一种采用管道式制备CL-20 / Estane5703炸药颗粒及其制备方法

By using a pipeline preparation method, CL-20 and Estane 5703 solutions are mixed in a spiral glass pipe to form uniformly coated spherical particles, which solves the problems of uneven particle size and agglomeration in the water suspension method and improves the safety and preparation efficiency of explosives.

CN118530079BActive Publication Date: 2026-07-17BEIJING INST OF TECH

Patent Information

Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
BEIJING INST OF TECH
Filing Date
2024-05-24
Publication Date
2026-07-17

AI Technical Summary

Technical Problem

The existing water suspension method for preparing CL-20/Estane5703 particles suffers from uneven particle size and agglomeration, which affects the safety of the explosive, and the process parameters are difficult to control precisely.

Method used

A pipeline preparation method is adopted, in which CL-20 and Estane5703 solutions are mixed through a spiral glass pipeline to form spherical particles, and uniform coating is formed by diffusion using dichloromethane solvent, thus avoiding the use of surfactants.

Benefits of technology

The CL-20/Estane5703 particles were made uniform in size and regular in morphology, which improved the safety of the explosive and the simplicity of the preparation process, and reduced the probability of impact-sensitive explosion.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118530079B_ABST
    Figure CN118530079B_ABST
Patent Text Reader

Abstract

本发明公开了一种采用管道式制备CL‑20 / Estane5703炸药颗粒及其制备方法,涉及含能材料顿感包覆技术领域,其技术要点为:连续相匀速在管道中流动,分散相通过注射器匀速注入玻璃管道中形成单分散液滴,通过螺旋玻璃管道控制液滴;二氯甲烷与水相微溶,液滴中二氯甲烷扩散进入水相,液滴中Estane5703析出包覆CL‑20颗粒;以液滴为模板形成CL‑20 / Estane5703球形颗粒,球形颗粒在螺旋玻璃管道中导流进入收集容器;过滤、烘干,收集CL‑20 / Estane5703球形颗粒。本发明方法制备的CL‑20 / Estane5703炸药颗粒形貌规则、粒径均一、涂层均匀,具有较高的重复性和一致性。