the safety margin design, the rubber pad can be simplified into an isosceles triangle of 60°, 60°, and 60°, and the included angle between the rubber pad and the belt layer is simplified to 30°. Point B is located at the center point of the base of the isosceles triangle. The stretching of point B is bound to the tire carcass material at the corresponding position. Then the stretching rate of the center point of the bottom edge of the rubber pad is the stretching rate of point B. Based on the cause analysis of common damage modes in area B, the inner end point C of the finished cross-section of the fabric in area B is taken as the equivalent deformation point.
[0023] The elongation at point A is represented by T. A The elongation at point B is represented by S. B The elongation at point C is represented by B. C This indicates that T... A S B B C It can be calculated using the following formula: in: AD is the diameter of the auxiliary drum; MD is the diameter of the forming drum; W is the width of the padding rubber; D is the width of the forming machine; S1 is the inner positioning of the steel wire wrapped fabric; B1 is the inner circumference of the steel wire ring. The second type: T is measured using a material distribution map method. A S B B C The specific steps to obtain it are as follows: (a) Prepare a material distribution diagram for the finished tire; (b) Determine the location of equivalent deformation points A, B, and C in the center region of the tire crown, the tire shoulder region, and the region near the inner end of the bead reinforcement layer, and determine the nominal diameter of the standard rim; use the nominal diameter of the standard rim to determine the position of the central axis of the standard rim; For safety reasons, the point of maximum deformation is taken as the equivalent deformation point of this region. Furthermore, it is assumed that the deformation of the inner liner rubber compound in contact with the carcass is bound to the same deformation point as the skeleton material, and can be ignored compared to the deformation of the rubber compound in this region.
[0024] like Figure 3 As shown, point A, the center of symmetry of the fetal body in the crown, is taken as the equivalent deformation point in region T; In area S, point B, corresponding to the thickest part of the inner liner at the bottom of the belt layer, is taken as the equivalent deformation point. Specifically, point B is the intersection of the line connecting the outer end of the tire tread width and the end of the widest belt layer with the tire carcass. Since the included angle of the edge of the belt layer under the rubber pad on the finished cross-section is usually no greater than 15°, and the angle between the upper contour edge and the bottom edge of the finished rubber pad is usually no greater than 30°, considering the safety margin design, the rubber pad can be simplified into an isosceles triangle of 60°, 60°, and 60°, and the included angle between the rubber pad and the belt layer can be simplified to 30°. Point B is located at the center point of the base of the isosceles triangle. The stretching of point B is bound to the tire carcass material at the corresponding position. Then the stretching rate of the center point of the bottom edge of the rubber pad is the stretching rate of point B. (c) Measure the distance L from point ABC on the material distribution diagram to the center axis of the standard rim. A L B L C .
[0025] (d)T A S B B C The calculation formula is as follows: T A =L A / (forming drum radius * μ) S B = L B / (forming drum radius * μ) B C =L C / (forming drum radius * μ) Among them, the radius of the forming drum is the circumference of the forming drum / 2π, and μ is the coefficient of thermal expansion of the carcass material, which varies slightly depending on the process technology of each company. Our company's process coefficient is approximately 1.04.
[0026] (3) The formulas for calculating the thickness of the T, S, and B zones of the semi-finished inner lining layer are derived from the formula: Design thickness of the inner lining layer = Minimum thickness of the zone × Maximum tensile strength of the zone. G T =H Tmin ×T A G S =H Smin ×S B GB =H Bmin ×B C Wherein: H Tmin H Smin H Bmin These are the minimum standard theoretical thicknesses of the inner linings in zones T, S, and B, respectively, after being stretched from semi-finished to finished product dimensions on the finished tire. The standard theoretical thickness H of the inner lining layer in the crown T zone, shoulder S zone, and bead B zone of the finished tire is determined based on whether the product is tubeless or not and the location of the inner end of the bead lining. This thickness is calculated from the semi-finished product to the finished product size after stretching. T H S H B The minimum value.
[0027] (4) Draw the outline drawing of the transition layer half component.
[0028] Specific examples Based on the different design experience and processing techniques of each manufacturer, the standard theoretical thickness of the inner lining in the T-zone, S-zone of the tire shoulder, and B-zone of the bead varies from semi-finished product to finished tire after stretching. For Fengshen tires, which are tubeless, the finished product cross-section H... T The minimum value is approximately 1.2~2 mm, H S The minimum value is approximately 2.0~2.5mm, H B The minimum value is approximately 2.0~2.5mm. For products with inner tubes, the finished product cross-section H... T The minimum value is approximately 1.2~2 mm, H S The minimum value is approximately 2.2~3.0 mm, H B The minimum value is approximately 2.2~3.2 mm.
[0029] 1. Taking tubeless tires, specifically 12R22.5 size, as an example: Step 1: Divide the area and determine the main reference area for the design, as shown in the attached diagram. Figure 1 Appendix Figure 2 The width of the area is determined. The inner positioning of the padding in this specification is 75mm, so the width of area 1 is 75mm. The inner and outer positioning of the platform with the thickest padding thickness on the tire shoulder are 73mm and 103mm respectively, and the width of the padding platform is 30mm. Considering tolerances and production versatility, the width of area 2 is 40mm.
[0030] Step 2: Determine H based on whether the product type is tubeless or tubeless and the manufacturing process. T H S H B The minimum values are 1.2 mm, 2.0 mm, and 2.0 mm, respectively.
[0031] Step 3: 5. Determine the design thickness of the semi-finished inner lining area. G T =H Tmin ×T A =1.2 * 1.89 = 2.26 ≈ 2.3 G S =H Smin ×S B =2.0 * 1.88 = 3.76 ≈ 3.8 G B =H Bmin ×B C =2.0 * 1.13 = 2.26 ≈ 2.3 The rest is the same as the existing transition layer thickness.
[0032] Step 4: Draw the outline of the semi-finished component of the transition layer, as shown in the attached diagram. Figure 4 Calculations show that the weight of the transition layer in each tire after the lightweight design is reduced by 0.95 kg compared to the original transition layer.
[0033] 2. For tubed tires, taking 12.00R20 as an example, Step 1: Divide the area and determine the main reference area for the design, as shown in the attached diagram. Figure 1 Appendix Figure 2 The width of the area is determined. The inner positioning of the padding in this specification is 40mm, so the width of area 1 is 40mm. The inner and outer positioning of the platform with the thickest padding thickness on the tire shoulder are 92mm and 104mm respectively, and the width of the padding platform is 12mm. Considering tolerances and production versatility, the width of area 2 is 40mm.
[0034] Step 2: Determine H based on whether the product type is tubeless or tubeless and the manufacturing process. T H S H B The minimum values are 1.2 mm, 2.2 mm, and 2.2 mm, respectively.
[0035] Step 3: 5. Determine the design thickness of the semi-finished inner lining area. G T =H Tmin ×T A =1.2 * 2.17 = 2.6 ≈ 2.6 G S =H Smin ×S B =2.2 * 2.16 = 4.75 ≈ 4.8 G B =HBmin ×B C =2.2 * 1.45 = 3.19 ≈ 3.2 The remaining areas have the same thickness as the existing transition layer.
[0036] Step 4: The outline drawing of the semi-finished component of the transition layer is attached. Figure 5 Calculations show that the weight of the transition layer in each tire after the weight reduction process is 2.54 kg less than the original transition layer weight.
[0037] The second type: T is measured using a material distribution map method. A S B B C The specific steps to obtain it are as follows: (a) Prepare a material distribution diagram for the finished tire; (b) Determine points A, B, and C. According to the 2010 edition of "China Tire Rim Valve", the nominal diameter d of the 12R22.5 standard rim is 571.5 mm, and the nominal diameter of the 12.00R20 standard rim is 508 mm. Use the nominal diameter of the standard rim to determine the position of the center axis of the standard rim. (c) Measure the distances L from the equivalent deformation points A, B, and C in the center region of the tire crown, the tire shoulder region, and the region near the inner end of the bead reinforcement layer to the central axis of the standard rim, respectively, from the material distribution diagram. A L B L C The specifications for 12R22.5 are 503.3mm, 495.24mm, and 317.44mm, respectively, while the specifications for 12.00R20 are 526.7mm, 510.5mm, and 340mm, respectively.
[0038] (4) 12R22.5 T A S B B C The calculation is as follows: T A =L A / (forming drum radius * μ) = 503.3 / (1665 / 2π*1.04)≈1.83; S B = L B / (forming drum radius * μ) = 495.24 / (1665 / 2π * 1.04) ≈ 1.8; B C =L C / (forming drum radius * μ) = 317.44 / (1665 / 2π * 1.04) ≈ 1.15; Among them, the radius of the forming drum is the circumference of the forming drum / 2π. The circumference of the forming drum of this specification is designed to be 1665mm. μ is the coefficient of thermal expansion of the carcass material, which our company takes as 1.04. 12.00R20 T A S B B C The calculation is as follows: T A =L A / (forming drum radius * μ) = 526.7 / (1500 / 2π*1.04)≈2.12; S B = L B / (forming drum radius * μ) = 510.5 / (1500 / 2π * 1.04) ≈ 2.05; B C =L C / (forming drum radius * μ) = 340 / (1500 / 2π * 1.04) ≈ 1.38; Among them, the radius of the forming drum is the circumference of the forming drum / 2π. The circumference of the forming drum of this specification is designed to be 1500mm. μ is the coefficient of thermal expansion of the carcass material, which our company takes as 1.04. (3) The thicknesses of the T, S, and B zones of the semi-finished inner lining layer are calculated as follows: 12R22.5 specification: G T =H Tmin ×T A =1.2 * 1.83 = 2.19 ≈ 2.2mm G S =H Smin ×S B =2.0 * 1.8 = 3.6 ≈ 3.6 mm G B =H Bmin ×B C =2.0 * 1.15 = 2.3 ≈ 2.3mm Among them: according to the company's process technology requirements, H Tmin Take 1.2mm, H Smin Take 2.0mm, H Bmin Take 2.0mm.
[0039] 12.00R20 specification: G T =H Tmin ×T A =1.2 * 2.12 = 2.54 ≈ 2.6 mm G S =H Smin ×S B=2.2 * 2.05 = 4.51 ≈ 4.6 mm G B =H Bmin ×B C =2.2 * 1.38 = 3.04 ≈ 3.1 mm Wherein: H T H S H B The minimum values are 1.2 mm, 2.2 mm, and 2.2 mm, respectively.
[0040] The remaining areas have the same thickness as the existing transition layer.
[0041] Step 4: The outline drawing of the transition layer semi-finished component for 12R22.5 and 12.00R20 specifications is attached. Figure 6 Appendix Figure 7 Calculations show that the weight of the transition layer in each tire after weight reduction is 0.98 kg less than that of the original transition layer, and 2.57 kg less.
[0042] Using the semi-part outlines obtained from Methods 1 and 2, inner liner semi-parts were fabricated. These semi-parts were then used to produce tires of 12R22.5 and 12.00R20 specifications. The finished product section thickness is shown in Table 1 below. This table shows that the inner liner designed using lightweight design methods 1 and 2 has a significantly thinner finished tire crown center inner liner thickness compared to traditional design methods. This improves the tire crown's heat dissipation performance, reducing crown voids and early crown burst damage during use. The increased inner liner thickness at the tire shoulder and the significantly increased inner liner thickness at the inner end of the U-shaped bead wrap provides better protection for the belt layer and steel wire wrap ends, enhancing tire air and pressure retention performance. This reduces problems encountered with traditional designs during use, such as inner liner cracks at the shoulder and bead areas, and reduces shoulder voids caused by leaking threads, thereby increasing tire lifespan.
[0043] Taking the 12R22.5 and 12.00R20 tires with a lightweight transition layer produced in January 2022 as examples, a total of 2000 tires were tracked, including 860 12R22.5 tires and 1140 12.00R20 tires, with a tracking period of 1.5 years. Simultaneously, 860 12R22.5 tires and 1140 12.00R20 tires of the conventional design produced in the same period were compared with those produced in the market. The main market defects related to the inner liner are shown in Table 2 below: The above description is only a preferred embodiment of the present invention, but the scope of protection of the present invention is not limited thereto. It should be noted that for those skilled in the art and any person skilled in the art, any equivalent substitutions or changes made to the technical solution and inventive concept of the present invention without departing from the overall concept of the present invention, as well as any changes and improvements made, should also be considered within the scope of protection of the present invention.
Claims
1. A method for lightweight design of semi-finished automotive tire inner liner, characterized in that: Specifically, the thickness of the tire crown center area, tire shoulder area, and area near the inner end of the bead reinforcement layer is optimized. (1) Based on the material distribution location on the material distribution map, The center area of the tire crown, located at the center of the finished tire crown, with the center of the tire crown as the center line, its width is the distance between the inner end of the pad rubber and the center line of the tire crown; it is called the T area; The tire shoulder area, located at the shoulder of the finished tire, has a total width equal to the inner liner arc length between the two ends of the rubber pad bottom width; this is called the S-zone. The area near the inner end of the bead reinforcement layer, whose width is between 10mm and 20mm from the inner end of the bead wrapping of the finished tire section, is called Zone B. (2) Based on safety considerations, the point of maximum deformation is taken as the equivalent deformation point of the region; and it is assumed that the deformation of the inner liner rubber material in contact with the tire carcass is bound to the same deformation point as the skeleton material, and the equivalent deformation points of the tire crown center region, tire shoulder region, and region near the inner end of the bead reinforcement layer are determined respectively. In the T region, the symmetrical center point A of the fetal body in the crown is taken as the equivalent deformation point; In area S, point B, corresponding to the thickest part of the inner liner at the bottom of the belt layer, is taken as the equivalent deformation point. The specific method for taking point B is the intersection of the line connecting the outer end of the tire tread width and the end of the widest belt layer with the tire body. In area B, take the inner end point C of the finished cross-section of the fabric wrapping as the equivalent deformation point; The elongation at point A is represented by T. A The elongation at point B is represented by S. B The elongation at point C is represented by B. C This indicates that the maximum tensile strengths of the central area of the tire crown, the tire shoulder area, and the area near the inner end of the bead reinforcement layer are T, respectively. A S B B C Determine T A S B B C There are two methods, which can be any one of the following two methods; The first type: T A S B B C Calculate it using the following formula: ; in: AD is the diameter of the auxiliary drum; MD is the diameter of the forming drum; W is the width of the padding; D is the width of the forming machine; S1 is the inner positioning of the steel wire wrapping cloth; B1 is the inner circumference of the steel wire ring; The second type: T is measured using a material distribution map method. A S B B C The specific steps to obtain it are as follows: (a) Prepare a material distribution diagram for the finished tire; (b) Determine the nominal diameter of the standard rim; (c) Measure the distances L from the equivalent deformation points A, B, and C in the center region of the tire crown, the tire shoulder region, and the region near the inner end of the bead reinforcement layer to the central axis of the standard rim, respectively, from the material distribution diagram. A L B L C ; (d)T A S B B C The calculation formula is as follows: T A =L A / (forming drum radius * μ) S B = L B / (forming drum radius * μ) B C =L C / (forming drum radius * μ) Wherein, the radius of the forming drum is the circumference of the forming drum / 2π, and μ is the coefficient of thermal expansion of the carcass material; (3) The formulas for calculating the thickness of the T, S, and B zones of the semi-finished inner lining layer are derived from the formula: Design thickness of the inner lining layer = Minimum thickness of the zone × Maximum tensile strength of the zone. G T =H Tmin ×T A G S =H Smin ×S B G B =H Bmin ×B C Wherein: H Tmin H Smin H Bmin These are the minimum standard theoretical thicknesses of the inner linings in zones T, S, and B, respectively, after being stretched from semi-finished to finished product dimensions on the finished tire.
2. The method for lightweight design of semi-finished automotive tire inner liner layer according to claim 1, characterized in that: In step (3), the standard theoretical thickness H of the inner lining layer in the crown T area, shoulder S area, and bead B area of the finished tire is determined based on whether the product has an inner tube or not and the position of the inner end of the bead wrapping. This thickness is calculated from the semi-finished product to the finished product size after stretching. T H S H B The minimum value.
3. The method for lightweight design of semi-finished automotive tire inner liner layer according to claim 1, characterized in that: In step (2), the equivalent deformation point B in area S is determined as follows: since the angle between the edge of the padding layer under the finished product cross section is no greater than 15°, and the angle between the edge of the upper contour of the finished padding layer and the bottom edge is no greater than 30°, considering the safety margin design, the padding layer can be simplified into an equilateral triangle of 60°, 60°, and 60°, and the angle between the padding layer and the belt layer is simplified to 30°. Point B is located at the center point of the base of the isosceles triangle. The stretching of point B is bound to the carcass material at the corresponding position. Then the stretching rate of the center point of the bottom edge of the padding layer is the stretching rate of point B.