正极极片及其制备方法、电池单体、电池及用电设备

By layering conductive coatings in aqueous cathode batteries, the adhesion to the current collector and water resistance are improved, solving the problem of poor cycle stability of aqueous cathode batteries and achieving higher battery stability and energy density.

CN117716540BActive Publication Date: 2026-07-17CONTEMPORARY AMPEREX TECHNOLOGY CO LTD

Patent Information

Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
CONTEMPORARY AMPEREX TECHNOLOGY CO LTD
Filing Date
2022-07-13
Publication Date
2026-07-17

AI Technical Summary

Technical Problem

Existing aqueous cathode batteries suffer from poor cycle stability, mainly due to the limited contact area between the current collector and the active material, which leads to increased interfacial resistance and affects battery performance.

Method used

By layering the water-based conductive coatings, the adhesion between the first water-based conductive coating and the current collector is improved, and the water resistance of the second water-based conductive coating is used to prevent the coating from dissolving during the preparation process, thereby improving the adhesion and electrical connection between the electrode layer and the current collector.

Benefits of technology

It improves the cycle stability and capacity retention of the battery, reduces the rate of resistance change and thickness non-uniformity, and enhances the performance consistency of the positive electrode sheet.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117716540B_ABST
    Figure CN117716540B_ABST
Patent Text Reader

Abstract

一种正极极片及其制备方法、电池单体、电池及用电设备,涉及电池领域。正极极片(24)包括集流体(240)、水性导电涂层以及电极层(243),水性导电涂层包括第一水性导电涂层(241)以及第二水性导电涂层(242),第一水性导电涂层(241)位于第二水性导电涂层(242)面向集流体(240)的一侧;第一水性导电涂层(241)与集流体(240)之间的剥离力≥50N / M;第二水性导电涂层(242)可溶于水且超声波清洗的溶解时间≥200s,电极层(243)与第二水性导电涂层(242)之间的剥离力≥40N / M。该正极极片(24)能够改善现有采用水性正极的电池存在的循环稳定性较差的问题。