易摊铺的沥青混合料及其制备方法和用途
By adding specific components to thin-layer overlay asphalt mixtures and carrying out shear development and mixing, the problems of high paving temperature and large scattering loss in thin-layer overlay construction are solved, achieving the construction effect of low temperature easy compaction and low loss.
Patent Information
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- CHONGQING ZONJO RENEWABLE RESOURCES DEV CO LTD
- Filing Date
- 2024-03-04
- Publication Date
- 2026-07-17
AI Technical Summary
Existing thin-layer overlay asphalt mixtures are prone to rapid temperature loss and are difficult to compact during paving, resulting in significant quality issues and substantial scattering losses, making it difficult to meet the requirements for thin-layer overlay construction.
The process involves mixing styrene-butadiene-styrene, styrene-isoprene-styrene, white oil, epoxidized soybean oil, furfural extract, glycerol monofatty acid esters, and antioxidants with molten matrix asphalt. This mixture is then sheared and developed to form the first mixture, which is then mixed with basalt and mineral filler to reduce paving temperature and control scattering losses.
It enables easy compaction at lower paving temperatures, improves the construction quality of thin overlays, and reduces Kentenberg scattering losses, making it suitable for thin-layer asphalt mixtures.