A bi-2212 superconducting coil former

By creating T-shaped grooves and setting T-shaped bosses on the winding bobbin, the problem of wire end damage during the heat treatment of Bi-2212 superconducting coils was solved, enabling non-destructive bobbin replacement and copper electrode installation.

CN117894548BActive Publication Date: 2026-11-24HEFEI INSTITUTE OF PHYSICAL SCIENCE CHINESE ACADEMY OF SCIENCES
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202410090256.X
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-01-22
Publication Date
2026-11-24
Estimated Expiration
2044-01-22

AI Technical Summary

Technical Problem

During the heat treatment process, the ends of the Bi-2212 superconducting coil are easily damaged. Existing technology requires the replacement of the frame, which can easily cause damage. Furthermore, the copper electrodes cannot be heat treated together with the coil.

Method used

T-shaped grooves are made on the winding bobbin, and T-shaped bosses are set on the fixing joint and copper electrode, so that the fixing joint can be embedded in the groove during heat treatment to avoid damage to the wire end, and the copper electrode can be directly replaced after heat treatment.

Benefits of technology

It effectively protects the wire ends, preventing damage during heat treatment and bobbin replacement, simplifying the operation process and reducing the risk of coil damage.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117894548B_ABST
    Figure CN117894548B_ABST
Patent Text Reader

Abstract

This invention discloses a Bi-2212 superconducting coil frame, comprising a winding frame, a fixing connector, and copper electrodes. The winding frame has an inlet slot and an outlet slot at both ends, and T-shaped grooves at both ends. During heat treatment of the superconducting coil, the two ends of the winding frame are connected to the fixing connector. After heat treatment, the two ends of the winding frame are connected to the copper electrodes. The advantage of this invention is that by providing T-shaped grooves on the winding frame and first T-shaped bosses and second T-shaped bosses on the fixing connector and copper electrodes respectively, which can be embedded in the T-shaped grooves, the wire ends on the superconducting coil frame are not damaged during heat treatment or when the fixing connector is replaced with a copper electrode.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of superconducting coil technology, specifically to a Bi-2212 superconducting coil frame. Background Technology

[0002] In the late 20th century, Japanese scientists discovered the Bi-Sr-Ca-Cu-O system and found that different compositions and structures could yield three superconducting phases: Bi-2201, Bi-2212, and Bi-2223. Bi-2201 has a superconducting transition temperature of around 20K and is mainly used for research on high-temperature superconductivity mechanisms. Bi-2223 has a superconducting transition temperature of around 110K and exhibits some current-carrying capacity at 77K. However, due to limitations in superconducting imaging mechanisms, current technology can only fabricate Bi-2223 tapes.

[0003] Bi-2212, as a high-temperature superconducting material, possesses an extremely high upper critical field and maintains strong current-carrying capacity even under high background fields. Furthermore, Bi-2212 is an isotropic superconducting material, which is beneficial for the fabrication of cable-in-conduit conductors (CICC). Moreover, Bi-2212 is manufactured using the powder-in-tube (PIT) method, which is simple to produce, low in cost, and suitable for large-scale mass production. To date, Bi-2212 is the only high-temperature superconducting material that can be fabricated into isotropic multi-filament circular wires, making it the only feasible choice for magnets in future high-field fusion reactors and particle colliders. In addition, currently, medical and scientific magnets are primarily made of low-temperature superconducting materials; the circular wire structure of Bi-2212 means that these magnets can be replaced with Bi-2212, and its performance will be significantly improved.

[0004] Like most superconducting materials, Bi-2212 requires heat treatment to exhibit a superconducting phase. However, the heat treatment process for Bi-2212 differs significantly from other superconducting materials. It requires a high-temperature, high-pressure, and oxygen-rich environment with multiple temperature steps and a long treatment time. Bi-2212 typically uses a silver sheath as the matrix material, as silver is less expensive than other oxygen-permeable metals. At a heat treatment temperature of 884℃, the Bi-2212 powder melts into a liquid. Liquid Bi-2212 is highly corrosive, corroding the surrounding silver matrix. During recrystallization, the superconducting phase exhibits dendritic growth, and in severe cases, it can penetrate the matrix material, exposing itself to external substances and thus reducing its performance. Furthermore, the formation of the Bi-2212 superconducting phase requires a certain amount of oxygen doping. However, most metals readily react with each other at high temperatures, consuming oxygen in the heat treatment furnace. Copper, often used as a test electrode, not only consumes oxygen but also readily reacts with Bi-2212. Therefore, copper is generally not heat-treated together with Bi-2212. After heat treatment, the Bi-2212 core wire is in a ceramic state, so Bi-2212 coils are typically manufactured using a winding-then-reaction process. During low-temperature testing, the heat-treated coil requires connector electrodes to connect the current leads. Because oxygen-free copper has low resistance at low temperatures and is inexpensive, it is generally used as the connector electrode. However, copper cannot be heat-treated with the coil. Therefore, two types of frames are used in Bi-2212 heat treatment: one for heat treatment and one for testing. This means that after the coil is heat-treated, the two frames need to be exchanged. The winding frame is fixed, so only the fixed connector protecting the wire ends in the heat-treated frame needs to be replaced with a copper electrode. However, the ends of the superconducting coils after heat treatment are in a ceramic state and are easily damaged. Therefore, there is an urgent need for a superconducting coil frame that is not easily damaged. Summary of the Invention

[0005] The technical problem to be solved by this invention is how to prevent damage to the wire ends on the superconducting coil frame.

[0006] To solve the above-mentioned technical problems, the present invention provides the following technical solution: A Bi-2212 superconducting coil frame includes a winding frame, a fixing connector and a copper electrode. The winding frame has an inlet groove and an outlet groove at both ends, and T-shaped grooves are also formed at both ends of the winding frame. During the heat treatment of the superconducting coil, the two ends of the winding skeleton are respectively connected to the fixed joint. The fixed joint is provided with a first vertical groove that communicates with the inlet groove or outlet groove. The fixed joint is also provided with a first T-shaped boss that can be embedded in the T-shaped groove. After the superconducting coil is heat-treated, the two ends of the winding skeleton are respectively connected to the copper electrodes. The copper electrodes are provided with a second vertical wire groove that communicates with the wire inlet groove or the wire outlet groove. The copper electrodes are also provided with a second T-shaped boss that can be embedded in the T-shaped groove.

[0007] The present invention provides a T-shaped groove on the winding frame and a fixing connector, and a first T-shaped boss and a second T-shaped boss on the copper electrode that can be embedded in the T-shaped groove, so that the wire ends on the superconducting coil frame will not be damaged during heat treatment or when the fixing connector is replaced with a copper electrode.

[0008] Preferably, when winding a single-layer superconducting coil, the winding frame is also provided with a helical groove, the two ends of which are connected to the inlet groove and the outlet groove, respectively.

[0009] Preferably, the inlet slot and outlet slot are symmetrically arranged with the T-shaped groove along the center line of the winding skeleton.

[0010] Preferably, the top of the copper electrode has a chamfer.

[0011] Preferably, the inner wall of the T-shaped groove is also provided with a threaded hole.

[0012] Preferably, the second T-shaped boss is provided with a through hole that is coaxial with the threaded hole.

[0013] Preferably, the fixing joint is made of a non-copper material.

[0014] Preferably, the fixing joint is made of a nickel-based alloy.

[0015] Compared with the prior art, the beneficial effects of the present invention are: The present invention provides a T-shaped groove on the winding frame and a fixing connector, and a first T-shaped boss and a second T-shaped boss on the copper electrode that can be embedded in the T-shaped groove, so that the wire ends on the superconducting coil frame will not be damaged during heat treatment or when the fixing connector is replaced with a copper electrode. Attached Figure Description

[0016] Figure 1 This is a schematic diagram of the structure of a single-layer superconducting coil skeleton according to an embodiment of the present invention; Figure 2 This is another structural schematic diagram of a single-layer superconducting coil skeleton according to an embodiment of the present invention; Figure 3 This is a schematic diagram of the structure of a single-layer winding skeleton according to an embodiment of the present invention; Figure 4 This is a schematic diagram of the structure of the multilayer superconducting coil skeleton according to an embodiment of the present invention; Figure 5 This is another structural schematic diagram of the multilayer superconducting coil skeleton according to an embodiment of the present invention; Figure 6 This is a schematic diagram of the structure of a multi-layer winding skeleton according to an embodiment of the present invention. Detailed Implementation

[0017] To facilitate understanding of the technical solution of the present invention by those skilled in the art, the technical solution of the present invention will now be further described in conjunction with the accompanying drawings.

[0018] In this application, unless otherwise expressly specified and limited, the terms "installation," "connection," "linking," and "fixing," etc., should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral part; they can refer to a mechanical connection, an electrical connection, or a communication connection; they can refer to a direct connection or an indirect connection through an intermediate medium; they can refer to the internal communication of two components or the interaction between two components. Those skilled in the art can understand the specific meaning of the above terms in this application according to the specific circumstances.

[0019] In this application, unless otherwise expressly specified and limited, the terms "first" and "second" are used for descriptive purposes only and should not be construed as indicating or implying relative importance or implicitly specifying the number of indicated technical features. Thus, a feature defined as "first" or "second" may explicitly or implicitly include one or more of that feature. In the description of this application, "multiple" means two or more, unless otherwise expressly and specifically limited.

[0020] See Figures 1 to 6 This embodiment discloses a Bi-2212 superconducting coil skeleton, including a winding skeleton 1, a fixed connector 2 and a copper electrode 3. The winding skeleton 1 has an inlet groove 101 and an outlet groove 102 respectively at both ends. T-shaped grooves 11 are also formed at both ends of the winding skeleton 1, and threaded holes 12 are formed on the inner wall of the T-shaped grooves 11.

[0021] During the heat treatment of the superconducting coil, the two ends of the winding frame 1 are respectively connected to the fixed joint 2. The fixed joint 2 is provided with a first vertical wire groove 201 that communicates with the wire inlet groove 101 or the wire outlet groove 102. Both ends of the fixed joint 2 are provided with a first T-shaped boss 21 that can be embedded in the T-shaped groove 11. The wire inlet groove 101 and the wire outlet groove 102 are symmetrically arranged with the T-shaped groove 11 along the center line of the winding frame 1.

[0022] Furthermore, the fixing joint 2 is made of a non-copper material; in this embodiment, the fixing joint 2 is made of a nickel-based alloy.

[0023] After the superconducting coil is heat-treated, the two ends of the winding frame 1 are respectively connected to the copper electrode 3. The copper electrode 3 is provided with a second vertical wire groove 301 that communicates with the wire inlet groove 101 or the wire outlet groove 102. The copper electrode 3 is also provided with a second T-shaped boss 31 that can be embedded in the T-shaped groove 11. Furthermore, the second T-shaped boss 31 is provided with a through hole 311 that is coaxial with the threaded hole. Specifically, the copper electrode 3 is fixed on the winding frame 1 by bolts passing through the through hole 311 of the second T-shaped boss 31 and connecting to the threaded hole 12 in the T-shaped groove 11.

[0024] The top of the copper electrode 3 is chamfered to match the barrel test rod used in later testing.

[0025] Furthermore, when winding a single-layer superconducting coil, a spiral groove 103 is also provided on the winding frame 1. The two ends of the spiral groove 103 are respectively connected to the inlet groove 101 and the outlet groove 102 for fixing the single-layer superconducting coil.

[0026] The working principle of the single-layer superconducting coil frame is as follows: During winding, the wire is first wound into the spiral groove 103 on the winding frame 1, and the wire end extends out along the inlet groove 101 and outlet groove 102. Then, the first T-shaped protrusion 21 of the fixing connector 2 is moved into the T-shaped groove of the winding frame 1 in the direction of the wire end. Since the inlet groove 101 and outlet groove 102 are symmetrically arranged with the T-shaped groove 11 along the center line of the winding frame 1, after the first T-shaped protrusion 21 on the fixing connector 2 is engaged with the T-shaped groove 11, the wire end extending from the inlet groove 101 and outlet groove 102 is exactly located in the first vertical groove 201 of the fixing connector 2. During heat treatment, it is only necessary to wrap the silver wire wrapped with glass fiber cloth around the connection of the first T-shaped protrusion 21 once to ensure that the fixing connector 2 will not fall off in the opposite direction of the translation. After heat treatment, the wrapped silver wire is removed, and the fixing connector 2 is then moved out in the opposite direction. Next, replace the copper electrode 3, using the same method as connecting and fixing the connector 2. Simply slide it in towards the wire end, and then use a bolt to pass through the through hole 311 of the second T-shaped boss 31 and connect it to the threaded hole 12 in the T-shaped groove 11, thus fixing the copper electrode 3 onto the winding frame 1. The installed coil still needs to undergo curing treatment, which is not within the scope of this invention. During testing, simply insert the superconducting coil frame into the barrel test sample rod.

[0027] The working principle of the multilayer superconducting coil frame is as follows: When winding a multilayer coil, a single-layer coil should be selected as much as possible, so that the inlet slot 101 and outlet slot 102 are at both ends of the winding frame 1, which facilitates testing using a barrel test rod without the need for additional current leads. Since the inlet slot 101 and outlet slot 102 of the multilayer coil are not on the same cylindrical surface, slots of different depths are cut on the winding frame 1 for inlet and outlet respectively. Slots of the same size as the inlet slot 101 and outlet slot 102 on the winding frame 1 can be cut on the fixed connector 2 and the winding frame 1, respectively. Similarly, the steps for replacing the fixed connector 2 with the copper electrode 3 and the installation and testing steps are the same as the working principle of the single-layer superconducting coil frame described above.

[0028] The present invention provides a T-shaped groove 11 on the winding frame 1 and a first T-shaped boss 21 and a second T-shaped boss 31 that can be embedded in the T-shaped groove 11 on the fixing connector 2 and the copper electrode 3, so that the wire ends on the superconducting coil frame will not be damaged during heat treatment or when the fixing connector 2 is replaced with the copper electrode 3.

[0029] It will be apparent to those skilled in the art that the present invention is not limited to the details of the exemplary embodiments described above, and that the invention can be implemented in other specific forms without departing from its spirit or essential characteristics. Therefore, the embodiments should be considered illustrative and non-limiting in all respects, and the scope of the invention is defined by the appended claims rather than the foregoing description. Thus, all variations falling within the meaning and scope of equivalents of the claims are intended to be included within the present invention, and no reference numerals in the claims should be construed as limiting the scope of the claims.

[0030] The above embodiments are merely examples of implementation methods of the invention. The scope of protection of the present invention is not limited to the above embodiments. For those skilled in the art, several modifications and improvements can be made without departing from the concept of the present invention, and these all fall within the scope of protection of the present invention.

Claims

1. A Bi-2212 superconducting coil former, characterized by: It includes a winding frame, a fixed connector and copper electrodes. The winding frame has an inlet groove and an outlet groove at both ends, and T-shaped grooves are also formed at both ends of the winding frame. During the heat treatment of the superconducting coil, the two ends of the winding skeleton are respectively connected to the fixed joint. The fixed joint is provided with a first vertical groove that communicates with the inlet groove or outlet groove. The fixed joint is also provided with a first T-shaped boss that can be embedded in the T-shaped groove. After the superconducting coil is heat-treated, the two ends of the winding skeleton are respectively connected to the copper electrode. The copper electrode is provided with a second vertical groove that communicates with the inlet groove or outlet groove. The copper electrode is also provided with a second T-shaped boss that can be embedded in the T-shaped groove. Both the inlet and outlet slots are symmetrically arranged with the T-shaped groove along the center line of the winding skeleton.

2. A Bi-2212 superconducting coil former according to claim 1, characterised in that: When winding a single-layer superconducting coil, a helical groove is also provided on the winding frame, and the two ends of the helical groove are respectively connected to the inlet groove and the outlet groove.

3. The Bi-2212 superconducting coil frame according to claim 1, characterized in that: The top of the copper electrode has a chamfer.

4. The Bi-2212 superconducting coil frame according to claim 1, characterized in that: The inner wall of the T-shaped groove is also provided with threaded holes.

5. The Bi-2212 superconducting coil frame according to claim 4, characterized in that: The second T-shaped boss is provided with a through hole that is coaxial with the threaded hole.

6. The Bi-2212 superconducting coil frame according to claim 1, characterized in that: The fixed joint is made of a non-copper material.

7. A Bi-2212 superconducting coil frame according to claim 6, characterized in that: The fixed joint is made of a nickel-based alloy.

Citation Information

Patent Citations

  • Bayonet type metal superconductive magnet framework and manufacturing method thereof

    CN103065756A

  • Superconducting coil and superconducting magnet device

    JP2004319777A