Railway slab crack detection method

By using a camera and ultrasonic phased array sensor carried by a track inspection trolley, combined with a photoelectric encoder and a computer, real-time and automated inspection of track slabs is achieved, solving the problems of low efficiency in traditional inspection and blind spots in ultrasonic inspection, and providing high-precision three-dimensional imaging of track slabs.

CN117740807BActive Publication Date: 2026-11-20SHANGHAI UNIV OF ENG SCI +2
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202311804439.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-12-26
Publication Date
2026-11-20
Estimated Expiration
2043-12-26

AI Technical Summary

Technical Problem

Traditional methods for detecting cracks in track slabs are inefficient and slow. Furthermore, ultrasonic phased array technology has blind spots when detecting cracks in track slabs, resulting in poor imaging effects and inaccurate detection results.

Method used

A track inspection trolley carrying a height-adjustable camera and an ultrasonic phased array sensor, combined with an optical encoder and a computer, enables real-time, automated inspection of the track slab surface and interior. Through a full-focus imaging algorithm and a virtual crack model, combined with isosurface extraction and interpolation calculations, a three-dimensional image of the track slab is generated.

Benefits of technology

It enables real-time, automated, and all-around inspection of track slabs, overcoming the problem of blind spots in ultrasonic inspection of track slab surfaces. The imaging results are more accurate, the inspection precision is high, and it can clearly show the complete cracks inside and outside the track slab.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117740807B_ABST
    Figure CN117740807B_ABST
Patent Text Reader

Abstract

The application discloses a kind of track slab crack detection methods, comprising the following steps: S1, track inspection trolley is driven to the steel rail of track slab to be detected;S2, with the movement of track inspection trolley, camera continuously shoots the track slab surface in front of track inspection trolley, photoelectric encoder real-time acquisition track inspection trolley wheel movement;S3, computer calculates the relative position of track slab crack according to wheel movement information, obtains the absolute position of track slab crack according to the picture of camera shooting, and calculates the geographical position of track slab crack in combination with relative position and absolute position;S4, when the picture of camera shooting shows that there is crack in track slab surface, start ultrasonic phased array sensor detection;S5, computer processes each slice data of track slab collected by ultrasonic phased array sensor, and obtains the three-dimensional imaging of complete track slab internal crack.The application overcomes track slab crack detection blind area, and detection precision is high.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to a method for detecting cracks in track slabs, belonging to the field of track slab crack detection technology. Background Technology

[0002] Track slabs are a crucial component of the entire track structure, directly bearing the load from the rails. Modern track slabs are pre-cast in the production workshop and then transported to the site for installation. During production, issues such as incomplete compaction can occur. Furthermore, prolonged exposure to air and environmental factors such as temperature changes, dynamic and static loads from trains, and rain erosion can lead to various cracks appearing on the surface and inside the track slabs. This poses a significant threat to the safe operation of trains, making crack detection of track slabs essential.

[0003] Traditional methods for detecting cracks in track slabs mainly rely on manual observation, which is subject to weather conditions, resulting in low efficiency and slow speed. Delayed detection can lead to significant dangerous losses. Ultrasonic testing technology, with its advantages of rapid energy propagation, strong penetration, and safe monitoring, has been widely used in non-destructive testing of various materials in recent years.

[0004] Chinese patent CN202010176415.X discloses an in-service blade damage detection robot. This robot includes a damage detection system, which comprises a camera module for capturing images of the blade surface and a phased array ultrasonic module for detecting internal blade damage. During detection, machine vision technology is used to identify the video data collected by the camera equipment, and coordinates and data are stored for damage such as cracks and corrosion on the blade surface. The phased array ultrasonic module's surface scanning mode can collect and store three-dimensional structural data of the blade's interior, and machine learning algorithms are used to improve the accuracy of automatic identification and localization of blade damage in ultrasonic imaging results.

[0005] Chinese patent CN202310724531.4 discloses a robot and method for detecting hidden dangers in the main beam of in-service wind turbine blades. The robot includes a curved surface adaptive phased array ultrasonic scanning structure and a camera detection system. The curved surface adaptive phased array ultrasonic scanning structure includes a curved surface adaptive unit and a phased array ultrasonic probe for detecting internal defects in the main beam of the blade. Under the action of the curved surface adaptive unit, the phased array ultrasonic probe is kept perpendicular to the detection surface and in close contact with the detection surface when moving on the curved surface. The camera detection system includes a drone main camera and a vehicle-mounted camera module installed under a wheeled mobile chassis. The drone main camera is used to detect environmental information in the robot's running direction, and the vehicle-mounted camera module is used to detect the working status of the curved surface adaptive phased array ultrasonic scanning structure and damage to the blade surface.

[0006] Concrete cracks can be classified into three types based on the form of external load: Type I (opening), Type II (slipping), and Type III (tearing). Cracks commonly found in track slabs belong to the combined Type I-II category. Due to the inherent characteristics of track slab cracks, blind spots exist when using ultrasonic phased array technology to detect track slab cracks, resulting in poor imaging effects and inaccurate detection results. Summary of the Invention

[0007] To address the aforementioned problems in the existing technology, the purpose of this invention is to provide a method for detecting cracks in track slabs.

[0008] To achieve the above objectives, the present invention adopts the following technical solution:

[0009] A method for detecting cracks in track slabs includes the following steps:

[0010] S1. The track inspection trolley is driven onto the rail of the track slab to be inspected. The front end of the track inspection trolley is equipped with a height-adjustable camera, and an ultrasonic phased array sensor is located below the camera. The track inspection trolley is equipped with a photoelectric encoder. The camera, ultrasonic phased array sensor, and photoelectric encoder are respectively connected to a computer.

[0011] S2. As the track inspection trolley moves, the camera continuously takes pictures of the track slab surface in front of the track inspection trolley and transmits the pictures to the computer. The photoelectric encoder collects the motion of the track inspection trolley wheels in real time and transmits the collected wheel motion information to the computer.

[0012] S3. The computer calculates the relative position of the track slab crack based on the wheel motion information, obtains the absolute position of the track slab crack based on the images taken by the camera, and calculates the geographical location of the track slab crack by combining the relative and absolute positions of the track slab crack.

[0013] S4. When the image captured by the camera shows that there are cracks on the surface of the track slab, the ultrasonic phased array sensor detection is started. The transmitting end of the ultrasonic phased array sensor emits ultrasonic waves perpendicular to the track slab at the same distance interval. Then, the receiving end of the ultrasonic phased array sensor receives the sound field signal reflected from the inside of the track slab, forming the full matrix data of each slice section, and then transmits the full matrix data of each slice section to the computer.

[0014] S5. The computer processes the data of each slice of the track slab acquired by the ultrasonic phased array sensor, forming a two-dimensional detection image of each slice. It then combines this with a virtual crack model to predict cracks in the blind zone, creating a complete slice image containing track slab cracks. Finally, it performs isosurface extraction and interpolation calculations on all slice images to obtain a complete three-dimensional image of the internal cracks of the track slab, achieving visualized detection of track slab cracks. This includes the following operations:

[0015] S51. The computer uses a full-focusing imaging algorithm to process the full matrix data of each slice section of the track slab acquired by the ultrasonic phased array sensor, and obtains a two-dimensional detection image of each slice.

[0016] S52. Perform edge trimming, binarization, and grayscale preprocessing on all the two-dimensional detection images of the slice sections to obtain clear contour information of the cracks;

[0017] S53. Predicting blind zone cracks in track slabs using virtual crack models from structural engineering: Concrete cracks can be classified into three types based on the different forms of external loads: Type I, Type II, and Type III. The cracks in the track slab belong to the Type I-II composite type. The propagation criterion for Type I-II concrete cracks states that during crack propagation, the difference between the stress intensity factor at the crack tip under external load and the stress intensity factor at the crack tip under virtual crack cohesion is... When the crack initiation toughness equals that of a type I-II composite crack, the crack is in a critical state of propagation. Combining the propagation criterion for type I-II cracks in concrete with the maximum circumferential stress criterion, the crack initiation equation for the specimen is obtained:

[0018] (2);

[0019] in:

[0020] (3);

[0021] In equations (2) and (3): , and , External loads and cohesion Type I and Type II stress intensity factors at the crack tip under action; To create a cracked corner; For type I concrete, the crack initiation toughness;

[0022] During crack propagation, the crack extends along the direction of the principal tensile strain at the crack tip, and the crack propagation angle is... Calculated by the following formula:

[0023] (4);

[0024] In equation (4): For the crack propagation angle, , , These are the shear strains at the crack tip under load, and The positive strain in the direction;

[0025] Set the initial crack length and step length Substituting the material parameters of the track slab and the load on the track slab at a certain moment into equation (4), the crack propagation angle can be obtained, and the crack propagation direction in the first step can be obtained; then, substituting the external load on the track slab at the next moment, the above process is repeated to obtain the trajectory of the crack in the blind zone of the track slab, and thus realize the prediction of the crack in the blind zone. The specific process is as follows:

[0026] In the pre-processed slice image, at the crack representing the boundary between the detection area and the blind area, two rows of pixel grids representing the crack are selected sequentially from top to bottom, and the pixel grids at the middle position of each are taken, denoted as . , Calculate the distance between them as the initial crack length. ,Right now:

[0027] (5);

[0028] Calculate step size for:

[0029] (6);

[0030] In equation (6), , These are the dimensions of the divided pixel grid;

[0031] Based on the initial crack length and step length and the calculated crack propagation angle The expansion path of the first step can be calculated, and the distance between the expansion path and the surrounding pixel grid points can be calculated. The closest point is selected as the new center position of the crack. The cracks are symmetrically distributed around the center position, and the width is the width of the initial crack. The length that can be predicted in each step is one grid length. In the next step, the newly predicted center position of the crack is... and The distance between them is used as the new initial crack length. Combined with step size and new crack propagation angle To make the next prediction, after n iterations, we finally obtain... The location of the cracks, along with their width, extends to the very top of the image, indicating the distribution of cracks on the surface of the track slab.

[0032] S54. Using the positional information of each image as a reference, perform isosurface extraction and interpolation calculations on the images in Matlab software to achieve spatial three-dimensional imaging of defects. The operation is as follows:

[0033] Each time, two slice images are selected, and two corresponding small squares are chosen from the image to form a voxel. Isosurface calculations are performed on each voxel, and this process is repeated for all slice images. An isosurface is the set of all points in space with the same gray value. This isosurface is a continuous three-dimensional surface, and its equation is established. Set a certain grayscale value Then the isosurface equation satisfies the following equation:

[0034] (7);

[0035] In equation (7), The equation of the surface where all gray values ​​are equal;

[0036] By calculating the function values ​​corresponding to the coordinates of each voxel vertex, the relationship between each vertex in the voxel and the isosurface is determined one by one. Then, the interpolation formula is used to perform interpolation calculations on the voxel boundary to calculate the gray value information of a certain point within the voxel. The interpolation formula is as follows:

[0037] (8);

[0038] In equation (8): where is the coefficient of each vertex in the voxel. Let be the coordinates of the vertices of each voxel. When the isosurface to be sought is a fixed value, that is... hour, Let be a constant value for the isosurface. The intersection line between the isosurface and each face of the voxel can be calculated using formula (8). Then, the equation of the boundary is... , Let the boundary value be the intersection line between the isosurface and each face of the voxel, thus obtaining:

[0039] (9);

[0040] in, , , , They are as follows:

[0041] (10);

[0042] In equations (9) and (10), , , , These are the coefficients of each volume element point in the isosurface;

[0043] In this way, by extracting isosurfaces and interpolating, the gray values ​​within all voxels are calculated, and three-dimensional reconstruction is completed to obtain a complete three-dimensional image of the track slab crack. The visual detection of track slab cracks can be achieved through three-dimensional imaging.

[0044] In one embodiment, in step S2, the camera takes pictures perpendicular to the track slab.

[0045] In one implementation, step S3 includes the following operations:

[0046] S31. The computer preprocesses the image with cracks captured by the camera and extracts crack features: The computer first performs image grayscale conversion, image filtering, image enhancement, and image binarization preprocessing on the image with cracks captured by the camera in sequence. Then, it extracts crack features from the preprocessed image. Among these, image enhancement processing refers to enhancing the image using a histogram equalization algorithm.

[0047] (1);

[0048] In formula (1): It represents the grayscale level of each pixel after equalization. It is the sum of the pixels in the image. It represents the number of pixels at the current grayscale level. It is the total number of gray levels in the image. It is the number of gray levels in the image. It is the gray level index in the image. ;

[0049] S32. The crack features in the extracted image are detected and classified by the SSD target detection algorithm to realize the crack detection on the surface of the track slab and mark the location of the crack. This location is the geographical location of the crack.

[0050] In one embodiment, in step S3, median filtering is used for image filtering.

[0051] In one embodiment, in step S4, the transmitting end of the ultrasonic phased array sensor sequentially and perpendicularly to the track plate, emits ultrasonic waves with a center frequency of 50kHz into the interior of the track plate at equal distance intervals.

[0052] In one embodiment, the ultrasonic phased array sensor includes a phased array probe bracket and an ultrasonic phased array probe mounted on the phased array probe bracket, wherein the ultrasonic phased array probe is connected to a computer signal.

[0053] In a preferred embodiment, the ultrasonic phased array probe is a dry-coupled ultrasonic phased array probe.

[0054] One embodiment is a CCD industrial camera.

[0055] In one embodiment, a ring light source is provided around the camera.

[0056] In one embodiment, the front end of the track inspection trolley is connected to a height-adjustable camera bracket, the camera is mounted on the upper end of the camera bracket, and the ultrasonic phased array sensor is mounted on the lower end of the camera bracket.

[0057] One embodiment includes a mobile power supply mounted on the track inspection trolley.

[0058] In one embodiment, the bottom of the track inspection trolley is provided with a drive motor for driving the wheels of the track inspection trolley to rotate, and the photoelectric encoder is located on the motor shaft of the drive motor.

[0059] In one embodiment, the track inspection trolley is equipped with an ultrasonic excitation source, which is connected to a computer and an ultrasonic phased array sensor. The computer controls the ultrasonic excitation source to excite and emit ultrasonic waves perpendicular to the track slab through the transmitting end of the ultrasonic phased array sensor.

[0060] In one embodiment, the track inspection trolley is equipped with a data acquisition controller, which is connected to a computer and a photoelectric encoder. The photoelectric encoder generates pulse electrical signals by rotating its code disk, and the generated pulse electrical signals are transmitted to the computer through the data acquisition controller to realize the acquisition of the wheel motion of the track inspection trolley.

[0061] Compared with the prior art, the beneficial technical effects of the present invention are as follows:

[0062] The track slab crack detection method provided by this invention can realize real-time, automated, and all-round detection of track slabs. The detection process is not easily affected by the environment. The obtained three-dimensional imaging of track slab cracks can show the complete cracks inside and outside the track slab. It overcomes the problem of blind spots in ultrasonic detection of track slab surfaces, and the imaging results are more accurate and the detection precision is high. Compared with the existing technology, it has significant innovation and application value. Attached Figure Description

[0063] Figure 1 This is a diagram showing the working state of the track slab crack detection device provided in this embodiment of the invention;

[0064] Figure 2 This is a schematic diagram of the track slab crack detection device provided in an embodiment of the present invention;

[0065] Figure 3 This is a schematic diagram of the ultrasonic phased array sensor in an embodiment of the present invention;

[0066] Figure 4 This is a flowchart of the track slab crack detection method in an embodiment of the present invention;

[0067] Figure 5 This is a three-dimensional reconstruction image of the track slab crack in an embodiment of the present invention;

[0068] The labels in the diagram are as follows:

[0069] 1. Track inspection trolley; 2. Camera; 3. Ultrasonic phased array sensor; 301. Phased array probe bracket; 302. Ultrasonic phased array probe; 4. Photoelectric encoder; 5. Computer; 6. Track slab; 7. Ring light source; 8. Camera bracket; 9. Mobile power supply; 10. Ultrasonic excitation source; 11. Data acquisition controller; 12. Track slab; 13. Track slab crack imaging. Detailed Implementation

[0070] The technical solution of the present invention will be further described clearly and completely below with reference to the accompanying drawings and embodiments.

[0071] Example

[0072] Combination Figures 1 to 3 As shown: The present invention provides a track slab crack detection device, including a track inspection trolley 1, a height-adjustable camera 2 at the front end of the track inspection trolley 1, an ultrasonic phased array sensor 3 below the camera 2, and a photoelectric encoder 4 on the track inspection trolley 1. The camera 2, the ultrasonic phased array sensor 3, and the photoelectric encoder 4 are respectively connected to a computer 5.

[0073] In this embodiment, the computer 5 is a vehicle-mounted computer installed on the track inspection trolley 1. During connection, the camera 2 and the ultrasonic phased array sensor 3 are connected to the computer 5 through data cables, ensuring the speed and stability of data transmission.

[0074] In this embodiment, the ultrasonic phased array sensor 3 includes a phased array probe bracket 301 and an ultrasonic phased array probe 302 mounted on the phased array probe bracket 301. The ultrasonic phased array probe 302 is connected to the computer 5 via signal transmission. In use, the ultrasonic phased array probe 302 emits ultrasonic waves perpendicular to the track slab 6 into the track slab. The ultrasonic phased array probe 302 can be a commercially available product; in this embodiment, the ultrasonic phased array probe 302 is a dry-coupled ultrasonic phased array probe.

[0075] In this embodiment, the camera 2 is a CCD industrial camera. Furthermore, a ring light source 7 is provided around the camera 2. This serves two purposes: firstly, it supplements the light source when the ambient light is weak, making the camera more sensitive and ensuring uniform lighting in the images captured by the camera 2, which is beneficial for identifying and extracting crack features; secondly, it ensures that the detection device can operate even at night.

[0076] In this embodiment, the front end of the track inspection trolley 1 is connected to a height-adjustable camera bracket 8. The camera 2 is mounted on the upper end of the camera bracket 8, and the ultrasonic phased array sensor 3 is mounted on the lower end of the camera bracket 8. The camera bracket 8 can be a commercially available product, such as a commercially available electric telescopic rod. The camera 2 is mounted on the upper telescopic end of the telescopic rod, and the ultrasonic phased array sensor 3 is mounted on the lower fixed end of the telescopic rod. The camera bracket 8 allows the height of the camera 2 to be adjusted. When the crack distribution range is large, the camera 2 rises, thereby expanding the camera's field of view; when the crack is small, the camera 2 lowers, reducing the field of view, making the image of the crack clearer.

[0077] In this embodiment, the track inspection trolley 1 is equipped with a mobile power supply 9 to provide mobile power to the electrical equipment in the inspection device.

[0078] In this embodiment, the bottom of the track inspection trolley 1 is provided with a drive motor (not shown in the figure) for driving the wheels of the track inspection trolley 1 to rotate, and the photoelectric encoder 4 is located on the motor shaft of the drive motor.

[0079] In this embodiment, the track inspection trolley 1 is equipped with an ultrasonic excitation source 10. The ultrasonic excitation source 10 is connected to the computer 5 and the ultrasonic phased array sensor 3. The computer 5 controls the ultrasonic excitation source 10 to excite and emit ultrasonic waves perpendicularly to the track slab 6 through the transmitting end of the ultrasonic phased array sensor 3. The ultrasonic excitation source 10 can be a commercially available product.

[0080] In this embodiment, the track inspection trolley 1 is equipped with a data acquisition controller 11. The data acquisition controller 11 is connected to the computer 5 and the photoelectric encoder 4. The photoelectric encoder 4 generates pulse electrical signals by rotating its code disk. The generated pulse electrical signals are transmitted to the computer 5 through the data acquisition controller 11 to realize the acquisition of the wheel motion of the track inspection trolley. The data acquisition controller 11 can be a commercially available product.

[0081] See Figure 4 As shown, the method for detecting track slab cracks using the track slab crack detection device of the present invention includes the following steps:

[0082] S1. The track inspection trolley 1 is driven onto the rail of the track slab 6 to be inspected. The front end of the track inspection trolley 1 is equipped with a height-adjustable camera 2. Below the camera 2 is an ultrasonic phased array sensor 3. The track inspection trolley 1 is equipped with a photoelectric encoder 4. The camera 2, ultrasonic phased array sensor 3, and photoelectric encoder 4 are respectively connected to a computer 5.

[0083] S2. As the track inspection trolley 1 moves, the camera 2 continuously takes pictures of the surface of the track plate 6 in front of the track inspection trolley 1 (when taking pictures, the camera 2 is perpendicular to the track plate 6), and transmits the pictures to the computer 5. The photoelectric encoder 4 collects the motion of the wheels of the track inspection trolley 1 in real time and transmits the collected wheel motion information to the computer 5.

[0084] S3. Computer 5 calculates the relative position of the track slab crack based on the wheel motion information, obtains the absolute position of the track slab crack based on the image taken by camera 2, and calculates the geographical location of the track slab crack by combining the relative and absolute positions; specifically including the following operations:

[0085] S31. Computer 5 preprocesses the image with cracks captured by the camera and extracts crack features: Computer 5 first performs image grayscale conversion, image filtering (specifically, median filtering is used to remove noise while better preserving edge details), image enhancement, and image binarization (specifically, a suitable threshold is selected for image binarization; in this embodiment, a grayscale value of 200 is chosen to make the contrast between the background and the cracks more obvious, thus facilitating the extraction of crack features) preprocessing on the preprocessed image. Then, crack features are extracted from the preprocessed image. The image enhancement process refers to using a histogram equalization algorithm to enhance the image.

[0086] (1);

[0087] In formula (1): It represents the grayscale level of each pixel after equalization. It is the sum of the pixels in the image. It represents the number of pixels at the current grayscale level. It is the total number of gray levels in the image. It is the number of gray levels in the image. It is the gray level index in the image. ;

[0088] S32. The crack features in the extracted image are detected and classified by the SSD target detection algorithm to realize the crack detection on the surface of the track slab and mark the location of the crack. This location is the geographical location of the crack.

[0089] S4. When the image captured by camera 2 shows that there are cracks on the surface of the track slab, the ultrasonic phased array sensor 3 starts to detect. The transmitting end of the ultrasonic phased array sensor 3 emits ultrasonic waves perpendicular to the track slab at the same distance intervals to the interior of the track slab (specifically: the transmitting end of the ultrasonic phased array sensor emits ultrasonic waves with a center frequency of 50kHz perpendicular to the track slab at the same distance intervals to the interior of the track slab. The ultrasonic waves used have a low frequency, and the sound wave energy is not easily attenuated in the track slab, which is conducive to the sound waves propagating deeper and improving the ultrasonic detection depth). Then, the receiving end of the ultrasonic phased array sensor 3 receives the sound field signal reflected from the interior of the track slab, forming the full matrix data of each slice section, and transmits the full matrix data of each slice section to computer 5.

[0090] S5 and computer 5 process the data of each slice of the track slab collected by ultrasonic phased array sensor 3, forming a two-dimensional detection image of each slice (i.e., attached image). Figure 4 The image is scanned (B-scan image), and combined with fracture mechanics theory in engineering, blind zone cracks are predicted to form a complete slice image containing track slab cracks. Then, isosurface extraction is performed on all slice images (i.e., appending...). Figure 4 The MC algorithm (and interpolation calculations) are used to obtain a complete 3D image of the internal cracks in the track slab, enabling visual detection of track slab cracks; specifically, the following operations are included:

[0091] S51 and Computer 5 use a full-focusing imaging algorithm (any existing full-focusing imaging algorithm will suffice) to process the full matrix data of each cross-section of the track slab acquired by the ultrasonic phased array sensor, obtaining a two-dimensional detection image of each slice (i.e., an attached image). Figure 4 (B-scan image in the image)

[0092] S52. Perform edge trimming, binarization, and grayscale preprocessing on all the two-dimensional detection images of the slice sections to obtain clear contour information of the cracks;

[0093] S53. Predicting blind zone cracks in track slabs using virtual crack models in structural engineering: Concrete cracks can be classified into three types based on the different forms of external loads: Type I (opening), Type II (slipping), and Type III (tearing). The cracks in the track slab belong to the I-II composite type. The propagation criterion for concrete Type I-II cracks states that during crack propagation, the difference between the stress intensity factor at the crack tip under external load and the stress intensity factor at the crack tip under virtual crack cohesion is... When the crack initiation toughness equals that of a type I-II composite crack, the crack is in a critical state of propagation. Combining the propagation criterion for type I-II cracks in concrete with the maximum circumferential stress criterion, the crack initiation equation for the specimen is obtained:

[0094] (2);

[0095] in:

[0096] (3);

[0097] In equations (2) and (3): , and , External loads and cohesion Type I and Type II stress intensity factors at the crack tip under action; To create a cracked corner; The crack initiation toughness of Type I concrete can be determined based on the experimentally measured crack initiation load of the track slab cement material. and initial crack length Calculated;

[0098] During crack propagation, the crack extends along the direction of the principal tensile strain at the crack tip, and the crack propagation angle is... Calculated by the following formula:

[0099] (4);

[0100] In equation (4): For the crack propagation angle, , , These are the shear strains at the crack tip under load, and The positive strain in the direction;

[0101] Set the initial crack length and step length Substituting the material parameters of the track slab and the load on the track slab at a certain moment into equation (4), the crack propagation angle can be obtained, and the crack propagation direction in the first step can be obtained; then, substituting the external load on the track slab at the next moment, the above process is repeated to obtain the trajectory of the crack in the blind zone of the track slab, and thus realize the prediction of the crack in the blind zone. The specific process is as follows:

[0102] In the pre-processed slice image, at the crack representing the boundary between the detection area and the blind area, two rows of pixel grids representing the crack are selected sequentially from top to bottom, and the pixel grids at the middle position of each are taken, denoted as . , Calculate the distance between them as the initial crack length. ,Right now:

[0103] (5);

[0104] Calculate step size for:

[0105] (6);

[0106] In equation (6), , These are the dimensions of the divided pixel grid;

[0107] Based on the initial crack length and step length and the calculated crack propagation angle The expansion path of the first step can be calculated, and the distance between the expansion path and the surrounding pixel grid points can be calculated. The closest point is selected as the new center position of the crack. The cracks are symmetrically distributed around the center position, and the width is the width of the initial crack. The length that can be predicted in each step is one grid length. In the next step, the newly predicted center position of the crack is... and The distance between them is used as the new initial crack length. Combined with step size and new crack propagation angle To make the next prediction, after n iterations, we finally obtain... The location of the cracks, along with their width, extends to the very top of the image, indicating the distribution of cracks on the surface of the track slab.

[0108] S54. Using the positional information of each image as a reference, perform isosurface extraction and interpolation calculations on the images in Matlab software to achieve spatial three-dimensional imaging of defects. The operation is as follows:

[0109] Each time, two slice layer cross-sectional images are selected, and two corresponding small squares are selected in the image to form a voxel. Isosurface calculation is performed on each voxel, and the isosurface processing of all slice layers is completed in sequence (this algorithm is attached). Figure 4 In the McLeod algorithm, the isosurface is the set of all points in space with the same gray value. This isosurface is a continuous three-dimensional surface, and the surface equation is established. Set a certain grayscale value Then the isosurface equation satisfies the following equation:

[0110] (7);

[0111] In equation (7), The equation of the surface where all gray values ​​are equal;

[0112] By calculating the function values ​​corresponding to the coordinates of each voxel vertex, the relationship between each vertex in the voxel and the isosurface is determined one by one. Then, the interpolation formula is used to perform interpolation calculations on the voxel boundary to calculate the gray value information of a certain point within the voxel. The interpolation formula is as follows:

[0113] (8);

[0114] In equation (8): where is the coefficient of each vertex in the voxel. Let be the coordinates of the vertices of each voxel. When the isosurface to be sought is a fixed value, that is... hour, Since the isosurface is a constant value, the intersection line between the isosurface and each face of the voxel can be calculated using formula (8). Then the equation of the boundary is: , Let the boundary value be the intersection line between the isosurface and each face of the voxel, thus obtaining:

[0115] (9);

[0116] in, , , , They are as follows:

[0117] (10);

[0118] In equations (9) and (10), , , , These are the coefficients of each volume element point in the isosurface;

[0119] Thus, by extracting isosurfaces and interpolating, the gray values ​​within all voxels are calculated, completing the 3D reconstruction and obtaining a complete 3D image of the track slab crack. This 3D imaging enables the visual detection of track slab cracks, and the detection results are as follows: Figure 5 As shown, from Figure 5 As can be seen, the present invention can not only detect cracks in the depth of the track slab model 12, but also cracks that extend all the way to the surface of the track slab model 12. The resulting track slab crack image 13 can more clearly show the cracks inside and outside the track slab, solving the problem of blind spots in ultrasonic detection of the track slab surface.

[0120] In summary, this invention overcomes the problem of blind spots in ultrasonic testing of track slab surfaces, enabling comprehensive, long-distance, and automated testing of track slabs with high efficiency. It can more clearly present cracks inside and outside the track slab, providing high visualization and real-time, effective diagnostic data for maintenance personnel, thus ensuring the safe and healthy operation of trains.

[0121] Finally, it should be pointed out that the above description is only a preferred embodiment of the present invention, but the scope of protection of the present invention is not limited thereto. Any changes or substitutions that can be easily conceived by those skilled in the art within the scope of the technology disclosed in the present invention should be included within the scope of protection of the present invention.

Claims

1. A method for detecting cracks in track slabs, characterized in that, Includes the following steps: S1. The track inspection trolley is driven onto the rail of the track slab to be inspected. The front end of the track inspection trolley is equipped with a height-adjustable camera, and an ultrasonic phased array sensor is located below the camera. The track inspection trolley is equipped with a photoelectric encoder. The camera, ultrasonic phased array sensor, and photoelectric encoder are respectively connected to a computer. S2. As the track inspection trolley moves, the camera continuously takes pictures of the track slab surface in front of the track inspection trolley and transmits the pictures to the computer. The photoelectric encoder collects the motion of the track inspection trolley wheels in real time and transmits the collected wheel motion information to the computer. S3. The computer calculates the relative position of the track slab crack based on the wheel motion information, obtains the absolute position of the track slab crack based on the images taken by the camera, and calculates the geographical location of the track slab crack by combining the relative and absolute positions of the track slab crack. S4. When the image captured by the camera shows that there are cracks on the surface of the track slab, the ultrasonic phased array sensor detection is started. The transmitting end of the ultrasonic phased array sensor emits ultrasonic waves perpendicular to the track slab at the same distance interval. Then, the receiving end of the ultrasonic phased array sensor receives the sound field signal reflected from the inside of the track slab, forming the full matrix data of each slice section, and then transmits the full matrix data of each slice section to the computer. S5. The computer processes the data of each slice of the track slab acquired by the ultrasonic phased array sensor, forming a two-dimensional detection image of each slice. It then combines this with a virtual crack model to predict cracks in the blind zone, creating a complete slice image containing track slab cracks. Finally, it performs isosurface extraction and interpolation calculations on all slice images to obtain a complete three-dimensional image of the internal cracks of the track slab, achieving visualized detection of track slab cracks. This includes the following operations: S51. The computer uses a full-focusing imaging algorithm to process the full matrix data of each slice section of the track slab acquired by the ultrasonic phased array sensor, and obtains a two-dimensional detection image of each slice. S52. Perform edge trimming, binarization, and grayscale preprocessing on all two-dimensional detection images of the slice sections to obtain clear contour information of the cracks; S53. Predicting blind zone cracks in track slabs using virtual crack models from structural engineering: Concrete cracks can be classified into three types based on the different forms of external loads: Type I, Type II, and Type III. The cracks in the track slab belong to the Type I-II composite type. The propagation criterion for Type I-II concrete cracks states that during crack propagation, the difference between the stress intensity factor at the crack tip under external load and the stress intensity factor at the crack tip under virtual crack cohesion is... When the crack initiation toughness equals that of a type I-II composite crack, the crack is in a critical state of propagation. Combining the propagation criterion for type I-II cracks in concrete with the maximum circumferential stress criterion, the crack initiation equation for the specimen is obtained: (2); in: (3); In equations (2) and (3): , and , External loads and cohesion Type I and Type II stress intensity factors at the crack tip under action; To create a cracked corner; For type I concrete, the crack initiation toughness; During crack propagation, the crack extends along the direction of the principal tensile strain at the crack tip, and the crack propagation angle is... Calculated by the following formula: (4); In equation (4): For the crack propagation angle, , , These are the shear strains at the crack tip under load, and The positive strain in the direction; Set the initial crack length and step length Substituting the material parameters of the track slab and the load on the track slab at a certain moment into equation (4), the crack propagation angle can be obtained, and the crack propagation direction in the first step can be obtained; then, substituting the external load on the track slab at the next moment, the above process is repeated to obtain the trajectory of the crack in the blind zone of the track slab, and thus realize the prediction of the crack in the blind zone. The specific process is as follows: In the pre-processed slice image, at the crack representing the boundary between the detection area and the blind area, two rows of pixel grids representing the crack are selected sequentially from top to bottom, and the pixel grids at the middle position of each are taken, denoted as . , Calculate the distance between them as the initial crack length. ,Right now: (5); Calculate step size for: (6); In equation (6), , These are the dimensions of the divided pixel grid; Based on the initial crack length and step length and the calculated crack propagation angle The expansion path of the first step can be calculated, and the distance between the expansion path and the surrounding pixel grid points can be calculated. The closest point is selected as the new center position of the crack. The cracks are symmetrically distributed around the center position, and the width is the width of the initial crack. The length that can be predicted in each step is one grid length. In the next step, the newly predicted center position of the crack is... and The distance between them is used as the new initial crack length. Combined with step size and new crack propagation angle To make the next prediction, after After several iterations, we finally obtain The location of the cracks, along with their width, extends to the very top of the image, indicating the distribution of cracks on the surface of the track slab. S54. Using the positional information of each image as a reference, perform isosurface extraction and interpolation calculations on the images in Matlab software to achieve spatial three-dimensional imaging of defects. The operation is as follows: Each time, two slice images are selected, and two corresponding small squares are chosen from the image to form a voxel. Isosurface calculations are performed on each voxel, and this process is repeated for all slice images. An isosurface is the set of all points in space with the same gray value. This isosurface is a continuous three-dimensional surface, and its equation is established. Set a certain grayscale value Then the isosurface equation satisfies the following equation: (7); In equation (7), The equation of the surface where all gray values ​​are equal; By calculating the function values ​​corresponding to the coordinates of each voxel vertex, the relationship between each vertex in the voxel and the isosurface is determined one by one. Then, the interpolation formula is used to perform interpolation calculations on the voxel boundary to calculate the gray value information of a certain point within the voxel. The interpolation formula is as follows: (8); In equation (8): where is the coefficient of each vertex in the voxel. Let be the coordinates of the vertices of each voxel. When the isosurface to be sought is a fixed value, that is... hour, Since the isosurface is a constant value, the intersection line between the isosurface and each face of the voxel can be calculated using formula (8). Then the equation of the boundary is: , Let the boundary value be the intersection line between the isosurface and each face of the voxel, thus obtaining: (9); in, , , , They are as follows: (10); In equations (9) and (10), , , , These are the coefficients of each volume element point in the isosurface; In this way, by extracting isosurfaces and interpolating, the gray values ​​within all voxels are calculated, and three-dimensional reconstruction is completed to obtain a complete three-dimensional image of the track slab crack. The visual detection of track slab cracks can be achieved through three-dimensional imaging.

2. The method for detecting cracks in track slabs according to claim 1, characterized in that: In step S2, the camera takes pictures perpendicular to the track plate.

3. The method for detecting cracks in track slabs according to claim 1, characterized in that: Step S3 includes the following operations: S31. The computer preprocesses the image with cracks captured by the camera and extracts crack features: The computer first performs image grayscale conversion, image filtering, image enhancement, and image binarization preprocessing on the image with cracks captured by the camera in sequence. Then, it extracts crack features from the preprocessed image. Among these, image enhancement processing refers to enhancing the image using a histogram equalization algorithm. (1); In formula (1): It represents the grayscale level of each pixel after equalization. It is the sum of the pixels in the image. This is the number of pixels at the current grayscale level. It is the total number of gray levels in the image. It is the number of gray levels in the image. It is the gray level index in the image. ; S32. The crack features in the extracted image are detected and classified by the SSD target detection algorithm to realize the crack detection on the surface of the track slab and mark the location of the crack. This location is the geographical location of the crack.

4. The method for detecting cracks in track slabs according to claim 1, characterized in that: In step S3, the median filtering method is used for image filtering processing.

5. The method for detecting cracks in track slabs according to claim 1, characterized in that: The camera is surrounded by a ring light source.

6. The method for detecting cracks in track slabs according to claim 1, characterized in that: The front end of the track inspection trolley is connected to a height-adjustable camera bracket, the camera is mounted on the upper end of the camera bracket, and the ultrasonic phased array sensor is mounted on the lower end of the camera bracket.

7. The method for detecting cracks in track slabs according to claim 1, characterized in that: The bottom of the track inspection trolley is equipped with a drive motor for driving the wheels of the track inspection trolley to rotate, and the photoelectric encoder is located on the motor shaft of the drive motor.

8. The method for detecting cracks in track slabs according to claim 1, characterized in that: The track inspection trolley is equipped with an ultrasonic excitation source, which is connected to a computer and an ultrasonic phased array sensor. The computer controls the ultrasonic excitation source to excite and emit ultrasonic waves perpendicular to the track slab through the transmitting end of the ultrasonic phased array sensor.

9. The method for detecting cracks in track slabs according to claim 1, characterized in that: The track inspection trolley is equipped with a data acquisition controller, which is connected to a computer and a photoelectric encoder. The photoelectric encoder generates pulse electrical signals by rotating its code disk. The generated pulse electrical signals are transmitted to the computer through the data acquisition controller to realize the acquisition of the wheel motion of the track inspection trolley.

Citation Information

Patent Citations

  • A robot for detecting damage to in-service blades

    CN111398418B

  • In-service wind power blade main beam hidden danger detection robot and detection method thereof

    CN116902240A

  • Bridge detection information management system

    CN113567247A

  • Signal acquisition device for ballastless track plate crack detection

    CN211856387U