Low-carbon cobalt-containing die steel, steel bar and preparation method

By optimizing the chemical composition and smelting process, low-carbon cobalt-containing die steel is prepared, forming M6C carbides and intermetallic compounds. This solves the shortcomings of existing die steels in terms of high-temperature strength and toughness, and achieves high-performance extrusion dies with high-temperature strength, toughness and wear resistance, thus extending the die life.

CN117802407BActive Publication Date: 2026-11-24DAYE SPECIAL STEEL CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202311857327.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-12-29
Publication Date
2026-11-24
Estimated Expiration
2043-12-29

AI Technical Summary

Technical Problem

Existing die steels are insufficient in terms of high-temperature strength, toughness, and ductility, resulting in short and unstable extrusion die lifespans, which cannot meet the requirements of high-performance extrusion dies with complex structures, high surface quality, and long service life.

Method used

By optimizing the chemical composition design and smelting and forging processes, low-carbon cobalt-containing mold steel is prepared, including steps such as vacuum induction melting, electroslag remelting and crystallization, to form M6C carbides and (Fe, Co)7W6 intermetallic compounds, which inhibit grain growth and improve toughness and hardness.

Benefits of technology

It improves the high-temperature strength, toughness and wear resistance of mold steel, meets the requirements of high-performance extrusion dies, extends the die life and ensures quality stability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0004642573090000101
    Figure BDA0004642573090000101
  • Figure BDA0004642573090000111
    Figure BDA0004642573090000111
Patent Text Reader

Abstract

This invention relates to a mold material, its preparation method, and its application, specifically to a low-carbon cobalt-containing mold steel, steel bar, and its preparation method. It is mainly used in high-performance extrusion molds for automobiles, energy, and communications, belonging to the field of mold steel manufacturing technology. The low-carbon cobalt-containing mold steel of this invention, by mass percentage, comprises: C: 0.17-0.23%, Si: 0.15-0.35%, Mn: 0.40-0.60%, S: ≤0.020%, P: ≤0.030%, Cr: 9.00-10.00%, Mo: 1.80-2.20%, W: 5.00-6.00%, Co: 9.50-10.50%, V: ≤0.30%, with the balance being iron. The preparation method of this invention for the low-carbon cobalt-containing mold steel ensures a uniform distribution of chemical composition and high / low magnification microstructure, resulting in high purity. Under certain heat treatment conditions, the strength and hardness of the material are improved, leading to molds made from this steel exhibiting good crack resistance and hot wear resistance.
Need to check novelty before this filing date? Find Prior Art

Citation Information

Patent Citations

  • Low-temperature high-toughness high-temperature high-intensity high-hardenability hot mould steel and preparation technology thereof

    CN111500928A