Reactor, converter, and power conversion device
By employing a magnetic core structure combining composite materials and powder-molded bodies, the reactor achieves optimized inductance and heat dissipation without increasing its size, solving the problem of adjusting inductance and heat dissipation in existing reactors, reducing eddy current losses and improving heat dissipation performance.
Patent Information
- Application Number
- CN202280056088.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2021-08-27
- Filing Date
- 2022-08-08
- Publication Date
- 2026-11-20
- Estimated Expiration
- 2042-08-08
AI Technical Summary
Existing reactors tend to be large-scale when adjusting inductance and heat dissipation, and it is difficult to optimize heat dissipation performance and inductance adjustment at the same time.
The magnetic core structure employs a combination of composite materials and pressed powder molding bodies. By constructing the first core from a composite material molding body and the second core from a pressed powder molding body, and by setting gaps between the winding parts, the material combination of the magnetic core is optimized to adjust the inductance and heat dissipation.
This technology enables reactors to simultaneously optimize inductance and heat dissipation without scaling up, reducing eddy current losses and improving the heat dissipation performance of the magnetic core.
Smart Images

Figure CN117813665B_ABST
Abstract
Description
Technical Field
[0001] The present disclosure relates to a reactor, a converter, and a power conversion device. This application claims priority based on Japanese Application No. 2021-138708 filed on August 27, 2021, the entire contents of which are incorporated herein by reference. Background Art
[0002] The reactor disclosed in Patent Document 1 includes a coil, a magnetic core, a case, and a cooling pipe. The coil is formed by spirally winding a winding wire. The number of the coil is one, and the coil has a cylindrical shape. The magnetic core has an inner core portion and an outer core portion. The inner core portion is disposed inside the coil. The outer core portion covers both end surfaces of the inner core portion, both end surfaces of the coil, and the outer peripheral surface of the coil. The inner core portion and the outer core portion are made of different materials. Specifically, the inner core portion is formed of a pressed powder molded body, and the outer core portion is formed of a composite material molded body. The case accommodates an assembly of the coil and the magnetic core therein. The assembly can be accommodated in the case by disposing the coil and the inner core portion in the case, filling the case with a raw material of the composite material, and curing the raw material. A refrigerant flows through the inside of the cooling pipe. The cooling pipe is spirally wound along the circumferential direction of the case so as to be in contact with the outer peripheral surface of the case. Description of Related Art Patent Document
[0003] Patent Document 1: Japanese Laid-Open Patent Publication No. 2013-74062 Summary of the Invention Problems to be Solved by the Invention
[0004] A reactor according to the present disclosure is a reactor including a coil and a magnetic core, the coil having a winding portion, the number of the winding portion is one, an outer peripheral surface of the winding portion includes a portion that comes into contact with an installation target of the reactor, the magnetic core comprising: an E-shaped first core portion and a T-shaped second core portion that are combined along an axial direction of the winding portion, and a gap portion disposed between the first core portion and the second core portion, the first core portion is configured by an integrated composite material molded body to form a first end core portion facing a first end surface of the winding portion, a first intermediate core portion having a portion disposed inside the winding portion, and a first side magnetic core portion and a second side magnetic core portion disposed on an outer periphery of the winding portion so as to sandwich the first intermediate core portion therebetween, The second core is formed by an integral powder-pressed molding body, which is a second end core facing the second end face of the winding part, and a second intermediate core having a portion disposed inside the winding part. The length of the second intermediate core along the axial direction of the winding portion is shorter than the length of the first intermediate core along the axial direction of the winding portion. The gap portion is located inside the winding portion, between the first intermediate core portion and the second intermediate core portion. The length from the second end face to the gap is more than 0.2 times and less than 0.49 times the length of the winding portion. The total volume Va of the first core, the second core, and the gap is 50 cm³. 3 Above and 500cm 3 the following.
[0005] The converter disclosed herein incorporates the reactor disclosed herein.
[0006] The power conversion device disclosed herein includes the converter disclosed herein. Attached Figure Description
[0007] Figure 1 This is a schematic perspective view showing the overall structure of the reactor according to Embodiment 1. Figure 2 This is a schematic side view showing the overall structure of the reactor according to Embodiment 1. Figure 3 This is a schematic perspective view showing the state of the reactor in Embodiment 1 when disassembled. Figure 4 This is a schematic top view showing the overall structure of the reactor according to Embodiment 1. Figure 5 This is a schematic diagram illustrating the power system configuration of a hybrid electric vehicle. Figure 6 This is a circuit diagram showing an example of a power conversion device equipped with a converter. Detailed Implementation
[0008] The problem this disclosure aims to solve The aforementioned assembly, due to the different materials used for the inner and outer cores, facilitates inductance adjustment. However, because the coil and inner core are embedded in the outer core, heat dissipation is difficult to adjust. This is because the surface of the assembly is essentially made only of the material used for the outer core. Furthermore, the assembly exhibits poor heat dissipation because the outer core is made of a composite material with relatively low thermal conductivity. Therefore, the aforementioned reactor improves heat dissipation by housing the assembly within a casing with a cooling tube wound around it. However, this results in a larger reactor due to the cooling tube wound around the casing.
[0009] One objective of this disclosure is to provide a reactor that is easy to adjust inductance and heat dissipation without being bulky. Another objective of this disclosure is to provide a converter incorporating the aforementioned reactor. Furthermore, a further objective of this disclosure is to provide a power conversion device incorporating the aforementioned converter.
[0010] The effect of this disclosure The reactor disclosed herein is easy to adjust inductance and heat dissipation without being large in size.
[0011] The converter and power conversion device disclosed herein have excellent heat dissipation without being large in size.
[0012] Description of Implementation Methods of this Disclosure First, the embodiments of this disclosure will be described and explained in parallel.
[0013] (1) The reactor involved in one aspect of this disclosure is a reactor having a coil and a magnetic core. The coil has a winding portion. The number of the winding portion is 1. The outer peripheral surface of the winding portion includes a portion that contacts the object on which the reactor is installed. The magnetic core has: The E-shaped first core and the T-shaped second core, which are combined along the axial direction of the winding portion, and The gap between the first core and the second core is provided. The first core is formed by an integral composite material molding body comprising a first end core facing the first end face of the winding portion, a first intermediate core having a portion disposed inside the winding portion, and a first side magnetic core and a second side magnetic core disposed on the outer periphery of the winding portion in a manner that sandwiches the first intermediate core. The second core is formed by an integral powder-pressed molding body, comprising a second end core facing the second end face of the winding portion, and a second intermediate core having a portion disposed inside the winding portion. The length of the second intermediate core along the axial direction of the winding portion is shorter than the length of the first intermediate core along the axial direction of the winding portion. The gap portion is disposed inside the winding portion between the first intermediate core portion and the second intermediate core portion. The length from the second end face to the gap is more than 0.2 times and less than 0.49 times the length of the winding portion. The total volume Va of the first core, the second core, and the gap is 50 cm³. 3 Above and 500cm 3 the following.
[0014] The aforementioned reactor is easy to adjust inductance. In particular, the reactor is easy to adjust inductance because there is no large gap between the first core and the second core. This is because the core is not made of a single material, but is configured to include a first core made of a molded composite material and a second core made of a pressed powder molded material.
[0015] Compared to conventional reactors, the above-mentioned reactor offers easier adjustment of heat dissipation. Conventional reactors are formed by embedding a core with higher thermal conductivity within a core with lower thermal conductivity. In other words, the surface of the magnetic core in conventional reactors is made of a single material. In contrast, the above-mentioned reactor forms its magnetic core by combining a first core and a second core along the axial direction of the winding portion; therefore, the surface of the magnetic core is made of different materials.
[0016] The aforementioned reactor exhibits improved heat dissipation. This is because the winding portion of the reactor includes a part that contacts the mounting object, allowing for efficient heat dissipation from the coil via the mounting object. In particular, compared to conventional reactors, the aforementioned reactor demonstrates significantly improved heat dissipation. According to conventional reactors, as described above, the surface of the magnetic core is composed solely of a core portion with relatively low thermal conductivity. In contrast, according to the aforementioned reactor, the surface of the magnetic core can include a surface composed of a pressed powder molded body with relatively high thermal conductivity.
[0017] The aforementioned reactor is preferably applied to reactors cooled by cooling components with varying cooling performance. The second core, with higher thermal conductivity, is positioned on the side of the cooling component with lower cooling performance, while the first core, with lower thermal conductivity, is positioned on the side with higher cooling performance. This ensures that the first and second cores are cooled equally, reducing the maximum temperature of the magnetic core.
[0018] The aforementioned reactor is not easily scaled up. As mentioned above, the heat dissipation of the aforementioned reactor is easy to adjust and improve, therefore it does not require cooling pipes as is the case with conventional reactors.
[0019] In the above-mentioned reactor, there is only one winding portion. Therefore, compared with the case where multiple winding portions are arranged in parallel along a direction orthogonal to the axial direction of the winding portion, the installation area in the direction orthogonal to the axial direction of the winding portion can be reduced.
[0020] The aforementioned reactor is easy to manufacture. This is because the reactor can be obtained simply by assembling a pre-fabricated first core and a second core into a coil.
[0021] The aforementioned reactor achieves low losses. In this reactor, the length of the second intermediate core is shorter than the length of the first intermediate core, resulting in a lower proportion of high-loss powder-pressed molded bodies compared to powder-pressed molded bodies. Furthermore, in this reactor, the gap is disposed inside the winding section, and the length from the second end face to the gap is more than 0.2 times the length of the winding section, making it difficult for leakage flux to penetrate the winding section. Therefore, eddy current losses occurring in the winding section are easily reduced. Moreover, the length from the second end face to the gap is less than 0.49 times the length of the winding section, thereby increasing the proportion of low-loss powder-pressed molded bodies inside the winding section compared to powder-pressed molded bodies. Furthermore, the aforementioned reactor can reduce the maximum temperature of the magnetic core as described above.
[0022] The aforementioned reactor can suppress problems such as leakage flux affecting peripheral equipment. In the aforementioned reactor, the gap portion is disposed inside the winding portion, and the length from the second end face to the gap portion is more than 0.2 times the length of the winding portion, thereby easily suppressing the leakage of magnetic flux to the outside of the winding portion.
[0023] Compared to the E-shaped case, the T-shaped second core is easier to manufacture. Therefore, compared to the E-shaped case, the T-shaped second core has higher precision and is easier to manufacture. Consequently, compared to the E-shaped case, the T-shaped second core is less likely to produce unwanted gaps when combined with the first core.
[0024] In the aforementioned reactors, the total volume Va is 50 cm³. 3 Above and 500cm 3 The following are converters applicable to electric vehicles, hybrid vehicles, or fuel cell vehicles.
[0025] Generally speaking, the larger the reactor, the more easily it generates heat and the more difficult it is to dissipate it. However, as mentioned above, the reactor described above is easy to improve heat dissipation, therefore even though the total volume Va is 50 cm³, it still achieves good heat dissipation. 3 The above methods can also help suppress fever.
[0026] (2) Preferably, in the reactor described in (1) above, The volume of the second core accounts for more than 25% and less than 40% of the total volume Va.
[0027] If the above ratio is above 25%, it is easier to improve the heat dissipation of the reactor. If the above ratio is below 40%, it is easier to reduce the losses of the reactor.
[0028] (3) Preferably, in the reactor described in (1) or (2) above, The volume of the second intermediate core accounts for more than 15% and less than 49% of the total volume of the first intermediate core, the second intermediate core, and the gap.
[0029] If the above ratio is above 15%, it is easier to improve the heat dissipation of the reactor. If the above ratio is below 49%, it is easier to reduce the losses of the reactor.
[0030] (4) Preferably, in any one of the reactors described in (1) to (3) above, The ratio of the thickness of the gap portion to the total length of the first intermediate core portion, the second intermediate core portion, and the thickness of the gap portion is 0.001 or more and 0.1 or less.
[0031] If the ratio is above 0.001, it is easy to ensure the specified inductance. If the ratio is below 0.1, the leakage flux is low, which makes it easier to improve the reduction effect of eddy current losses.
[0032] (5) Preferably, in any one of the reactors described in (1) to (4) above, The thickness of the gap is 0.1 mm or more and 2 mm or less.
[0033] If the thickness is 0.1mm or more, it is easy to ensure the specified inductance. If the thickness is 2mm or less, the leakage flux is low, which makes it easier to improve the reduction of eddy current losses.
[0034] (6) Preferably, in any one of the reactors described in (1) to (5) above, It includes a molding resin portion that covers at least a portion of the magnetic core and forms the gap portion.
[0035] In the aforementioned reactor, the gap is made of molding resin, which facilitates maintaining the distance between the end faces of the first intermediate core and the second intermediate core. Furthermore, the reactor effectively protects the magnetic core covered by the molding resin from external environmental factors.
[0036] In the aforementioned reactor, the gap portion can easily be formed from a portion of the molding resin part. The reason is as follows: The gap portion formed from a portion of the molding resin part is formed as follows: A composition combining a coil and a magnetic core is prepared. The material constituting the molding resin part transitions from the outside of the composition to the end faces of the first intermediate core and the second intermediate core within the winding portion. Even if the total volume Va is 50 cm³... 3 In addition, by making the length from the second end face to the gap less than 0.49 times the length of the winding portion, the constituent materials of the molding resin portion can easily transition between the end faces.
[0037] (7) Preferably, in any one of the reactors described in (1) to (6) above, The reactor constitutes a converter for electric vehicles, hybrid vehicles, or fuel cell vehicles.
[0038] The aforementioned reactor is suitable for constituting the aforementioned converter.
[0039] (8) Preferably, in any one of the reactors described in (1) to (7) above, The pressed powder molded body is a molded body comprising raw material powder including soft magnetic powder. The content of the soft magnetic powder in the pressed powder molded body is 85% by volume or more and 99% by volume or less.
[0040] Compared with the molded articles of composite materials, the above-mentioned pressed powder molded articles are easier to improve magnetic properties.
[0041] (9) Preferably, in any one of the reactors described in (1) to (8) above, The molded body of the composite material is a molded body in which soft magnetic powder is dispersed in resin. The content of the soft magnetic powder in the molded body of the composite material is more than 20% by volume and less than 80% by volume.
[0042] Compared to powder-pressed moldings, the moldings of the above-mentioned composite materials are easier to form, even complex shapes, based on the ease of adjusting magnetic properties.
[0043] (10) The converter involved in one aspect of this disclosure, It has any one of the reactors described in (1) to (9) above.
[0044] The converter described above has the aforementioned reactor, thus achieving low loss without large size while maintaining excellent heat dissipation.
[0045] (11) The power conversion device involved in one aspect of this disclosure, A converter that has the above (10) features.
[0046] The aforementioned power conversion device has the aforementioned converter, thus achieving low loss without large size while maintaining excellent heat dissipation.
[0047] Detailed Description of the Embodiments of this Disclosure The embodiments of this disclosure will now be described in detail with reference to the accompanying drawings. The same reference numerals in the drawings denote the same names of objects.
[0048] Implementation Method 1 [Reactor] Combination Figures 1 to 4 The reactor 1 of Embodiment 1 will be described below. The reactor 1 includes a coil 2 and a magnetic core 3. The coil 2 has a winding portion 21. The number of winding portions 21 is one. One feature of the reactor 1 of this embodiment is that it satisfies the following requirements (a) to (f).
[0049] (a) such as Figure 2 As shown, the outer peripheral surface 25 of the winding portion 21 includes a portion that contacts the installation object 100 of the reactor 1. (b) such as Figure 1 As shown, the magnetic core 3 has an E-shaped first core 3f and a T-shaped second core 3s arranged along the axial direction of the winding portion 21, and a gap portion 3g disposed between the first core 3f and the second core 3s. (c) The first core 3f is composed of a molded body of composite material, and the second core 3s is composed of a pressed powder molded body. (d) The first intermediate core 31f of the first core 3f and the second intermediate core 31s of the second core 3s have specific lengths. (e) The gap 3g is located in a specific location. (f) The volume of the magnetic core 3 is a specific size.
[0050] For ease of explanation, Figure 4 Coil 2 is shown with a double-dotted line. In the following description, the first direction D1, the second direction D2, and the third direction D3 as defined below are sometimes used. The first direction D1 is the direction along the axial direction of the winding part 21. The second direction D2 is the direction along the parallel direction of the first intermediate core 31f, the first side core 321 and the second side core 322, which will be described later. The third direction D3 is a direction that is orthogonal to both the first direction D1 and the second direction D2.
[0051] [Coil] like Figure 3As shown, the coil 2 has a hollow winding portion 21. The winding portion 21 is constructed by winding a single, unjointed wire into a spiral shape. There is one winding portion 21. In the reactor 1 of this embodiment, the number of winding portions 21 is one, thereby shortening the length along the second direction D2 compared to the case where multiple winding portions are arranged side by side along a direction orthogonal to the axial direction of the winding portion.
[0052] The winding portion 21 is rectangular cylindrical in shape. Rectangle includes rectangle and square. In this embodiment, the end face of the winding portion 21 is rectangular frame-shaped. Because the winding portion 21 is rectangular cylindrical, it is easier to increase the contact area between the winding portion 21 and the object 100 compared to a circular cylindrical winding portion with the same cross-sectional area. Therefore, the reactor 1 can easily dissipate heat to the object 100 via the winding portion 21. Furthermore, it is easier to stably mount the winding portion 21 onto the object 100. An example of the object 100 is a cooling base or the inner bottom surface of a housing described later. The corners of the winding portion 21 are rounded. Unlike this embodiment, the winding portion 21 is cylindrical. A circle includes a perfect circle and an ellipse.
[0053] The winding can utilize publicly available winding methods. In this embodiment, the winding employs a wrapped flat-angle wire. The conductor of the wrapped flat-angle wire is made of copper flat-angle wire. The insulating coating of the wrapped flat-angle wire is made of enamel. The winding portion 21 is composed of an edge-winding coil formed by winding the wrapped flat-angle wire along its edge.
[0054] The first end 21a and the second end 21b of the winding portion 21 are respectively located at the first and second ends in the axial direction of the winding portion 21, and in this embodiment, they are pulled outwards from the winding portion 21. Although the first end 21a and the second end 21b are not shown in the figure, the insulating covering is removed and the wire is exposed. Figure 2 As shown, the exposed wires in this embodiment extend outwards from the molded resin portion 4, which will be described later. A terminal member is connected to the exposed wires. The terminal member is not shown in the diagram. An external device is connected to the coil 2 via this terminal member. The external device is not shown in the diagram. The external device is a power source, etc., that supplies power to the coil 2.
[0055] The outer peripheral surface 25 of the winding portion 21 has a portion that contacts the mounting object 100 of the reactor 1. Therefore, the reactor 1 can easily improve heat dissipation. The outer peripheral surface 25 has a portion that protrudes in the third direction D3 of the magnetic core 3. That is, the length of the winding portion 21 along the third direction D3 is longer than the length of the magnetic core 3 along the third direction D3. In this embodiment, the winding portion 21 is rectangular cylindrical in shape, so the outer peripheral surface 25 of the winding portion 21 has four flat surfaces. In this embodiment, one of the four flat surfaces is the portion that contacts the mounting object 100. Therefore, the winding portion 21 can ensure sufficient contact area relative to the mounting object 100. Therefore, the reactor 1 can easily further improve heat dissipation. In this embodiment, the aforementioned contact portion of the winding portion 21 is exposed from the molding resin portion 4 described later. Therefore, the heat of the coil 2 can be easily released via the mounting object 100.
[0056] [Magnetic core] like Figure 1 As shown, the magnetic core 3 is a composite obtained by combining a first core portion 3f and a second core portion 3s along a first direction D1. A gap portion 3g, described later, is provided between the first core portion 3f and the second core portion 3s. The magnetic core 3 can be constructed by combining the first core portion 3f and the second core portion 3s along the first direction D1, thus improving the workability of the reactor 1. The combination of the first core portion 3f and the second core portion 3s is of the ET type. This combination makes it easier to adjust the inductance and heat dissipation. The first core portion 3f is formed from a molded composite material, described later. The second core portion 3s is formed from a powder-pressed molded material, described later.
[0057] The total volume Va of the first core 3f, the second core 3s, and the gap 3g is 50 cm³. 3 Above and 500cm 3 The total volume V is 50 cm³. 3 Above and 500cm 3 The reactor 1 described below is suitable for converters in electric vehicles, hybrid vehicles, or fuel cell vehicles. Because the winding portion 21 has a part that contacts the object 100, and the second core 3s is composed of a powder-formed body, even though the total volume Va is 50 cm³, it is still possible to achieve this. 3 The above also facilitates the release of heat from the magnetic core 3. The total volume Va is 500 cm³. 3 Therefore, reactor 1 is less likely to be excessively large. The total volume Va mentioned above is further 60 cm³. 3 Above and 400cm 3 The following is particularly preferred: 70cm 3 Above and 300cm 3The volume of the gap 3g is the volume of the space surrounded by the end face of the first intermediate core 31f, the end face of the second intermediate core 31s, and the virtual outer peripheral surface. The so-called virtual outer peripheral surface is the outer peripheral surface obtained by extending the outer peripheral surface of the first intermediate core 31f along the first direction D1.
[0058] (First Core) like Figure 4 As shown, the planar shape of the first core 3f is E-shaped. The planar shape of the first core 3f refers to its shape as viewed from a third direction (D3). The same concept of planar shape applies to the second core 3s described later. The first core 3f has a first end core 33f, a first intermediate core 31f, a first side core 321, and a second side core 322. The first end core 33f faces the first end face of the winding portion 21. "Facing" means that the first end core 33f and the first end face of the winding portion 21 are directly opposite each other. The first intermediate core 31f has a portion disposed inside the winding portion 21. The first side core 321 and the second side core 322 are disposed facing each other, sandwiching the first intermediate core 31f. The first side core 321 and the second side core 322 are disposed on the outer periphery of the winding portion 21.
[0059] like Figure 3 As shown, the first core 3f is a molded body integrally formed by the first end core 33f, the first intermediate core 31f, the first side magnetic core 321, and the second side magnetic core 322. The first end core 33f connects the first intermediate core 31f, the first side magnetic core 321, and the second side magnetic core 322. The first side magnetic core 321 and the second side magnetic core 322 are disposed at both ends of the first end core 33f. The first intermediate core 31f is disposed at the center of the first end core 33f. The first core 3f is constructed from a molded body of composite material, as described later.
[0060] In this embodiment, the first end core portion 33f is a thin prismatic shape. The shape of the first intermediate core portion 31f corresponds to the inner circumferential shape of the winding portion 21. In this embodiment, the first intermediate core portion 31f is a quadrangular prism shape. The corners of the first intermediate core portion 31f are... Figure 3 The core portion is shown as square, but in reality, the corners are rounded along the inner circumferential surface of the corners of the winding portion 21. The first side core portion 321 and the second side core portion 322 have the same shape. In this embodiment, the first side core portion 321 and the second side core portion 322 are thin prismatic in shape.
[0061] The combined cross-sectional area of the first side magnetic core portion 321 and the second side magnetic core portion 322 is the same as the cross-sectional area of the first intermediate core portion 31f and the cross-sectional area of the second intermediate core portion 31s. Here, the cross-sectional area refers to the cross-sectional area of a cutting plane orthogonal to the first direction D1.
[0062] like Figure 4 As shown, the length L1f of the first intermediate core portion 31f along the first direction D1 is shorter than the length of the winding portion 21 along the first direction D1. The length of the winding portion 21 along the first direction D1 refers to the length along the first direction D1 between the first end face and the second end face of the winding portion 21. When there are gaps between the turns of the winding portion 21, the length of the winding portion 21 along the first direction D1 includes the length of the gaps between the turns. The length of the first intermediate core portion 31f along the second direction D2 is longer than the lengths of the first side core portion 321 and the second side core portion 322 along the second direction D2. Figure 1 As shown, the length of the first intermediate core 31f along the third direction D3 is the same as the length of the first side core 321 along the third direction D3 and the length of the second side core 322 along the third direction D3.
[0063] like Figure 4 As shown, the length L21f of the first side magnetic core portion 321 along the first direction D1 is the same as the length L22f of the second side magnetic core portion 322 along the first direction D1. Lengths L21f and L22f are longer than length L1f and longer than the length of the winding portion 21 along the first direction D1. The length of the first side magnetic core portion 321 along the second direction D2 is the same as the length of the second side magnetic core portion 322 along the second direction D2. Figure 1 As shown, the length of the first side magnetic core portion 321 along the third direction D3 is the same as the length of the second side magnetic core portion 322 along the third direction D3.
[0064] (Second Core) like Figure 4 As shown, the second core 3s has a T-shaped planar shape. The second core 3s has a second end core 33s and a second intermediate core 31s. The second end core 33s faces the second end face of the winding portion 21. "Facing" means that the second end core 33s and the second end face of the winding portion 21 are face-to-face. The second intermediate core 31s has a portion disposed inside the winding portion 21.
[0065] like Figure 3As shown, the second core 3s is a molded body integrally formed by the second end core 33s and the second intermediate core 31s. The second intermediate core 31s is located at the center of the second end core 33s. The second core 3s is composed of a powder pressing molded body described later. Compared with an E-shaped powder pressing molded body, a T-shaped powder pressing molded body is easier to manufacture. Therefore, compared with an E-shaped powder pressing molded body, a T-shaped powder pressing molded body has higher precision and is easier to manufacture. Therefore, compared with the E-shaped case, when the T-shaped second core 3s is combined with the first core 3f, no unwanted gaps are generated.
[0066] The second end core 33s has the same shape as the first end core 33f. That is, the second end core 33s is a thin prism. The second intermediate core 31s is a quadrangular prism. The corners of the second intermediate core 31s are rounded along the inner circumferential surface of the corner of the winding portion 21.
[0067] like Figure 4 As shown, the length L1s of the second intermediate core 31s along the first direction D1 is shorter than the length L1f. The combined length of lengths L1s and L1f is shorter than the individual lengths L21f and L22f. The length of the second intermediate core 31s along the second direction D2 is the same as the length of the first intermediate core 31f along the second direction D2. Figure 1 As shown, the length of the second intermediate core 31s along the third direction D3 is the same as the length of the first intermediate core 31f along the third direction D3.
[0068] like Figure 4 As shown, the length L3s of the second end core 33s along the first direction D1 is the same as the length L3f of the first end core 33f along the first direction D1. The length of the second end core 33s along the second direction D2 is the same as the length of the first end core 33f along the second direction D2. The length of the second end core 33s along the second direction D2 is longer than the length of the winding portion 21 along the second direction D2. Figure 1 As shown, the length of the second end core 33s along the third direction D3 is the same as the length of the first end core 33f along the third direction D3. Figure 2 As shown, the length of the second end core 33s along the third direction D3 is shorter than the length of the winding portion 21 along the third direction D3. Figure 1 As shown, the length of the second end core 33s along the third direction D3 is the same as the length of the second intermediate core 31s along the third direction D3.
[0069] An example of the volume ratio Vps, obtained by multiplying (volume Vs / total volume Va) by 100, is 25% or more and 40% or less. Volume Vs is the volume of the second core 3s. Total volume Va, as described above, is the sum of the volumes of the first core 3f, the second core 3s, and the gap 3g. If the volume ratio Vps is 25% or more, the heat dissipation of the reactor 1 is easily improved. If the volume ratio Vps is 40% or less, the losses of the reactor 1 are easily reduced. The volume ratio Vps is further preferably 27% or more and 38% or less, and particularly preferably 29% or more and 36% or less.
[0070] An example of the volume ratio Vpm, obtained by multiplying (volume Vms / total volume Vma) by 100, is 5% or more and 49% or less. Volume Vms is the volume of the second intermediate core 31s. Total volume Vma is the sum of the volumes of the first intermediate core 31f, the second intermediate core 31s, and the gap 3g. If the ratio Vpm is 15% or more, the heat dissipation of reactor 1 is easily improved. If the ratio Vpm is 49% or less, the losses of reactor 1 are easily reduced. The ratio Vpm is further preferably 20% or more and 40% or less, and particularly preferably 25% or more and 35% or less.
[0071] The first core portion 3f and the second core portion 3s are combined such that the end faces of the first side core portion 321 and the second side core portion 322 are in contact with the end face of the second end core portion 33s. A gap is provided between the end face of the first intermediate core portion 31f and the end face of the second intermediate core portion 31s. A gap portion 3g, described later, is provided between the end face of the first intermediate core portion 31f and the end face of the second intermediate core portion 31s.
[0072] The molded composite material constituting the first core 3f is a molded body in which soft magnetic powder is dispersed in resin. The molded composite material is obtained by filling a mold with a flowable raw material containing soft magnetic powder dispersed in uncured resin and then curing the resin. The content of soft magnetic powder in the resin of the molded composite material can be easily adjusted. Therefore, the magnetic properties of the molded composite material are easily adjusted. Moreover, even shapes more complex than those of powder-molded composite materials are easily formed. An example of the soft magnetic powder content in the molded composite material is 20% by volume or more and 80% by volume or less. An example of the resin content in the molded composite material is 20% by volume or more and 80% by volume or less. The above contents are values when the molded composite material is 100% by volume.
[0073] The 3S pressed powder molded body constituting the second core is a molded body obtained by compressing soft magnetic powder. Pressed powder molded bodies can increase the proportion of soft magnetic powder in the core compared to molded bodies made of composite materials. Therefore, pressed powder molded bodies easily improve magnetic properties. Magnetic properties are specific permeability and saturation flux density. Furthermore, pressed powder molded bodies have excellent heat dissipation because they contain less resin and more soft magnetic powder compared to molded bodies made of composite materials. An example of the magnetic powder content in the pressed powder molded body is 85% by volume or more and 99% by volume or less. This content is the value when the pressed powder molded body is 100% by volume.
[0074] The particles constituting soft magnetic powder can be soft magnetic metal particles, coated particles, or soft magnetic non-metal particles. Coated particles include soft magnetic metal particles and an insulating coating portion disposed around the outer periphery of the soft magnetic metal particles. The soft magnetic metal can be pure iron or an iron-based alloy. An example of an iron-based alloy is an Fe-Si alloy or an Fe-Ni alloy. An example of an insulating coating portion is phosphate. An example of a soft magnetic non-metal is ferrite.
[0075] An example of the resin used in the molded composite material is a thermosetting resin or a thermoplastic resin. An example of a thermosetting resin is an epoxy resin, phenolic resin, silicone resin, or polyurethane resin. An example of a thermoplastic resin is a polyphenylene sulfide resin, a polyamide resin, a liquid crystal polymer, a polyimide resin, or a fluoropolymer. An example of a polyamide resin is nylon 6, nylon 66, or nylon 9T.
[0076] Molded composite materials can contain ceramic fillers. Examples of ceramic fillers include alumina or silica gel. Ceramic fillers contribute to improved heat dissipation and electrical insulation.
[0077] The content of soft magnetic powder in the molded composite material and the content of soft magnetic powder in the pressed powder molded material are considered equivalent to the area ratio of soft magnetic powder in the cross-section of the molded material. The content of soft magnetic powder in the molded material is determined as follows: Images are obtained by observing the cross-section of the molded material using a SEM (scanning electron microscope). The cross-section of the molded material is arbitrary. The SEM magnification is 200x or higher and 500x or lower. At least 10 images are obtained. The total cross-sectional area is 0.1 cm². 2 One observation image can be obtained for a single cross-section, or multiple observation images can be obtained for a single cross-section. Image processing is performed on each observation image to extract the particle contours. Image processing may include, for example, binarization. The area ratio of soft magnetic particles in each observation image is calculated, and the average area ratio is determined. This average value is considered as the content of the soft magnetic powder.
[0078] As described above, the first core 3f is formed from a molded composite material, and the second core 3s is formed from a pressed powder molded body. By having the first core 3f formed from a molded composite material and the second core 3s formed from a pressed powder molded body, the inductance can be easily adjusted without relying on the long gap 3g, and the heat dissipation can also be easily adjusted. Furthermore, the reactor 1's heat dissipation is easily improved by having the second core 3s formed from a pressed powder molded body with relatively high thermal conductivity.
[0079] (Gap) The gap portion 3g is disposed inside the winding portion 21. The gap portion 3g is disposed between the end face of the first intermediate core portion 31f and the end face of the second intermediate core portion 31s. Because the gap portion 3g is disposed inside the winding portion 21, leakage flux is less likely to penetrate the winding portion 21 compared to when it is disposed outside the winding portion 21. Therefore, eddy current losses occurring in the winding portion 21 are easily reduced. The gap portion 3g is made of a component formed of a material with a specific permeability lower than that of the first core portion 3f and the second core portion 3s. In this embodiment, the gap portion 3g is composed of a portion of the molding resin portion 4, which will be described later.
[0080] An example of the ratio of the thickness of the gap portion 3g to the total length of the lengths L1f, L1s, and the thickness of the gap portion 3g is 0.001 or more and 0.1 or less. The thickness of the gap portion 3g refers to its length Lg along the first direction D1. If the ratio is 0.001 or more, it is easy to ensure the specified inductance. If the ratio is 0.1 or less, leakage flux is low, making it easier to improve the reduction effect of eddy current losses. The ratio is further preferably 0.01 or more and 0.08 or less, and particularly preferably 0.02 or more and 0.06 or less.
[0081] An example of the thickness of the gap portion 3g is 0.1mm or more and 2mm or less. If the thickness is 0.1mm or more, it is easy to ensure the specified inductance. If the thickness is 2mm or less, the leakage flux is low, which makes it easier to improve the reduction effect of eddy current loss. The thickness is further preferably 0.3mm or more and 1.75mm or less, and particularly preferably 0.5mm or more and 1.5mm or less.
[0082] An example of the length Le along the first direction D1 from the second end face of the winding portion 21 to the gap portion 3g is 0.2 times or more and 0.49 times or less the length of the winding portion 21 along the first direction D1. The length Le refers to the length along the first direction D1 between the position in the gap portion 3g closest to the second end face and the second end face.
[0083] Because the length Le is more than 0.2 times the length of the winding portion 21 along the first direction D1, leakage flux is less likely to penetrate the winding portion 21. Therefore, it is easier to reduce eddy current losses occurring in the winding portion 21. The closer the length Le is to 0.5 times the length of the winding portion 21 along the first direction D1, that is, the closer the position of the gap portion 3g is to the center of the winding portion 21 along the first direction D1, the easier it is to improve the reduction effect of eddy current losses.
[0084] By making the length Le less than 0.49 times the length of the winding portion 21 along the first direction D1, the proportion of molded parts of composite materials with lower loss than powder-pressed molded parts can be increased, thus making the reactor 1 a low-loss product. Furthermore, by making the length Le less than 0.49 times the length of the winding portion 21 along the first direction D1, it is easier to manufacture the gap portion 3g, which is composed of a portion of the molding resin portion 4. The gap portion 3g, composed of a portion of the molding resin portion 4, is formed as follows: A composition is prepared by combining the coil 2 and the magnetic core 3. The material constituting the molding resin portion 4 is made to transition from the outside of the composition towards the end face of the first intermediate core portion 31f and the end face of the second intermediate core portion 31s inside the winding portion 21. By making the length Le less than 0.49 times the length of the winding portion 21 along the first direction D1, even if the total volume Va is 50 cm³, 3 The above also facilitates the transition of the constituent materials of the molding resin part 4 to the aforementioned end faces. The shorter the length Le, the easier it is for the constituent materials of the molding resin part 4 to transition to the aforementioned end faces.
[0085] The length Le is preferably more than 0.2 times and less than 0.4 times the length of the winding portion 21 along the first direction D1, and more preferably more than 0.25 times and less than 0.375 times the length of the winding portion 21 along the first direction D1.
[0086] [Molding Resin Department] like Figure 1 As shown, the molding resin portion 4 covers at least a portion of the magnetic core 3 and forms the gap portion 3g. The molding resin portion 4 may cover the outer periphery of the magnetic core 3 but not the outer periphery of the coil 2, or it may cover both the outer periphery of the magnetic core 3 and the outer periphery of the coil 2. For ease of explanation, Figure 4 The molding resin section 4, which will be described later, is omitted.
[0087] like Figure 2As shown, in this embodiment, the molding resin portion 4 covers a portion of the outer periphery of the assembly of the coil 2 and the magnetic core 3. Therefore, the assembly is substantially protected from external environmental influences. In this embodiment, the flat surface on the object-side of the outer peripheral surface 25 of the coil 2 is exposed from the molding resin portion 4. The surface of the outer peripheral surface 25 of the coil 2 excluding the flat surface on the object-side is covered by the molding resin portion 4. The entire outer periphery of the magnetic core 3 is covered by the molding resin portion 4. The molding resin portion 4 is disposed between the winding portion 21 and the first intermediate core portion 31f, between the winding portion 21 and the second intermediate core portion 31s, and between the end face of the first intermediate core portion 31f and the end face of the second intermediate core portion 31s. Through this molding resin portion 4, the coil 2 and the magnetic core 3 are integrated. An example of the resin of the molding resin portion 4 is the same resin as the resin of the molded composite material described above. The resin of the molding resin portion 4, like the molded composite material, may contain ceramic fillers.
[0088] 〔other〕 Although the reactor 1 is not shown in the diagram, it may include at least one of the following: a housing, an adhesive layer, and a retaining member. The housing internally houses the assembly of the coil 2 and the magnetic core 3. This assembly within the housing may be embedded in a sealing resin portion. The housing is mounted on a cooling base or similar fixture. The adhesive layer fixes the assembly to the cooling base or the inner bottom surface of the housing, or fixes the housing to the cooling base or similar fixture. The retaining member is positioned between the coil 2 and the magnetic core 3 to ensure insulation between them.
[0089] In reactor 1, the thickness of the gap 3g is not increased, making it easy to adjust the inductance. This is because the magnetic core 3 is not made of a single material, but is configured to include a first core 3f made of a composite material molding body and a second core 3s made of a powder molding body.
[0090] The reactor 1 is designed to improve heat dissipation. Because the winding portion 21 includes a part that contacts the mounting object 100, the heat from the coil 2 can be effectively released via the mounting object 100. Furthermore, this is because the surface of the magnetic core 3 can include a surface composed of a pressed powder molded body with relatively high thermal conductivity.
[0091] The reactor 1 can be preferably applied to a reactor cooled by a cooling component with inconsistent cooling performance. A second core 3s with high thermal conductivity is positioned on the side of the cooling component with low cooling performance, and a first core 3f with low thermal conductivity is positioned on the side of the cooling component with high cooling performance. Thus, the first core 3f and the second core 3s are cooled equally, and the maximum temperature of the magnetic core 3 is reduced.
[0092] Reactor 1 is not easily made large. As described above, reactor 1 is easy to adjust and has improved heat dissipation, and can be installed without cooling pipes as is the case with conventional reactors.
[0093] The reactor 1 achieves low losses. This is because the length L1s is shorter than the length L1f, resulting in a smaller proportion of powder-pressed molded bodies with losses greater than those of the composite material molded bodies. Furthermore, because the gap 3g is disposed inside the winding section 21, and the length Le is more than 0.2 times the length of the winding section 21, leakage flux is less likely to intrude into the winding section 21. Therefore, eddy current losses occurring in the winding section 21 are easily reduced. Moreover, because the length Le is less than 0.49 times the length of the winding section 21, the proportion of composite material molded bodies with lower losses than those of powder-pressed molded bodies can be increased inside the winding section 21. Furthermore, the maximum temperature of the magnetic core 3 is thus reduced as described above.
[0094] The reactor 1 can suppress problems such as the impact on peripheral equipment by reducing leakage flux. The gap 3g is disposed inside the winding part 21, and its length Le is more than 0.2 times the length of the winding part 21, so it is easy to suppress the leakage of magnetic flux to the outside of the winding part 21.
[0095] The reactor 1 can easily form the gap portion 3g using a portion of the molding resin part 4. The length Le is less than 0.49 times the length of the winding part 21. That is, the gap that forms the gap portion 3g is close to the second end face of the winding part 21. Therefore, even if the total volume Va is 50 cm³, 3 In addition, it is also easy to make the constituent material of the molding resin part 4 transition between the end face of the first intermediate core part 31f and the end face of the second intermediate core part 31s inside the winding part 21.
[0096] Implementation Method 2 [Converter / Power Conversion Device] The reactor 1 of Embodiment 1 can be applied to applications that meet the following energizing conditions. These energizing conditions include, for example, a maximum DC current of approximately 100A to 1000A, an average voltage of approximately 100V to 1000V, and an operating frequency of approximately 5kHz to 100kHz. The reactor 1 of Embodiment 1, as a representative example, can be applied to components of converters mounted on vehicles 1200 such as electric vehicles, hybrid vehicles, or fuel cell vehicles, or to components of power conversion devices equipped with such converters.
[0097] like Figure 5 As shown, vehicle 1200 includes a main battery 1210, a power conversion device 1100 connected to the main battery 1210, and a motor 1220 driven by power supplied from the main battery 1210 for driving. A representative example of motor 1220 is a three-phase AC motor, which drives the wheels 1250 during driving and functions as a generator during regeneration. In the case of a hybrid electric vehicle, vehicle 1200 includes an engine 1300 in addition to the motor 1220. Figure 5 In the text, the charging port of vehicle 1200 is referred to as a socket, but it may be a plug-in type.
[0098] The power conversion device 1100 includes a converter 1110 connected to the main battery 1210 and an inverter 1120 connected to the converter 1110 and performing DC-AC conversion. In this example, the converter 1110 boosts the input voltage of the main battery 1210 (between 200V and 300V) to between 400V and 700V when the vehicle 120 is in motion, supplying power to the inverter 1120. During regeneration, the converter 1110 steps down the input voltage from the motor 1220 via the inverter 1120 to a DC voltage suitable for the main battery 1210, charging the main battery 1210. The input voltage is DC. When the vehicle 1200 is in motion, the inverter 1120 converts the DC boosted by the converter 1110 into a specified AC voltage to supply power to the motor 1220; during regeneration, it converts the AC output from the motor 1220 into DC and outputs it to the converter 1110.
[0099] like Figure 6 As shown, the converter 1110 includes multiple switching elements 1111, a drive circuit 1112 that controls the operation of the switching elements 1111, and a reactor 1115, and performs input voltage conversion by repeatedly switching ON and OFF. Input voltage conversion here refers to boosting and bucking. The switching elements 1111 utilize power devices such as field-effect transistors and insulated-gate bipolar transistors. The reactor 1115 utilizes the property of a coil to impede changes in the current flowing through the circuit, thus smoothing the current change when the current increases or decreases due to switching operations. The reactor 1115 is the reactor 1 of Embodiment 1. With the reactor 1, which offers excellent heat dissipation and low losses without becoming bulky, the power conversion device 1100 and the converter 1110 can also be expected to achieve miniaturization, improved heat dissipation, and lower losses.
[0100] In addition to the converter 1110, the vehicle 1200 also includes a power supply converter 1150 connected to the main battery 1210, and an auxiliary power supply converter 1160 connected to the auxiliary battery 1230 (which serves as the power source for the auxiliary equipment 1240) and the main battery 1210, which converts the high voltage of the main battery 1210 to a low voltage. The converter 1110 is a representative example of a DC-DC converter, but the power supply converter 1150 and the auxiliary power supply converter 1160 perform AC-DC conversion. Some power supply converters 1150 also perform DC-DC conversion. The reactors of the power supply converter 1150 and the auxiliary power supply converter 1160 have the same configuration as the reactor 1 in Embodiment 1, and reactors with different sizes and shapes can be appropriately applied. Furthermore, the reactor 1 in Embodiment 1 can also be applied to converters that only perform boost conversion or converters that only perform buck conversion, which are converters that convert input power.
[0101] The present invention is not limited to the examples above but is represented by the claims, and is intended to include all modifications within the meaning and scope of the claims. Explanation of reference numerals in the attached figures
[0102] 1. Reactor 2 coils 21 winding portion, 21a first end, 21b second end 25 outer perimeter 3 magnetic core, 3f first core, 3s second core 31f first intermediate core, 31s second intermediate core 321 First side magnetic core section, 322 Second side magnetic core section 33f first end core, 33s second end core 3g gap 4. Molding Resin Section L1f, L1s, L21f, L22f, L3f, L3s, Le length D1 First Direction, D2 Second Direction, D3 Third Direction 100 Setting Objects 1100 power conversion device, 1110 converter 1111 Switching element, 1112 Drive circuit, 1115 Reactor 1120 inverter Converters for 1150 power supply units and 1160 auxiliary power supplies 1200 vehicles 1210 main battery, 1220 motor, 1230 auxiliary battery 1240 auxiliary machinery, 1250 wheels 1300 engine
Claims
1. A reactor comprising a coil and a magnetic core, wherein, The coil has a winding portion. The number of the winding portion is 1. The outer peripheral surface of the winding portion includes a portion that contacts the object on which the reactor is installed. The magnetic core has: The E-shaped first core and the T-shaped second core, which are combined along the axial direction of the winding portion, and The gap between the first core and the second core is provided. The first core is formed by an integral composite material molding body comprising a first end core facing the first end face of the winding portion, a first intermediate core having a portion disposed inside the winding portion, and a first side magnetic core and a second side magnetic core disposed on the outer periphery of the winding portion in a manner that sandwiches the first intermediate core. The second core is formed by an integral powder-pressed molding body, comprising a second end core facing the second end face of the winding portion, and a second intermediate core having a portion disposed inside the winding portion. The length of the second intermediate core along the axial direction of the winding portion is shorter than the length of the first intermediate core along the axial direction of the winding portion. The gap portion is disposed inside the winding portion between the first intermediate core portion and the second intermediate core portion. The length from the second end face to the gap is more than 0.2 times and less than 0.49 times the length of the winding portion. The total volume Va of the first core, the second core, and the gap is 50 cm³. 3 Above and 500cm 3 the following.
2. The reactor according to claim 1, wherein, The volume of the second core is more than 25% and less than 40% of the total volume Va.
3. The reactor according to claim 1 or claim 2, wherein, The volume of the second intermediate core accounts for more than 15% and less than 49% of the total volume of the first intermediate core, the second intermediate core, and the gap.
4. The reactor according to claim 1 or claim 2, wherein, The ratio of the thickness of the gap portion to the total length of the first intermediate core portion, the second intermediate core portion, and the thickness of the gap portion is 0.001 or more and 0.1 or less.
5. The reactor according to claim 1 or claim 2, wherein, The thickness of the gap is 0.1 mm or more and 2 mm or less.
6. The reactor according to claim 1 or claim 2, wherein, It includes a molding resin portion that covers at least a portion of the magnetic core and forms the gap portion.
7. The reactor according to claim 1 or claim 2, wherein, The reactor constitutes a converter for electric vehicles or hybrid vehicles.
8. The reactor according to claim 7, wherein, The reactor constitutes the converter in a fuel cell vehicle.
9. The reactor according to claim 1 or claim 2, wherein, The pressed powder molded body is a molded body comprising raw material powder including soft magnetic powder. The content of the soft magnetic powder in the pressed powder molded body is 85% by volume or more and 99% by volume or less.
10. The reactor according to claim 1 or claim 2, wherein, The molded body of the composite material is a molded body in which soft magnetic powder is dispersed in resin. The content of the soft magnetic powder in the molded body of the composite material is more than 20% by volume and less than 80% by volume.
11. A converter, wherein, A reactor comprising any one of claims 1 to 10.
12. A power conversion device, wherein, It has the converter as described in claim 11.
Citation Information
Patent Citations
Electric reactor
JP2013074062A
Pharmaceutical composition including phosphate binder particle
JP2021138708A
Compound magnetic core
JP2000294429A
Shunt reactor
JP2004047828A