A method for manufacturing a herringbone monolithic composite ceramic tube

CN117781064BActive Publication Date: 2026-08-28YANTAI KINGWAY SCI & TECH
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202311843157.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-12-29
Publication Date
2026-08-28
Estimated Expiration
2043-12-29

AI Technical Summary

Technical Problem

[0004]本发明的目的是提供一种人字形整体复合陶瓷管的制备方法,以解决上述T型管道冲刷非常强、不耐高温和不耐腐蚀的问题

Benefits of technology

[0023](1)本发明的分流采用人字形圆弧过渡,内衬陶瓷为整体烧制而成,消除了陶瓷与陶瓷之间的拼接间隙,保证了耐磨和耐腐性能,其外层金属管通过人工打磨或机械整形的方式使陶瓷与金属管之间紧密贴合,不需要胶水固定,可以应用于高温工况。

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117781064B_ABST
    Figure CN117781064B_ABST
Patent Text Reader

Abstract

The application discloses a preparation method of a herringbone integral composite ceramic pipe, which comprises the following steps: (1) adopting a grouting process to cast ceramic into a prefabricated mold, and then high-temperature sintering to form a herringbone integral ceramic lining; (2) respectively cutting two metal elbows along the axial direction of the inlet center, splicing together for welding to form a herringbone integral metal pipe, and then cutting the herringbone integral metal pipe along the axial direction into two halves; (3) placing the herringbone integral ceramic lining in the middle of the two herringbone integral metal pipes, and then splicing together for welding to obtain a herringbone integral composite ceramic pipe. The herringbone integral composite ceramic pipe has the advantages that compared with a traditional T-shaped right-angle three-way pipe, fluid resistance is smaller, service life is longer, the ceramic lining is integrally sintered, there is no splicing gap between ceramics, the ceramics are closely combined with the metal pipe, the ceramics are not separated, wear resistance is good, and the herringbone integral composite ceramic pipe can be used in high-temperature or strong-corrosion working conditions.
Need to check novelty before this filing date? Find Prior Art

Citation Information

Patent Citations

  • Silicon carbide ceramic continuous flow reactor / condenser and manufacturing method thereof

    CN109678515A

  • Wear-resistant pipe

    US4633913A