一种吸湿透气仿皮超纤面料的制备工艺及产品

By combining microfiber top and bottom coatings with polyurethane and microfiber, a moisture-wicking and breathable imitation leather microfiber fabric is prepared. This solves the problem of insufficient moisture absorption and breathability of existing microfiber leather fabrics, improves softness and comfort, and is suitable for a variety of products.

CN118480200BActive Publication Date: 2026-07-17DONGGUAN KEDI IND CO LTD

Patent Information

Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
DONGGUAN KEDI IND CO LTD
Filing Date
2024-05-08
Publication Date
2026-07-17

AI Technical Summary

Technical Problem

Existing microfiber leather fabrics have low moisture absorption and breathability, which affects wearing comfort.

Method used

By employing a composite process of microfiber top coating and microfiber bottom coating, combined with polyurethane and microfiber, and through coating, drying, washing and texturing treatments, a moisture-wicking and breathable imitation leather microfiber fabric with a leather-like texture is prepared.

Benefits of technology

It improves the moisture absorption, breathability and softness of the fabric, making it suitable for shoe uppers, bags and protective shells for electronic products, with good texture and fashion.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0004827545760000021
    Figure BDA0004827545760000021
  • Figure BDA0004827545760000022
    Figure BDA0004827545760000022
  • Figure BDA0004827545760000031
    Figure BDA0004827545760000031
Patent Text Reader

Abstract

本申请涉及超纤皮面料的领域,具体公开了一种吸湿透气仿皮超纤面料的制备工艺及产品。一种吸湿透气仿皮超纤面料的制备工艺,包括以下制备步骤:S1、将超纤面涂料涂覆于第一皮纹纸,将超纤底涂料涂覆于第二皮纹纸,后将超纤面涂料和超纤底涂料进行复合,干燥,撕离第一皮纹纸和第二皮纹纸,制得仿皮超纤面料初品;S2、将制得的仿皮超纤面料初品进行水洗、揉纹处理,制得吸湿透气仿皮超纤面料。本申请的制备工艺制得的仿皮超纤面料具有较好的柔软性、吸湿性和透气性,适用于鞋垫、鞋面、箱包和电子产品保护外壳装饰等中,不易褶皱,舒适性好。