一种利用助剂强化回收溢出气态氟化物的方法
By heating the additives with silicon-rich materials, the problem of low fluoride overflow rate is solved, achieving efficient recovery of fluorine resources and improvement of phosphoric acid quality, which is applicable to a variety of fluorine-containing industrial processes.
Patent Information
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- WUHAN INST OF TECH
- Filing Date
- 2024-04-26
- Publication Date
- 2026-07-17
AI Technical Summary
Existing technologies have low fluoride spillover and recovery rates, resulting in underutilization of fluorine resources and a lack of effective optimization of related processes.
An additive is mixed with a silicon-rich substance, and the overflowing gaseous fluoride is recovered through a heating reaction. The chemical structure and properties of the additive reduce interfacial tension, enhance dispersibility and permeability, and increase the fluoride overflow rate.
It significantly improves the fluorine spillover rate, enhances the quality of phosphoric acid, and the process is simple and easy to implement, making it suitable for various fluorine-containing industrial processes.
Smart Images

Figure CN118387847B_ABST