A membrane electrode structure
By introducing a structure combining a breathable membrane and a silicone rubber coating into the membrane electrode, and designing drainage holes and a grid pad, the problem of water flooding during membrane electrode operation was solved, enabling rapid water discharge and improved electrochemical reaction efficiency.
Patent Information
- Application Number
- CN202410181399.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-02-18
- Publication Date
- 2026-11-20
- Estimated Expiration
- 2044-02-18
AI Technical Summary
In existing membrane electrodes, water is difficult to drain in time during operation, leading to flooding and affecting battery reaction efficiency.
The structure adopts a combination of a breathable membrane and a silicone rubber coating. The breathable membrane is located on both sides of the catalyst-coated proton exchange membrane, and the silicone rubber coating is provided with drainage holes. Water between the breathable membrane and the catalyst-coated proton exchange membrane flows back to the gas outlet side of the first gas diffusion layer through the drainage holes. Combined with the grid pad and drainage hole design, the rapid discharge of water is promoted.
It effectively reduces the impact of water on airflow, increases airflow velocity, ensures rapid water discharge, and enhances the efficiency of electrochemical reactions.
Smart Images

Figure CN118016939B_ABST
Abstract
Description
Technical Field
[0001] This application relates to the field of fuel cells, and in particular to a membrane electrode structure. Background Technology
[0002] Fuel cells are considered an important green energy technology because they can directly convert chemical energy into electrical energy through electrochemical reactions. The membrane electrode assembly (MEA) is the most crucial component of a fuel cell. As the site of the electrochemical reaction, the MEA plays a key role, and its characteristics directly determine the overall performance of the fuel cell. Currently, the MEA is composed of a catalyst-coated proton exchange membrane, a catalyst, an electronic conductor, and a gas diffusion layer.
[0003] In a fuel cell, membrane electrode assemblies (MEAs) are stacked alternately with bipolar plates, with each MEA located between two adjacent bipolar plates. Gas channels are provided on both sides of each bipolar plate. During operation, air and hydrogen flow to opposite sides of the catalyst-coated proton exchange membrane. Air and hydrogen are guided by the gas channels on opposite sides of the adjacent bipolar plates, while air is diffused by a first gas diffusion layer, and hydrogen by a second gas diffusion layer.
[0004] In the existing membrane electrode assembly (MEA) technology, water is continuously generated on the cathode side of the MEA during operation of the fuel cell. If the water cannot be drained in time, flooding will occur, and the water will cover the membrane surface, blocking the reaction and thus reducing the battery reaction efficiency. Summary of the Invention
[0005] In order to reduce the problem of water being difficult to drain in time during the operation of the membrane electrode, which affects the battery reaction efficiency, this application provides a membrane electrode structure.
[0006] The membrane electrode structure provided in this application adopts the following technical solution: A membrane electrode structure includes a catalyst-coated proton exchange membrane, a first gas diffusion layer, a second gas diffusion layer, and a permeable membrane. The first gas diffusion layer and the second gas diffusion layer are located on opposite sides of the catalyst-coated proton exchange membrane, and the permeable membrane is located between the first gas diffusion layer and the catalyst-coated proton exchange membrane. A silicone rubber coating is provided on the side of the permeable membrane away from the first gas diffusion layer. The silicone rubber coating has drainage holes, which are located near the gas outlet side of the first gas diffusion layer.
[0007] By adopting the above technical solution, during membrane electrode operation, air and hydrogen flow to opposite sides of the catalyst-coated proton exchange membrane under the guidance of the gas flow channel. Hydrogen and oxygen react on the side of the catalyst-coated proton exchange membrane closer to the first gas diffusion layer to form water. During this process, as air diffuses along the first gas diffusion layer, some of it passes through the water-permeable membrane and the silicone rubber coating on its surface, reaching the area between the water-permeable membrane and the catalyst-coated proton exchange membrane. In this area, it reacts to form water. The silicone rubber coating has high selectivity for water, allowing it to remain between the water-permeable membrane and the catalyst-coated proton exchange membrane. The water between these membranes then flows back to the outlet side of the first gas diffusion layer through the drain hole, allowing it to be quickly discharged from the membrane electrode under the pressure difference of the air. During membrane electrode operation, air is mainly distributed on the side of the first gas diffusion layer away from the catalyst-coated proton exchange membrane, which helps reduce the influence of water on air flow, increases air velocity, and enables the rapid removal of water from the membrane electrode.
[0008] Optionally, a third gas diffusion layer is provided between the permeable membrane and the catalyst-coated proton exchange membrane.
[0009] By employing the above technical solution, the third gas diffusion layer can conduct air that has passed through the permeable membrane, promoting the electrochemical reaction. Furthermore, the third gas diffusion layer can reduce the probability of water contacting the catalyst-coated proton exchange membrane, allowing the catalyst on the proton exchange membrane to exert its catalytic effect to the fullest extent, thereby improving the efficiency of the electrochemical reaction.
[0010] Optionally, the thickness of the first gas diffusion layer is less than the thickness of the third gas diffusion layer.
[0011] By adopting the above technical solution, the first gas diffusion layer and the third gas diffusion layer are disposed on the same side of the catalyst-coated proton exchange membrane. Both the first gas diffusion layer and the third gas diffusion layer are used to diffuse air. It is necessary to control the total thickness of the two layers. By making the thickness of the first gas diffusion layer smaller than the thickness of the third gas diffusion layer, it is beneficial to make it easier for air to diffuse from the first gas diffusion layer to the permeable membrane.
[0012] Optionally, the breathable membrane is a polysulfone membrane or a polyethersulfone membrane.
[0013] By adopting the above technical solutions, polysulfone membranes and polyethersulfone membranes have good mechanical properties and high temperature resistance, and can better adapt to the high temperature environment during fuel cell operation.
[0014] Optionally, the breathable membrane is provided with a grid pad on the side away from the first gas diffusion layer. The grid pad has grid holes arranged in a single row. The length direction of the grid holes is the same as the overall gas diffusion direction of the first gas diffusion layer, and the arrangement direction of adjacent grid holes is perpendicular to the length direction of the grid holes. The drainage holes of the breathable membrane are located within the distribution range of the grid holes of the grid pad.
[0015] By adopting the above technical solution, the grid pad occupies the space between the breathable membrane and the third gas diffusion layer. The space of the grid holes of the grid pad can serve as a drainage channel, which helps to accelerate the flow and discharge of water between the breathable membrane and the third gas diffusion layer.
[0016] Optionally, the width of the grille openings gradually increases along the direction close to the drain hole.
[0017] By adopting the above technical solution, the water between the breathable membrane and the third gas diffusion layer flows towards the drain hole, and the width of the grid holes gradually increases along the direction of the drain hole, so that the resistance of water flow gradually decreases, which is conducive to promoting drainage.
[0018] Optionally, the drainage hole is an elongated hole, and the length direction of the elongated hole is arranged along the arrangement direction of the grid holes of the grid pad.
[0019] By adopting the above technical solution, the drainage hole is set as an elongated hole. Under the premise that the area of the exhaust hole is fixed, the drainage hole can be concentrated as close as possible to the exhaust side of the first gas diffusion layer, which is conducive to improving drainage efficiency.
[0020] Optionally, the silicone rubber coating has an air inlet on the side near the air inlet side of the first gas diffusion layer. There are multiple air inlets, and the arrangement direction of the multiple air inlets is the same as the arrangement direction of the grid holes of the grid pad. Each air inlet corresponds to one grid hole.
[0021] By adopting the above technical solution, during the process of air passing through the breathable membrane and the silicone rubber coating, the position of the silicone rubber coating corresponding to the air inlet is not covered by the silicone rubber coating, which makes the air flow speed larger and the air pressure relatively larger. This helps to form a thrust on the water between the breathable membrane and the third gas diffusion layer towards the drain hole, which is beneficial to further improve the drainage efficiency between the breathable membrane and the third gas diffusion layer.
[0022] Optionally, the grid pad is bonded and fixed to the breathable membrane by the silicone rubber coating.
[0023] By adopting the above technical solution, the grating pad is bonded and fixed to the breathable membrane through a silicone rubber coating, making the grating pad and the breathable membrane a whole, which facilitates assembly. Furthermore, using a silicone rubber coating to bond the grating pad and the breathable membrane eliminates the need for a special adhesive, saving processing steps.
[0024] Optionally, the grid pad is provided with a border-shaped indentation strip around its perimeter, and the thickness of the silicone rubber coating in the area corresponding to the indentation strip is greater than the thickness in the other areas.
[0025] By adopting the above technical solution, when the silicone rubber coating is bonded to the grid pad on the breathable membrane, the thickness of the silicone rubber coating in the area corresponding to the indentation of the grid pad is greater, which helps to seal the gap space between the first gas diffusion layer and the third gas diffusion layer.
[0026] In summary, this application includes at least one of the following beneficial technical effects: 1. When the membrane electrode is working, during the diffusion of air along the first gas diffusion layer, some of the water passes through the water-permeable membrane and the silicone rubber coating on the surface of the water-permeable membrane and reaches the area between the water-permeable membrane and the catalyst-coated proton exchange membrane. In this area, water is formed by reaction. The silicone rubber coating has high selectivity for water, which can keep the water between the water-permeable membrane and the catalyst-coated proton exchange membrane. The water between the water-permeable membrane and the catalyst-coated proton exchange membrane then flows back to the gas outlet side of the first gas diffusion layer through the drain hole, so that the water is discharged from the membrane electrode as soon as possible under the action of air pressure difference.
[0027] 2. The grid pad occupies the space between the breathable membrane and the third gas diffusion layer. The space of the grid holes in the grid pad can serve as a drainage channel, which helps to accelerate the flow and discharge of water between the breathable membrane and the third gas diffusion layer. Attached Figure Description
[0028] Figure 1 This is a schematic diagram of the membrane electrode structure in this embodiment.
[0029] Figure 2 This is a schematic diagram used in this embodiment to illustrate the connection relationship between the first diffusion layer and the third diffusion layer.
[0030] Figure 3 yes Figure 2 A magnified view of point A in the middle.
[0031] Explanation of reference numerals in the attached figures: 1. Catalyst-coated proton exchange membrane; 11. Mounting frame; 2. First gas diffusion layer; 21. Outlet side; 3. Second gas diffusion layer; 4. Third gas diffusion layer; 5. Permeable membrane; 51. Silicone rubber coating; 511. Drain hole; 512. Inlet hole; 6. Grille pad; 61. Grille hole; 62. Drainage channel; 63. Indentation strip; 7. Seal. Detailed Implementation
[0032] The following is in conjunction with the appendix Figure 1-3 This application will be described in further detail.
[0033] This application discloses a membrane electrode structure. (Refer to...) Figure 1 The membrane electrode structure includes a catalyst-coated proton exchange membrane 1, a first gas diffusion layer 2, a second gas diffusion layer 3, a third gas diffusion layer 4, and a permeable membrane 5. The catalyst-coated proton exchange membrane 1 is provided with a mounting frame 11. The first gas diffusion layer 2 and the second gas diffusion layer 3 are located on both sides of the catalyst-coated proton exchange membrane 1, respectively. The first gas diffusion layer 2 and the second gas diffusion layer 3 are respectively connected to the mounting frame 11 of the catalyst-coated proton exchange membrane 1 through a frame-shaped sealing member 7.
[0034] The third gas diffusion layer 4 is located between the first gas diffusion layer 2 and the catalyst-coated proton exchange membrane 1, and the permeable membrane 5 is located between the first gas diffusion layer 2 and the third gas diffusion layer 4. The permeable membrane 5 is made of polysulfone or polyethersulfone. A silicone rubber coating 51 is provided on the side of the permeable membrane 5 away from the first gas diffusion layer 2. The silicone rubber coating 51 has drainage holes 511, which are the parts of the silicone rubber coating 51 that are not covered on the surface of the permeable membrane 5. The drainage holes 511 are close to the gas outlet side 21 of the first gas diffusion layer 2. The gas outlet side 21 of the first gas diffusion layer 2 is the side on which gas is discharged after passing through the first gas diffusion layer 2.
[0035] When the membrane electrode is working, air and hydrogen flow to both sides of the catalyst-coated proton exchange membrane 1 under the guidance of the gas flow channel. The air is guided and diffused by the first gas diffusion layer 2, and the hydrogen is guided and diffused by the second gas diffusion layer 3.
[0036] During the diffusion of air along the first gas diffusion layer 2, some of it passes through the silicone rubber coating 51 on the surface of the water-permeable membrane and reaches the gap space between the air-permeable membrane 5 and the third gas diffusion layer. Water is generated on both sides of the first gas diffusion layer 2. The water on the side of the first gas diffusion layer 2 away from the catalyst-coated proton exchange membrane 1 is discharged through the gas channel on the bipolar plate. The water on the side of the first gas diffusion layer 2 close to the catalyst-coated proton exchange membrane 1 is kept between the air-permeable membrane 5 and the catalyst-coated proton exchange membrane 1 under the action of the silicone rubber coating 51. The water between the air-permeable membrane 5 and the catalyst-coated proton exchange membrane 1 then flows back to the gas outlet side 21 of the first gas diffusion layer 2 through the drain hole 511, so that the water is discharged from the membrane electrode as soon as possible under the action of the air pressure difference.
[0037] The thickness of the first gas diffusion layer 2 and the thickness of the third gas diffusion layer 4 are both less than the thickness of the second gas diffusion layer 3. The thickness of the first gas diffusion layer 2 is less than the thickness of the third gas diffusion layer 4, making it easier for air to diffuse from the first gas diffusion layer to the breathable membrane 5.
[0038] Reference Figure 1 and Figure 2A grid pad 6 is provided on the side of the breathable membrane 5 away from the first gas diffusion layer 2. The grid pad 6 can be made of non-woven fabric or woven fabric, or it can be made of the same material as the breathable membrane 5. The grid pad 6 is bonded and fixed to the breathable membrane 5 by a silicone rubber coating 51. The grid pad 6 has grid holes 61, which are arranged in a single row. The arrangement direction of adjacent grid holes 61 is perpendicular to the length direction of the grid holes 61. The length direction of the grid holes 61 is the same as the overall diffusion direction of the gas on the first gas diffusion layer 2. The width of the grid holes 61 gradually increases along the direction close to the drain hole 511. The drain hole 511 of the breathable membrane 5 is located within the distribution range of the grid holes 61 of the grid pad 6.
[0039] The grid pad 6 occupies the space between the breathable membrane 5 and the third gas diffusion layer 4. The space of the grid holes 61 of the grid pad 6 can serve as a drainage channel 62, which helps to accelerate the flow and discharge of water between the breathable membrane 5 and the third gas diffusion layer 4. The width of the grid holes 61 gradually increases towards the drain hole 511, which helps to reduce the resistance to water flow along the grid holes 61.
[0040] It is worth mentioning that in this embodiment, the grating pad 6 is directly bonded to the breathable membrane 5 via the silicone rubber coating 51, making the grating pad 6 and the breathable membrane 5 a single unit for easy assembly. When the grating pad 6 and the breathable membrane 5 are connected as a single unit, the materials of the breathable membrane 5 and the grating pad 6 can be bonded together using silicone rubber coating first, and then cut simultaneously, eliminating the need for separate cutting. In another embodiment, the grating pad 6 can also be bonded to the already solidified silicone rubber coating 51 using other adhesives.
[0041] Reference Figure 1 The drainage hole 511 is an elongated hole, and its length is arranged along the arrangement direction of the grid holes 61 of the grid pad 6. Under the premise that the drainage area of the drainage hole 511 is constant, the drainage hole 511 can be concentrated as close as possible to the gas outlet side 21 of the first gas diffusion layer 2, which is beneficial to improving drainage efficiency.
[0042] Reference Figure 1 and Figure 3 An air inlet 512 is provided on the side of the silicone rubber coating 51 near the air inlet side of the first gas diffusion layer 2. A drain hole 511 is located on the part of the silicone rubber coating 51 that is not covered on the surface of the breathable membrane 5. Multiple air inlets 512 are provided, and their arrangement direction is the same as that of the grid holes 61 of the grid pad 6. Each air inlet 512 corresponds to one grid hole 61. The position on the silicone rubber coating 51 corresponding to the air inlet 512 is not covered by the silicone rubber coating 51. The air velocity passing through the air inlet 512 is relatively high, which helps to create a thrust towards the drain hole 511 on the water between the breathable membrane 5 and the third gas diffusion layer 4, thus improving drainage efficiency.
[0043] Reference Figure 1 and Figure 3 The grid pad 6 has a frame-shaped indentation strip 63 around its perimeter. When the silicone rubber coating 51 adheres to the breathable membrane 5 and the grid pad 6, the coating thickness of the silicone rubber coating 51 in the area corresponding to the indentation strip 63 is greater than the thickness in the other areas, which helps to seal the gap space between the first gas diffusion layer 2 and the third gas diffusion layer 4.
[0044] The implementation principle of a membrane electrode structure in this application embodiment is as follows: When the membrane electrode is working, air and hydrogen flow to both sides of the catalyst-coated proton exchange membrane 1 under the guidance of the gas flow channel. The air is guided and diffused by the first gas diffusion layer 2, and the hydrogen is guided and diffused by the second gas diffusion layer 3. Under the catalytic action of the catalyst, hydrogen forms protons and electrons. After passing through the catalyst-coated proton exchange membrane 1, the protons reach the side where the first gas diffusion layer 2 is located, and the electrons reach the side where the first gas diffusion layer 2 is located after passing through the conductor. This causes hydrogen and oxygen to react on the side of the catalyst-coated proton exchange membrane 1 near the first gas diffusion layer 2 to form water.
[0045] During the above process, as the air diffuses along the first gas diffusion layer 2, some of it passes through the water-permeable membrane and the silicone rubber coating 51 on the surface of the water-permeable membrane, reaching the area between the water-permeable membrane and the catalyst-coated proton exchange membrane 1. In this area, it reacts to form water. The silicone rubber coating 51 has high selectivity for water, allowing it to remain between the water-permeable membrane 5 and the catalyst-coated proton exchange membrane 1. The water between the water-permeable membrane 5 and the catalyst-coated proton exchange membrane 1 then flows back to the outlet side 21 of the first gas diffusion layer 2 through the drain hole 511, allowing the water to be quickly discharged from the membrane electrode under the pressure difference of the air. During the operation of the membrane electrode, the air is mainly distributed on the side of the first gas diffusion layer 2 away from the catalyst-coated proton exchange membrane 1, which helps to reduce the influence of water on the airflow, increases the airflow velocity, and enables the water to be quickly carried out of the membrane electrode.
[0046] The above are all preferred embodiments of this application, and are not intended to limit the scope of protection of this application. Therefore, all equivalent changes made in accordance with the structure, shape and principle of this application should be covered within the scope of protection of this application.
Claims
1. A membrane electrode structure, characterized in that, The device includes a catalyst-coated proton exchange membrane (1), a first gas diffusion layer (2), a second gas diffusion layer (3), and a permeable membrane (5). The first gas diffusion layer (2) and the second gas diffusion layer (3) are located on opposite sides of the catalyst-coated proton exchange membrane (1), and the permeable membrane (5) is located between the first gas diffusion layer (2) and the catalyst-coated proton exchange membrane (1). The permeable membrane (5) has a silicone rubber coating (51) on the side away from the first gas diffusion layer (2). The silicone rubber coating (51) has a drainage hole (511) near the outlet side (21) of the first gas diffusion layer (2). A third gas diffusion layer (4) is provided between the breathable membrane (5) and the catalyst-coated proton exchange membrane (1); a grid pad (6) is provided on the side of the breathable membrane (5) away from the first gas diffusion layer (2), the grid pad (6) has grid holes (61), the grid holes (61) are arranged in a single row, the length direction of the grid holes (61) is the same as the overall gas diffusion direction of the first gas diffusion layer (2), and the arrangement direction of adjacent grid holes (61) is perpendicular to the length direction of the grid holes (61); the drainage holes (511) of the breathable membrane (5) are located within the distribution range of the grid holes (61) of the grid pad (6).
2. The membrane electrode structure according to claim 1, characterized in that: The breathable membrane (5) is a polysulfone membrane or a polyethersulfone membrane.
3. The membrane electrode structure according to claim 1, characterized in that: The thickness of the first gas diffusion layer (2) is less than the thickness of the third gas diffusion layer (4).
4. The membrane electrode structure according to claim 1, characterized in that: The width of the grille hole (61) gradually increases along the direction close to the drain hole (511).
5. A membrane electrode structure according to claim 1, characterized in that: The drainage hole (511) is an elongated hole, and the length direction of the elongated hole is set along the arrangement direction of the grid holes (61) of the grid pad (6).
6. The membrane electrode structure according to claim 1, characterized in that: The silicone rubber coating (51) has an air inlet hole (512) on the side near the air inlet side of the first gas diffusion layer (2). There are multiple air inlets (512), and the arrangement direction of the multiple air inlets (512) is the same as the arrangement direction of the grid holes (61) of the grid pad (6). Each air inlet hole (512) corresponds to one grid hole (61).
7. A membrane electrode structure according to claim 1, characterized in that: The grid pad (6) is bonded and fixed to the breathable membrane (5) by the silicone rubber coating (51).
8. A membrane electrode structure according to claim 7, characterized in that: The grid pad (6) has a frame-shaped embossed strip (63) around its perimeter, and the silicone rubber coating (51) has a coating thickness in the area corresponding to the embossed strip (63) that is greater than the thickness in the other areas.
Citation Information
Patent Citations
Membrane electrode with improved mass transfer property and preparation method thereof