Extreme high temperature cycle resistant wire for aerospace
By designing aerospace cables with multi-core structures and specific material combinations, the problems of durability and weight increase of existing cables under extreme high-temperature environments have been solved, achieving cable stability and lightweighting under high-temperature conditions.
Patent Information
- Application Number
- CN202410164932.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-02-05
- Publication Date
- 2026-11-24
- Estimated Expiration
- 2044-02-05
AI Technical Summary
Existing aerospace cables cannot meet the high-temperature resistance requirements under extreme high-temperature environments, and wrapping them with high-temperature resistant insulation materials increases the weight of the wire harness and the difficulty of processing.
Design an aerospace-grade high-temperature resistant cycling wire with a multi-core structure, including multiple stranded insulated cores, a shielding layer, and a sheath. The insulation layer consists of a polyimide composite film, a nano-quartz fiber yarn braided layer, and a nano-silicone resin coating layer. The shielding layer is made of nickel-plated copper wire braid, and the sheath consists of a blended slurry and a nano-quartz fiber yarn braided layer.
It achieves the durability of wires in high-temperature environments of 450-550℃, reduces the weight and processing difficulty of wire harnesses, and has the ability to resist electromagnetic interference, meeting the multi-core design requirements of the aerospace field.
Smart Images

Figure CN117854820B_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of cable technology, and in particular relates to an aerospace-grade high-temperature cycling resistant wire. Background Technology
[0002] The basic requirements for aerospace cables are light weight, small diameter, high temperature resistance, and good abrasion resistance. In addition, they should be resistant to fuel oils, lubricating oils, and other chemical solvents. High-performance cable materials are extremely important for improving structural efficiency and extending cable lifespan, and are one of the goals of aerospace materials research.
[0003] Currently, high-temperature resistant cables used in aerospace applications have the following problems: the insulation layer is made of fluoroplastics, and the maximum long-term operating temperature of the cable is 200-250℃, which can only be used in general high-temperature environments. For environments with extreme high-temperature requirements (450℃-500℃), high-temperature resistant insulation materials must be wrapped around the wire harness. This method not only increases the difficulty of wire harness processing, but also increases the outer diameter and weight of the wire harness, thereby increasing the difficulty of installation and laying. Summary of the Invention
[0004] The purpose of this invention is to overcome the above-mentioned problems in the prior art and provide an aerospace-grade high-temperature resistant cycling wire. This wire has high-temperature resistance, a multi-core structure, eliminates the difficulty of wire harness bundling, and meets the requirements of multi-core design.
[0005] To achieve the above-mentioned technical objectives and effects, the present invention is implemented through the following technical solution: An aerospace-grade high-temperature resistant cycling wire includes multiple stranded insulated cores and a shielding layer covering the outside of the multiple insulated cores, wherein the shielding layer is covered with a sheath. The insulated core includes a conductor and an insulating layer covering the outside of the conductor, wherein the conductor includes multiple stranded single-core copper wires; The insulating layer includes a polyimide composite film layer, a first braided layer, and a first resin coating layer that are tightly arranged from the inside out. The sheath includes a second braided layer and a second resin coating layer applied to the outside of the second braided layer.
[0006] Furthermore, the number of insulated wire cores is at least two.
[0007] Furthermore, the conductor contains 7-37 single-core copper wires; The single-core copper wire is silver-plated copper wire or nickel-plated copper wire; The diameter of the single-core copper wire is 0.10-0.45mm.
[0008] Furthermore, the polyimide composite film layer is formed by wrapping a polyimide composite film around the outside of the conductor. The polyimide composite film has two wrapping layers, and the wrapping directions of the two polyimide composite films are opposite. The polyimide composite film is prepared by laminating a high-temperature resistant material layer onto both sides of the polyimide film as a base film. The material of the high-temperature resistant material layer is polytetrafluoroethylene or polytetrafluoroethylene.
[0009] Furthermore, the material of the first woven layer is nano-quartz fiber yarn, and the first woven layer is formed by weaving nano-quartz fiber yarn on the outside of the polyimide composite film layer; The exterior of the nano-quartz fiber yarn is coated with an aluminum oxide coating by a plasma spraying machine. The alumina has a particle size of 50-100 μm.
[0010] Furthermore, both the first resin coating layer and the second resin coating layer are made of nano-silicone resin. The particle size of the nano-silicone resin is 50-100 nm.
[0011] Furthermore, the shielding layer is made of nickel-plated copper wire braided with a braiding density of not less than 75% and the nickel plating layer thickness of the nickel-plated copper wire is not less than 0.2 μm.
[0012] Furthermore, the second woven layer includes a protective layer and a quartz fiber layer arranged from the inside out; The protective layer is formed by coating the outside of the shielding layer with a blended slurry and then drying it. The blended slurry is applied in 1-2 coats, and drying is required after each coat of the blended slurry. The quartz fiber layer is formed by weaving nano-quartz fiber yarn onto the outside of the protective layer; The exterior of the nano-quartz fiber yarn is coated with an aluminum oxide coating by a plasma spraying machine. The alumina has a particle size of 50-100 μm.
[0013] Furthermore, the preparation process of the blended slurry is as follows: Under an ice-water bath, silane and anhydrous ethanol are added to the reaction vessel and stirred for 1-2 hours. After stirring, silane coupling agent, xylene, and hydrochloric acid are added to the reaction vessel, the temperature is raised to 50-60°C, and stirring is continued for 1-2 hours. After standing and separating into layers, the acid water layer is removed to obtain a mixture. The mixture is then evaporated in a rotary evaporator for 4-6 hours to obtain a precursor slurry. The precursor slurry, carbon fiber powder, and graphite powder are placed in a magnetic stirrer and magnetically stirred for 2-6 hours to ensure uniform mixing, thus preparing a blended slurry.
[0014] Furthermore, the mass ratio of silane, anhydrous ethanol, silane coupling agent, xylene, and hydrochloric acid added to the reaction vessel is 1:1.1-2.6:0.5-1.2:0.5-1.2:2.0-4.0; The hydrochloric acid concentration is 0.05-0.10 mmol / L; The mass ratio of the precursor slurry, carbon fiber powder, and graphite powder in the magnetic stirrer is 1:0.10-0.60:0.01-0.10; The silane includes any one or a combination of at least two of methyltrimethoxysilane, methyltriethoxysilane, tetramethyldivinylsilane, tetramethoxysilane, or tetramethyldivinyldisiloxane; The silane coupling agent includes any one of KH-550, KH-560 or KH-570.
[0015] Compared with the prior art, the beneficial effects of the present invention are: 1. This invention provides an aerospace-grade high-temperature resistant cycling wire. This wire has extreme high-temperature resistance and features a multi-core structure, eliminating the difficulty of wire harness bundling and meeting the requirements of multi-core design.
[0016] 2. The aerospace-grade high-temperature resistant cyclic wire provided by the present invention has an insulation layer composed of a polyimide composite film layer, a high-temperature resistant first braided layer, and a first resin coating layer coated on the outer layer of the first braided layer. The wire prepared by this invention can withstand high temperatures of 450-550℃.
[0017] 3. The aerospace-grade high-temperature resistant cycling wire provided by this invention adopts a multi-core structure, which eliminates the difficulty of wire harness bundling and avoids the situation where additional high-temperature resistant materials are wrapped around the wire harness, resulting in an increase in the weight of the wire harness. Through the design of this multi-core structure, the needs of actual working conditions can be met.
[0018] 4. The aerospace-grade high-temperature resistant cyclic wire provided by this invention has a shielding layer made of nickel-plated copper wire braid, which not only makes the product resistant to extreme high temperatures, but also suitable for working environments that require isolation from external electromagnetic interference, thus having a wide range of applications. Attached Figure Description
[0019] The accompanying drawings, which are included to provide a further understanding of the invention and form part of this application, illustrate exemplary embodiments of the invention and, together with their description, serve to explain the invention and do not constitute an undue limitation thereof. In the drawings: Figure 1 This is a schematic diagram of the structure of the present invention; Figure 2 This is a schematic diagram of the structure of the insulated wire core of the present invention.
[0020] The reference numerals in the attached drawings are as follows: 10, insulated core; 20, shielding layer; 30, sheath; 1, conductor; 2, insulation layer; 21, polyimide composite film layer; 22, first braided layer; 23, first resin coating layer; 31, second braided layer; 32, second resin coating layer. Detailed Implementation
[0021] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.
[0022] like Figures 1 to 2 As shown, an embodiment of the present invention provides an aerospace-grade high-temperature cycling-resistant wire, comprising multiple stranded insulated cores 10 and a shielding layer 20 covering the multiple insulated cores 10, the shielding layer 20 being covered by a sheath 30; wherein, the number of insulated cores 10 is at least two. The insulated core 10 includes a conductor 1 and an insulating layer 2 covering the outside of the conductor 1. The conductor 1 includes multiple stranded single-core copper wires; wherein the number of single-core copper wires in the conductor 1 is 7-37. The single-core copper wire should be silver-plated or nickel-plated copper wire with a nominal diameter of 0.10-0.45mm; The insulating layer 2 includes a polyimide composite film layer 21, a first braided layer 22, and a first resin coating layer 23 that are tightly arranged from the inside out. The polyimide composite film layer 21 is formed by wrapping a polyimide composite film around the outside of the conductor 1. The polyimide composite film has two wrapping layers, and the wrapping directions of the two polyimide composite films are opposite. The thickness of the polyimide composite film layer 21 is 0.108-0.264 mm; Polyimide composite film is made by laminating a layer of high-temperature resistant material onto both sides of a polyimide film using a method of layer-by-layer melting and precision pressing. The thickness of the base film is 0.015-0.017 mm, and the thicknesses of the double-sided composite high-temperature resistant material layers of the base film are 0.010-0.012 mm and 0.002-0.004 mm, respectively. The high-temperature resistant material layer is made of perfluoroethylene or polytetrafluoroethylene; The first woven layer 22 is made of nano-quartz fiber yarn. The first woven layer 22 is formed by weaving nano-quartz fiber yarn on the outside of the polyimide composite film layer 21. The weaving density is not less than 95%, and the weaving thickness is 0.25-0.45 mm. The SiO2 content in the nano-quartz fiber yarn is not less than 99.95%. The SiO2 content in the nano-quartz fiber yarn is not less than 99.95%. The high-purity nano-quartz fiber yarn has properties such as high temperature resistance, low thermal conductivity, high strength and good insulation. The insulation performance is effectively improved by coating the first woven layer 22 woven from the nano-quartz fiber yarn with a first resin coating layer 23. The outer surface of the nano-quartz fiber yarn is coated with an alumina coating using a plasma spraying machine; the alumina has a particle size of 50-100 μm. The first resin coating layer 23 is made of nano-silicone resin. Specifically, the first resin coating layer 23 is formed by coating the outside of the first braided layer 22 with nano-silicone resin solution and then drying it. The nano-silicone resin solution is coated in 1-2 times, and drying is required after each coating of nano-silicone resin solution. The thickness of the first resin coating layer 23 is 0.005-0.015 mm; The pH value of the nano-silicone resin solution used is between 8 and 9, and it does not bubble or crack after being placed at 500-800℃ for 24 hours. The nano-silicone resin solution is a 50-60% methyl silicone resin solution with ethanol as the solvent, and the particle size of the methyl silicone resin is 50-100 nm.
[0023] The shielding layer 20 is made of nickel-plated copper wire braid with a braiding density of not less than 75% and a nickel plating layer thickness of not less than 0.2um. The shielding layer 20 is made of metal wire braid, which enables the wire to not only withstand extreme high temperatures, but also meet the requirements for isolating external electromagnetic interference.
[0024] The sheath 30 includes a second braided layer 31 and a second resin coating layer 32 coated on the outside of the second braided layer 31; The second woven layer includes a protective layer arranged from the inside out and a quartz fiber layer; The protective layer is formed by coating the outside of the shielding layer 20 with a blended slurry and then drying it. The blended slurry is coated 1-2 times, and drying is required after each coating of the blended slurry. The preparation process of the blended slurry is as follows: Silane and anhydrous ethanol are added to the reaction vessel under an ice-water bath and stirred for 1-2 hours. After stirring, silane coupling agent, xylene and hydrochloric acid are added to the reaction vessel, the temperature is raised to 50-60℃, and stirring is continued for 1-2 hours. After standing and separating, the acid water layer is removed to obtain a mixture. The mixture is then evaporated by a rotary evaporator for 4-6 hours to obtain a precursor slurry. The precursor slurry, carbon fiber powder and graphite powder are placed in a magnetic stirrer and magnetically stirred for 2-6 hours to make them uniformly mixed, thus preparing the blended slurry. The mass ratio of silane, anhydrous ethanol, silane coupling agent, xylene, and hydrochloric acid added to the reaction vessel is 1:1.1-2.6:0.5-1.2:0.5-1.2:2.0-4.0. The hydrochloric acid concentration is 0.05-0.10 mmol / L; The mass ratio of the precursor slurry, carbon fiber powder, and graphite powder in the magnetic stirrer is 1:0.10-0.60:0.01-0.10; The silane includes any one or a combination of at least two of methyltrimethoxysilane, methyltriethoxysilane, tetramethyldivinylsilane, tetramethoxysilane, or tetramethyldivinyldisiloxane; The silane coupling agent includes any one of KH-550, KH-560 or KH-570; The preparation of the blended slurry uses a single silane or multiple silanes as raw materials and co-hydrolyzes and condenses them through a silane coupling agent. The initially prepared silicone resin precursor slurry has high temperature resistance. The prepared precursor slurry is blended with carbon fiber, which is carbon fiber powder with a particle size of 50-100um. This can improve the performance of the silicone resin precursor and improve the heat resistance of the final protective layer. The quartz fiber layer is formed by weaving nano-quartz fiber yarn onto the outside of the protective layer; the weaving density is not less than 95%, and the weaving thickness is 0.25-0.45 mm; the SiO2 content in the nano-quartz fiber yarn is not less than 99.95%. The outer surface of the nano-quartz fiber yarn is coated with an alumina coating using a plasma spraying machine; the alumina particle size is 50-100um. The mechanical properties of the wire at high temperatures are improved by spraying an aluminum oxide coating onto the outside of the nano-quartz fiber yarn. This is mainly because under high temperature conditions, a reaction occurs between the first braided layer 22 and the first resin coating layer coated on the outside of the first braided layer 22, as well as between the quartz fiber layer and the second resin coating layer 32 coated on the outside of the quartz fiber layer, which reduces the mechanical properties. By spraying aluminum oxide onto the outside of the nano-quartz fiber yarn used in the first braided layer 22 and the quartz fiber layer, the reaction is isolated, thereby improving the mechanical properties of the wire. The second resin coating layer 32 is made of the same material as the first resin coating layer 23. That is, the second resin coating layer 32 is formed by coating the outside of the second braided layer 31 with a nano-silicone resin solution and then drying it. The nano-silicone resin solution is coated in 1-2 times, and drying is required after each coating of the nano-silicone resin solution. The thickness of the second resin coating layer 32 is 0.005-0.015 mm; The pH value of the nano-silicone resin solution used is between 8 and 9, and it does not bubble or crack after being placed at 500-800℃ for 24 hours; the nano-silicone resin solution is a 50-60% methyl silicone resin solution, the solvent is ethanol, and the particle size of the methyl silicone resin is 50-100nm.
[0025] The following detailed description of an aerospace-grade high-temperature cycling-resistant wire provided by the embodiments of the present invention, in conjunction with specific examples and comparative examples, provides an in-depth description of such a wire.
[0026] Example 1 This embodiment provides an aerospace-grade high-temperature resistant cycling wire, including four stranded insulated cores 10 and a shielding layer 20 covering the four insulated cores 10. The shielding layer 20 is covered with a sheath 30. The four insulated cores 10 are stranded into a cable. The insulated core 10 consists of a conductor 1 and an insulation layer 2 covering the outside of the conductor 1. The conductor 1 is made of 7 silver-plated copper wires with a nominal diameter of 0.30mm twisted together. During the twisting process, the silver-plated copper wires are semi-compacted or compacted to ensure the roundness of the conductor 1 formed by the multiple silver-plated copper wires. The insulating layer 2 is composed of a polyimide composite film layer 21, a first braided layer 22 and a first resin coating layer 23 that are tightly arranged from the inside out. The polyimide composite film layer 21 is formed by wrapping a polyimide composite film around the conductor 1. The polyimide composite film has two wrapping layers, and the two polyimide composite films are wrapped in opposite directions. The thickness of the polyimide composite film layer 21 is 0.186 mm. The wrapping overlap rate of each polyimide composite film layer is 52.5%; Polyimide composite film is prepared by laminating a high-temperature resistant material layer on both sides of a polyimide film as a base film. The material of the high-temperature resistant material layer is polytetrafluoroethylene propylene. In the polyimide composite film, the thickness of the base film is 0.016 mm, and the thicknesses of the high-temperature resistant material layers on both sides of the base film are 0.011 mm and 0.003 mm, respectively. The first woven layer 22 is made of high-temperature resistant nano-quartz fiber yarn with a SiO2 content of 99.95%. The first woven layer 22 is formed by weaving nano-quartz fiber yarn on the outside of the polyimide composite film layer 21, with a weaving density of 95% and a weaving thickness of 0.35 mm. The outside of the nano-quartz fiber yarn is coated with an alumina coating by a plasma spraying machine. The particle size of the alumina is 75 μm. The first resin coating layer 23 is formed by coating the outside of the first braided layer 22 with a nano-silicone resin solution and then drying it. The thickness of the first resin coating layer 23 is 0.010 mm. The first resin coating layer is coated in two layers, and drying is required after each coating of nano-silicone resin solution. The pH value of the nano-silicone resin solution is 9; the nano-silicone resin solution is a 60% methyl silicone resin solution, the solvent is ethanol, and the particle size of the methyl silicone resin is 75nm; The shielding layer 20 is made of nickel-plated copper wire braid with a braiding density of 75% and a nickel plating layer thickness of 0.2µm. The sheath 30 includes a second braided layer 31 and a second resin coating layer 32 coated on the outside of the second braided layer 31. The second braided layer includes a protective layer and a quartz fiber layer arranged from the inside out. The protective layer is formed by coating the outside of the shielding layer 20 with a blended slurry and then drying it. The blended slurry is coated once. The quartz fiber layer is formed by weaving nano-quartz fiber yarn with a SiO2 content of 99.95% on the outside of the protective layer. The weaving density is 95% and the weaving thickness is 0.35 mm. The outside of the nano-quartz fiber yarn is coated with an alumina coating by a plasma spraying machine. The particle size of the alumina is 75 μm. The preparation process of the blended slurry is as follows: Step 1.1: Under an ice-water bath, add silane and anhydrous ethanol to the reaction vessel and stir for 1.5 hours. After stirring, continue to add silane coupling agent KH-550, xylene, and hydrochloric acid to the reaction vessel. The mass ratio of silane, anhydrous ethanol, silane coupling agent, xylene, and hydrochloric acid added to the reaction vessel is 1:2:0.6:0.6:4.0; the concentration of hydrochloric acid is 0.05-0.10 mmol / L. The silane used is methyltrimethoxysilane and methyltriethoxysilane, and the mass ratio of methyltrimethoxysilane to methyltriethoxysilane in the silane is 1:1; Step 1.2: Heat to 55℃, continue stirring for 1.5h, let stand to separate into layers, remove the acidic water layer to obtain the mixture; Step 1.3: The mixture is rotary evaporated for 5 hours to obtain the precursor slurry; Step 1.4: Take the precursor slurry, carbon fiber powder and graphite powder, and add them to a magnetic stirrer in a mass ratio of 1:0.20:0.05. Stir magnetically for 3 hours to mix them evenly and prepare a blended slurry. The carbon fiber powder has a diameter of 75 μm.
[0027] The second resin coating layer 32 is made of the same material as the first resin coating layer 23. That is, the second resin coating layer 32 is formed by coating the outside of the second braided layer 31 with a nano-silicone resin solution and then drying it. The nano-silicone resin solution is coated in two layers, and drying is required after each coating of the nano-silicone resin solution. The thickness of the second resin coating layer 32 is 0.010 mm; The pH value of the nano-silicone resin solution used is 8; the nano-silicone resin solution is a 60% methyl silicone resin solution, the solvent is ethanol, and the particle size of the methyl silicone resin is 75nm.
[0028] Example 2 This embodiment provides an aerospace-grade high-temperature resistant cycling wire, including six stranded insulated cores 10 and a shielding layer 20 covering the six stranded insulated cores 10, with a sheath 30 covering the shielding layer 20. The insulated core 10 consists of a conductor 1 and an insulating layer 2 covering the outside of the conductor 1. The conductor 1 is made of 10 nickel-plated copper wires with a nominal diameter of 0.45 mm twisted together. The insulating layer 2 is composed of a polyimide composite film layer 21, a first braided layer 22, and a first resin coating layer 23, which are tightly arranged inside and out. The polyimide composite film layer 21 is formed by wrapping a polyimide composite film around the conductor 1. There are two wrapping layers of polyimide composite film, and the wrapping directions of the two polyimide composite films are opposite. The thickness of the polyimide composite film layer 21 is 0.108 mm. The polyimide composite film is prepared by laminating a high-temperature resistant material layer on both sides of the polyimide film as a base film. The high-temperature resistant material layer is made of polytetrafluoroethylene. In the polyimide composite film, the thickness of the base film is 0.015 mm, and the thicknesses of the high-temperature resistant material layers on both sides of the base film are 0.010 mm and 0.002 mm, respectively. The first woven layer 22 is made of high-temperature resistant nano-quartz fiber yarn with a SiO2 content of 99.95%. The first woven layer 22 is formed by weaving nano-quartz fiber yarn on the outside of the polyimide composite film layer 21, with a weaving density of 96% and a weaving thickness of 0.25 mm. The outside of the nano-quartz fiber yarn is coated with an alumina coating by a plasma spraying machine. The particle size of the alumina is 50 μm. The first resin coating layer 23 is formed by coating the outside of the first braided layer 22 with a nano-silicone resin solution and then drying it. The thickness of the first resin coating layer 23 is 0.005 mm. The first resin coating layer 23 is coated in one step, and drying is required after coating with the nano-silicone resin solution. The pH value of the nano-silicone resin solution used is 9; the nano-silicone resin solution is a 50% methyl silicone resin solution, the solvent is ethanol, and the particle size of the methyl silicone resin is 50nm. The shielding layer 20 is made of nickel-plated copper wire braid with a braiding density of 80% and a nickel plating layer thickness of 0.3µm. The sheath 30 includes a second braided layer 31 and a second resin coating layer 32 coated on the outside of the second braided layer 31. The second braided layer includes a protective layer and a quartz fiber layer arranged from the inside out. The protective layer is formed by coating the outside of the shielding layer 20 with a blended slurry and then drying it. The blended slurry is coated twice, and drying is required after each coating. The quartz fiber layer is formed by weaving nano-quartz fiber yarn with a SiO2 content of 99.95% on the outside of the protective layer. The weaving density is 96% and the weaving thickness is 0.45 mm. The outside of the nano-quartz fiber yarn is coated with an alumina coating by a plasma spraying machine. The particle size of the alumina is 50 μm. The preparation process of the blended slurry is the same as that of the blended slurry in Example 1.
[0029] The second resin coating layer 32 is made of the same material as the first resin coating layer 23. That is, the second resin coating layer 32 is formed by coating the outside of the second braided layer 31 with a nano-silicone resin solution and then drying it. The nano-silicone resin solution is coated in one step, and drying is required after each coating of the nano-silicone resin solution. The thickness of the second resin coating layer 32 is 0.005 mm; The pH value of the nano-silicone resin solution used is 8; the nano-silicone resin solution is a 60% methyl silicone resin solution, the solvent is ethanol, and the particle size of the methyl silicone resin is 150nm.
[0030] Example 3 This embodiment provides an aerospace-grade high-temperature cycling-resistant wire, including two stranded insulated cores 10 and a shielding layer 20 covering the outside of the two stranded insulated cores 10, with a sheath 30 covering the outside of the shielding layer 20.
[0031] The insulated core 10 consists of a conductor 1 and an insulating layer 2 covering the outside of the conductor 1. The conductor 1 is made of 37 silver-plated copper wires with a nominal diameter of 0.10 mm twisted together. The insulating layer 2 is composed of a polyimide composite film layer 21, a first braided layer 22, and a first resin coating layer 23, which are tightly arranged inside and out. The polyimide composite film layer 21 is formed by wrapping a polyimide composite film around the conductor 1. There are two wrapping layers of polyimide composite film, and the wrapping directions of the two polyimide composite films are opposite. The thickness of the polyimide composite film layer 21 is 0.264 mm. The polyimide composite film is prepared by using a polyimide film as the base film and bonding a high-temperature resistant material layer to both sides of the polyimide film. The material of the high-temperature resistant material layer is polytetrafluoroethylene. In the polyimide composite film, the thickness of the base film is 0.017 mm, and the thicknesses of the high-temperature resistant material layers on both sides of the base film are 0.012 mm and 0.004 mm, respectively. The first woven layer 22 is made of high-temperature resistant nano-quartz fiber yarn with a SiO2 content of 99.95%. The first woven layer 22 is formed by weaving nano-quartz fiber yarn on the outside of the polyimide composite film layer 21, with a weaving density of 98% and a weaving thickness of 0.45 mm. The outside of the nano-quartz fiber yarn is coated with an alumina coating by a plasma spraying machine. The particle size of the alumina is 75 μm. The first resin coating layer 23 is formed by coating the outside of the first braided layer 22 with a nano-silicone resin solution and then drying it. The thickness of the first resin coating layer 23 is 0.015 mm. The first resin coating layer is completed by coating in two layers. After coating with the nano-silicone resin solution, it needs to be dried. The pH value of the nano-silicone resin solution used is 8; the nano-silicone resin solution is a 60% methyl silicone resin solution, the solvent is ethanol, and the particle size of the methyl silicone resin is 75nm.
[0032] The shielding layer 20 is made of nickel-plated copper wire braid with a braiding density of 85% and a nickel plating layer thickness of 0.2µm.
[0033] The sheath 30 includes a second braided layer 31 and a second resin coating layer 32 coated on the outside of the second braided layer 31. The second braided layer includes a protective layer and a quartz fiber layer arranged from the inside out. The protective layer is formed by coating the outside of the shielding layer 20 with a blended slurry and then drying it. The blended slurry is coated once. The quartz fiber layer is formed by weaving nano-quartz fiber yarn with a SiO2 content of 99.95% on the outside of the protective layer. The weaving density is 96% and the weaving thickness is 0.25 mm. The outside of the nano-quartz fiber yarn is coated with an alumina coating by a plasma spraying machine. The particle size of the alumina is 75 μm. The preparation process of the blended slurry is the same as that of the blended slurry in Example 1.
[0034] The second resin coating layer 32 is made of the same material as the first resin coating layer 23. That is, the second resin coating layer 32 is formed by coating the outside of the second braided layer 31 with a nano-silicone resin solution and then drying it. The nano-silicone resin solution is coated in two layers, and drying is required after each coating of the nano-silicone resin solution. The thickness of the second resin coating layer 32 is 0.015 mm; The pH value of the nano-silicone resin solution used is 8; the nano-silicone resin solution is a 55% methyl silicone resin solution, the solvent is ethanol, and the particle size of the methyl silicone resin is 75nm.
[0035] Comparative Example The comparison example uses AF-200 type wire, whose performance parameters are as follows: The normal operating temperature range is -40 to 200℃; Test voltage of 1000V AC for 1 minute.
[0036] Experimental Example 1 The aerospace-grade high-temperature cycling-resistant wires from Examples 1-3 were subjected to insulation resistance testing, withstand voltage testing, and low-temperature testing. The withstand voltage test conditions were: a test voltage of 2500V AC at power frequency, and a test time of 5 minutes; the low-temperature test temperature was -65±2℃. The test results are as follows: In Examples 1-3, the aerospace-grade high-temperature cycling-resistant wires prepared were able to withstand a low-temperature test of -65±2℃. After the low-temperature test, the wires were subjected to a test voltage of 2500V AC for 5 minutes without breakdown, indicating that the performance of the aerospace-grade high-temperature cycling-resistant wires provided in this application is superior to that of the existing AF-200 model wires.
[0037] Experiment Example 2 The aerospace high-temperature resistant cycling wires provided in Examples 1-3 were subjected to high-temperature resistance tests. The selected wires were of the same length. During the test, both ends of the wires were fixed to prevent loosening from affecting the test results. After the test, the wires were allowed to cool to room temperature before electrical performance tests were performed and any changes in appearance were recorded. Tests showed that the aerospace-grade high-temperature resistant cycling wires provided in Examples 1-3 could withstand temperatures of 450℃-550℃ and functioned normally. Specific test data results are shown in Table 1.
[0038] Test 1: After the wires were treated at 450℃ for 40 minutes, they were taken out and subjected to electrical performance testing. The test was repeated 20 times. The wires in Examples 1-3 did not crack and all functions were normal. Test 2: After the wires were treated at 500℃ for 40 minutes, they were taken out and subjected to electrical performance testing. The test was repeated 4 times. The wires in Examples 1-3 did not crack and all functions were normal. Test 3: After treating the wire at 550℃ for 30 minutes, the wire was taken out and subjected to electrical performance testing. The test was repeated twice. The wires in Examples 1-3 all functioned normally.
[0039] This invention provides an aerospace-grade high-temperature resistant cyclic wire. The insulation layer is composed of a polyimide composite film layer, a high-temperature resistant first braided layer, and a first resin coating layer applied to the outside of the first braided layer. The thickness of each layer is controlled, allowing the wire to withstand temperatures of 450-550℃, thus meeting the requirements for high-temperature applications and reducing the difficulty of wire processing. Furthermore, for the aerospace field, lightweight cables are required; this wire solves the problem of increased weight caused by wrapping the wire bundle with high-temperature resistant insulation material, and also reduces the difficulty of installation and laying. A shielding layer 20 is formed by braiding nickel-plated copper wire, enabling the product to not only withstand extreme high temperatures but also meet the requirement of isolating external electromagnetic interference.
[0040] In the description of this specification, references to terms such as "an embodiment," "example," "specific example," etc., indicate that a specific feature, structure, material, or characteristic described in connection with that embodiment or example is included in at least one embodiment or example of the invention. In this specification, illustrative expressions of the above terms do not necessarily refer to the same embodiment or example. Furthermore, the specific features, structures, materials, or characteristics described may be combined in any suitable manner in one or more embodiments or examples.
[0041] The foregoing has shown and described the basic principles, main features, and advantages of the present invention. Those skilled in the art should understand that the present invention is not limited to the above embodiments. The embodiments and descriptions in the specification are merely illustrative of the principles of the invention. Various changes and modifications can be made to the invention without departing from its spirit and scope, and all such changes and modifications fall within the scope of the claimed invention.
Claims
1. An aerospace extreme high temperature cycle resistant wire, characterized by: It includes multiple stranded insulated wire cores (10) and a shielding layer (20) covering the outside of the multiple strands of insulated wire cores (10), the shielding layer (20) being covered with a sheath (30). The insulated core (10) includes a conductor (1) and an insulating layer (2) covering the outside of the conductor (1), wherein the conductor (1) includes multiple stranded single-core copper wires; The insulating layer (2) includes a polyimide composite film layer (21), a first braided layer (22) and a first resin coating layer (23) that are tightly arranged from the inside and outside. The material of the first braided layer (22) is nano-quartz fiber yarn, and the outside of the nano-quartz fiber yarn is coated with an aluminum oxide coating. The sheath (30) includes a second braided layer (31) and a second resin coating layer (32) coated on the outside of the second braided layer (31). The second braided layer (31) includes a protective layer and a quartz fiber layer arranged from the inside out. The protective layer is formed by coating the outside of the shielding layer (20) with a blended slurry and then drying it. The blended slurry is prepared by the following process: silane is mixed with anhydrous ethanol, and then silane coupling agent, xylene and hydrochloric acid are added and reacted to obtain a precursor slurry. The precursor slurry is then mixed with carbon fiber powder and graphite powder to prepare the blended slurry. The quartz fiber layer is formed by weaving nano-quartz fiber yarn on the outside of the protective layer, and the outside of the nano-quartz fiber yarn is coated with an aluminum oxide coating. The alumina coating is used to isolate the interfacial reaction between the nano-quartz fiber yarn and the resin coating layer under high-temperature cycling conditions, thereby improving the mechanical properties of the wire.
2. The extreme high temperature resistant cycled wire for aerospace applications of claim 1, wherein: The number of insulated wire cores (10) is at least two.
3. The extreme high temperature resistant cycled wire for aerospace applications of claim 1, wherein: The conductor (1) contains 7-37 single-core copper wires; The single-core copper wire is silver-plated copper wire or nickel-plated copper wire; The diameter of the single-core copper wire is 0.10-0.45mm.
4. The aerospace-grade high-temperature cycling-resistant wire according to claim 1, characterized in that: The polyimide composite film layer (21) is formed by wrapping a polyimide composite film around the conductor (1). The polyimide composite film has two wrapping layers, and the wrapping directions of the two polyimide composite films are opposite. The polyimide composite film is prepared by laminating a high-temperature resistant material layer onto both sides of the polyimide film as a base film. The material of the high-temperature resistant material layer is polytetrafluoroethylene or polytetrafluoroethylene.
5. The aerospace-grade high-temperature cycling-resistant wire according to claim 1, characterized in that: The first woven layer (22) is formed by weaving nano-quartz fiber yarn on the outside of the polyimide composite film layer (21); The exterior of the nano-quartz fiber yarn is coated with an aluminum oxide coating by a plasma spraying machine. The alumina has a particle size of 50-100 μm.
6. The aerospace-grade high-temperature cycling-resistant wire according to claim 1, characterized in that: The first resin coating layer (23) and the second resin coating layer (32) are both made of nano-silicone resin; The particle size of the nano-silicone resin is 50-100 nm.
7. The aerospace-grade high-temperature cycling-resistant wire according to claim 1, characterized in that: The shielding layer (20) is made of nickel-plated copper wire with a braiding density of not less than 75% and a nickel plating layer thickness of not less than 0.2 μm.
8. The aerospace-grade high-temperature cycling-resistant wire according to claim 1, characterized in that: The protective layer is formed by coating the outside of the shielding layer (20) with a blended slurry and then drying it. The blended slurry is coated in 1-2 times, and drying is required after each coating of the blended slurry. The exterior of the nano-quartz fiber yarn is coated with an aluminum oxide coating by a plasma spraying machine. The alumina has a particle size of 50-100 μm.
9. The aerospace-grade high-temperature cycling-resistant wire according to claim 8, characterized in that, The preparation process of the blended slurry is as follows: Under an ice-water bath, silane and anhydrous ethanol are added to the reaction vessel and stirred for 1-2 hours. After stirring, silane coupling agent, xylene, and hydrochloric acid are added to the reaction vessel, the temperature is raised to 50-60°C, and stirring is continued for 1-2 hours. After standing and separating into layers, the acid water layer is removed to obtain a mixture. The mixture is then evaporated in a rotary evaporator for 4-6 hours to obtain a precursor slurry. The precursor slurry, carbon fiber powder, and graphite powder are placed in a magnetic stirrer and magnetically stirred for 2-6 hours to ensure uniform mixing, thus preparing a blended slurry.
10. An aerospace-grade high-temperature cycling-resistant wire according to claim 9, characterized in that, The mass ratio of silane, anhydrous ethanol, silane coupling agent, xylene, and hydrochloric acid added to the reaction vessel is 1:1.1-2.6:0.5-1.2:0.5-1.2:2.0-4.0; The hydrochloric acid concentration is 0.05-0.10 mmol / L; The mass ratio of the precursor slurry, carbon fiber powder, and graphite powder in the magnetic stirrer is 1:0.10-0.60:0.01-0.10; The silane includes any one or a combination of at least two of methyltrimethoxysilane, methyltriethoxysilane, tetramethyldivinylsilane, tetramethoxysilane, or tetramethyldivinyldisiloxane; The silane coupling agent includes any one of KH-550, KH-560 or KH-570.
Citation Information
Patent Citations
Carbon / carbon composite sealing material and its preparing method
CN1156167A
Compensating cable for high-temperature-resistant fireproof thermocouple and process of compensating cable
CN117079875A
High-temperature-resistant cable insulation structure
CN213366164U