A HEMT contact hole structure and a method for manufacturing the same
By forming a contact hole structure with an upper hole with inclined sidewalls and a lower hole with a concave bottom in the barrier layer of the GaN HEMT device, the problems of high contact resistance and difficulty in removing etching impurities are solved, resulting in lower on-resistance and higher filling process reliability.
Patent Information
- Application Number
- CN202211116949.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-09-14
- Publication Date
- 2026-11-20
- Estimated Expiration
- 2042-09-14
AI Technical Summary
In the prior art, the contact hole structure of GaN HEMT devices has the problems of high contact resistance and difficulty in removing impurities during the etching process, which affects the device performance.
An upper hole with inclined sidewalls is formed in the barrier layer, and a lower hole with a concave bottom surface is formed by adjusting the etching parameters to form a contact hole. This increases the effective opening during the etching process, facilitates the removal of impurities, and improves the reliability of subsequent filling processes.
It reduces contact resistance, improves the reliability of the filling process, enhances the uniformity of the electric field on the bottom surface of the contact hole, and reduces the on-resistance of the device. It is suitable for both gold-free and metal-filled processes.
Smart Images

Figure CN117747420B_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of semiconductor integrated circuit manufacturing and relates to a HEMT contact hole structure and its preparation method. Background Technology
[0002] Gallium nitride (GaN), a typical representative of third-generation wide-bandgap semiconductor materials, is widely used in high-temperature, high-frequency, and high-power electronic systems due to its advantages such as high bandgap width, high critical electric field strength, and high electron saturation drift velocity. For AlGaN / (Al)GaN high electron mobility transistors (HEMTs), the performance of the ohmic contacts is crucial; low ohmic contact resistance can reduce the on-resistance of power devices and the knee voltage of RF devices, thereby increasing the current output capability of the devices.
[0003] The ohmic contacts of conventional GaN HEMT devices are typically fabricated using reactive ion etching (RIE) or inductively coupled plasma etching (ICP), and their structures are as follows: Figure 1 As shown, the structure includes a semiconductor structure 01, a substrate 011, a buffer layer 012, a channel layer 013, a barrier layer 014, and a contact hole 0141. This method involves etching a contact hole with a rectangular cross-section into the barrier layer of the GaN HEMT structure, and then filling the contact hole with a source / drain ohmic contact metal layer.
[0004] In GaN HEMT devices, the source and drain contacts are ohmic contacts, fabricated on the same side of the device. To reduce ohmic contact resistance, a portion of the barrier layer on the device surface needs to be etched away to form contact holes, which are typically rectangular in cross-section. These rectangular profile contact holes have relatively high ohmic contact resistance, requiring an Au-free process for mass production. The resulting ohmic contact resistance is higher than that of gold-based processes, hindering the reduction of on-resistance. During barrier layer etching, precise control of the etching rate and thickness is crucial; therefore, byproducts from the barrier layer and plasma reaction must be removed promptly. However, removing etching byproducts is difficult with rectangular profile contact holes, easily leaving residues that affect the etching rate and impurities in the barrier layer, impacting device performance.
[0005] Therefore, there is an urgent need to find a method for preparing HEMT contact holes that can reduce the contact resistance of HEMT contact holes and facilitate the removal of impurities generated during the etching process. Summary of the Invention
[0006] In view of the shortcomings of the prior art described above, the purpose of this invention is to provide a HEMT contact hole structure and its preparation method, so as to solve the problems of high contact resistance and difficulty in removing impurities generated during the etching process in the prior art.
[0007] To achieve the above and other related objectives, the present invention provides a method for preparing a HEMT contact hole, comprising the following steps:
[0008] A semiconductor structure is provided, the semiconductor structure comprising a substrate, a buffer layer, a channel layer, a barrier layer and a dielectric layer stacked sequentially upwards;
[0009] A patterned photoresist layer is formed on the upper surface of the dielectric layer, and a plurality of openings are formed through the dielectric layer and spaced apart based on the patterned photoresist layer;
[0010] Based on the opening, the barrier layer is etched to obtain an upper hole in the barrier layer, and the bottom surface of the upper hole is spaced apart from the upper surface of the channel layer by a first preset distance.
[0011] The barrier layer at the bottom of the upper hole is etched to form a lower hole with a concave bottom surface. The upper hole and the lower hole form a contact hole. The concave tip of the lower hole is spaced a second preset distance from the upper surface of the channel layer. The bottom surface of the contact hole is at a preset angle to the horizontal plane where the upper surface of the channel layer is located.
[0012] Optionally, the substrate may be made of at least one of sapphire, SiC, Si, GaN and diamond.
[0013] Optionally, after forming the opening and before forming the upper hole, the step of removing the photoresist layer is further included.
[0014] Optionally, the method for forming the upper aperture includes reactive ion etching and inductively coupled plasma etching; the method for forming the lower aperture includes reactive ion etching and inductively coupled plasma etching.
[0015] Optionally, the angle between the sidewall of the upper hole and the horizontal plane containing the bottom surface of the upper hole is greater than 90°.
[0016] Optionally, the lateral etching rate of the process forming the upper hole is less than the lateral etching rate of the process etching the bottom of the lower hole.
[0017] Optionally, the first preset distance is greater than the second preset distance.
[0018] Optionally, the range of the second preset distance is 1nm to 2nm.
[0019] Optionally, the preset angle ranges from 5° to 15°.
[0020] The present invention also provides a HEMT contact hole structure, comprising:
[0021] Substrate;
[0022] A buffer layer is located on the upper surface of the substrate;
[0023] A channel layer is located on the upper surface of the buffer layer;
[0024] A barrier layer is located on the upper surface of the channel layer;
[0025] Multiple contact holes are spaced apart and embedded in the barrier layer. Each contact hole includes an upper hole portion and a lower hole portion. The bottom surface of the lower hole portion is concave. The tip of the concave corner of the lower hole portion is spaced apart from the upper surface of the channel layer by a second preset distance. The bottom surface of the contact hole and the horizontal plane containing the upper surface of the channel layer form a preset angle.
[0026] As described above, the HEMT contact hole structure and its fabrication method of the present invention, in the process of forming the contact hole, first forms the upper hole portion with inclined sidewalls, and then adjusts the etching parameters to etch the bottom surface of the upper hole portion to form the lower hole portion with a concave bottom angle, so as to obtain the contact hole composed of the upper hole portion and the lower hole portion. Because the sidewalls of the upper hole portion are inclined, the effective opening during the etching process is enlarged, which facilitates the timely removal of impurities during the etching process and avoids the impact of residual etching impurities on the performance of the device. At the same time, because the sidewalls of the contact hole have an inclination angle, the process window of the subsequent filling process is relatively larger, which facilitates the filling of the contact hole, avoids the deposition of voids, improves the reliability of the filling process, and the contact hole is suitable for both gold-free filling processes and metal filling processes, making the process more flexible. Furthermore, due to the inclined sidewalls of the contact holes, the concave tip of the bottom surface of the contact holes protrudes towards the channel layer, and the included angle between the bottom surfaces of the contact holes is greater than the included angle between the sidewalls and the bottom surface of the contact holes. This reduces the electric field strength at the edge of the bottom surface of the contact holes while enhancing the electric field strength at the tip of the bottom surface of the contact holes, making the electric field strength at the bottom surface of the contact holes relatively uniform. It also causes the carrier concentration below the contact holes to gradually increase from the tip of the bottom surface of the contact holes to the edge of the bottom surface of the contact holes, increasing the number of carriers participating in tunneling to the source and drain of the device. The thickness of the barrier layer below the bottom surface of the contact holes gradually increases from the tip of the bottom surface of the contact holes to the edge of the contact holes, thereby making the number of carriers tunneling to the source and drain of the device at the bottom of the contact holes more uniform, reducing the overall on-resistance of the device, and having high industrial application value. Attached Figure Description
[0027] Figure 1 The diagram shows a cross-sectional view of the HEMT contact hole.
[0028] Figure 2 The diagram shows the process flow of the HEMT contact hole preparation method of the present invention.
[0029] Figure 3 The diagram shows a cross-sectional view of the semiconductor structure used in the method for preparing the HEMT contact hole of the present invention.
[0030] Figure 4 The diagram shows a cross-sectional structure after the opening is formed, illustrating the method for preparing the HEMT contact hole according to the present invention.
[0031] Figure 5 The diagram shows a cross-sectional structure after the upper hole portion is formed, which is a method for preparing HEMT contact holes according to the present invention.
[0032] Figure 6 The diagram shows a cross-sectional structure of the HEMT contact hole after the contact hole is formed, according to the method for preparing the HEMT contact hole of the present invention.
[0033] Figure 7 The diagram shown is a cross-sectional view of the HEMT contact hole preparation method of the present invention after removing the dielectric layer.
[0034] Component designation explanation
[0035] 01 Semiconductor Structure
[0036] 011 Substrate
[0037] 012 Buffer Layer
[0038] 013 Channel layer
[0039] 014 Barrier Layer
[0040] 0141 Contact Hole
[0041] 1. Semiconductor Structure
[0042] 11 Substrate
[0043] 12 Buffer Layer
[0044] 13. Channel layer
[0045] 14. Barrier Layer
[0046] 141 Upper hole
[0047] 142 Lower hole
[0048] 143 Contact Hole
[0049] 15. Dielectric layer
[0050] 151 Opening
[0051] 16 photoresist layers Detailed Implementation
[0052] The following specific examples illustrate the implementation of the present invention. Those skilled in the art can easily understand other advantages and effects of the present invention from the content disclosed in this specification. The present invention can also be implemented or applied through other different specific embodiments, and various details in this specification can also be modified or changed based on different viewpoints and applications without departing from the spirit of the present invention.
[0053] Please see Figures 2 to 7 It should be noted that the illustrations provided in this embodiment are only schematic representations of the basic concept of the present invention. Therefore, the drawings only show the components related to the present invention and are not drawn according to the actual number, shape and size of the components in the actual implementation. In the actual implementation, the form, quantity and proportion of each component can be arbitrarily changed, and the layout of the components may also be more complex.
[0054] Example 1
[0055] This embodiment provides a method for preparing HEMT contact holes, such as... Figure 2 The diagram shown is a process flow chart of the method for preparing the HEMT contact hole, including the following steps:
[0056] S1: A semiconductor structure is provided, the semiconductor structure comprising a substrate, a buffer layer, a channel layer, a barrier layer and a dielectric layer stacked sequentially upwards;
[0057] S2: A patterned photoresist layer is formed on the upper surface of the dielectric layer, and a plurality of openings are formed through the dielectric layer and spaced apart based on the patterned photoresist layer;
[0058] S3: Based on the first opening, the barrier layer is etched to obtain an upper hole in the barrier layer, and the bottom surface of the upper hole is spaced apart from the upper surface of the channel layer by a first preset distance;
[0059] S4: Etch the barrier layer at the bottom of the upper hole to form a lower hole with a concave bottom surface. The upper hole and the lower hole form a contact hole. The concave tip of the lower hole is spaced a second preset distance from the upper surface of the channel layer. The bottom surface of the contact hole is at a preset angle to the horizontal plane where the upper surface of the channel layer is located.
[0060] Please see Figures 3 to 4 Perform steps S1 and S2: Provide a semiconductor structure 1, the semiconductor structure 1 including a substrate 11, a buffer layer 12, a channel layer 13, a barrier layer 14 and a dielectric layer 15 stacked upwards; form a patterned photoresist layer 16 on the upper surface of the dielectric layer 15, and form a plurality of openings 151 that penetrate the dielectric layer 15 and are spaced apart based on the patterned photoresist layer 16.
[0061] As an example, such as Figure 3 The diagram shown is a cross-sectional view of the semiconductor structure 1. The substrate 11 is made of at least one of sapphire, SiC, Si, GaN, and diamond, or other suitable materials. In this embodiment, SiC is used as the substrate 11.
[0062] Specifically, the buffer layer 12 includes at least one of AlN, AlGaN, GaN, and InN layers, or other suitable semiconductor layer materials. In this embodiment, an AlN / AlGaN composite layer is used as the buffer layer 12.
[0063] Specifically, when the buffer layer 12 is a single-layer structure, the thickness of the buffer layer 12 can be set according to the actual situation while ensuring device performance, and is not limited here.
[0064] Specifically, when the buffer layer 12 is a composite layer, the thickness of each film layer in the buffer layer 12 can be set according to the actual situation while ensuring device performance, and is not limited here.
[0065] Specifically, the channel layer 13 is made of GaN, AlGaN, InGaN, or other suitable semiconductor materials. In this embodiment, a pure GaN thin film is used as the channel layer 13.
[0066] Specifically, the material of the barrier layer 14 includes In x Al y Ga 1-x-y N, Al x Ga 1-x N、In x Al 1-x N or other suitable materials. In this embodiment, In is used. x Al y Ga 1-x-y N serves as the barrier layer 14.
[0067] Specifically, the dielectric layer 15 is made of silicon nitride or other suitable dielectric materials. In this embodiment, silicon nitride is used as the dielectric layer 15.
[0068] Specifically, while ensuring device performance, the thickness of the dielectric layer 15 can be set according to the actual situation, and is not limited here.
[0069] Specifically, the method for forming the photoresist layer 16 includes coating or other suitable methods.
[0070] Specifically, since the method for patterning the photoresist layer 16 is a conventional method, it will not be described in detail here.
[0071] Specifically, such as Figure 4 The diagram shown is a cross-sectional view of the structure after the opening 151 is formed. The method for forming the opening 151 includes dry etching or other suitable methods. In this embodiment, the opening 151 is formed using inductively coupled plasma etching (a type of dry etching).
[0072] Specifically, while ensuring device performance, the size of the opening 151 can be selected according to the actual situation, and is not limited here.
[0073] Please see again Figures 5 to 7 Then, perform steps S3 and S4: etch the barrier layer 14 based on the opening 151 to obtain an upper hole 141 located in the barrier layer 14, the bottom surface of the upper hole 141 being spaced apart from the upper surface of the channel layer 13 by a first preset distance; etch the barrier layer 14 at the bottom of the upper hole 141 to form a lower hole 142 with a concave bottom surface, the upper hole 141 and the lower opening 142 forming a contact hole 143, the concave tip of the lower hole 142 being spaced apart from the upper surface of the channel layer 13 by a second preset distance, and the bottom surface of the contact hole 143 forming a preset angle with the horizontal plane where the upper surface of the channel layer 13 is located.
[0074] As an example, after forming the opening 151 and before forming the upper hole 141, the step of removing the photoresist layer 16 is also included.
[0075] Specifically, since the method for removing the photoresist layer 16 is a conventional method, it will not be described in detail here.
[0076] As an example, the method for forming the upper hole 141 includes reactive ion etching, inductively coupled plasma etching, or other suitable etching methods; the method for forming the lower hole 142 includes reactive ion etching, inductively coupled plasma etching, or other suitable etching methods.
[0077] Specifically, such as Figure 5 The diagram shown is a cross-sectional view of the upper hole 141 after it has been formed. The opening size of the upper hole 141 can be selected according to the actual situation while ensuring the performance of the device. It is not limited here.
[0078] As an example, the angle between the sidewall of the upper hole 141 and the horizontal plane where the bottom surface of the upper hole 141 is located is greater than 90°, that is, the opening size of the upper hole 141 is larger than the size of the bottom surface of the upper hole 141, and the sidewall of the upper hole 141 is inclined.
[0079] Specifically, provided that the angle between the upper hole 141 and the horizontal plane where the bottom surface of the upper hole 141 is located is greater than 90° and the device performance is guaranteed, the angle between the side wall of the upper hole 141 and the horizontal plane where the bottom surface of the upper hole 141 is located can be selected according to the actual situation, and is not limited here.
[0080] As an example, the lateral etching rate of the process forming the upper hole is less than the lateral etching rate of the process etching the bottom of the lower hole.
[0081] Specifically, due to the anisotropy of dry etching, the lateral and longitudinal etching rates during the etching process are controlled by adjusting the etching parameters of the etching equipment. This, in turn, controls the morphology of the upper hole 141 and the lower hole 142, i.e., the morphology of the contact hole 143. For example, when using inductively coupled plasma etching, it is necessary to make the sidewalls of the etched holes steep. This can be achieved by reducing the proportion of suppressant gas in the etching gas, decreasing the gas pressure, or increasing the bias power of the equipment. However, adjusting the equipment process parameters to control the lateral etching rate is accompanied by changes in the etching selectivity. Therefore, it is necessary to reasonably adjust the etching process parameters to ensure the size and morphology of the holes.
[0082] As an example, the first preset distance is greater than the second preset distance.
[0083] Specifically, provided that the value of the first preset distance is greater than the value of the second preset distance, the value of the first preset distance can be selected according to the actual situation.
[0084] Specifically, the first preset distance is greater than the second preset distance, so that there is enough space in the barrier layer 14 at the bottom of the upper hole 141 to form the lower hole 142 with a concave bottom surface.
[0085] As an example, the second preset distance is in the range of 1nm to 2nm, so that the charge carriers located at the bottom of the contact hole 143 can tunnel to the source and drain.
[0086] Specifically, such as Figure 6 As shown, this is a cross-sectional structural diagram after the contact hole 143 is formed. Since the bottom surface of the lower hole 142 is concave, that is, the bottom surface has a sharp point, which in turn causes the bottom of the source and drain of the contact hole 142 to have a sharp point. By utilizing the sharp point effect, a strong electric field is formed at the sharp point at the bottom of the contact hole 143, so that the charge carriers in the channel layer 13 can tunnel to the source and drain of the device.
[0087] Specifically, since the angle between the sidewall and the bottom surface of the contact hole 143 is greater than 90°, compared with a rectangular cross-section contact hole, the electric field intensity at the tip of the angle between the bottom surface and the sidewall of the contact hole 143 can be reduced. At the same time, a tip is formed at the bottom of the contact hole 143, resulting in an enhanced electric field intensity at the tip of the bottom of the contact hole 143. This makes the electric field distribution at the source and drain of the device more uniform, which facilitates the tunneling of charge carriers located below the contact hole 143 to the source and drain of the device, thereby reducing the overall on-resistance of the device.
[0088] Specifically, the included angle between the bottom surfaces of the contact holes 143 is greater than the included angle between the sidewall of the contact holes 143 and the bottom surface of the contact holes 143, and the included angle between the bottom surface of the contact holes 143 and the sidewall of the contact holes 143 is greater than 95°.
[0089] Specifically, since the included angle between the bottom surfaces of the contact holes 143 is greater than the included angle between the sidewall of the contact holes 143 and the bottom surface of the contact holes 143, the carrier concentration in the channel layer 13 from the tip of the bottom surface of the contact holes 143 to the edge of the bottom surface of the contact holes 143 gradually increases. Compared with contact holes with horizontal bottom surfaces (where the carriers in the channel layer 13 are mostly concentrated at the tip of the bottom edge of the contact hole), more carriers participate in the tunneling process, thereby allowing more carriers to tunnel to the source and drain of the device, reducing the overall on-resistance of the device.
[0090] As an example, the range of the preset angle is 5° to 15°.
[0091] Specifically, since the carrier concentration below the contact hole 143 gradually increases from the tip of the bottom surface of the contact hole 143 to the edge of the bottom surface of the contact hole 143, and the preset angle ranges from 5° to 15°, the thickness of the barrier layer 14 below the contact hole 143 gradually increases from the tip of the bottom surface of the contact hole 143 to the edge of the bottom surface of the contact hole 143, and the increase is small. This makes it easier for the carriers below the bottom surface of the contact hole 143 to have similar tunneling probabilities, while preventing the distance between the bottom surface of the contact hole 143 and the upper surface of the channel layer 13 from being too large, which would affect the tunneling of carriers in the channel layer 13 into the source or drain of the device.
[0092] Specifically, since the angle between the sidewall of the contact hole 143 and the horizontal plane containing the upper surface of the channel layer 13 is greater than 90°, that is, the sidewall of the contact hole 143 is inclined, the effective opening of the etching becomes larger during the etching process of forming the contact hole 143. This facilitates the timely removal of by-products generated during the etching process, avoids the problem of incomplete removal of impurities generated during subsequent etching, which affects the device performance, and enhances the controllability and precision of etching.
[0093] Specifically, because the sidewall of the contact hole 143 is inclined and the angle between the sidewall of the contact hole 143 and the horizontal plane on the upper surface of the channel layer 13 is greater than 90°, a larger process window is provided, which facilitates the subsequent deposition of filling materials and avoids the phenomenon of deposition voids, making the subsequent filling process more reliable. At the same time, the contact hole 143 is suitable for both gold-free filling processes and metal filling processes, and has greater process flexibility.
[0094] Specifically, such as Figure 7 The diagram shown is a cross-sectional view of the structure after the dielectric layer 15 is removed. After forming the contact hole 143, the process also includes removing the dielectric layer 15 from the upper surface of the barrier layer 14.
[0095] Specifically, since the process of removing the dielectric layer 15 is a conventional process, it is not limited here.
[0096] The HEMT contact hole fabrication method of this embodiment first forms an upper hole portion 141 with inclined sidewalls. The angle between the sidewall of the upper hole portion 141 and the horizontal plane containing the upper surface of the channel layer 13 is greater than 90°. This increases the effective opening size during etching, facilitating the timely removal of etching byproducts and avoiding the problem of incomplete removal of etching impurities, which could affect device performance. At the same time, the inclined sidewalls of the contact hole 143 provide a larger process window, facilitating the deposition of subsequent filling materials and avoiding the formation of deposition voids. This results in higher reliability of the subsequent filling process. Furthermore, the contact hole 143 is suitable for both gold-free and metal-filled processes, offering greater process flexibility. Furthermore, since the angle between the sidewall and the bottom surface of the contact hole 143 is greater than 95°, the electric field strength at the tip of the angle between the sidewall and the bottom surface of the contact hole 143 is reduced. At the same time, a tip is formed on the bottom surface of the contact hole 143, which enhances the electric field at the tip of the bottom of the contact hole 143. This avoids the electric field at the bottom of the contact hole 143 from concentrating at the tip of the angle between the sidewall and the bottom surface of the contact hole 143, making the electric field at the bottom of the contact hole 143 relatively uniform.
[0097] Example 2
[0098] This embodiment provides a HEMT contact hole structure, such as Figure 7 The diagram shows a cross-sectional view of the HEMT contact hole structure, including a substrate 11, a buffer layer 12, a channel layer 13, a barrier layer 14, and contact holes 143. The buffer layer 12 is located on the upper surface of the substrate 11; the channel layer 13 is located on the upper surface of the buffer layer 12; and the barrier layer 14 is located on the upper surface of the channel layer 13. A plurality of spaced-apart contact holes 143 are embedded in the barrier layer 14. Each contact hole 143 includes an upper hole portion 141 and a lower hole portion 142. The bottom surface of the lower hole portion 142 is concave, and the tip of the concave angle of the lower hole portion 142 is spaced from the upper surface of the channel layer 13 by a second predetermined distance. The bottom surface of the contact hole 143 forms a predetermined angle with the horizontal plane containing the upper surface of the channel layer 13.
[0099] Specifically, while ensuring device performance, the thickness of the substrate 11 can be selected according to the actual situation, and is not limited here.
[0100] Specifically, the buffer layer 12 can be a multi-layer structure or a single-layer structure. When the buffer layer 12 is a multi-layer structure, the thickness of each film layer in the buffer layer 12 can be set according to the actual situation while ensuring device performance, and is not limited here. When the buffer layer 12 is a single-layer film structure, the thickness of the buffer layer 12 can be set according to the actual situation while ensuring device performance, and is not limited here.
[0101] Specifically, while ensuring device performance, the thickness of the channel layer 13 can be set according to the actual situation, and is not limited here.
[0102] Specifically, while ensuring device performance, the thickness of the barrier layer 14 can be set according to the actual situation, and is not limited here.
[0103] Specifically, the angle between the sidewall of the contact hole 143 and the horizontal plane containing the bottom surface of the upper hole 141 is greater than 90°, that is, the sidewall of the upper hole 141 is inclined, and the cross-sectional dimension of the bottom surface of the upper hole 141 is smaller than the size of the opening of the upper hole 141.
[0104] Specifically, the lower hole 142 is the bottom of the contact hole 143. The angle between the bottom surface of the contact hole 143 and the horizontal plane containing the upper surface of the channel layer 13 is in the range of 5° to 15°, that is, the angle between the sidewall of the contact hole 143 and the bottom surface of the contact hole 143 is greater than 95°. The distance between the bottom surface of the contact hole 143 and the upper surface of the channel layer 13 gradually increases along the direction from the tip of the bottom surface of the contact hole 143 to the edge of the bottom surface of the contact hole 143. The tip of the bottom surface of the contact hole 143 protrudes toward the channel layer 13.
[0105] Specifically, because the bottom surface of the contact hole 143 is concave, it has a pointed tip, which enhances the electric field strength near the tip. Furthermore, the angle between the sidewall and the bottom surface of the contact hole 143 is greater than 95°, and the angle between the bottom surface of the contact hole 143 and the horizontal plane containing the upper surface of the channel layer 13 is between 5° and 15°. However, due to the small size of the device, the angle between the sidewall and the bottom surface of the contact hole 143 is smaller than the angle between the bottom surfaces of the contact hole 143. This causes the electric field strength from the tip to the edge of the bottom surface of the contact hole 143 to gradually increase, and the carrier concentration in the channel layer 13 below the tip to the edge of the bottom surface of the contact hole 143 to gradually increase, allowing more carriers to participate in tunneling to the source and drain of the device. Furthermore, the thickness of the barrier layer 14 below the tip to the edge of the bottom surface of the contact hole 143 gradually increases, balancing the uniformity of carrier tunneling in the channel layer 13 below the contact hole 143 and reducing the overall on-resistance of the device.
[0106] Specifically, the tip of the bottom surface of the lower hole 142 is located in the middle region of the bottom surface of the lower hole 142, so as to improve the electric field distribution at the bottom of the contact hole 143 and make the electric field distribution near the bottom surface of the contact hole 143 more uniform. Here, more uniform refers to the contact hole without a concave bottom surface.
[0107] In this embodiment, the HEMT contact hole structure is constructed by setting the sidewall of the contact hole 143 as an inclined surface. The bottom surface of the contact hole 143 is set in a concave shape, so that the bottom surface of the contact hole 143 faces the tip of the channel layer 13. This increases the angle between the sidewall of the contact hole 143 and the bottom surface of the contact hole 143, reduces the electric field strength at the edge of the bottom surface of the contact hole 143, and enhances the electric field strength at the tip of the bottom surface of the contact hole 143. This makes the electric field strength at the bottom surface of the contact hole 143 relatively uniform. At the same time, the carrier concentration below the contact hole 143 gradually increases from the tip to the edge of the bottom surface of the contact hole 143, increasing the number of carriers participating in tunneling to the source and drain of the device. Since the thickness of the barrier layer 14 below the bottom surface of the contact hole 143 gradually increases from the tip to the edge of the bottom surface of the contact hole 143, the amount of carriers tunneling to the source and drain of the device from the bottom of the contact hole 143 is more uniform, reducing the overall on-resistance of the device.
[0108] In summary, the HEMT contact hole structure and its preparation method of the present invention first form an upper hole portion with a beveled surface, and then etch the bottom surface of the upper hole portion to form a lower hole portion with a concave bottom surface, thereby obtaining a contact hole with a concave bottom surface. Since the sidewall of the upper hole portion has an inclination angle, the effective opening of the etching is enlarged, which facilitates the timely removal of by-products during the etching process and avoids the problem of device performance being affected by the introduction of impurities during the etching process. At the same time, it makes the process window of the subsequent filling process larger, which facilitates the filling of the contact hole, avoids the phenomenon of deposited voids, improves the reliability of the process, and the contact hole is suitable for both gold-free filling processes and metal filling processes, with higher process flexibility. Furthermore, since the angle between the sidewall and bottom surface of the contact hole is greater than 95°, and the angle between the bottom surfaces of the contact hole is greater than the angle between the sidewall and bottom surface, the electric field strength at the edge of the bottom surface of the contact hole is reduced while the electric field strength at the tip of the bottom surface is enhanced. This makes the electric field strength at the bottom surface of the contact hole relatively uniform, and the carrier concentration below the contact hole gradually increases from the tip to the edge of the bottom surface, increasing the number of carriers participating in tunneling to the source and drain of the device. Because the thickness of the barrier layer below the bottom surface of the contact hole gradually increases from the tip to the edge of the bottom surface, the number of carriers tunneling to the source and drain of the device from the bottom of the contact hole becomes more uniform, reducing the overall on-resistance of the device. Therefore, this invention effectively overcomes the various shortcomings of the prior art and has high industrial applicability.
[0109] The above embodiments are merely illustrative of the principles and effects of the present invention and are not intended to limit the invention. Any person skilled in the art can modify or alter the above embodiments without departing from the spirit and scope of the present invention. Therefore, all equivalent modifications or alterations made by those skilled in the art without departing from the spirit and technical concept disclosed in the present invention should still be covered by the claims of the present invention.
Claims
1. A method for preparing a HEMT contact hole, characterized in that, Includes the following steps: A semiconductor structure is provided, the semiconductor structure comprising a substrate, a buffer layer, a channel layer, a barrier layer and a dielectric layer stacked sequentially upwards; A patterned photoresist layer is formed on the upper surface of the dielectric layer, and a plurality of openings are formed through the dielectric layer and spaced apart based on the patterned photoresist layer; Based on the opening, the barrier layer is etched to obtain an upper hole in the barrier layer. The bottom surface of the upper hole is spaced apart from the upper surface of the channel layer by a first preset distance. The angle between the sidewall of the upper hole and the horizontal plane where the bottom surface of the upper hole is located is greater than 90°. The barrier layer at the bottom of the upper hole is etched to form a lower hole with a concave bottom surface. The upper hole and the lower hole form a contact hole. The concave tip of the lower hole is spaced apart from the upper surface of the channel layer by a second preset distance. The bottom surface of the contact hole and the horizontal plane containing the upper surface of the channel layer form a preset angle. The preset angle ranges from 5° to 15°. The second preset distance ranges from 1 nm to 2 nm.
2. The method for preparing HEMT contact holes according to claim 1, characterized in that: The substrate is made of at least one of sapphire, SiC, Si, GaN and diamond.
3. The method for preparing HEMT contact holes according to claim 1, characterized in that: After forming the opening, but before forming the upper hole, the step of removing the photoresist layer is also included.
4. The method for preparing HEMT contact holes according to claim 1, characterized in that: The method for forming the upper hole includes reactive ion etching and inductively coupled plasma etching; the method for forming the lower hole includes reactive ion etching and inductively coupled plasma etching.
5. The method for preparing a HEMT contact hole according to claim 1, characterized in that: The lateral etching rate of the process forming the upper hole is less than the lateral etching rate of the process etching the bottom of the lower hole.
6. The method for preparing HEMT contact holes according to claim 1, characterized in that: The first preset distance is greater than the second preset distance.
7. A HEMT contact hole structure, characterized in that, include: Substrate; A buffer layer is located on the upper surface of the substrate; A channel layer is located on the upper surface of the buffer layer; A barrier layer is located on the upper surface of the channel layer; Multiple spaced contact holes are embedded in the barrier layer. Each contact hole includes an upper hole portion and a lower hole portion. The bottom surface of the lower hole portion is concave. The tip of the concave corner of the lower hole portion is spaced apart from the upper surface of the channel layer by a second preset distance. The bottom surface of the contact hole and the horizontal plane containing the upper surface of the channel layer form a preset angle. The angle between the sidewall of the upper hole portion and the horizontal plane containing the bottom surface of the upper hole portion is greater than 90°. The preset angle ranges from 5° to 15°. The second preset distance ranges from 1 nm to 2 nm.
Citation Information
Patent Citations
Transistor device and preparation method thereof
CN111106169A
Semiconductor device and method for fabricating the same
US20050087763A1