A method for mass production of an absolute optical path wavelength division multiplexing device

By accurately measuring and splicing the fiber length of the wavelength division multiplexing tube, the problem of optical path difference in the existing technology has been solved, realizing the fabrication of large-scale, high-precision absolute optical path wavelength division multiplexing devices, which are suitable for phased array systems.

CN117741870BActive Publication Date: 2026-11-24THE 44TH INST OF CHINA ELECTRONICS TECH GROUP CORP
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202311758069.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-12-20
Publication Date
2026-11-24
Estimated Expiration
2043-12-20

AI Technical Summary

Technical Problem

Existing technologies make it difficult to manufacture large-scale, high-precision absolute optical path wavelength division multiplexing (OSWDM) devices, resulting in optical path differences between batches and making them incompatible on the same system, which limits their application in large factories.

Method used

By preparing wavelength division multiplexing tubes of specific wavelengths, measuring the optical path value using an optical frequency domain reflectometer and cutting the fiber length, and combining this with a fiber optic fusion splicer for precise splicing, the optical path consistency of each wavelength channel is ensured, and phase consistency testing is performed. Finally, the device is packaged into an absolute optical path wavelength division multiplexing device.

Benefits of technology

It achieves high precision and reproducibility of absolute optical path wavelength division multiplexing devices, expands the wavelength manufacturing range, improves production efficiency, and is suitable for phased array systems.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117741870B_ABST
    Figure CN117741870B_ABST
Patent Text Reader

Abstract

This invention belongs to the field of microwave optoelectronic devices, specifically relating to a method for large-scale fabrication of absolute optical path wavelength division multiplexing (WDM) devices. The method includes: preparing a wavelength division multiplexing tube of a specific wavelength; measuring the optical path value of the WDM using an optical frequency domain reflectometer, and cutting the fiber length of the WDM using a fiber cleaver according to the optical path value; measuring the pigtail length of an external optical device using an optical frequency domain reflectometer, and cutting the pigtail length; repairing the fiber of the WDM using a fiber fusion splicer; precisely splicing the fiber of the WDM to the external optical device; performing phase consistency testing on the wavelength and signal modulation frequency of each channel of the fabricated WDM; coiling and fixing the fiber with adhesive, and sealing it to obtain the fabricated absolute optical path wavelength division multiplexing device. The absolute optical path wavelength division multiplexing device of this invention has a constant optical path, fixed length, strong reproducibility, and expands the wavelength fabrication range of wavelength division multiplexing devices.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of microwave optoelectronic devices, specifically relating to a method for large-scale fabrication of absolute optical path wavelength division multiplexing devices. Background Technology

[0002] Microwave optical transmission, as one of the core transmission methods for signals such as local oscillators and clocks in modern radar and telemetry systems, has requirements for large-scale, high-precision phase delays between subarrays and absolute transmission distances. Applying wavelength division multiplexing (WDM) technology can save on circuit materials. For the circuit design of microwave optical transmission with these requirements, this paper presents a technique for large-scale fabrication of absolute optical path wavelength division multiplexing devices to achieve phase consistency in microwave signal fiber optic transmission. This is of great significance for improving production efficiency, quality control, and product performance parameters.

[0003] In recent years, the existing technology "A Method and System for High-Precision Fabrication of Dense Wavelength Division Multiplexing Devices" introduced for the first time a method for high-precision OFDR testing of fiber length, demonstrating a new approach to fabricating relatively long dense wavelength division multiplexing devices. While this has greatly improved fabrication accuracy, it also presents several challenges. For example, it cannot achieve absolute optical path length; different batches of products exhibit optical path differences, preventing their application in the same system. This leads to incompatibility between multiple batches of the same type of phased array radar measurement and control systems, causing significant difficulties in system calibration and control. Furthermore, its scale is limited, failing to meet the production requirements of large factories and the demand for large-scale distributed phased array radars. Summary of the Invention

[0004] To address the shortcomings of existing technologies, this invention proposes a method for large-scale fabrication of absolute optical path wavelength division multiplexing (OSWDM) devices, the method comprising:

[0005] S1: Prepare wavelength division multiplexing tubes for specific wavelengths;

[0006] S2: Measure the optical path length of the wavelength division multiplexing tube using an optical frequency domain reflectometer, and cut the fiber length of the wavelength division multiplexing tube using a fiber optic cleaver based on the optical path length.

[0007] S3: Measure the length of the pigtail of the external optical device using an optical frequency domain reflectometer, and cut the pigtail to the desired length;

[0008] S4: Use a fiber optic fusion splicer to repair the optical fibers of the wavelength division multiplexing tube.

[0009] S5: Perform precision fusion splicing between the optical fiber of the wavelength division multiplexing tube and the external optical device.

[0010] Preferably, the wavelengths of the wavelength division multiplexing tubes of the specific wavelengths include 1545.32nm, 1551.72nm, 1548.51nm and 1310nm.

[0011] Preferably, step S2 specifically includes:

[0012] The optical path length of each wavelength division multiplexing tube was measured using an optical frequency domain reflectometer to obtain the optical path length value of each wavelength division multiplexing tube channel;

[0013] Set the optical path reference value, and calculate the cutting size of each wavelength division multiplexer tube based on the optical path value and the optical path reference value;

[0014] The optical fiber of the wavelength division multiplexing tube is cut using an optical fiber cleaver according to the cutting size.

[0015] Preferably, the process of splicing and repairing the optical fiber of the wavelength division multiplexing (WDM) tube includes: connecting the COM end of the WDM tube corresponding to the 1548.51nm wavelength optical path to the reflector end of the WDM tube corresponding to the 1551.72nm wavelength optical path; connecting the COM end of the WDM tube corresponding to the 1551.72nm wavelength optical path to the reflector end of the WDM tube corresponding to the 1545.32nm wavelength optical path; connecting the COM end of the WDM tube corresponding to the 1545.32nm wavelength optical path to the reflector end of the WDM tube corresponding to the 1310nm wavelength optical path; and using the combining fiber end of the WDM tube corresponding to the 1310nm wavelength optical path as the total port of the absolute optical path wavelength division multiplexing device.

[0016] Preferably, the process of precisely splicing the optical fiber of the wavelength division multiplexing tube to the external optical device includes: the transmission end of all wavelength division multiplexing tubes is connected to the optical device of the corresponding wavelength, and the reflection end of the wavelength division multiplexing tube corresponding to the 1548.51nm wavelength optical path is connected to the CH28 detector.

[0017] Preferably, the following step is included after step S5:

[0018] S6: Perform phase consistency tests on the wavelength and signal modulation frequency of each channel of the fabricated wavelength division multiplexing device;

[0019] S7: The optical fiber is coiled and fixed with adhesive, and then sealed to obtain the fabricated absolute optical path wavelength division multiplexing device.

[0020] The beneficial effects of this invention are as follows: The absolute optical path wavelength division multiplexing (WDM) device manufactured by this invention has a fixed optical path length and high reproducibility. It solves the problem of batch-to-batch variations in multiple fabrications. This invention expands the wavelength fabrication range of WDM devices, supplementing the fabrication of specific wavelength channels with vector network analyzer measurement technology. Furthermore, the fabrication accuracy of this invention is high, reaching up to three decimal places. It is not limited to dense WDM applications but extends to all bands of communication optical wavelengths; because the optical path is fixed, the fabrication process can be solidified, significantly improving product production efficiency, and it can also be applied to phased array systems. Attached Figure Description

[0021] Figure 1 This is a schematic diagram of the fiber cut length of the wavelength division multiplexing tube in this invention;

[0022] Figure 2 This is a schematic diagram of fiber optic splicing repair in the wavelength division multiplexing tube of the present invention;

[0023] Figure 3 This is a block diagram illustrating the principle of the absolute optical path wavelength division multiplexing optoelectronic device in this invention. Detailed Implementation

[0024] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.

[0025] This invention proposes a method for large-scale fabrication of absolute optical path wavelength division multiplexing (OSWDM) devices, the method comprising the following:

[0026] S1: Prepare wavelength division multiplexing tubes for specific wavelengths.

[0027] Prepare wavelength division multiplexing (WDM) tubes with specific wavelengths, including CH40 (1545.32nm), CH32 (1551.72nm), CH36 (1548.51nm), and 1310nm. Using these four specific wavelength WDM tubes, fabricate a hybrid CWDM / DWDM, laser emission, and photoelectric detection optoelectronic device—an absolute optical path wavelength division multiplexing (ABSWDM) device—with five wavelengths: CH40 (1545.32nm), CH32 (1551.72nm), CH36 (1548.51nm), CH28 (1554.94nm), and 1310nm.

[0028] Table 1. Parameters of Absolute Optical Path Wavelength Division Multiplexing Devices

[0029]

[0030] S2: Measure the optical path length of the wavelength division multiplexing tube using an optical frequency domain reflectometer, and cut the fiber length of the wavelength division multiplexing tube using a fiber optic cleaver based on the optical path length.

[0031] The optical path length of each wavelength division multiplexing (WDM) tube was measured using an optical frequency domain reflectometer to obtain the optical path length value of each WDM tube channel. Specifically, taking into account the characteristics of the linear sweep frequency light source of the optical frequency domain reflectometer and the parallel transmission between different wavelengths of the dense wavelength division multiplexing (DWDM) device, the optical path length of each wavelength transmission channel of the DWDM device was measured to obtain the optical path length value of each wavelength channel of the DWDM device.

[0032] Set the optical path reference value, and calculate the cutting dimensions of each wavelength division multiplexer tube based on the optical path value and the optical path reference value.

[0033] The optical fiber of the wavelength division multiplexing tube is cut using an optical fiber cleaver according to the cutting size.

[0034] Preferably, the length of the optical fiber cut into the wavelength division multiplexing tube is as follows: Figure 1 As shown.

[0035] S3: Measure the length of the pigtail of the external optical device using an optical frequency domain reflectometer, and cut the pigtail length.

[0036] Preferably, the cut lengths of the pigtails can be as follows:

[0037] The total length of the CH40 detector's fiber optic pigtail is 550.000mm. The white protective sleeve is removed 270.000mm from the end of the pigtail.

[0038] The total length of the CH32 detector's fiber optic pigtail is 550.000mm. The white protective sleeve is removed 260.000mm from the end of the pigtail sleeve.

[0039] The total length of the CH36 detector's fiber optic pigtail is 600.000 mm. Remove the white protective sleeve 315.000 mm from the end of the pigtail.

[0040] The total length of the CH28 detector's fiber optic pigtail is 610.000 mm. The white protective sleeve is removed 345.000 mm from the end of the pigtail sleeve.

[0041] The total length of the 1310nm laser pigtail is 500.000mm. Remove the white protective sleeve 250.000mm from the end of the pigtail.

[0042] The total length of the FC / APC jumper cable at the COM port is 240.000mm. Remove the white protective sleeve 175.000mm from the COM port.

[0043] Preferably, the length error is controlled within ±0.100mm. The fixed loss during the fiber optic dicing process is 9.000mm.

[0044] S4: Use a fiber optic fusion splicer to repair the optical fibers of the wavelength division multiplexing tube.

[0045] like Figure 2 As shown, the reflector of each wavelength division multiplexer (WDM) is sequentially connected to the WDM corresponding to the next wavelength optical path. Specifically, the COM terminal of the WDM corresponding to the 1548.51nm wavelength optical path is connected to the reflector of the WDM corresponding to the 1551.72nm wavelength optical path; the COM terminal of the WDM corresponding to the 1551.72nm wavelength optical path is connected to the reflector of the WDM corresponding to the 1545.32nm wavelength optical path; and the COM terminal of the WDM corresponding to the 1545.32nm wavelength optical path is connected to the reflector of the WDM corresponding to the 1310nm wavelength optical path. Since the final reflection only has one wavelength, one less CH28 WDM can be used.

[0046] The combining fiber end of the wavelength division multiplexing tube corresponding to the 1310nm wavelength optical path is used as the total port of the absolute optical path wavelength division multiplexing device.

[0047] S5: Perform precision fusion splicing between the optical fiber of the wavelength division multiplexing tube and the external optical device.

[0048] The external optical devices include CH40 detector, CH32 detector, CH36 detector, CH28 detector, and a 1310nm laser. The transmission ends of all wavelength division multiplexers (WDMs) are connected to the corresponding wavelength optical devices. Specifically, the transmission end of the WDM corresponding to the 1548.51nm wavelength optical path is connected to the CH36 detector, the transmission end of the WDM corresponding to the 1551.72nm wavelength optical path is connected to the CH32 detector, and the transmission end of the WDM corresponding to the 1545.32nm wavelength optical path is connected to the CH40 detector; and the reflection end of the WDM corresponding to the 1548.51nm wavelength optical path is connected to the CH28 detector.

[0049] Preferably, the accuracy of each optical fiber is controlled within ±0.500mm during fusion splicing.

[0050] S6: Perform phase consistency tests on the wavelength and signal modulation frequency of each channel of the fabricated wavelength division multiplexing device.

[0051] Phase consistency tests were performed on the wavelength and signal modulation frequency of each channel of the fabricated wavelength division multiplexing device. The 1310nm laser was tested using a vector network analyzer to ensure its accuracy was within ±2.000mm.

[0052] The process of testing a 1310nm laser using a vector network analyzer includes:

[0053] Connect the test connection lines. Connect the optical receiver to port 2 of the vector network analyzer via a connector, and connect the transmitter to port 1 to form a measurement loop.

[0054] During testing, the vector network analysis setup includes two test curves, with measurement mode S21 selected. One curve measures logarithmic amplitude (primarily for fiber optic delay), and the other measures phase. First, time-domain transformation is selected on the logarithmic amplitude curve to define the large measurement range. Then, maximum value tracking is chosen in the cursor function to find the delay value corresponding to the maximum amplitude. Next, the cursor is set on the phase test curve, and the phase value at each frequency point is found (measuring the phase delay value of one channel at a time).

[0055] When measuring the maximum amplitude delay, a large test range should be determined first, and then the maximum value should be gradually approached. The cursor center should be at the peak point; if the cursor is at the edge of the screen, the maximum value may not have been found.

[0056] S7: The optical fiber is coiled and fixed with adhesive, and then sealed to obtain the fabricated absolute optical path wavelength division multiplexing device.

[0057] The spliced ​​optical fiber is coiled inside the structural component with a minimum radius of curvature and then fixed with adhesive. The fiber routing and exit positions within the cavity are as follows: Figure 3 As shown; then the device is sealed to complete the fabrication of the absolute optical path wavelength division multiplexing optoelectronic device product.

[0058] The above-described embodiments further illustrate the purpose, technical solution, and advantages of the present invention. It should be understood that the above-described embodiments are merely preferred embodiments of the present invention and are not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc., made to the present invention within the spirit and principles of the present invention should be included within the protection scope of the present invention.

Claims

1. A method for large-scale fabrication of absolute optical path wavelength division multiplexing (OSWDM) devices, characterized in that, include: S1: Prepare wavelength division multiplexing tubes for specific wavelengths; S2: Measure the optical path length of the wavelength division multiplexing (WDM) tube using an optical frequency domain reflectometer, and cut the fiber length of the WDM tube using a fiber optic cleaver based on the optical path length; the specific process includes: The optical path length of each wavelength division multiplexing tube was measured using an optical frequency domain reflectometer to obtain the optical path length value of each wavelength division multiplexing tube channel; Set the optical path reference value, and calculate the cutting size of each wavelength division multiplexer tube based on the optical path value and the optical path reference value; The optical fiber of the wavelength division multiplexing tube is cut using an optical fiber cleaver according to the cutting size; S3: Measure the length of the pigtail of the external optical device using an optical frequency domain reflectometer, and cut the pigtail to the desired length; S4: Use a fiber optic fusion splicer to repair the optical fibers of the wavelength division multiplexing tube. S5: Perform precision fusion splicing between the optical fiber of the wavelength division multiplexing tube and the external optical device.

2. The method for large-scale fabrication of absolute optical path wavelength division multiplexing devices according to claim 1, characterized in that, The wavelengths of the wavelength division multiplexing tubes with specific wavelengths include 1545.32nm, 1551.72nm, 1548.51nm and 1310nm.

3. The method for large-scale fabrication of an absolute optical path wavelength division multiplexing device according to claim 1, characterized in that, The process of splicing and repairing the optical fibers of a wavelength division multiplexing (WDM) tube includes: connecting the COM terminal of the WDM tube corresponding to the 1548.51nm wavelength optical path to the reflector terminal of the WDM tube corresponding to the 1551.72nm wavelength optical path; connecting the COM terminal of the WDM tube corresponding to the 1551.72nm wavelength optical path to the reflector terminal of the WDM tube corresponding to the 1545.32nm wavelength optical path; connecting the COM terminal of the WDM tube corresponding to the 1545.32nm wavelength optical path to the reflector terminal of the WDM tube corresponding to the 1310nm wavelength optical path; and using the combining fiber end of the WDM tube corresponding to the 1310nm wavelength optical path as the main port of the absolute optical path wavelength division multiplexing device.

4. The method for large-scale fabrication of an absolute optical path wavelength division multiplexing device according to claim 1, characterized in that, The process of precisely splicing the optical fiber of the wavelength division multiplexing tube to the external optical device includes: the transmission end of all wavelength division multiplexing tubes is connected to the optical device of the corresponding wavelength, and the reflection end of the wavelength division multiplexing tube corresponding to the 1548.51nm wavelength optical path is connected to the CH28 detector.

5. A method for large-scale fabrication of an absolute optical path wavelength division multiplexing device according to claim 1, characterized in that, The following steps are included after step S5: S6: Perform phase consistency tests on the wavelength and signal modulation frequency of each channel of the fabricated wavelength division multiplexing device; S7: The optical fiber is coiled and fixed with adhesive, and then sealed to obtain the fabricated absolute optical path wavelength division multiplexing device.

Citation Information

Patent Citations

  • Optical fiber shape sensor based on torsional stress release principle and manufacturing method

    CN116182734A

  • Group velocity dispersion measuring device and group velocity dispersion measuring method

    US6856723B1