一种岩土固化用矿物掺合料及其制备方法

By mixing and grinding modified steel slag and phosphorus slag with slag, cement clinker and grinding aids, the problems of low early strength and poor water stability of cement solidification materials are solved, achieving efficient and environmentally friendly soil and rock solidification effect, which is suitable for in-situ solidification of tunnel slag in highway construction.

CN117923830BActive Publication Date: 2026-07-17GUIZHOU HIGHWAY ENG GRP

Patent Information

Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
GUIZHOU HIGHWAY ENG GRP
Filing Date
2024-01-19
Publication Date
2026-07-17

AI Technical Summary

Technical Problem

Existing soil and rock solidification materials such as cement have problems such as large drying shrinkage, easy cracking, poor water stability, and insufficient impermeability. Furthermore, industrial by-products such as steel slag and phosphorus slag have low early strength and high expansion when directly applied, making it difficult to meet the engineering durability requirements.

Method used

Mineral admixtures are prepared by mixing modified steel slag and phosphorus slag with slag, cement clinker and grinding aids, and then grinding them. The modification treatment improves the compatibility and hydration activity of steel slag and phosphorus slag, reduces the expansion rate, and enhances early strength and water stability.

Benefits of technology

It significantly improves the early strength and water stability of soil and rock solidification materials, reduces transportation costs, and achieves efficient on-site solidification of tunnel excavated soil, possessing good engineering performance and environmental benefits.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_1
    Figure SMS_1
Patent Text Reader

Abstract

本发明属于岩土固化技术领域,涉及一种岩土固化用矿物掺合料及其制备方法。将矿物原料混合,然后加入助磨添加剂,随后转入粉磨装置中进行粉磨,得到岩土固化用矿物掺合料;所述助磨添加剂用量为矿物原料的0.2%~0.3%;按照重量份数计算,所述矿物原料包括如下组分:矿渣20%~30%;改性钢渣25%~35%;改性磷渣5%~10%;二水石膏2%~5%;余量为水泥熟料。本发明通过对磷渣和钢渣分别改性,首先通过粒径较小的钢渣微粉嵌设磷渣的空隙,再通过粒径较小的磷渣微粉嵌合钢渣的空隙,最后将其混合粉磨,提高矿物原料的混合均匀性,提高矿物掺合料的作用效果。