A leak-proof device and leak-proof method for welding a molten salt pipe
By utilizing the solidification and expansion of liquid metal and the deformation of shape memory alloy in the leak-proof device, combined with the cooling effect of the Tesla valve, the leakage problem caused by easy cracking of welded joints in molten salt pipes is solved, achieving rapid sealing and solidification of molten salt.
Patent Information
- Application Number
- CN202211700738.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-12-29
- Publication Date
- 2026-11-24
- Estimated Expiration
- 2042-12-29
AI Technical Summary
In existing technologies, welded joints in molten salt pipes are prone to cracking, leading to molten salt leakage, and there is a lack of effective leakage prevention solutions.
The system employs a leak-proof device, including an annular flow channel, a protective shell, an inner steel layer, a salt discharge cavity, a shape memory alloy, and a cooling buffer cavity. It utilizes the solidification characteristics of liquid metal and the elastic deformation of shape memory alloy, combined with the reverse blocking effect of the Tesla valve, to achieve self-sealing and deformation sealing.
It effectively prevents molten salt leakage by using the solidification and expansion of liquid metal and the deformation and blockage of shape memory alloy, combined with the cooling effect of Tesla valve, to achieve rapid sealing and solidification of molten salt.
Smart Images

Figure CN118268762B_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of solar thermal power generation technology, specifically to a leak-proof device and method for welding molten salt pipes. Background Technology
[0002] The thermal storage system is a core component of a tower solar thermal power plant. Molten salt, as the thermal storage medium, is an integral part of the thermal storage system. The environmental problems that may arise during the use of molten salt mainly include molten salt leakage and nitrogen oxide emissions. Molten salt leakage is a relatively common accident in solar thermal power plants, especially in large-scale molten salt systems. The main reasons for molten salt leakage are: (1) the flow and heat release process of molten salt will cause significant thermal stress on the thermal storage pipelines; (2) at high operating temperatures, the components of molten salt have a significant corrosive effect on the thermal storage system. It is worth noting that corrosion and cracking of the welded parts of the pipelines are one of the main ways of molten salt leakage. However, there is currently no practical and feasible technical method to solve the problem of molten salt leakage in an emergency. Therefore, it is necessary to design a leakage prevention device to solve the problem of molten salt leakage in the welded parts of the pipelines. Summary of the Invention
[0003] The purpose of this invention is to solve the problems in the background art by providing a leak-proof device and method for welding molten salt pipes, so as to solve the problem of molten salt leakage after the welded joint of the molten salt pipe cracks.
[0004] The above-mentioned technical objective of the present invention is achieved through the following technical solution: A leak-proof device for welding molten salt pipes includes: an annular flow channel, a protective shell, an inner steel layer, a salt drain cavity, a shape memory alloy, a filler, and a cooling buffer cavity; the inner steel layer and the salt drain cavity are disposed within the protective shell, the annular flow channel is disposed within the inner steel layer, the filler is connected to the annular flow channel, the salt drain cavity is positioned aligned with the weld seam of the connected molten salt pipe, the shape memory alloy is connected to the salt drain cavity, and the cooling buffer cavity is disposed on both sides of the salt drain cavity.
[0005] Preferably, the cooling buffer chamber is a square cavity, and the cooling buffer chamber is connected to the salt drain cavity through a pipe.
[0006] Preferably, the cooling buffer chamber includes: a cooling chamber, a reverse Tesla valve, and a forward Tesla valve. The reverse Tesla valve is connected to the brine drain chamber, and the two ends of the forward Tesla valve are respectively connected to the cooling chamber and the reverse Tesla valve. The forward Tesla valve is open from the reverse Tesla valve to the cooling chamber, and the reverse Tesla valve is blocked from the brine drain chamber to the forward Tesla valve.
[0007] Preferably, the cooling chamber inlet is a throttling orifice.
[0008] A leak-proof method for welding molten salt pipes includes the following steps: S1. Install the leak prevention device: Install the leak prevention device at the weld position between the connected molten salt pipes; S2. Injecting high-temperature liquid metal: High-temperature liquid metal is injected into the annular flow channel through a filling device. The freezing point of the liquid metal is higher than the temperature of the molten salt in the molten salt tube. S3, Cooling liquid metal: Liquid metal in the annular flow channel will change from liquid to solid because the ambient temperature is lower than its freezing point temperature; S4. Self-sealing of the leak prevention device: After the liquid metal cools and becomes solid, its volume expands, squeezing the inner steel layer and forming an overall self-pressurizing seal of the leak prevention device. S5. When molten salt leaks at the weld, the molten salt will gradually fill the vent cavity; the shape memory alloy deforms elastically when heated and extends towards the molten salt weld, blocking the crack in the molten salt tube. S6. The leaked molten salt flows into the buffer cooling chamber and gradually solidifies; S7. Due to the solidification of the leaked molten salt, the shape memory alloy's retractable structural flow channel is squeezed, causing the shape memory alloy to be unable to return to its original shape and achieve the deformation sealing effect.
[0009] Preferably, in step S6, the leaked molten salt is squeezed into the reverse Tesla valve. Under the reverse blocking effect, the leaked molten salt slowly flows into the Tesla valve and gradually solidifies. When the molten salt is gradually injected into the reverse Tesla valve, the gas remaining in the pipeline is compressed and driven to flow towards the reverse Tesla valve and enter the cooling chamber. Since the inlet of the cooling chamber is a throttling orifice, the incoming gas produces a throttling cooling effect, thereby rapidly cooling the leaked salt cavity and accelerating the solidification of the molten salt.
[0010] The reverse Tesla valve can block leaking molten salt, slowing down the leakage, and at the same time can accelerate the filling of the salt leakage cavity with molten salt, accelerating the deformation of the shape memory alloy and achieving a timely deformation sealing effect.
[0011] Preferably, in step S6, by setting a positive Tesla valve, a one-way gas flow channel is formed, which allows the compressed gas to quickly enter the cooling chamber, be throttled and generate a cooling effect, cool the salt discharge cavity and accelerate the solidification of molten salt; in addition, the positive Tesla valve 12 can prevent a large amount of gas from flowing back and maintain a sufficient amount of gas in the cooling chamber.
[0012] In summary, the beneficial effects of this invention are as follows: 1. The present invention provides a leak-proof device and method for welding molten salt pipes, which utilizes the temperature characteristics of liquid metal to cause it to transform from liquid to solid, resulting in volume expansion and achieving self-pressurizing sealing.
[0013] 2. The leak-proof device and leak-proof method for welding molten salt pipes described in this invention uses a shape memory alloy, which undergoes elastic deformation when heated, thus achieving a deformation sealing effect.
[0014] 3. The leakage prevention device and method for welding molten salt pipes described in this invention adopts a Tesla valve, which has a reverse blocking effect, forming a blockage for leaking molten salt, and then the molten salt cools down and solidifies to form a secondary seal. Attached Figure Description
[0015] Figure 1 This is a schematic diagram of the anti-leakage device according to Embodiment 1 of the present invention; Figure 2 This is a schematic axial cross-sectional view of the anti-leakage device according to Embodiment 1 of the present invention; Figure 3 This is a schematic diagram of the leakage process 1 in Embodiment 1 of the present invention; Figure 4 This is a schematic diagram of the leakage process 2 in Embodiment 1 of the present invention; Figure 5 This is a schematic diagram of leakage process 3 in Embodiment 1 of the present invention; Figure 6 This is a schematic diagram of leakage process 4 in Embodiment 1 of the present invention; Figure 7 This is a schematic diagram of the leakage process 5 in Embodiment 1 of the present invention; Figure 8 This is a schematic diagram of the anti-leakage device according to Embodiment 2 of the present invention; Figure 9 This is a schematic axial cross-sectional view of the anti-leakage device of Embodiment 2 of the present invention; Figure 10 This is a schematic diagram of the leakage process 1 in Embodiment 2 of the present invention; Figure 11 This is a schematic diagram of leakage process 2 in Embodiment 2 of the present invention; Figure 12 This is a schematic diagram of the leakage process 3 in Embodiment 2 of the present invention; Figure 13 This is a schematic diagram of leakage process 4 in Embodiment 2 of the present invention; Figure 14 This is a schematic diagram of the leakage process 5 in Embodiment 2 of the present invention. Detailed Implementation
[0016] The following specific embodiments are merely illustrative of the present invention and are not intended to limit the invention. After reading this specification, those skilled in the art can make modifications to these embodiments without contributing any inventive step, but such modifications are protected by patent law as long as they fall within the scope of the claims of the present invention.
[0017] The present invention will now be described in detail with reference to the accompanying drawings and embodiments.
[0018] Example 1: according to Figures 1-2 As shown, a leak-proof device 2 for welding molten salt pipes includes: an annular flow channel 3, a protective shell 4, an inner steel layer 5, a salt draining cavity 7, a shape memory alloy 8, a filler 9, and a cooling buffer chamber 15; the inner steel layer 5 and the salt draining cavity 7 are disposed inside the protective shell 4, the annular flow channel 3 is disposed inside the inner steel layer 5, the filler 9 is connected to the annular flow channel 3, the salt draining cavity 7 is disposed at the weld seam 6 of the connected molten salt pipe 1, the shape memory alloy 8 is connected to the salt draining cavity 7, the cooling buffer chamber 15 is disposed on both sides of the salt draining cavity 7, the cooling buffer chamber 15 is a square cavity, and the cooling buffer chamber 15 is connected to the salt draining cavity 7 through a pipe.
[0019] A leak-proof method for welding molten salt pipes includes the following steps: S1. Install the above-mentioned leak prevention device 2: Install the leak prevention device 2 at the weld 6 position between the connected molten salt pipes 1; S2. Adding high-temperature liquid metal: High-temperature liquid metal is added to the annular flow channel 3 through the filler 9. The freezing point of the liquid metal is higher than the temperature of the molten salt in the molten salt tube. S3, Cooling liquid metal: The liquid metal in the annular flow channel 3 will change from liquid to solid because the ambient temperature is lower than its freezing point temperature; S4. Self-sealing of the leak prevention device: After the liquid metal cools and becomes solid, its volume expands and squeezes the inner steel 5, forming an overall self-pressurizing seal of the leak prevention device 2. S5. When molten salt leaks at the weld, the molten salt will gradually fill the salt leakage cavity 7; the shape memory alloy 8 deforms elastically when heated and extends towards the molten salt weld 6 to block the crack point of the molten salt tube. S6. The leaked molten salt flows into the buffer cooling chamber 15 and gradually solidifies; S7. Due to the solidification of the leaked molten salt, the shape memory alloy's retractable structural flow channel is squeezed, causing the shape memory alloy to be unable to return to its original shape and achieve the deformation sealing effect.
[0020] Figures 3-7 The image shows the self-sealing process after a molten salt pipe weld ruptures: 1 Figure 3 This is the initial state; 2. When crack 13 appears in weld 6, molten salt leaks out of the molten salt pipe, such as... Figure 4 ; 3. Molten salt gradually fills the salt drain cavity 7 and flows into the buffer cooling cavity 15; 4. The molten salt 14 in the salt venting cavity 7 comes into contact with the shape memory alloy 8. Due to the elastic deformation of the shape memory alloy 8 under heat, it extends towards the weld 6 until it approaches the weld crack 13, achieving a sealing effect. Figure 5 As shown; 5. As the shape memory alloy 8 occupies the area attached to the molten salt tube, the temperature of the molten salt gradually decreases as it moves away from the molten salt tube wall until it solidifies. When the leaked molten salt 14 solidifies, it squeezes the shrinkage structure flow channel of the shape memory alloy 8. At the same time, the molten salt at the weld crack is always in contact with the shape memory alloy at a high temperature. Therefore, the shape memory alloy 8 is always in a deformed state, which plays a role in blocking and sealing.
[0021] Example 2: according to Figures 8-9 As shown, a leak-proof device 2 for welding molten salt pipes includes: an annular flow channel 3, a protective shell 4, an inner steel layer 5, a salt discharge cavity 7, a shape memory alloy 8, a filler 9, and a cooling buffer cavity 15; the inner steel layer 5 and the salt discharge cavity 7 are disposed inside the protective shell 4, the annular flow channel 3 is disposed inside the inner steel layer 5, the filler 9 is connected to the annular flow channel 3, the salt discharge cavity 7 is disposed at the weld seam 6 of the connected molten salt pipe 1, the shape memory alloy 8 is connected to the salt discharge cavity 7, and the cooling buffer cavity 15 is disposed on both sides of the salt discharge cavity 7.
[0022] The cooling buffer chamber 15 includes a cooling chamber 10, a reverse Tesla valve 11, and a forward Tesla valve 12. The reverse Tesla valve 11 is connected to the salt drain chamber 7. The two ends of the forward Tesla valve 12 are connected to the cooling chamber 10 and the reverse Tesla valve 11, respectively. The forward Tesla valve 12 is open from the reverse Tesla valve 11 to the cooling chamber 10. The reverse Tesla valve 11 is blocked from the salt drain chamber 7 to the forward Tesla valve 12. The inlet of the cooling chamber 10 is a throttling orifice.
[0023] A leak-proof method for welding molten salt pipes includes the following steps: S1. Install the above-mentioned leak prevention device 2: Install the leak prevention device 2 at the weld 6 position between the connected molten salt pipes 1; S2. Adding high-temperature liquid metal: High-temperature liquid metal is added to the annular flow channel 3 through the filler 9. The freezing point of the liquid metal is higher than the temperature of the molten salt in the molten salt tube. S3, Cooling liquid metal: The liquid metal in the annular flow channel 3 will change from liquid to solid because the ambient temperature is lower than its freezing point temperature; S4. Self-sealing of the leak prevention device: After the liquid metal cools and becomes solid, its volume expands and squeezes the inner steel 5, forming an overall self-pressurizing seal of the leak prevention device 2. S5. When molten salt leaks at the weld, the molten salt will gradually fill the salt leakage cavity 7; the shape memory alloy 8 deforms elastically when heated and extends towards the molten salt weld 6 to block the crack point of the molten salt tube. S6. The leaked molten salt will be squeezed into the reverse Tesla valve 11. Under the reverse blocking effect, the leaked molten salt slowly flows into the Tesla valve and gradually solidifies. When the molten salt is gradually injected into the reverse Tesla valve 11, the gas remaining in the pipeline will be compressed and driven to flow towards the reverse Tesla valve 11 and enter the cooling chamber 10. Since the inlet of the cooling chamber 10 is a throttling orifice, the incoming gas will produce a throttling cooling effect, thereby rapidly cooling the salt leakage cavity 7 and accelerating the solidification of the molten salt. By setting the forward Tesla valve 12, a one-way gas flow channel is formed, which allows the compressed gas to quickly enter the cooling chamber 10, be throttled and produce a cooling effect, cool the salt leakage cavity 7 and accelerate the solidification of the molten salt. In addition, the forward Tesla valve 12 can prevent a large amount of gas from flowing back and maintain a sufficient amount of gas in the cooling chamber 10. S7. Due to the solidification of the leaked molten salt, the shape memory alloy's retractable structural flow channel is squeezed, causing the shape memory alloy to be unable to return to its original shape and achieve the deformation sealing effect.
[0024] Figures 10-14 The image shows the self-sealing process after a molten salt pipe weld ruptures: 1 Figure 10 This is the initial state; 2. When crack 13 appears in weld 6, molten salt leaks out of the molten salt pipe, such as... Figure 11 ; 3. Molten salt gradually fills the salt discharge cavity 7 and flows into the reverse Tesla valve 11; 4. Due to the reverse blocking effect of Tesla valve 11, two streams of molten salt will be formed opposing each other in the flow path intersection area, which will hinder the flow of molten salt, such as... Figure 12 As shown; 5. The molten salt 14 in the salt venting cavity 7 comes into contact with the shape memory alloy 8. Due to the elastic deformation of the shape memory alloy 8 under heat, it extends towards the weld 6 until it approaches the weld crack 13, achieving a sealing effect. Figure 13 As shown; The gas in pipeline 6, under the pressure of the molten salt flowing out, is gradually driven into the positive Tesla valve 12 and then into the cooling chamber 10. Due to the throttling effect at the inlet of the cooling chamber 10, a cooling effect is generated, which rapidly cools the salt draining chamber 7 and accelerates the solidification of the molten salt. Note: The closer the cooling chamber 10 is to the salt draining chamber 7, the better the cooling effect.
[0025] 7. As the shape memory alloy 8 occupies the area attached to the molten salt tube, the temperature of the molten salt gradually decreases as it moves away from the molten salt tube wall until it solidifies. When the leaked molten salt 14 solidifies, it squeezes the shrinkage structure flow channel of the shape memory alloy 8. At the same time, the molten salt at the weld crack is always in contact with the shape memory alloy at a high temperature. Therefore, the shape memory alloy 8 is always in a deformed state, which plays a role in blocking and sealing.
Claims
1. A leak-proof device for welding a molten salt pipe, characterized by, include: The annular flow channel (3), protective shell (4), inner steel (5), salt drain cavity (7), shape memory alloy (8), filler (9), and cooling buffer cavity (15) are arranged inside the protective shell (4), the annular flow channel (3) is arranged inside the inner steel (5), the filler (9) is connected to the annular flow channel (3), the salt drain cavity (7) is arranged at the weld (6) of the connected molten salt pipe (1), the shape memory alloy (8) is connected to the salt drain cavity (7), and the cooling buffer cavity (15) is arranged on both sides of the salt drain cavity (7).
2. A leak-proof device for welding a molten salt pipe according to claim 1, wherein The cooling buffer chamber (15) is a square cavity, and the cooling buffer chamber (15) is connected to the salt discharge cavity (7) through a pipe.
3. A leak-proof device for welding molten salt pipes according to claim 1, characterized in that, The cooling buffer chamber (15) includes a cooling chamber (10), a reverse Tesla valve (11), and a forward Tesla valve (12). The reverse Tesla valve (11) is connected to the salt drain chamber (7). The two ends of the forward Tesla valve (12) are connected to the cooling chamber (10) and the reverse Tesla valve (11), respectively. The forward Tesla valve (12) is open from the reverse Tesla valve (11) to the cooling chamber (10), and the reverse Tesla valve (11) is blocked from the salt drain chamber (7) to the forward Tesla valve (12).
4. A leak-proof device for welding molten salt pipes according to claim 3, characterized in that, The inlet of the cooling chamber (10) is a throttling orifice.
5. A leak-proof method for welding molten salt pipes, characterized in that, Includes the following steps: S1. Install the leak prevention device (2) as described in any one of claims 1-4: Install the leak prevention device (2) at the weld (6) position between the connected molten salt pipes (1); S2. Adding high-temperature liquid metal: Through the filler (9), high-temperature liquid metal is added to the annular flow channel (3), wherein the freezing point of the liquid metal is higher than the temperature of the molten salt in the molten salt tube; S3, Cooling liquid metal: The liquid metal in the annular flow channel (3) will change from liquid to solid because the ambient temperature is lower than its freezing point temperature; S4. Self-sealing of the anti-leakage device: After the liquid metal cools and becomes solid, its volume expands and squeezes the inner steel (5), forming an overall self-pressurizing seal of the anti-leakage device (2). S5. When molten salt leaks at the weld, the molten salt will gradually fill the salt leakage cavity (7); the shape memory alloy (8) deforms elastically under heat and extends towards the molten salt weld (6) to block the crack point of the molten salt pipe. S6. The leaked molten salt flows into the cooling buffer chamber (15) and gradually solidifies; S7. Due to the solidification of the leaked molten salt, the shape memory alloy's retractable structural flow channel is squeezed, causing the shape memory alloy to be unable to return to its original shape and achieve a deformation sealing effect.
6. The method according to claim 5, characterized in that, In step S6, the leaked molten salt will be squeezed into the reverse Tesla valve (11). Under the reverse blocking effect, the leaked molten salt slowly flows into the Tesla valve and gradually solidifies. When the molten salt is gradually injected into the reverse Tesla valve (11), the gas remaining in the pipeline will be compressed and driven to flow to the reverse Tesla valve (11) and enter the cooling chamber (10). Since the inlet of the cooling chamber (10) is a throttling orifice, the gas entering will generate a throttling cooling effect, thereby playing a role in rapidly cooling the salt leakage cavity (7) and accelerating the solidification of the molten salt.
7. The method according to claim 6, characterized in that, In step S6, by setting a positive Tesla valve (12), a one-way gas flow channel is formed, which allows the compressed gas to quickly enter the cooling chamber (10), and generate a cooling effect due to the throttling effect, thereby cooling the salt discharge cavity (7) and accelerating the solidification of molten salt. In addition, the positive Tesla valve (12) can prevent a large amount of gas from flowing back and maintain a sufficient amount of gas in the cooling chamber (10).
Citation Information
Patent Citations
Coating pipeline welded structure
CN208605758U
Tube welding method and tube welding device
JP2006136911A