Microneedle manufacturing method

By simultaneously performing pressurization and drying processes within a pressurized chamber, the problems of active ingredient leakage and poor quantification in the manufacture of biodegradable microneedles are solved, achieving the effects of simplifying the process and improving productivity.

CN118401277BActive Publication Date: 2026-11-24DAEWOONG THERAPEUTICS INC
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202280082313.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2021-12-14
Filing Date
2022-04-04
Publication Date
2026-11-24
Estimated Expiration
2042-04-04

AI Technical Summary

Technical Problem

In existing biodegradable microneedle manufacturing methods, the active ingredients are prone to leakage during decompression or vacuum processes, resulting in poor quantification and complex procedures, making it difficult to guarantee the quality and production efficiency of microneedles.

Method used

The pressurization and drying processes are carried out simultaneously in a pressurized chamber. Convection is generated by air injection and discharge to achieve the filling and drying of raw materials, simplifying the process and improving quantitative accuracy.

Benefits of technology

Simultaneous pressurization and drying processes within the pressurization chamber simplify the process, improve the quantification of active ingredients, reduce the possibility of microneedle contamination, and increase productivity.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118401277B_ABST
    Figure CN118401277B_ABST
Patent Text Reader

Abstract

An embodiment of the present invention provides a microneedle manufacturing method, comprising the following steps: coating a raw material containing an effective ingredient onto one or more recessed portions formed in a microneedle mold; and placing the microneedle mold coated with the raw material into a pressurized chamber, and pressurizing the raw material with the internal pressure of the pressurized chamber in order to fill the microstructure of the recessed portion, wherein during the pressurization step, air injection and air discharge are performed simultaneously in the pressurized chamber to generate convection within the pressurized chamber, thereby simultaneously performing the filling and drying of the raw material.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to a microneedle manufacturing method, and more specifically, to a microneedle manufacturing method that simplifies the process and improves the quantification of the active ingredient by simultaneously performing pressure and drying processes on the active ingredient coated on the microneedle mold. Background Technology

[0002] Generally, the purpose of microneedling formulations is to penetrate the skin to deliver ingredients that achieve a target effect. In microneedling formulations, microneedles with diameters and heights of only tens to thousands of micrometers are used to penetrate the stratum corneum, the main barrier to ingredient delivery through the skin. Using these microneedles, the target ingredient reaches the epidermis or dermis, manifesting its effect at the site of application, or through the body's circulatory system.

[0003] Microneedles can be broadly classified into metal microneedles and biodegradable microneedles.

[0004] Metal microneedles come in the following forms: hollow microneedles, which have a path for the delivery of the desired component and are hollow like a conventional injection needle; and solid microneedles, which have the component coated on their surface and delivered.

[0005] On the other hand, biodegradable microneedles are primarily in the form of solid microneedles, and are manufactured by coating the surface of the microneedle with a component or forming it together with a biodegradable polymer. After application to the skin, the component is delivered while the microneedle degrades. In manufacturing these biodegradable microneedles, they are generally produced by injecting the active ingredient constituting the microneedle into a mold formed by sculpting the microneedle shape.

[0006] At this time, as Figure 1 As shown, conventional methods for manufacturing biodegradable microneedles include the following steps: coating an active ingredient onto a mold; allowing the active ingredient to penetrate into the microstructures within the mold under reduced pressure or vacuum; and drying the active ingredient within the mold to form microneedles.

[0007] However, this conventional method of manufacturing biodegradable microneedles has the following problems: during decompression or vacuum processes, due to the leakage of active ingredients and bubbles in the mold to the outside (when the bubbles burst, the active ingredients overflow the concave carving of the mold), there may be quantitative deviations in the active ingredients in the microneedles.

[0008] Existing technical documents

[0009] Korean Patent Registration Publication No. 10-1747099 (June 8, 2017) Summary of the Invention

[0010] The technical problem to be solved by the invention

[0011] The present invention addresses the problems of the prior art. The purpose of the present invention is to simplify the process and improve the quantification of the effective ingredients by simultaneously applying pressure and drying the effective ingredients coated on the microneedle mold.

[0012] means for solving technical problems

[0013] To achieve the objectives described above, one aspect of the present invention provides a microneedle manufacturing method, comprising the following steps: coating a raw material containing an effective ingredient onto one or more recessed portions formed in a microneedle mold; and placing the microneedle mold coated with the raw material into a pressurized chamber, and pressurizing the raw material with the internal pressure of the pressurized chamber in order to fill the microstructure of the recessed portion, wherein during the pressurization step, air injection and air discharge are simultaneously performed in the pressurized chamber to generate convection within the pressurized chamber, thereby simultaneously performing the filling and drying of the raw material.

[0014] In one embodiment of the present invention, the microneedle manufacturing method is characterized in that, when the air pressure injected into the pressurized chamber is X bar and the air pressure discharged from the pressurized chamber is Y bar, the internal pressure XY bar of the pressurized chamber is 1.5 bar or more.

[0015] In one embodiment of the present invention, the microneedle manufacturing method is characterized in that the air pressure injected into the pressurized chamber is 2 bar or more, and the air pressure discharged from the pressurized chamber is 0.5 bar or more.

[0016] In one embodiment of the present invention, the microneedle manufacturing method is characterized in that the microneedle mold is manufactured by injection molding of thermoplastic resin.

[0017] In one embodiment of the present invention, the microneedle manufacturing method is characterized in that the thermoplastic resin is selected from at least one of the group consisting of polyethylene terephthalate (PET), polyvinyl chloride (PVC), and polypropylene (PP).

[0018] In one embodiment of the present invention, the microneedle manufacturing method is characterized in that the concave portion of the microneedle mold is a pointed concave portion, which exists independently.

[0019] To achieve the objectives described above, another aspect of the present invention provides a microneedle manufacturing method, comprising the following steps: placing a plurality of microneedle molds on a fixture; applying a raw material containing an active ingredient to one or more recessed portions formed in the microneedle molds; fixing one or more of the fixtures to a tray; and placing the tray into a pressurizing chamber and pressurizing the raw material with the internal pressure of the pressurizing chamber in order to fill the microstructure of the recessed portion, wherein during the pressurizing step, air injection and air discharge are simultaneously performed in the pressurizing chamber to generate convection within the pressurizing chamber, thereby simultaneously performing the filling and drying of the raw material.

[0020] In one embodiment of the present invention, the microneedle manufacturing method is characterized in that, when the air pressure injected into the pressurized chamber is X bar and the air pressure discharged from the pressurized chamber is Y bar, the internal pressure XY bar of the pressurized chamber is 1.5 bar or more.

[0021] In one embodiment of the present invention, the microneedle manufacturing method is characterized in that the air pressure injected into the pressurized chamber is 2 bar or more, and the air pressure discharged from the pressurized chamber is 0.5 bar or more.

[0022] Invention Effects

[0023] According to one aspect of the present invention, in the microneedle manufacturing method of the present invention, the process can be simplified and the quantitativeity of the raw material material coated on the concave part of the microneedle mold can be improved by simultaneously performing the pressurization and drying process in the pressurization chamber, and the exposure to the external environment can be reduced during the manufacturing process to reduce the possibility of microneedle contamination.

[0024] Furthermore, a large number of microneedles can be formed in the pressurized chamber using a fixture that can hold multiple microneedle molds and a tray that can fix multiple fixtures, thus improving the productivity of microneedles.

[0025] The effects of the present invention are not limited to those described above, but should be understood to include all effects that can be inferred from the composition of the invention as described in the detailed description or technical solution of the present invention. Attached Figure Description

[0026] Figure 1 This diagram is a conceptual representation of a microneedle manufacturing method based on previous technologies.

[0027] Figure 2 This is a flowchart of a microneedle manufacturing method based on an embodiment of the present invention.

[0028] Figure 3This is a diagram conceptually illustrating a microneedle manufacturing method in the case of a dot-coating method within the recessed portion of a mold based on an embodiment of the present invention.

[0029] Figure 4 This is a diagram conceptually illustrating a microneedle manufacturing method in the case of an overall mold coating method based on an embodiment of the present invention.

[0030] Figure 5 This is a flowchart of a microneedle manufacturing method based on another embodiment of the present invention.

[0031] Figure 6 This is a diagram conceptually illustrating a microneedle manufacturing method in the case of a dot-coating method within the recessed portion of a mold based on another embodiment of the present invention.

[0032] Figure 7 This is a diagram conceptually illustrating a microneedle manufacturing method in the case of an overall mold coating method based on another embodiment of the present invention.

[0033] Figures 8 to 13 Examples of microneedle generation are shown, based on the internal pressure of the pressurized chamber and according to the type of polymer. Detailed Implementation

[0034] The present invention will now be described with reference to the accompanying drawings. However, the present invention can be implemented in various different ways and is therefore not limited to the embodiments described herein. Furthermore, in the drawings, parts unrelated to the description have been omitted for clarity, and similar reference numerals are used for similar parts throughout the specification.

[0035] Throughout the specification, when a part is referred to as being "connected" to other parts, this includes not only "direct connection" but also "indirect connection" with other components in between. Furthermore, when a part is referred to as "including" a certain constituent element, unless otherwise stated otherwise, it implies that other constituent elements may also be present, rather than excluding other constituent elements.

[0036] Hereinafter, embodiments of the present invention will be described in detail with reference to the accompanying drawings.

[0037] Figure 2 This is a flowchart of a microneedle manufacturing method based on an embodiment of the present invention. Figure 3 This diagram conceptually illustrates a microneedle manufacturing method based on a dot-coating method within the recessed portion of a mold according to an embodiment of the present invention. Figure 4 This is a diagram conceptually illustrating a microneedle manufacturing method in the case of an overall mold coating method based on an embodiment of the present invention.

[0038] refer to Figures 2 to 4The microneedle manufacturing method of the present invention includes the following steps: preparing a microneedle mold (100) (S110); coating a raw material (120) onto the recessed portion (110) of the microneedle mold (100) (S120); and filling and drying the raw material (120) by pressurizing it in a pressurized chamber (30) (S130).

[0039] More specifically, the microneedle manufacturing method of the present invention comprises the following steps: a step of preparing a microneedle mold (100) (S110); a step of coating a raw material (120) containing an effective ingredient onto one or more recessed portions (110) formed in the microneedle mold (100) (S120); and a step of placing the microneedle mold (100) coated with the raw material (120) into a pressurizing chamber (30) and pressurizing the raw material (120) with the internal pressure of the pressurizing chamber (30) in order to fill the microstructure (111) of the recessed portion (110) with the raw material (120) (S130). In the pressurizing step (S130), air injection and air discharge are performed simultaneously in the pressurizing chamber (30) to generate convection in the pressurizing chamber (30), thereby simultaneously performing the filling and drying of the raw material (120).

[0040] In step (S110) of preparing the microneedle mold (100), injection molding is performed using an injection device by melting, flowing, cooling, and demolding thermoplastic resin, thereby manufacturing a microneedle mold (100) including one or more recessed portions. At this time, one side of the microneedle mold (100) may include one or more recessed portions (110), and the other side may be flat. The recessed portions (110) function as molds for the microneedles formed in subsequent steps and may have the same shape as the microneedles.

[0041] At this time, the recessed portion (110) may include a tip recessed portion. As used in this specification, the term "tip recessed portion" refers to a recessed portion formed by reducing the cross-sectional area from the upper surface of a plane to the lower surface constituting the tip in order to achieve a typical microneedle shape, thereby recessing from said upper surface. The terms "upper surface" and / or "lower surface" as used in this specification are used to determine the relative positional relationship of the components, not to determine their absolute positions.

[0042] On the other hand, the microneedle mold (100) can be formed from a robust material. The microneedle mold (100) can be made from any suitable material, but is preferably formed from plastic resin.

[0043] More specifically, the microneedle mold (100) may be at least one selected from the group consisting of polyethylene terephthalate (PET), polyvinyl chloride (PVC), and polypropylene (PP), but is not limited thereto.

[0044] Traditionally, silicon materials are expensive and difficult to use in single applications, requiring repeated use. However, this makes it difficult to verify the cleaning effectiveness (CV) of the micro-engraved portions of the microneedles and the silicon permeability to cleaning solvents. Furthermore, with silicon materials, due to physical and chemical degradation and their relatively weak hardness, it is difficult to verify the generation of debris during the manufacturing or cleaning process and the lifespan of the silicon mold.

[0045] Furthermore, in the mold manufacturing process using silicon materials, silicon cannot provide protection against external air or foreign objects. Therefore, the dried microneedles need to be demolded from the silicon mold and repackaged. In this process, it is practically difficult to individually and tightly package the microneedles of such a small size. Instead, the microneedles need to be packaged in a bag or a cap-like container while exposed to air.

[0046] The airtightness and stability of the packaging container are factors that have a significant impact on the quality maintenance of the internal drug. It must be able to completely protect the internal microneedle drug from physicochemical deformation or deterioration through simulation of the final product's transportation conditions and mechanical testing.

[0047] The microneedle mold (100) of the present invention can function as a primary packaging container that fits completely against the microneedles, without the need to demold and repackage the microneedles formed in the embossed portion (110), and can be configured in a form that can be removed before use. As a result, the microneedle packaging process is simplified, and the quality of the microneedles can be easily maintained.

[0048] In step (S120) of coating the raw material (120) onto the recessed portion (110) of the microneedle mold (100), the raw material (120) can be supplied from the reservoir to the microneedle mold (100) through a single dispensing part and coated onto the recessed portion (110). However, the method of coating the raw material (120) is not limited to this. If necessary, the raw material (120) can also be coated onto the recessed portion (110) through multiple dispensing parts located at positions adjacent to each of the multiple recessed portions (110).

[0049] At this time, refer to Figure 3 and Figure 4 The coating of the raw material (120) can be performed by applying more than one drop to each of the recessed portions (110), or by applying it to the entire upper surface of the microneedle mold (100) on which the recessed portions (110) are formed.

[0050] The raw material (120) may contain one or more of the group consisting of metals, nonmetals, biodegradable polymers and active pharmaceutical ingredients, depending on the intended use of the microneedles. For example, the raw material (120) may be a composition containing active ingredients, or a composition containing metals, nonmetals, biodegradable polymers, or a combination of two or more of them, but is not limited thereto.

[0051] In the step (S130) of pressurizing the raw material (120) coated on the recessed portion (110) in the pressurizing chamber (30), the raw material (120) is pressurized by the internal pressure of the pressurizing chamber (30) in order to fill the microstructure (111) of the recessed portion (110) with the raw material (120).

[0052] When the pressurized chamber (30) is shielded, if air is injected through the injection port (31) of the pressurized chamber (30) and the pressure of the pressurized chamber (30) increases, the raw material (120) will be subjected to pressure due to the gas pressure inside the pressurized chamber (30). The microbubbles contained in the raw material (120) will naturally detach from the raw material (120) and be removed, and the raw material (120) will fill the microstructure (111) in the recessed part (110).

[0053] At this time, air is simultaneously discharged through the outlet (32) of the pressurized chamber (30), causing convection to occur in the pressurized chamber (30), thereby enabling the drying of the raw material (120) to be performed simultaneously.

[0054] That is, in the microneedle manufacturing method of the present invention, the raw material (120) coated on the recessed portion (110) of the microneedle mold (100) can be simultaneously pressurized and dried in the pressurized chamber (30) to simplify the process and improve the quantitativeity of the raw material (120), and can reduce exposure to the external environment during the manufacturing process to reduce the possibility of microneedle contamination.

[0055] On the other hand, when the air pressure injected into the pressurized chamber (30) through the injection port (31) is X bar and the air pressure discharged from the pressurized chamber (30) through the discharge port (32) is Y bar, the internal pressure XY bar of the pressurized chamber (30) is 1.5 bar or more, preferably 2 bar or more.

[0056] Furthermore, the air pressure injected into the pressurized chamber (30) is 2 bar or more, preferably 2.5 bar or more, and the air pressure discharged from the pressurized chamber (30) can be 0.5 bar or more.

[0057] That is, air injection and air discharge are performed simultaneously in the pressurized chamber (30), and the internal pressure of the pressurized chamber (30) is maintained at 1.5 bar or more, preferably at 2 bar or more, so that the filling and drying of the raw material (120) can be carried out smoothly. If the internal pressure of the pressurized chamber (30) is less than 1.5 bar, the raw material (120) cannot be smoothly filled into the microstructure (111) in the recessed part (110), and the microbubbles contained in the raw material (120) may not be able to detach naturally from the raw material (120).

[0058] Figure 5 This is a flowchart of a microneedle manufacturing method based on another embodiment of the present invention. Figure 6 This diagram conceptually illustrates a microneedle manufacturing method in the case of a dot-coating method within the recessed portion of a mold based on another embodiment of the present invention. Figure 7 This is a diagram conceptually illustrating a microneedle manufacturing method in the case of an overall mold coating method based on another embodiment of the present invention.

[0059] The following mainly describes the differences and additions from the above embodiment.

[0060] refer to Figures 5 to 7 The microneedle manufacturing method of the present invention comprises the following steps: preparing a microneedle mold (100) (S210); placing a plurality of microneedle molds (100) on a jig (10) (S220); applying a raw material (120) to the recessed portion (110) of the microneedle mold (100) (S230); fixing one or more of the jigs (10) to a tray (20) (S240); and placing the tray (20) into a pressure chamber. (S250) In order to fill the microstructure (111) of the recessed part (110) with the internal pressure of the pressurized chamber (30), in the pressurized step (S250), air injection and air discharge are performed simultaneously in the pressurized chamber (30) to generate convection in the pressurized chamber (30), thereby simultaneously performing the filling and drying of the raw material (120).

[0061] In the step (S220) of placing multiple microneedle molds (100) onto the fixture (10), the fixture (10) may be formed as a plate, and its upper surface may have multiple placement portions (not shown) capable of positioning the microneedle molds (100). The placement portions may be formed by groove structures with shapes corresponding to the shape of the microneedle molds (100).

[0062] The fixture (10) is in the form of N×M (where N and M are numbers) and can be configured to accommodate microneedle molds (100), with a total of N×M microneedle molds (100) that can be accommodated on one fixture (10).

[0063] In step (S230) of coating the raw material (120) onto the recessed portion (110) of the microneedle mold (100), the raw material (120) can be supplied from the reservoir to the microneedle mold (100) through a single dispensing part and coated onto the recessed portion (110). However, the coating method of the raw material (120) is not limited to this. If necessary, the raw material (120) can also be coated onto the recessed portion (110) through multiple dispensing parts located at positions adjacent to each of the multiple recessed portions (110).

[0064] At this time, refer to Figure 6 and Figure 7 The coating of the raw material (120) can be performed by applying more than one drop to each of the recessed portions (110), or by applying it to the entire upper surface of the microneedle mold (100) on which the recessed portions (110) are formed.

[0065] In step (S240) of fixing one or more clamps (10) to the tray (20), the tray (20) may be a multi-layer tray, and multiple clamps (10) may be fixed on one tray (20) in multiple layers. Furthermore, multiple clamps (10) may be fixed on one layer of the tray (20).

[0066] In this way, by using a fixture (10) that can accommodate multiple microneedle molds (100) and a tray (20) that can fix multiple fixtures (10), a large number of microneedles can be formed in the pressurized chamber (30), thus improving the productivity of microneedles.

[0067] Figures 8 to 13 Examples of microneedle generation are shown, based on the internal pressure of the pressurized chamber and according to the type of polymer.

[0068] refer to Figures 8 to 13 Four polymers were used as raw materials: polyvinyl alcohol (PVA), carboxymethyl cellulose (CMC), polyvinylpyrrolidone (PVP), and hyaluronic acid (HA). After each polymer underwent pressurization and drying in a pressurized chamber, the presence or absence of microneedles was measured. The ideal maximum microneedle size was 650 μm. The presence or absence of microneedles was determined by whether a microneedle tip was formed and whether it had a size greater than 400 μm.

[0069] refer to Figure 8For four polymers coated on a microneedle mold, a pressurization and drying process was performed for 48 hours in an environment where the air pressure injected into the pressurization chamber was 2 bar, the air pressure discharged from the pressurization chamber was 1 bar, and the internal pressure of the pressurization chamber was 1 bar. At this time, for the four polymers, microneedles with a size of 400 μm or larger without forming microneedle tips were identified.

[0070] refer to Figure 9 For four polymers coated on a microneedle mold, a 48-hour pressurization and drying process was performed in an environment where the air pressure injected into the pressurized chamber was 3 bar, the air pressure discharged from the pressurized chamber was 1 bar, and the internal pressure of the pressurized chamber was 2 bar. At this time, for the polyvinyl alcohol (PVA) polymer, microneedles with tips forming microneedles and a size of 400 μm or larger were confirmed to have formed; for the other three polymers, no microneedles were confirmed to have formed.

[0071] refer to Figure 10 For four polymers coated on a microneedle mold, a 48-hour pressurization and drying process was performed in an environment where the air pressure injected into the pressurized chamber was 4 bar, the air pressure discharged from the pressurized chamber was 1 bar, and the internal pressure of the pressurized chamber was 3 bar. At this time, for the polyvinylpyrrolidone (PVP) polymer, microneedles with tips forming microneedles and a size of over 400 μm were confirmed to have formed; for the other three polymers, no microneedles were confirmed to have formed.

[0072] refer to Figure 11 For four polymers coated on a microneedle mold, a pressurization and drying process was performed for 48 hours in an environment where the air pressure injected into the pressurized chamber was 5 bar, the air pressure discharged from the pressurized chamber was 1 bar, and the internal pressure of the pressurized chamber was 4 bar. At this time, for all four polymers, microneedles with microneedle tips and a size of more than 400 μm were confirmed to have been formed.

[0073] refer to Figure 12 For four polymers coated on a microneedle mold, a pressurization and drying process was performed for 48 hours in an environment where the air pressure injected into the pressurized chamber was 6 bar, the air pressure discharged from the pressurized chamber was 1 bar, and the internal pressure of the pressurized chamber was 5 bar. At this time, for all four polymers, microneedles with microneedle tips and a size of more than 400 μm were confirmed to have been formed.

[0074] refer to Figure 13For four polymers coated on a microneedle mold, a pressurization and drying process was performed for 48 hours in an environment where the air pressure injected into the pressurized chamber was 7 bar, the air pressure discharged from the pressurized chamber was 1 bar, and the internal pressure of the pressurized chamber was 6 bar. At this time, for all four polymers, microneedles with microneedle tips and a size of more than 400 μm were confirmed to have been formed.

[0075] The above description of the present invention is merely illustrative. Those skilled in the art should understand that other specific modifications can be readily made without altering the technical concept or essential features of the invention. Therefore, it should be understood that the embodiments described above are merely illustrative in all respects and are not intended to limit the scope. For example, the constituent elements described as a single type can also be implemented separately, and similarly, the constituent elements described separately can also be implemented in combination.

[0076] The scope of this invention is defined by the claims described below, and all modifications or variations derived from the meaning and scope of the claims and from their equivalents shall be construed as being included within the scope of this invention.

[0077] Symbol Explanation

[0078] 100-microneedle mold

[0079] 110-Intaglio section

[0080] 111-Microstructure

[0081] 120 - Raw Material

[0082] 10-Clamp

[0083] 20-pallets

[0084] 30-Pressurized Chamber

[0085] 31-Injection Port

[0086] 32-Discharge outlet

Claims

1. A microneedle manufacturing method comprising the steps of: a step of applying a raw material substance containing an active ingredient to one or more concave portions formed in a microneedle mold; and a step of placing the microneedle mold to which the raw material substance is applied in a pressurized chamber, and pressurizing the raw material substance with an internal pressure of the pressurized chamber in order to fill the raw material substance in fine structures of the concave portions. In the pressurizing step, air injection and air discharge are simultaneously performed in the pressurized chamber, and a convection phenomenon is generated in the pressurized chamber, thereby simultaneously performing filling and drying of the raw material substance.

2. The microneedle manufacturing method according to claim 1, wherein when an air pressure injected into the pressurized chamber is X bar and an air pressure discharged from the pressurized chamber is Y bar, an internal pressure X-Y bar of the pressurized chamber is 1.5 bar or more.

3. The microneedle manufacturing method according to claim 2, wherein the air pressure injected into the pressurized chamber is 2 bar or more, and the air pressure discharged from the pressurized chamber is 0.5 bar or more.

4. The microneedle manufacturing method according to claim 1, wherein the microneedle mold is manufactured by injection molding a thermoplastic plastic resin.

5. The microneedle manufacturing method according to claim 4, wherein the thermoplastic plastic resin is at least one or more selected from the group consisting of polyethylene terephthalate (PET), polyvinyl chloride (PVC), and polypropylene (PP).

6. The microneedle manufacturing method according to claim 1, wherein the concave portions of the microneedle mold are tip concave portions, and each of the tip concave portions is independently present.

7. A microneedle manufacturing method comprising the steps of: a step of placing a plurality of microneedle molds on a jig; a step of applying a raw material substance containing an active ingredient to one or more concave portions formed in the microneedle molds; a step of fixing one or more of the jigs to a tray; and a step of placing the tray in a pressurized chamber, and pressurizing the raw material substance with an internal pressure of the pressurized chamber in order to fill the raw material substance in fine structures of the concave portions. In the pressurizing step, air injection and air discharge are simultaneously performed in the pressurized chamber, and a convection phenomenon is generated in the pressurized chamber, thereby simultaneously performing filling and drying of the raw material substance.

8. The microneedle manufacturing method according to claim 7, wherein when an air pressure injected into the pressurized chamber is X bar and an air pressure discharged from the pressurized chamber is Y bar, an internal pressure X-Y bar of the pressurized chamber is 1.5 bar or more.

9. The microneedle manufacturing method according to claim 8, wherein the air pressure injected into the pressurized chamber is 2 bar or more, and the air pressure discharged from the pressurized chamber is 0.5 bar or more.

Citation Information

Patent Citations

  • Method of Preparing Micro-Needle Using Biocompatible Polymer

    KR101747099B1

  • Method and apparatus for producing functional membrane

    JP2009082207A

  • Manufacturing method of micro needle

    KR101694317B1