A method for preparing a mammalian plastinated specimen

By dehydrating, degreasing, vacuum impregnating, and curing the fur and bone materials of mammal specimens, the problem of unrealistic appearance caused by imperfect fur treatment is solved, and lifelike plastinated specimens are prepared, which are suitable for museum preservation and teaching.

CN117898281BActive Publication Date: 2026-11-24HENAN ZHONGBO TECH CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202311748997.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-12-19
Publication Date
2026-11-24
Estimated Expiration
2043-12-19

AI Technical Summary

Technical Problem

Existing mammal specimens are not realistic in appearance due to imperfect fur treatment, making them inconvenient for observation and display.

Method used

By employing steps such as dehydration and degreasing, vacuum impregnation, and curing, the fur and bone specimen materials of mammals are separated and plasticized to make the fur soft and attached to the bone, forming a lifelike specimen.

Benefits of technology

The prepared mammalian plastinated specimens have soft fur, complete structure, and strong realism, making them easy to observe and display, and suitable for museum preservation and teaching.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117898281B_ABST
    Figure CN117898281B_ABST
Patent Text Reader

Abstract

This invention relates to the field of plastination technology, specifically to a method for preparing plastinated mammal specimens. The method involves separating the fur and bones of a mammal specimen, then plastinizing each separately. After plastination, the fur is cleaned to maintain its softness. The cleaned fur is then applied to the plastinated bones and flesh, and finally cured, resulting in a more realistic plastinated mammal specimen. The mammal specimens prepared using this method are made from real animal fur. The animal's fur, supported by muscles and bones, retains its shape and structure without alteration, exhibiting a strong sense of realism. This facilitates later specimen observation and is convenient to use. It can be used for pet preservation and display by the general public, for the preservation and display of special specimens in museums, and for teaching and learning by teachers and students in animal husbandry colleges.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of bioplasticization technology, specifically to a method for preparing a mammalian morphological plastinated specimen. Background Technology

[0002] Currently, the mammal specimens commonly used in school teaching and learning include: model specimens, taxidermy specimens, and specimens preserved in formalin bottles. Model specimens have a simple structure, but there is a certain deviation between teaching and real specimens, and they cannot show the true structure of the specimen. Tranquilization specimens have a complex preparation process, which is not easy to control. The specimens are easily damaged, the skeleton cannot be preserved, the grease is not easy to remove, and they are prone to insects and mold. They cannot be preserved for a long time. Formalin-preserved specimens have great limitations. They can only preserve small animals, are not easy to preserve, are easily damaged, and are not aesthetically pleasing.

[0003] The application of plastination technology in the field of biological anatomy specimens has a history of nearly 20 years. The plastination technology is a technique that replaces the water in organs and tissues with a mixture of liquid silicone resin, which can preserve the tissues permanently. Biological plastinated specimens produced using plastination technology have advantages such as being non-toxic, odorless, long-term preservation, easy to use, and able to be stored in the air for a long time.

[0004] Currently, plastination technology is mainly applied to muscles, blood vessels, and the combination of bones and muscles. This involves plastinating the entire organism to reveal the position and adjacent relationships of various organs and structures. However, the animal's fur is not displayed during this process because existing methods for processing fur are inadequate. The resulting fur specimens often have hard skin and insufficiently soft hair, making the specimens less lifelike. Therefore, a method for preparing mammalian plastination specimens that can make animal fur softer, resulting in more realistic plastination specimens that are easier to observe and display later, is a pressing problem that needs to be solved. Summary of the Invention

[0005] The purpose of this invention is to provide a method for preparing plastinated mammalian specimens, in order to solve the problem that existing mammalian specimens are not realistic in appearance due to imperfect fur treatment, thus making them inconvenient to observe and display.

[0006] To achieve the above objectives, the present invention adopts the following technical solution: a method for preparing a mammalian plastinated specimen, comprising the following steps: S1. Material selection and corrosion prevention; S2, Anatomy The specimen material treated with S1 was cut along the midline of the chest and abdomen, and the skin and superficial fascia were separated. Then the skin was peeled off to obtain the skin and bone specimen material after peeling. Remove fat and fascia from the fur and bone specimen materials, and freeze-dry the fur for later use; The internal organs of the bone and flesh specimen were completely removed, and then bleached. After bleaching, the bone and flesh specimen was sutured back to its original position along the incision with surgical sutures. S3. The fur and bone specimen materials obtained in S2 are sequentially dehydrated and degreased, vacuum impregnated, shaped and cleaned to obtain plasticized fur and bone specimen materials. S4. Clean the fur obtained in S3. S41. Use dimethyl silicone oil liquid silicone thinner to clean off excess silicone from the fur. S42. Soak the cleaned fur in D80 solvent oil for 3-5 days, then allow the kerosene to evaporate completely at room temperature, and comb the fur clean. S43. Soak the fur obtained in S42 in D80 solvent oil again for 2-3 days, and then let the kerosene evaporate completely at room temperature. Then comb the fur to make it naturally and neatly. S5, Reset The fur processed in S4 was fixed onto the plastinated bone and flesh specimen material obtained in S3, and the fur was sutured along the original incision. S6, Curing The specimen obtained in S5 was placed in a curing chamber. The first silicone curing agent was injected into the deep muscle layer of the plastinated bone and flesh specimen material to cure the silicone mixture. Then, the vapor of the second silicone curing agent was used to steam the specimen to cure it as a whole.

[0007] Furthermore, in S1, a complete mammalian carcass without external injury, fracture, or lesion is selected as the specimen material.

[0008] Furthermore, in S1, the animal specimen is perfused with formalin at a volume concentration of 15-20%, and the formalin is permeated to various parts of the specimen through the femoral artery and common carotid artery. After perfusion, the animal specimen is immersed in formalin at a volume concentration of 8-10% for 3-4 months to achieve preservation.

[0009] Furthermore, in step S2, the detached bone and flesh specimen material is bleached in a hydrogen peroxide solution with a mass concentration of 10-15% for 2-3 days.

[0010] Furthermore, in step S3, the fur and bone specimen materials are soaked in acetone solution for 80-90 days to obtain dehydrated and degreased specimen materials.

[0011] Furthermore, in S3, the dehydration and degreasing temperature is -25 to -20°C; the initial mass concentration of the acetone solution is 65 to 75%, which is gradually increased to 95 to 98% and then soaked for 14 to 21 days; during the dehydration and degreasing process, the acetone solution is replaced every two weeks.

[0012] Furthermore, in step S3, the dehydrated and degreased specimen material is placed in a silica gel mixture in a vacuum pressure chamber and left to stand for 60-70 days. During the standing period, the pressure of the vacuum pressure chamber is adjusted from 0.1 kPa to 1.5 kPa. The silica gel mixture is squeezed into the dehydrated and degreased specimen to displace the acetone solution, thus obtaining the impregnated specimen.

[0013] Further, in S3, the silicone mixture includes 100 parts by weight of silicone, 2 to 10 parts by weight of silicone vulcanizing agent C-14 accelerator, and 1 to 5 parts by weight of silane coupling agent curing agent.

[0014] Furthermore, in step S3, the specimen that has been soaked is removed from the silicone and shaped according to the required form; excess silicone and burrs on the muscles and bones are cleaned with a knife.

[0015] Furthermore, in S6, the curing time is 10-15 days, the curing temperature is 40-50°C, the first silicone curing agent is a silicone coupling agent, and the second silicone curing agent is propyl orthosilicate.

[0016] The beneficial effects of this invention are: 1. This invention involves peeling off the fur from mammal specimens and then using methods such as dehydration and degreasing, vacuum impregnation, and curing to plasticize and shape the muscles. The operation is relatively simple and the reagent cost is low. 2. The mammalian morphological plastinated specimen of the present invention is made from real animal fur. The animal fur is based on muscles and bones, and its shape and structure are intact and unchanged, with a strong sense of realism, which is conducive to the later observation of the specimen. Moreover, it is relatively convenient to use and can be used for the preservation and display of pets by the general public, the preservation and display of special specimens in museums, and teaching and learning by teachers and students in animal husbandry colleges. 3. The mammalian fur plastinated specimens of the present invention are non-toxic and odorless, easy to preserve for a long time, can be reused many times, and do not harm the health of users. Attached Figure Description

[0017] Figure 1 This is a plastinated specimen of a wolf from Embodiment 1 of the present invention; Figure 2 This is a plasticized specimen of an alpaca from Embodiment 2 of the present invention; Figure 3 This is a diagram of the plastinated horse specimen from Embodiment 3 of the present invention. Detailed Implementation

[0018] The technical solutions of the present invention will be clearly and completely described below with reference to the accompanying drawings in the embodiments of the present invention.

[0019] The principle of this invention is as follows: Select intact mammal carcasses without external injuries, fractures, or lesions as specimen materials. After preservation treatment, separate the fur and flesh from the bones and flesh of the specimens.

[0020] For preservation, formalin with a volume concentration of 15-20% is injected into the specimen. Formalin is then permeated into various parts of the specimen through the femoral artery and common carotid artery. After perfusion, the animal specimen is immersed in formalin with a volume concentration of 8-10% for 3-4 months. The fur of the preserved specimen is then peeled off to obtain the fur specimen material and the bone and flesh specimen material.

[0021] After cleaning the specimen materials obtained above, the fur and flesh are subjected to plasticization treatment. The plasticization process includes steps such as dehydration and degreasing, vacuum impregnation, shaping and cleaning. Since these are existing and mature technologies, they will not be described in detail here.

[0022] Clean the plasticized fur, removing the silicone from the fur. First, use dimethyl silicone oil liquid silicone thinner to clean off the excess silicone from the fur. Then, soak the cleaned fur in D80 solvent oil for 3-5 days. After that, allow the kerosene to evaporate completely at room temperature. Use a comb to clean the fur. Finally, soak the fur obtained from S42 in D80 solvent oil again for 2-3 days. After that, allow the kerosene to evaporate completely at room temperature again. Use a comb to comb the fur naturally and neatly.

[0023] The cleaned fur is then placed over the bone and flesh specimen, and then cured. A silicone coupling agent is injected into the deep muscle layer of the plastinated bone and flesh specimen material to cure the silicone mixture. Finally, the specimen is cured by steaming with propyl orthosilicate vapor.

[0024] The method of this invention produces mammalian plastinated specimens with soft fur that adheres to the mammal's bones and flesh, making the specimens more vivid and lifelike. This facilitates later specimen observation and allows for observation of the internal structure of the mammal's body. It also makes it convenient for museums to preserve and display special specimens, as well as for teaching by teachers and learning by students in animal husbandry colleges.

[0025] Example 1 S1. Select complete wolf carcasses without external injuries, fractures, or lesions as specimen materials and preserve them with formalin solution; S2, Anatomy The wolf specimen material, which had been treated with S1 preservatives, was cut open along the middle of the chest and abdomen. The fur and superficial fascia were separated, and then the fur was peeled off to obtain the stripped fur and bone specimen material. Remove fat and fascia from the fur and bone specimen materials, and freeze-dry the fur for later use; The internal organs of the bone and flesh specimen were completely removed, and then bleached with hydrogen peroxide solution. After bleaching, the bone and flesh specimen was sutured back to its original position along the incision with surgical sutures. S3. The fur and bone specimen materials obtained in S2 are sequentially dehydrated and degreased, vacuum impregnated, shaped and cleaned to obtain plasticized fur and bone specimen materials. S4. Clean the fur obtained in S3. S41. Use dimethyl silicone oil liquid silicone thinner to clean off excess silicone from the fur. S42. Soak the cleaned fur in D80 solvent oil for 3-5 days, then allow the kerosene to evaporate completely at room temperature, and comb the fur clean. S43. Soak the fur obtained in S42 in D80 solvent oil again for 2-3 days, and then let the kerosene evaporate completely at room temperature. Then comb the fur to make it naturally and neatly. S5, Reset The fur processed in S4 was fixed onto the plastinated bone and flesh specimen material obtained in S3, and the fur was sutured along the original incision. S6, Curing The specimen obtained from S5 was placed in a curing chamber, and a silicone coupling agent was injected into the deep muscle layer of the plastinated bone and flesh specimen material to cure the silicone mixture. Then, the specimen was cured by steaming with propyl orthosilicate vapor.

[0026] The plastinated wolf specimen prepared in this embodiment is shown in the attached figure. Figure 1 As shown.

[0027] Example 2 S1. Select complete alpaca carcasses without external injuries, fractures, or lesions as specimen materials and treat them with formalin solution for preservation. S2, Anatomy The wolf specimen material, which had been treated with S1 preservatives, was cut open along the middle of the chest and abdomen. The fur and superficial fascia were separated, and then the fur was peeled off to obtain the stripped fur and bone specimen material. Remove fat and fascia from the fur and bone specimen materials, and freeze-dry the fur for later use; The internal organs of the bone and flesh specimen were completely removed, and then bleached with hydrogen peroxide solution. After bleaching, the bone and flesh specimen was sutured back to its original position along the incision with surgical sutures. S3. The fur and bone specimen materials obtained in S2 are sequentially dehydrated and degreased, vacuum impregnated, shaped and cleaned to obtain plasticized fur and bone specimen materials. S4. Clean the fur obtained in S3. S41. Use dimethyl silicone oil liquid silicone thinner to clean off excess silicone from the fur. S42. Soak the cleaned fur in D80 solvent oil for 3-5 days, then allow the kerosene to evaporate completely at room temperature, and comb the fur clean. S43. Soak the fur obtained in S42 in D80 solvent oil again for 2-3 days, and then let the kerosene evaporate completely at room temperature. Then comb the fur to make it naturally and neatly. S5, Reset The fur processed in S4 was fixed onto the plastinated bone and flesh specimen material obtained in S3, and the fur was sutured along the original incision. S6, Curing The specimen obtained from S5 was placed in a curing chamber, and a silicone coupling agent was injected into the deep muscle layer of the plastinated bone and flesh specimen material to cure the silicone mixture. Then, the specimen was cured by steaming with propyl orthosilicate vapor.

[0028] The plastinated wolf specimen prepared in this embodiment is shown in the attached figure. Figure 2 As shown.

[0029] Example 3 S1. Select complete horse carcasses without external injuries, fractures, or lesions as specimen materials and treat them with formalin solution for preservation. S2, Anatomy The wolf specimen material, which had been treated with S1 preservatives, was cut open along the middle of the chest and abdomen. The fur and superficial fascia were separated, and then the fur was peeled off to obtain the stripped fur and bone specimen material. Remove fat and fascia from the fur and bone specimen materials, and freeze-dry the fur for later use; The internal organs of the bone and flesh specimen were completely removed, and then bleached with hydrogen peroxide solution. After bleaching, the bone and flesh specimen was sutured back to its original position along the incision with surgical sutures. S3. The fur and bone specimen materials obtained in S2 are sequentially dehydrated and degreased, vacuum impregnated, shaped and cleaned to obtain plasticized fur and bone specimen materials. S4. Clean the fur obtained in S3. S41. Use dimethyl silicone oil liquid silicone thinner to clean off excess silicone from the fur. S42. Soak the cleaned fur in D80 solvent oil for 3-5 days, then allow the kerosene to evaporate completely at room temperature, and comb the fur clean. S43. Soak the fur obtained in S42 in D80 solvent oil again for 2-3 days, and then let the kerosene evaporate completely at room temperature. Then comb the fur to make it naturally and neatly. S5, Reset The fur processed in S4 was fixed onto the plastinated bone and flesh specimen material obtained in S3, and the fur was sutured along the original incision. S6, Curing The specimen obtained from S5 was placed in a curing chamber, and a silicone coupling agent was injected into the deep muscle layer of the plastinated bone and flesh specimen material to cure the silicone mixture. Then, the specimen was cured by steaming with propyl orthosilicate vapor.

[0030] The plastinated wolf specimen prepared in this embodiment is shown in the attached figure. Figure 3 As shown.

[0031] This invention is not limited to the preferred embodiments described above. Anyone can derive other forms of products under the guidance of this invention. However, regardless of any changes made in their shape or structure, any technical solution that is the same as or similar to this application falls within the protection scope of this invention.

Claims

1. A method for preparing a mammalian plastinated specimen, characterized in that, Includes the following steps: S1. Material selection and corrosion prevention; S2, Anatomy The specimen material treated with S1 was cut along the midline of the chest and abdomen, and the skin and superficial fascia were separated. Then the skin was peeled off to obtain the skin and bone specimen material after peeling. Remove fat and fascia from the fur and bone specimen materials, and freeze-dry the fur for later use; The internal organs of the bone and flesh specimen were completely removed, and then bleached. After bleaching, the bone and flesh specimen was sutured back to its original position along the incision with surgical sutures. S3. The fur and bone specimen materials obtained in S2 are sequentially dehydrated and degreased, vacuum impregnated, shaped and cleaned to obtain plasticized fur and bone specimen materials. S4. Clean the fur obtained in S3. S41. Use dimethyl silicone oil liquid silicone thinner to clean off excess silicone from the fur. S42. Soak the cleaned fur in D80 solvent oil for 3-5 days, then allow the D80 solvent oil to evaporate completely at room temperature, and comb the fur clean. S43. Soak the fur obtained in S42 in D80 solvent oil again for 2-3 days, and then let the D80 solvent oil evaporate completely at room temperature. Then comb the fur to make it naturally and neatly. S5, Reset The fur processed in S4 was fixed onto the plastinated bone and flesh specimen material obtained in S3, and the fur was sutured along the original incision. S6, Curing The specimen obtained in S5 was placed in a curing chamber. The first silicone curing agent was injected into the deep muscle layer of the plastinated bone and flesh specimen material to cure the silicone mixture. Then, the vapor of the second silicone curing agent was used to steam the specimen to cure it as a whole.

2. The method for preparing a mammalian plastinated specimen according to claim 1, characterized in that: In S1, a complete mammalian carcass without external injury, fracture, or lesion is selected as the specimen material.

3. The method for preparing a mammalian plastinated specimen according to claim 1, characterized in that: In step S1, the animal specimen is perfused with formalin at a volume concentration of 15-20%. Formalin is then permeated into various parts of the specimen through the femoral artery and common carotid artery. After perfusion, the animal specimen is immersed in formalin at a volume concentration of 8-10% for 3-4 months to achieve preservation.

4. The method for preparing a mammalian plastinated specimen according to claim 1, characterized in that: In step S2, the detached bone and flesh specimen material is bleached in a hydrogen peroxide solution with a mass concentration of 10-15% for 2-3 days.

5. The method for preparing a mammalian plastinated specimen according to claim 1, characterized in that: In step S3, the fur and bone specimen materials are soaked in acetone solution for 80-90 days to obtain dehydrated and degreased specimen materials.

6. The method for preparing a mammalian plastinated specimen according to claim 5, characterized in that: In step S3, the dehydration and degreasing temperature is -25 to -20°C; the initial mass concentration of the acetone solution is 65 to 75%, which is gradually increased to 95 to 98% and then soaked for 14 to 21 days; during the dehydration and degreasing process, the acetone solution is replaced every two weeks.

7. The method for preparing a mammalian plastinated specimen according to claim 5, characterized in that: In step S3, the dehydrated and degreased specimen material is placed in a silica gel mixture in a vacuum pressure chamber and left to stand for 60-70 days. During the standing period, the pressure of the vacuum pressure chamber is adjusted from 0.1 kPa to 1.5 kPa. The silica gel mixture is squeezed into the dehydrated and degreased specimen to displace the acetone solution, thus obtaining the impregnated specimen.

8. The method for preparing a mammalian plastinated specimen according to claim 7, characterized in that: In S3, the silicone mixture includes 100 parts by weight of silicone, 2 to 10 parts by weight of silicone curing agent C-14 accelerator, and 1 to 5 parts by weight of silane coupling agent curing agent.

9. The method for preparing a mammalian plastinated specimen according to claim 7, characterized in that: In step S3, the specimen that has been soaked is removed from the silicone and shaped according to the required form; excess silicone and burrs on the muscles and bones are cleaned with a knife.

10. The method for preparing a mammalian plastinated specimen according to claim 1, characterized in that: In S6, the curing time is 10-15 days, the curing temperature is 40-50℃, the first silicone curing agent is a silicone coupling agent, and the second silicone curing agent is propyl orthosilicate.

Citation Information

Patent Citations

  • Animal muscle plasticizing specimen and preparing method thereof

    CN109619086A

  • Manufacturing method of plasticized specimen of endangered wild animal