Method for repairing a microthreaded connection failure
By using microscopic magnification and high-speed milling to repair micro-threaded connections, the problem of failure of micro-threaded connections in electronic packaging components was solved, achieving high-precision, rapid, and low-cost repair.
Patent Information
- Application Number
- CN202311811735.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-27
- Publication Date
- 2026-11-20
- Estimated Expiration
- 2043-12-27
AI Technical Summary
Existing technologies are insufficient for efficiently repairing failures in micro-threaded connections of M1.0 and below, especially in electronic packaging components, where conventional methods suffer from poor positioning accuracy, low cutting speed, and are unsuitable for the use of coolant.
The location of the failed residual screw was located using microscopic magnification, the residual screw was removed by high-speed milling, and the screw was positioned by microscope. Appropriate tools and cutting parameters were selected, and the screw was cooled with alcohol instead of cutting fluid. The threaded hole was then remade.
It achieves high-precision and rapid repair of micro-threaded connections, suitable for electronic packaging components, with significantly lower cost and cycle time than scrap disposal, resulting in substantial economic benefits.
Smart Images

Figure CN117773241B_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of thread repair technology, specifically relating to a method for repairing failures in micro-threaded connections. Background Technology
[0002] Precision thin-walled housing components assembled using M1.0 and smaller micro-threaded connections are widely used in the electronic packaging industry. After packaging, these components require telecommunications testing, and frequent test failures necessitate repeated disassembly and rework. Due to the small thread diameter and fine threads of these screws, screw seizing or even breakage is unavoidable during assembly and disassembly. Failed screws need to be removed, and the threaded holes re-fabricated for repair; otherwise, the component faces scrapping, resulting in significant economic losses. Currently, the conventional method of removing failed screws by drilling with a fitter is only suitable for larger screws (M2 and above) due to poor positioning accuracy and low cutting speed. Electrical discharge machining (EDM) screw removal, requiring coolant, is unsuitable for electronically packaged components.
[0003] There are no reports yet of a method for repairing micro-threaded connections that uses microscopic magnification to locate the position of residual screws and then removes them by high-speed milling before remaking the threaded holes. Summary of the Invention
[0004] The purpose of this invention is to provide a method for repairing failures in micro-threaded connections of M1.0 and below. The method uses microscopic magnification to locate the position of the failed residual screw and high-speed milling to remove the failed residual screw. It has high positioning accuracy and fast cutting speed, and is suitable for micro screws. No coolant is required during the repair process, making it suitable for electronic packaging components.
[0005] This invention provides a method for repairing failures in micro-threaded connections, the method comprising the following steps:
[0006] Step 1: Preparation
[0007] Step 1.1: Use masking tape to protect all exposed gaps in the components.
[0008] Step 1.2: Reinforce the remaining screws with a high-strength, penetrating threadlocker.
[0009] Step 2, clamping and positioning
[0010] During clamping, use the outer shape for rough positioning, and after the pressure plate is tightened, use a microscope to align the center position of the remaining screws.
[0011] Step 3: Remove any remaining screws and re-drill the threaded pilot hole.
[0012] Step 3.1: Select the cutting tool
[0013] Use a cutting tool for stainless steel, with a tool diameter slightly smaller than the bottom hole of the threaded hole;
[0014] Step 3.2: Determine cutting parameters
[0015] Step 3.3, Milling Holes
[0016] Mill a hole at the location of the remaining screw to remove the remaining screw, and at the same time machine the screw bottom hole;
[0017] Step 3.4, Cooling
[0018] During the machining process, the cutting tool is cooled by brushing it with alcohol; cutting fluid is not used.
[0019] Step 4: Remake the threaded hole
[0020] The threaded hole is re-threaded by using a cutting tap at the threaded hole location;
[0021] Step 5: After repairing the threaded hole, re-encapsulate the component and tighten it with screws. The repair work is now complete.
[0022] Preferably, step 1.1 specifically involves, in order to prevent foreign objects such as chips from entering the encapsulated component during the repair process, paper tape is used to protect all exposed gaps of the component before repair, and the tape used is required to leave no residue after removal.
[0023] Preferably, step 1.2 specifically involves, in order to prevent residual screws from rotating and affecting the milling process, using a high-strength liquid penetrating thread-locking agent to reinforce the residual screws before processing.
[0024] Preferably, in step 3.1, when the bottom hole of the M1.0 thread is φ0.73, a φ0.7 end mill is selected.
[0025] Preferably, in step 3.2, the spindle speed is not less than 20,000 r / min, the feed rate is not more than 1,500 mm / min, and the depth of cut is not more than 0.03 mm.
[0026] Preferably, in step 3.3, the residual screw at M1.0 is milled. hole.
[0027] The beneficial effects of this invention are:
[0028] This invention provides a method for repairing failed micro-threaded connections. It employs microscopic magnification to locate the position of residual screws and then uses high-speed milling to remove them. This method offers high positioning accuracy and fast cutting speed, making it suitable for micro-screws. Furthermore, it eliminates the need for coolant during the repair process, making it applicable to electronic packaging components. Moreover, using this repair method, the cost of repairing a single thread on a housing component is approximately 200 yuan, with a repair cycle of 2 days. Compared to scrapping the entire housing component, which results in losses exceeding 2000 yuan and a repair cycle of over 10 days, the cost and cycle are only 1 / 10 and 1 / 5 of the cost and cycle of scrapping, respectively, demonstrating significant economic and social benefits. Attached Figure Description
[0029] Figure 1 Partial schematic diagram of a precision thin-walled housing assembly
[0030] Figure 2 Partial schematic diagram of a precision thin-walled housing part
[0031] Figure 3 Repair process for micro-threaded connections in precision thin-walled housing components Detailed Implementation
[0032] The technical solutions provided by the present invention will be described in detail below with reference to specific embodiments. It should be understood that the following specific embodiments are only used to illustrate the present invention and are not intended to limit the scope of the present invention.
[0033] A typical precision thin-walled housing assembly generally consists of a housing and a cover plate, connected by threaded fastenings. See [link / details]. Figure 1 After a threaded connection fails, the remaining screws must be removed, and the threaded hole (M1.0) on the housing must be re-drilled. See [link / reference]. Figure 2 .
[0034] The remaining screws were removed using high-speed milling on a high-speed machining center. Figure 3 This describes the process flow for repairing threaded holes.
[0035] This invention provides a method for repairing failures in micro-threaded connections, the method comprising the following steps:
[0036] Step 1: Preparation
[0037] Step 1.1: Use masking tape to protect all exposed gaps in the components.
[0038] To prevent foreign objects such as chips from entering the encapsulated components during the repair process, paper tape is used to protect all exposed gaps of the components before repair. The tape used must leave no residue after removal.
[0039] Step 1.2: Reinforce the remaining screws with a high-strength liquid penetrating threadlocker.
[0040] To prevent residual screws from rotating and affecting the milling process, a high-strength liquid penetrating threadlocker is used to reinforce the residual screws before machining.
[0041] Step 2, clamping and positioning
[0042] During clamping, use the outer shape for rough positioning, and after the pressure plate is tightened, use a microscope to align the center position of the remaining screws.
[0043] Step 3: Remove any remaining screws and re-drill the threaded pilot hole.
[0044] Step 3.1: Select the cutting tool
[0045] Use cutting tools for stainless steel, with the tool diameter slightly smaller than the bottom hole of the threaded hole. For example, if the bottom hole of an M1.0 thread is φ0.73, select a φ0.7 end mill.
[0046] Step 3.2: Determine cutting parameters
[0047] The spindle speed is not less than 20,000 r / min, the feed rate is not more than 1,500 mm / min, and the depth of cut is not more than 0.03 mm.
[0048] Step 3.3, Milling Holes
[0049] Mill a hole at the location of the remaining screw to remove it. Simultaneously, machine the screw pilot hole, such as at the location of the M1.0 remaining screw. hole.
[0050] Step 3.4, Cooling
[0051] During the machining process, the cutting tool is cooled by brushing it with alcohol; cutting fluid is not used.
[0052] Step 4: Remake the threaded hole
[0053] Use a cutting tap to re-thread the hole at the location of the threaded hole and re-thread it.
[0054] Step 5: After repairing the threaded hole, re-encapsulate the component and tighten it with screws. The repair work is now complete.
[0055] Example:
[0056] Taking the installation of an M1.0 screw housing assembly as an example, repair the M1.0 threaded hole.
[0057] To prevent foreign objects such as chips from entering the encapsulated components during the repair process, 3M paper tape was used to protect all exposed gaps.
[0058] Apply high-strength liquid Loctite Threadlocker 290 to the threads of the failed screw and allow it to cure at room temperature for at least 24 hours to prevent the screw from rotating during subsequent milling.
[0059] The housing assembly was machined using a Swiss Mikron HSM700 high-speed milling machine. It was roughly positioned on the worktable and clamped by the outer shape. A 20x microscope was mounted on the machine tool spindle to locate the position of the failed screw and ensure that the positional error was controlled within 0.05mm.
[0060] After alignment, use a φ0.7 tungsten carbide end mill to mill a hole at the location of the failed screw. Remove any remaining screws and re-drill the M1.0 threaded pilot hole. During the machining process, cool the tool with a brush dipped in alcohol. The machining parameters are as follows:
[0061] Spindle speed 25000 r / min, feed rate 1500 mm / min, depth of cut 0.02 mm.
[0062] After remaking the threaded bottom hole, use an M1.0 cutting tap to re-thread at the remade threaded bottom hole to further remove the original screw residue. At the same time, remake the M1.0 threaded hole.
[0063] After the threaded hole was repaired, the component was re-encapsulated and tightened with screws, and the repair work was completed.
[0064] The above description is only the best specific embodiment of the present invention, but the protection scope of the present invention is not limited thereto. Any changes or substitutions that can be easily conceived by those skilled in the art within the technical scope disclosed in the present invention should be included within the protection scope of the present invention.
[0065] The contents not described in detail in this specification are common knowledge to those skilled in the art.
Claims
1. A method for repairing failures in micro-threaded connections, characterized in that, The method includes the following steps: Step 1: Preparation Step 1.1: Use masking tape to protect all exposed gaps in the components. Step 1.2: Reinforce the remaining screws with a high-strength, penetrating threadlocker; Step 2, clamping and positioning During clamping, use the outer shape for rough positioning, and after the pressure plate is tightened, use a microscope to align the center position of the remaining screws. Step 3: Remove any remaining screws and re-drill the threaded pilot hole. Step 3.1: Select the cutting tool Use a cutting tool for stainless steel, with a tool diameter slightly smaller than the bottom hole of the threaded hole; Step 3.2: Determine cutting parameters Step 3.3, Milling Holes Mill a hole at the location of the remaining screw to remove the remaining screw, and at the same time machine the screw bottom hole; Step 3.4, Cooling During the machining process, the cutting tool is cooled by brushing it with alcohol; cutting fluid is not used. Step 4: Remake the threaded hole The threaded hole is re-threaded by using a cutting tap at the threaded hole location; Step 5: After repairing the threaded holes, re-encapsulate the component and tighten it with screws. The repair work is now complete. Step 1.1 specifically involves using paper tape to protect all exposed gaps in the component before repair to prevent foreign objects from entering the encapsulated component during the repair process. The tape used must leave no residue after removal. Step 1.2 specifically involves using a high-strength liquid penetrating threadlocker to reinforce the residual screws before milling to prevent them from rotating and affecting the milling process. In step 3.1, when the bottom hole of the M1.0 thread is φ0.73, a φ0.7 end mill is selected; In step 3.2, the spindle speed is not less than 20,000 r / min, the feed rate is not more than 1,500 mm / min, and the depth of cut is not more than 0.03 mm; In step 3.3, mill φ at the M1.0 residual screw location. hole.
Citation Information
Patent Citations
A quick milling unit for nuclear power station pressure vessel kills kingbolt
CN205032780U