绿色发光杂化卤化锰材料及其制备方法和应用
By designing zero-dimensional hybrid manganese halide materials, the preparation and stability problems of existing scintillation materials have been solved, enabling efficient X-ray imaging applications with excellent radiative emission performance and low self-absorption.
CN117801018BActive Publication Date: 2026-07-17JINING UNIV
Patent Information
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- JINING UNIV
- Filing Date
- 2023-11-15
- Publication Date
- 2026-07-17
Smart Images

Figure CN117801018B_ABST
Abstract
本发明公开了一种绿色发光杂化卤化锰材料及其制备方法和应用,包括以下步骤:S1将含溴有机磷盐和溴化锰混合于丙酮溶液中,在60‑65℃下水浴加热搅拌至完全溶解,随后将混合溶液装入烧杯中;S2将烧杯在室温下静置,过滤,用丙酮洗涤,70‑80℃下干燥1‑2h后得到绿色发光杂化卤化锰材料;步骤S1中,含溴有机磷盐为(3‑溴丙基)三苯基溴化磷或(4‑溴丁基)三苯基溴化磷。本发明制备了两种具有优异发光性能的零维杂化锰基卤化物,其具有接近统一的PLQYs和可忽略的自吸收,具有非凡的辐射发光(RL)性能,产光量超过65000光子 / MeV,远远超过商用LuAG:Ce的25000光子 / MeV。