A method for repairing a pipe root weld
By using a quick-assembly and disassembly angle pendulum mechanism in the construction of long-distance pipelines, and by utilizing the angle pendulum method and current switching technology, the concave defect in the weld was solved, the welding quality was improved and the construction cost was reduced.
Patent Information
- Application Number
- CN202410099229.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-01-24
- Publication Date
- 2026-11-24
- Estimated Expiration
- 2044-01-24
AI Technical Summary
In the construction of long-distance pipelines, the use of root pass welding and parametric repair welding can easily produce concave defects, resulting in unqualified welds and increased construction costs.
A quick-release angular pendulum mechanism is adopted. When the tungsten electrode swings to the edge of the burn-through area, a larger pulse current is used. The arc force is used to push the molten iron towards the back and side of the weld. By switching between base current and peak current, concave defects are avoided.
It effectively solved the problems of concave weld seams and incomplete penetration, improved welding quality, and reduced construction costs.
Smart Images

Figure CN117754095B_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of welding technology, and in particular relates to a repair welding method for pipe root welding. Background Technology
[0002] Currently, in the construction of long-distance pipelines, due to terrain limitations in mountainous and paddy field areas, the U-shaped bevel, zero-gap assembly, and pulsed tungsten inert gas welding (TIG) without oscillation for the root pass are often used. However, due to thinner blunt edges in some areas during beveling and misalignment caused by the elliptical shape of the pipe during assembly, burn-through defects can occur in some places. If the root pass welding process and parameters are used for repair welding, the results are often poor, easily resulting in concavity and making the entire weld unqualified. This necessitates cutting and re-welding the final joint, incurring significant construction costs.
[0003] At the burn-through area, due to surface tension, the edge thickness is thicker than the normal blunt edge. Regardless of whether a straight pull (without oscillation) or a flat swing method is used, it is difficult to exceed the edge of the burn-through area due to the limitations of the tungsten electrode size and the bevel edge. Furthermore, the arc force cannot push the molten iron in the molten pool to the side, causing the edge area to melt and flow towards the part of the weld without molten iron, resulting in the problem of the bottom of the weld forming being concave. Summary of the Invention
[0004] The main technical problem solved by this invention is that the current methods of using root pass welding and parameter repair welding are prone to causing concavity, resulting in unqualified welds.
[0005] To solve the above-mentioned technical problems, the present invention adopts the following technical solution:
[0006] A method for repairing pipe root welds includes the following steps:
[0007] S1): Clean the burned area;
[0008] S2): Add a welded corner pendulum kit;
[0009] S3): Arc initiation welding;
[0010] S4): Welding complete.
[0011] Furthermore, in step 1, the cleaning process requires grinding both ends of the burned-through area into a wedge shape.
[0012] Furthermore, the angular pendulum assembly that is welded in step 2 is a detachable connection.
[0013] Furthermore, step 3 specifically includes the following steps:
[0014] S3-1): Low-current arc initiation: Current range is 30-50A;
[0015] S3-2): Gradual current rise: Linear gradual current rise, duration 0.5-2S;
[0016] S3-3): Wire feeding: Wire feeding speed: 1.5-3m / min;
[0017] S3-4): Head travel: Travel speed: 50-150mm / min
[0018] S3-5): Welding: Use a welding torch to weld the burned-through area. The specific welding parameters are as follows:
[0019] Peak current: 160-250A;
[0020] Base current: 20-60% of peak current;
[0021] Base time: equal to oscillation time;
[0022] Peak time: equal to the dwell time on both sides;
[0023] Swing speed: 0.5-1.5 m / min;
[0024] Swing amplitude: 1-4mm;
[0025] Dwell time on both sides: 0.2-0.5 seconds.
[0026] Furthermore, during welding in steps S3-5, the oscillation angle needs to be adjusted according to the width of the burn-through area. Specifically, a trial oscillation is performed first, with fine adjustments made to the oscillation amplitude as the tungsten electrode oscillates to both sides of the burn-through area. Then, the welding speed is calculated based on the oscillation angle, and the welding speed is controlled to decrease inversely as the oscillation angle increases, and increase inversely as the oscillation angle decreases. The specific speed is calculated using the following formula:
[0027] V = (A1 + a) / (A + a) * v1;
[0028] Where V is the welding speed, A1 is the set amplitude, A is the amplitude after fine adjustment, the coefficient is a, and v1 is the set welding speed.
[0029] Furthermore, after welding is completed in step S4, the process proceeds to current decay, wire stop, retraction, arc extinguishing, and delayed gas shut-off.
[0030] Furthermore, the gas used in the gas cut-off procedure is argon.
[0031] Furthermore, the angular pendulum kit in step 2 includes a machine head mounted on the pipe via a quick-release mechanism and an angular pendulum mechanism mounted on the machine head.
[0032] Furthermore, the angular pendulum mechanism includes an angular pendulum motor, an angular pendulum reducer connected to the angular pendulum motor, and a quick-release component connected to the angular pendulum reducer. A welding torch and an angle adjustment component for adjusting the angle of the welding torch are fixedly connected to the quick-release component.
[0033] The beneficial effects of this invention are:
[0034] The present invention utilizes a quick-assembly and disassembly angular pendulum mechanism. When the tungsten electrode swings to the edge of the burn-through area, a larger pulse current is used. The arc force pushes the molten iron towards the back and sides of the weld, preventing weld concavity. During the swing, a base current is used to cool the molten pool. When swinging to the other side, the current is converted to a peak current. Because of the angular pendulum mechanism, the arc force can push the molten iron towards the rear and sides of the weld, effectively solving the defects of concavity and incomplete penetration. Furthermore, the angular pendulum mechanism allows for quick and convenient assembly and disassembly of the angular pendulum assembly. Attached Figure Description
[0035] To more clearly illustrate the technical solutions in the embodiments of the present invention or the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.
[0036] Figure 1 This is a schematic diagram of the grinding wedge shape (the cross-section line represents the root weld bead);
[0037] Figure 2 This is a flowchart;
[0038] Figure 3 This is a schematic diagram of the welding process;
[0039] Figure 4 This is a schematic diagram of an angular pendulum mechanism;
[0040] 1. Pipe to be welded; 2. Angle swing mechanism; 21. Welding torch; 22. Angle swing motor; 23. Angle swing reducer; 24. Angle adjustment component; 25. Quick release component; 3. Machine head; 4. Quick release structure. Detailed Implementation
[0041] The preferred embodiments of the present invention will now be described in detail with reference to the accompanying drawings, so that the advantages and features of the present invention can be more easily understood by those skilled in the art, thereby providing a clearer and more explicit definition of the scope of protection of the present invention. Specific Implementation Example 1:
[0043] like Figures 1 to 4 As shown, a method for repairing pipe root welds includes the following steps:
[0044] S1): Clean the burned area; specifically, cleaning requires grinding both ends of the burned area into a wedge shape.
[0045] S2): Installing a swivel welding kit; the swivel welding kit in step 2 includes a machine head 3 mounted on the pipe 1 via a quick-release mechanism 4 and a swivel mechanism 2 mounted on the machine head 3. Specifically, the swivel mechanism 2 includes a swivel motor 22, a swivel reducer 23 connected to the swivel motor 22, and a quick-release component 25 connected to the swivel reducer 23. A welding torch 21 and an angle adjusting component 24 for adjusting the angle of the welding torch 21 are fixedly connected to the quick-release component 25. The swivel welding kit in this invention uses the automatic walking vehicle invented by our company (application number: CN202110807198.4).
[0046] S3): Arc initiation welding; specifically, step 3 is divided into the following steps:
[0047] S3-1): Low-current arc initiation: Current range is 30-50A;
[0048] S3-2): Gradual current rise: Linear gradual current rise, duration 0.5-2S;
[0049] S3-3): Wire feeding: Wire feeding speed: 1.5-3m / min;
[0050] S3-4): Head travel: Travel speed: 50-150mm / min
[0051] S3-5): Welding: Use a welding torch to weld the burned-through area. The specific welding parameters are as follows:
[0052] Peak current: 160-250A;
[0053] Base current: 20-60% of peak current;
[0054] Base time: equal to oscillation time;
[0055] Peak time: equal to the dwell time on both sides;
[0056] Swing speed: 0.5-1.5 m / min;
[0057] Swing amplitude: 1-4mm;
[0058] Dwell time on both sides: 0.2-0.5 seconds. Specifically, during welding in steps S3-5, the angle of the oscillation needs to be adjusted according to the width of the burn-through area. Specifically, a trial oscillation is performed first, with fine-tuning of the amplitude while oscillating. The welding is complete when the tungsten electrode oscillates to both sides of the burn-through area. Then, based on the oscillation angle, the welding speed is calculated, and the welding speed is controlled to decrease inversely as the oscillation angle increases, and increase inversely as the oscillation angle decreases. The specific speed is calculated using the following formula:
[0059] V = (A1 + a) / (A + a) * v1;
[0060] Where V is the welding speed, A1 is the set amplitude, A is the fine-tuned amplitude, the coefficient is a, and v1 is the set welding speed.
[0061] S4): Welding complete. Specifically, after welding in step S4, the process proceeds to current decay, wire stop, retraction, arc extinguishing, and delayed gas shut-off. Specifically, the gas used in the gas shut-off procedure is argon.
[0062] The principle of this invention is to utilize a quick-assembly and disassembly angled pendulum mechanism. By employing an angled pendulum method, when the tungsten electrode swings to the edge of the burn-through area, a larger pulse current is used. The arc force pushes the molten iron towards the back and sides of the weld, preventing weld concavity. During the swing, a base current is used to cool the molten pool. When swinging to the other side, the current is converted to a peak current. Due to the angled pendulum mechanism, the arc force can push the molten iron towards the rear and sides of the weld, effectively solving the defects of concavity and incomplete penetration. Because the angled pendulum mechanism can be quickly assembled and disassembled, repair welding angled pendulum kits can be used conveniently without spending excessive time on disassembly and assembly.
[0063] The above description is merely an embodiment of the present invention and does not limit the patent scope of the present invention. Any equivalent structural transformations made based on the content of the present invention specification and drawings, or direct or indirect applications in other related technical fields, are similarly included within the patent protection scope of the present invention.
Claims
1. A method for repairing pipe root welds, characterized in that: Includes the following steps: S1): Clean the burned area; S2): Add a welded corner pendulum kit; S3): Arc initiation welding; Step S3 specifically includes the following steps: S3-1): Low-current arc initiation: current range is 30-50A; S3-2): Gradual current increase: Linear gradual current increase, duration 0.5-2s; S3-3): Wire feeding: Wire feeding speed: 1.5-3m / min; S3-4): Head travel: Travel speed: 50-150mm / min; S3-5): Welding: Use a welding torch to weld the burned-through area. The specific welding parameters are as follows: Peak current: 160-250A; Base current: 20-60% of peak current; Base time: equal to oscillation time; Peak time: equal to the dwell time on both sides; Swing speed: 0.5-1.5 m / min; Swing amplitude: 1-4mm; Dwell time on both sides: 0.2-0.5s; S4): Welding complete; During welding in step S3-5, the oscillation angle needs to be adjusted according to the width of the burn-through area. Specifically, a trial oscillation is performed first, with fine adjustments to the amplitude while oscillating. The oscillation is complete when the tungsten electrode reaches both sides of the burn-through area. Then, the welding speed is calculated based on the oscillation angle value, and the welding speed is controlled to decrease inversely as the oscillation angle increases, and increase inversely as the oscillation angle decreases. The welding speed is calculated using the following formula: V = ((A1+a) / (A+a))*v1; Where V is the welding speed, A1 is the set amplitude, A is the amplitude after fine adjustment, the coefficient is a, and v1 is the set welding speed.
2. The repair welding method for pipe root welding according to claim 1, characterized in that: In step S1, cleaning requires grinding both ends of the burned area into a wedge shape.
3. The repair welding method for pipe root welding according to claim 1, characterized in that: In step S2, the angle pendulum assembly that is welded is detachably connected to the pipe to be welded.
4. The repair welding method for pipe root welding according to claim 1, characterized in that: After welding is completed in step S4, the process proceeds to current decay, wire stop, retraction, arc extinguishing, and delayed gas shut-off.
5. The repair welding method for pipe root welding according to claim 4, characterized in that: The gas used in the delayed gas shut-off procedure is argon.
6. The repair welding method for pipe root welding according to claim 1, characterized in that: The angular pendulum kit in step S2 includes a machine head (3) mounted on the pipe (1) via a quick-release mechanism (4) and an angular pendulum mechanism (2) mounted on the machine head (3).
7. A repair welding method for pipe root welding according to claim 6, characterized in that: The angular pendulum mechanism (2) includes an angular pendulum motor (22), an angular pendulum reducer (23) connected to the angular pendulum motor (22), and a quick-release component (25) connected to the angular pendulum reducer (23). A welding torch (21) and an angle adjustment component (24) for adjusting the angle of the welding torch (21) are fixedly connected to the quick-release component (25).
Citation Information
Patent Citations
An automated walking trolley for pipe welding
CN113523674B
Soldering process of SCSiMn2H steel
CN105643052A
High-speed automatic argon arc root welding method for long-distance pipeline
CN116511656A