Method and apparatus for stress corrosion prediction of grooved heat transfer tubes, device and medium

By screening the influencing factors of stress corrosion and constructing a stress corrosion prediction model, the problem of difficulty in assessing the stress corrosion risk of heat transfer tubes is solved, and efficient and accurate stress corrosion prediction is achieved, which is applicable to thin-walled heat transfer tubes in the nuclear power field.

CN118606594BActive Publication Date: 2026-11-24CHINA NUCLEAR POWER DESIGN COMPANY +1
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202410557451.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-05-07
Publication Date
2026-11-24
Estimated Expiration
2044-05-07

AI Technical Summary

Technical Problem

Existing technologies struggle to accurately predict the stress corrosion risk of dented heat transfer tubes, especially in the nuclear power sector, where complex and diverse influencing factors exacerbate the stress corrosion failure risk due to surface damage to the heat transfer tubes, and an effective assessment model is lacking.

Method used

By acquiring sample stress corrosion results data and multiple candidate stress corrosion influencing factors, input variables are selected, and the mapping relationship is determined using box plots. A stress corrosion prediction model is then constructed to predict the target stress corrosion results.

Benefits of technology

It improves the efficiency and accuracy of stress corrosion prediction, is applicable to stress corrosion assessment of dented heat transfer tubes, has high applicability, and can scientifically assess the impact of dented surface defects on the corrosion performance of thin-walled tubes.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118606594B_ABST
    Figure CN118606594B_ABST
Patent Text Reader

Abstract

This application discloses a method, apparatus, equipment, and medium for predicting stress corrosion of a dented heat transfer tube, relating to the field of stress corrosion assessment technology. The method includes: acquiring sample stress corrosion result data and multiple candidate stress corrosion influencing factors causing the sample stress corrosion results; selecting input variables from the multiple candidate stress corrosion influencing factors; plotting a box plot based on the sample stress corrosion result data and the input variables, and determining the mapping relationship between the sample stress corrosion result data and the input variables based on the distribution pattern of the quartile values ​​in the box plot; constructing a stress corrosion prediction model based on the mapping relationship between the sample stress corrosion result data and the input variables; and predicting the target stress corrosion result data of the dented heat transfer tube using the stress corrosion prediction model. This application can improve the efficiency of stress corrosion prediction.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application relates to the field of stress corrosion assessment technology, and in particular to a method and apparatus for predicting stress corrosion of a heat transfer tube with dents, an electronic device, and a computer-readable storage medium. Background Technology

[0002] Stress corrosion cracking has long been a typical failure mode for austenitic stainless steel and nickel-based alloys, and a common problem that many industries, including the nuclear power sector, urgently need to solve. Stress corrosion cracking is the result of the interaction between materials, environment, and stress. Due to the complexity of its formation mechanism, there are many technical challenges in experimental research and engineering assessment of stress corrosion. The surface damage state of stainless steel or nickel-based alloy heat transfer tube components affects the mechanical properties of the metal, such as wear resistance and stress corrosion resistance. In engineering fields including nuclear power, various thin-walled heat transfer tubes in heat exchangers inevitably suffer surface damage defects due to improper manufacturing processes, transportation impacts, installation collisions, jamming, and foreign object impacts during operation. These damages exacerbate the risk of stress corrosion failure in heat transfer tubes, posing a threat to the safe operation of the equipment.

[0003] Currently, due to the numerous factors affecting stress corrosion cracking of components, it is difficult to quantitatively assess the prediction of stress corrosion (such as stress corrosion crack propagation) of typical components under specific service conditions. This generally requires extensive experimental research, which takes a long time.

[0004] Therefore, it is necessary to address the difficulty in constructing existing stress corrosion prediction technologies. Summary of the Invention

[0005] This application aims to address at least one of the technical problems existing in the prior art. To this end, this application proposes a method and apparatus for predicting stress corrosion of a dented heat transfer tube, electronic equipment, and a computer-readable storage medium, which can improve the efficiency of stress corrosion prediction.

[0006] To achieve the above objectives, a first aspect of this application proposes a method for predicting stress corrosion of a dented heat transfer tube, the method comprising:

[0007] Obtain sample stress corrosion results data and multiple candidate stress corrosion influencing factors that cause the sample stress corrosion results;

[0008] Input variables were selected from multiple candidate factors affecting stress corrosion.

[0009] A box plot is drawn based on the sample stress corrosion results data and the input variables, and the mapping relationship between the sample stress corrosion results data and the input variables is determined based on the distribution pattern of the quartile values ​​in the box plot.

[0010] Based on the mapping relationship between the sample stress corrosion results data and the input variables, a stress corrosion prediction model is constructed.

[0011] The stress corrosion prediction model is used to predict the target stress corrosion results of the dented heat transfer tube.

[0012] Optionally, the acquisition of sample stress corrosion result data and multiple candidate stress corrosion influencing factors that cause the sample stress corrosion results includes:

[0013] Multiple candidate factors influencing stress corrosion were obtained;

[0014] Based on multiple candidate stress corrosion influencing factors, indentations were created on the initial sample to obtain the target sample;

[0015] The target sample is placed in a preset corrosion environment, and corrosion state data of the target sample is acquired at predetermined intervals.

[0016] Statistical analysis was performed on all the acquired corrosion state data to obtain the stress corrosion result data of the sample.

[0017] Optionally, the candidate stress corrosion influencing factors include sample indentation type and sample indentation depth;

[0018] The step of creating a dent in the initial sample based on multiple candidate stress corrosion influencing factors to obtain the target sample includes:

[0019] The punch is determined based on the type of indentation in the sample.

[0020] Obtain the impact mode, and obtain the mapping relationship between the first energy and the dent depth corresponding to the impact mode;

[0021] By using the mapping relationship between the first energy and the indentation depth, the indentation depth of the sample is mapped to obtain the target energy;

[0022] The target sample is obtained by applying the target energy to the initial sample using the impact method and the punch.

[0023] Optionally, the first energy-dent depth mapping relationship includes candidate energy-dent depth mapping relationships corresponding to multiple candidate dent types;

[0024] The step of mapping the sample indentation depth using the mapping relationship between the first energy and the indentation depth to obtain the target energy includes:

[0025] Based on the sample dent type, the candidate energy and dent depth mapping relationship corresponding to multiple candidate dent types is filtered to obtain the second energy and dent depth mapping relationship;

[0026] By utilizing the second energy-dimple depth mapping relationship, the sample dimple depth is mapped to obtain the target energy.

[0027] Optionally, the input variables include sample loading stress and sample indentation depth, and the mapping relationship includes a positive correlation between the sample stress corrosion result data and the sample loading stress, and a quadratic curve relationship between the sample stress corrosion result data and the sample indentation depth;

[0028] The step of constructing the stress corrosion prediction model based on the mapping relationship between the sample stress corrosion results data and the input variables includes:

[0029] Based on the positive correlation between the sample stress corrosion results and the sample loading stress, a first formula is constructed.

[0030] Based on the quadratic curve relationship between the stress corrosion results of the sample and the indentation depth of the sample, a second formula is constructed.

[0031] The stress corrosion prediction model is determined based on the first formula and the second formula.

[0032] Optionally, the step of constructing the stress corrosion prediction model based on the mapping relationship between the sample stress corrosion result data and the input variables further includes:

[0033] By integrating the first formula and the second formula, we obtain the first integrated formula;

[0034] A third formula is constructed based on the sample loading stress and the sample indentation depth, which indicates the multiplicative relationship between the sample loading stress and the sample indentation depth.

[0035] The stress corrosion prediction model is determined based on the first integrated formula and the third formula.

[0036] Optionally, determining the stress corrosion prediction model based on the first integration formula and the third formula includes:

[0037] The first integrated formula and the third formula are integrated to obtain the second integrated formula;

[0038] Obtain the environmental factors of sample corrosion;

[0039] The stress corrosion prediction model is obtained by multiplying the sample corrosion environment factor and the second integrated formula.

[0040] Optionally, the sample stress corrosion results data include the crack length of the sample cross-section, and the stress corrosion prediction model is shown in the following formula:

[0041] L=β*(p0+p1x+p2y+p3x 2 +p4xy+ε);

[0042] Where L is the crack length of the sample cross section, x is the dent depth of the sample, y is the loading stress of the sample, β is the corrosion environment factor of the sample, p0, p1, p2, p3, and p4 are all coefficients, and ε is the random error.

[0043] Optionally, the input variable includes the sample dent type, and the stress corrosion prediction model includes candidate stress corrosion prediction models corresponding to the sample dent type;

[0044] The data predicting the target stress corrosion result of the dented heat transfer tube using the stress corrosion prediction model includes:

[0045] The type of the dented heat transfer tube is detected to obtain the target dent type;

[0046] If the target dent type is consistent with the sample dent type, then the dented heat transfer pipe is predicted using the candidate stress corrosion prediction model corresponding to the sample dent type, and the target stress corrosion result data is obtained.

[0047] Optionally, the prediction of the target stress corrosion result data of the dented heat transfer tube using the stress corrosion prediction model includes:

[0048] Obtain the correspondence between the sample nondestructive testing signal and multiple input variables;

[0049] Based on the aforementioned correspondence, the stress corrosion prediction model is transformed to obtain the signal stress corrosion prediction model.

[0050] The dented heat transfer tube was subjected to non-destructive testing to obtain the target non-destructive testing signal;

[0051] The target non-destructive testing signal is input into the signal stress corrosion prediction model to predict corrosion and obtain the target stress corrosion result data.

[0052] To achieve the above objectives, a second aspect of this application provides a stress corrosion prediction device for a dented heat transfer tube, the device comprising:

[0053] The acquisition module is used to acquire sample stress corrosion result data and multiple candidate stress corrosion influencing factors that cause the sample stress corrosion results;

[0054] The filtering module is used to filter input variables from multiple candidate stress corrosion influencing factors;

[0055] The determination module is used to draw a box plot based on the sample stress corrosion result data and the input variables, and to determine the mapping relationship between the sample stress corrosion result data and the input variables based on the distribution pattern of the quartile values ​​in the box plot;

[0056] A construction module is used to construct a stress corrosion prediction model based on the mapping relationship between the sample stress corrosion result data and the input variables;

[0057] The prediction module is used to predict the target stress corrosion result data of the dented heat transfer pipe through the stress corrosion prediction model.

[0058] To achieve the above objectives, a third aspect of this application provides an electronic device, which includes a memory and a processor. The memory stores a computer program, and the processor executes the computer program to implement the stress corrosion prediction method for the dented heat transfer tube described in the first aspect.

[0059] To achieve the above objectives, a fourth aspect of this application provides a computer-readable storage medium storing a computer program that, when executed by a processor, implements the stress corrosion prediction method for dented heat transfer tubes described in the first aspect.

[0060] In this embodiment, input variables are first selected from multiple candidate stress corrosion influencing factors. A box plot is then used to determine the mapping relationship between the sample stress corrosion results data and the input variables. Based on this mapping relationship, a stress corrosion prediction model is constructed, and predictions are then made using this model. Specifically, the distribution pattern of the quartile values ​​in the box plot indicates the mapping relationship between the sample stress corrosion results data and the input variables, thus enabling the construction of the stress corrosion prediction model. Finally, the constructed stress corrosion prediction model can be used to predict the target stress corrosion results data of the dented heat transfer pipe. This embodiment improves the efficiency of stress corrosion prediction.

[0061] Additional aspects and advantages of this application will be set forth in part in the description which follows, and in part will be obvious from the description, or may be learned by practice of this application. Attached Figure Description

[0062] Figure 1 This is a flowchart of the stress corrosion prediction method for a dented heat transfer tube provided in the embodiments of this application;

[0063] Figure 2 yes Figure 1 The flowchart for step 101 in the document;

[0064] Figure 3A This is a schematic diagram illustrating the energy-depth mapping relationship of a triangular prism-shaped indentation;

[0065] Figure 3B This is a schematic diagram illustrating the energy-depth mapping relationship of a hemispherical indentation;

[0066] Figures 4A-4D This is a schematic diagram illustrating the relationship between input variables and crack length in the sample cross-section;

[0067] Figures 5A-5B This is a schematic diagram showing the relationship between the crack length of the sample cross section and the loading stress on the sample.

[0068] Figures 6A-6B This is a schematic diagram showing the relationship between the crack length and the indentation depth of the sample cross-section;

[0069] Figure 7 yes Figure 1 The flowchart for step 104 in the document;

[0070] Figure 8 yes Figure 1 The flowchart for step 104 in the document;

[0071] Figure 9 yes Figure 1 The flowchart for step 105 in the document;

[0072] Figure 10 This is a schematic diagram of the stress corrosion prediction device with a dented heat transfer tube provided in the embodiments of this application;

[0073] Figure 11 This is a schematic diagram of the structure of the electronic device provided in the embodiments of this application. Detailed Implementation

[0074] To make the objectives, technical solutions, and advantages of this application clearer, the following detailed description is provided in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are merely illustrative and not intended to limit the scope of this application.

[0075] It should be noted that although functional modules are divided in the device schematic diagram and a logical order is shown in the flowchart, in some cases, the steps shown or described may be performed in a different order than the module division in the device or the order in the flowchart. The terms "first," "second," etc., in the specification, claims, and the aforementioned drawings are used to distinguish similar objects and are not necessarily used to describe a specific order or sequence.

[0076] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as commonly understood by one of ordinary skill in the art to which this application belongs. The terminology used herein is for the purpose of describing embodiments of this application only and is not intended to limit this application.

[0077] Stress corrosion cracking has long been a typical failure mode for austenitic stainless steel and nickel-based alloys, and a common problem that many industries, including the nuclear power sector, urgently need to solve. Stress corrosion cracking is the result of the interaction between materials, environment, and stress. Due to the complexity of its formation mechanism, there are many technical challenges in experimental research and engineering assessment of stress corrosion. The surface damage state of stainless steel or nickel-based alloy heat transfer tubes affects the mechanical properties of the metal, such as wear resistance and stress corrosion resistance. Thin-walled heat transfer tubes in various heat exchangers in engineering fields, including nuclear power, inevitably suffer surface damage defects due to improper manufacturing processes, transportation impacts, installation collisions, jamming, and foreign object impacts during operation. These damages exacerbate the risk of stress corrosion failure, posing a threat to the safe operation of the equipment. Furthermore, because many factors influence stress corrosion cracking of components, it is difficult to quantitatively assess the stress corrosion sensitivity and stress corrosion crack propagation of typical components under specific service conditions. This requires extensive experimental research, which is time-consuming and costly. To date, the industry still lacks predictive and assessment models for stress corrosion crack initiation and cracking in typical nickel-based alloys (such as 690 and 600) and austenitic stainless steels with surface defects.

[0078] Currently, data on stress corrosion of surface-damaged dented tubes is extremely scarce, severely limiting the assessment and prediction of stress corrosion in heat transfer tubes with such surface defects. Furthermore, due to the complexity of stress corrosion influencing factors and the diversity of service environments, these factors exhibit highly nonlinear and strongly coupled relationships. Current methods for predicting and assessing the initiation and propagation of stress corrosion cracks in some thin-walled tubes generally rely on data parameter correlation or mechanistic modeling. This makes it difficult to accurately characterize the mapping relationship between crack initiation and propagation and the various influencing parameters, and similarly fails to support the industry's prediction and assessment of stress corrosion in thin-walled heat transfer tubes with surface-damaged nickel-based alloys and austenitic stainless steel.

[0079] Therefore, the main objective of this application is to establish a fundamental predictive model for stress corrosion of surface-dented heat transfer tubes that integrates multiple factors, and to further refine the model by combining it with non-destructive testing signals from in-service inspections in nuclear power plants. This model can address the service safety assessment of such components. Therefore, there is an urgent need to conduct systematic research on surface-dented defects in nickel-based alloys and austenitic stainless steel, scientifically assess the impact of surface defects of different scales on the microstructure and corrosion performance of thin-walled tubes, establish corresponding predictive assessment models, and correlate these models with non-destructive testing results of heat transfer tubes from nuclear power plants for service performance evaluation.

[0080] The stress corrosion prediction method, apparatus, electronic device, and storage medium for dented heat transfer tubes provided in this application are specifically illustrated through the following embodiments. First, the stress corrosion prediction method for dented heat transfer tubes in this application is described.

[0081] Please refer to Figure 1 , Figure 1 An optional flowchart of a method for predicting stress corrosion in dented heat transfer tubes is disclosed. Figure 1 The method may include, but is not limited to, steps 101 to 105.

[0082] Step 101: Obtain the sample stress corrosion result data and multiple candidate stress corrosion influencing factors that cause the sample stress corrosion results;

[0083] Step 102: Select input variables from multiple candidate stress corrosion influencing factors;

[0084] Step 103: Draw a box plot based on the sample stress corrosion results data and input variables, and determine the mapping relationship between the sample stress corrosion results data and input variables based on the distribution pattern of the quartile values ​​in the box plot.

[0085] Step 104: Based on the mapping relationship between the sample stress corrosion results data and the input variables, a stress corrosion prediction model is constructed.

[0086] Step 105: Predict the target stress corrosion result data of the dented heat transfer tube using the stress corrosion prediction model.

[0087] Steps 101 to 105, as illustrated in this embodiment, firstly, input variables are selected from multiple candidate stress corrosion influencing factors. Secondly, a box plot is used to determine the mapping relationship between the sample stress corrosion result data and the input variables. Based on this mapping relationship, a stress corrosion prediction model is constructed, and then prediction is performed using this model. Specifically, the distribution pattern of the quartile values ​​in the box plot can indicate the mapping relationship between the sample stress corrosion result data and the input variables, thus ensuring high accuracy of the constructed stress corrosion prediction model. Finally, the constructed stress corrosion prediction model can be used to predict the target stress corrosion result data of the dented heat transfer pipe. This embodiment improves the efficiency of stress corrosion prediction. Furthermore, the stress corrosion prediction model provided in this application has high prediction accuracy and high applicability.

[0088] In step 101 of some embodiments, the sample stress corrosion result data refers to the data obtained by subjecting a dented pipe (such as a dented heat transfer pipe) to stress corrosion in a corrosive environment. For example, the sample stress corrosion result data includes the sample oxide film thickness, the sample cross-sectional crack length, and the sample surface crack length. Taking the sample oxide film thickness as an example, the sample oxide film thickness of the dented heat transfer pipe is 1 mm after 100 hours in a corrosive environment.

[0089] The degree of stress corrosion experienced by dented pipe fittings varies, resulting in different stress corrosion outcomes. This difference in stress corrosion degree is reflected in the different candidate stress corrosion influencing factors, which characterize the factors or elements affecting the degree of stress corrosion. Multiple candidate stress corrosion influencing factors include sample dent type, sample loading stress, sample dent depth, number of impacts, and sample cross-dents. Among these, sample dent type, number of impacts, and sample cross-dents are categorical variables, while sample loading stress and sample dent depth are numerical variables. For example, sample dent types include hemispherical and triangular prism types. The number of impacts includes one and more than one. Sample cross-dents include cross-dents and non-cross-dents. Sample loading stress is a positive number, for example, within [0,2], and the unit is multiples. Sample dent depth is a positive number, for example, within [0,1], and the unit is mm.

[0090] Therefore, in one embodiment, reference is made to Figure 2 Step 101 includes:

[0091] Step 201: Obtain multiple candidate factors affecting stress corrosion;

[0092] Step 202: Based on multiple candidate stress corrosion influencing factors, indentation is created on the initial sample to obtain the target sample;

[0093] Step 203: Place the target sample in a preset corrosion environment and acquire corrosion status data of the target sample at predetermined intervals.

[0094] Step 204: Perform statistical analysis on all acquired corrosion state data to obtain sample stress corrosion result data.

[0095] In step 201, for stress corrosion tests on heat transfer tubes with dent defects, multiple candidate stress corrosion influencing factors include sample dent type, sample loading stress, sample dent depth, number of sample impacts, and sample cross-dents. These candidate stress corrosion influencing factors can be obtained by consulting relevant stress corrosion test standards.

[0096] In step 202, the initial sample (also called the initial specimen) can be prepared according to the stress corrosion test standard, using heat transfer tube materials, including C-rings, U-bends, and reverse U-bends. Indentation defects are prepared on the outer surface of the initial sample to obtain the target sample.

[0097] The relevant technologies address stress corrosion testing and evaluation of thin-walled heat transfer tubes with surface defects, specifically stress corrosion testing and evaluation of tubes with surface scratches. However, the methods and mechanisms of surface scratches differ from those of surface indentations. Compared to scratches, the pre-production of surface indentations is more difficult, typically due to the challenge in controlling the defect morphology and depth. Furthermore, there is a lack of predictive models for the initiation and cracking of stress corrosion cracks in nickel-based and stainless steel components caused by different types of surface damage, which would be insufficient to guide the prediction and evaluation of stress corrosion damage in thin-walled tubes.

[0098] In one embodiment, multiple stress corrosion influencing factors include sample indentation type and sample indentation depth, and step 202 includes:

[0099] Determine the punch type based on the sample dent type;

[0100] Obtain the impact mode, and obtain the mapping relationship between the first energy and the dent depth corresponding to the impact mode;

[0101] By utilizing the mapping relationship between the first energy and the indentation depth, the indentation depth of the sample is mapped to obtain the target energy;

[0102] The target sample is obtained by applying the target energy to the initial sample using an impact method and a punch.

[0103] Specifically, this embodiment primarily employs impact methods to provide impact energy for preparing dent defects. Impact methods include energy control techniques such as free fall, drop hammer impact, pressing, and pendulum impact. By exploring the relationship between energy and depth on the outer surface of the heat transfer tube under different impact methods, the mapping relationship between energy and depth is solidified, and surface dent depths for different samples are determined based on different energies. For example, assuming the impact method is pendulum impact, the corresponding dent depths under different energies are first collected. Then, data fitting techniques (such as least squares method) can be used to determine the mapping relationship, finally obtaining the first energy-dent depth mapping relationship corresponding to the pendulum impact method.

[0104] The advantage of the above embodiments is that they fully demonstrate the different energy and dent depth mapping relationships under different impact methods, thereby improving the accuracy of manufacturing target samples.

[0105] In one embodiment, the first energy-dimple depth mapping relationship includes candidate energy-dimple depth mapping relationships corresponding to multiple candidate dimple types; the process of mapping the sample dimple depth using the first energy-dimple depth mapping relationship to obtain the target energy may include:

[0106] Based on the sample indentation type, the candidate energy and indentation depth mapping relationship corresponding to multiple candidate indentation types is filtered to obtain the second energy and indentation depth mapping relationship;

[0107] By utilizing the mapping relationship between the second energy and the indentation depth, the indentation depth of the sample is mapped to obtain the target energy.

[0108] In one example, using a pendulum impact method to prepare hemispherical and triangular prism-shaped defects, a spherical punch and a triangular prism punch are selected to prepare circular and strip-shaped indentations, respectively. The punch is made of stainless steel with a hardness matching that of nickel-based 690 alloy. The rear end dimension of the punch is variable to control the mass. Material selection: a relatively hard material to avoid the effects of impact wear. Mass range: 10 to 50g; Punch angle: α = 60°; Dimension design: L (length) ≤ 2mm, H (height) ≤ 1mm. Figure 3A As shown, if the indentation is triangular prism-shaped, then the energy-depth mapping relationship is D = 92E + 48. Where D represents depth in mm and E represents energy in J. Figure 3B As shown, if the indentation is hemispherical, then the depth-energy mapping relationship is D = 2.7E. 2 +58E+51. Where D represents depth and E represents energy. For example, if the sample indentation type is triangular prism and the sample indentation depth is 200mm, then using D=92E+48, the target energy is calculated to be 1.65(J).

[0109] The advantage of the above embodiments is that they can fully reflect the different energy and dent depth mapping relationships corresponding to different dent types under the same impact mode, thereby improving the accuracy of determining the target energy.

[0110] In step 203, the corrosive environment refers to the environment in which the target sample is located, such as the primary loop of a nuclear power plant, the secondary loop of a nuclear power plant, or the corrosion loop of a typical chemical heat exchanger. The target sample will undergo stress corrosion in the corrosive environment, thus exhibiting different corrosion states. Corrosion state data can be obtained by sampling and analyzing the target sample. Specifically, corrosion state data of the target sample can be acquired at predetermined intervals (e.g., every 100 hours). The corrosion state data includes surface morphology, crack initiation and propagation states, crack initiation area, initiation time, propagation rate, and crack length.

[0111] In step 204, statistical analysis is performed on all acquired corrosion state data to obtain sample stress corrosion result data. This data includes sample oxide film thickness, sample cross-sectional crack length, sample surface crack length, and sample propagation rate. For example, statistical analysis of all acquired surface morphologies yields the sample oxide film thickness of the target sample. Similarly, statistical analysis of all acquired crack lengths yields the sample cross-sectional crack length or sample surface crack length of the target sample. Likewise, statistical analysis of all acquired propagation rates yields the sample propagation rate of the target sample. Likewise, based on crack initiation and propagation states, statistical analysis of crack initiation areas, initiation times, etc., yields other types of sample stress corrosion result data, which will not be elaborated upon here.

[0112] In steps 201 to 204, by first creating the dent and then analyzing the stress corrosion results of the sample, the dent defect can be effectively created and analyzed.

[0113] In step 102 of some embodiments, through analysis and sorting of multiple candidate stress corrosion influencing factors, a total of several variables are included, such as sample indentation type, sample loading stress, sample indentation depth, number of sample impacts, and sample cross-indentations. The analysis shows that sample indentation type, sample indentation depth, and sample loading stress are key variables affecting the cross-sectional crack length.

[0114] In one embodiment, step 102 includes:

[0115] Evaluate the impact of each candidate stress corrosion influencing factor on the sample stress corrosion results data;

[0116] Multiple input variables were selected from various stress corrosion influencing factors based on their impact.

[0117] For example, the importance and attributes of each candidate stress corrosion influencing factor are analyzed and evaluated to obtain the influence degree. If the influence degree is greater than the influence degree threshold, the candidate stress corrosion influencing factor is determined as an input variable. In one embodiment, the sample indentation type, sample indentation depth, and sample loading stress can be selected as input variables, and the sample cross-sectional crack length can be selected as an output variable.

[0118] It should be noted that analysis of all stress corrosion cross-sectional crack data revealed that, due to the diversity of influencing factors and the complexity of experimental process control, the relationship between multiple input variables and the crack length of the sample cross-section could not be determined. For example, referring to... Figure 4A When the sample loading stress is constant, the relationship between the sample indentation depth and the sample cross-sectional crack length is not obvious. (Refer to...) Figure 4BWhen the depth of the indentation in the sample is constant, the relationship between the loaded stress on the sample and the crack length in the sample cross-section is not obvious. (Refer to...) Figure 4C The relationship between the sample loading stress / sample indentation depth and the sample cross-sectional crack length is not obvious. (Refer to...) Figure 4D The relationship between the sample loading stress / sample indentation depth and the sample cross-sectional crack length is not obvious.

[0119] In step 103 of some embodiments, a box plot can be used to reflect the central location and distribution range of one or more sets of continuous quantitative data. This embodiment utilizes the distribution patterns of quartile values ​​in the box plot to determine the mapping relationship between sample stress corrosion results and input variables. The mapping relationship includes a positive correlation between sample stress corrosion results and sample loading stress, and a quadratic curve relationship between sample stress corrosion results and sample indentation depth.

[0120] Taking the crack length of the sample section as an example, such as Figure 5A As shown, the horizontal axis represents the sample's loading stress (in multiples), and the vertical axis represents the crack length of the sample's cross-section (in mm). From Figure 5A The box plot shows that although the overall data sample is discretely distributed, the quartile values ​​generally exhibit a linear relationship, leading to the conclusion that the crack length of the sample cross-section is positively correlated with the sample loading stress. Specifically, when the sample loading stress is 0.7 times the normal stress, the quartile value of the crack length in the sample cross-section is approximately 0.1; when the sample loading stress is 0.8 times the normal stress, the quartile value of the crack length in the sample cross-section is approximately 1.8, and so on. Figure 5B As shown, the horizontal axis represents the quantiles of the sample's loading stress (in multiples), and the vertical axis represents the quantiles of the crack length in the sample's cross-section (in mm). Figure 5B It can be seen that, under the same indentation depth, the crack length of the sample cross-section continuously increases with the increase of the sample loading stress. Under the same sample loading stress, such as Figure 6A As shown, the horizontal axis represents the depth of the indentation in the sample (in mm), and the vertical axis represents the length of the crack in the sample cross-section (in mm). Figure 6A The box plot shows that although the overall data sample is discretely distributed, the quartile values ​​generally exhibit a curved pattern, leading to the conclusion that the crack length of the sample cross-section and the sample loading stress have a quadratic curve relationship. Alternatively, as shown... Figure 6B As shown, the horizontal axis represents the depth of the indentation in the sample (in mm), and the vertical axis represents the length of the crack in the sample cross-section (in mm). Figure 6B It can be seen that, under the same loading stress conditions, as the depth of the indentation in the sample increases, the crack length of the sample cross section first increases and then decreases.

[0121] In step 104 of some embodiments, a stress corrosion prediction model can be constructed based on the mapping relationship between sample stress corrosion result data and input variables. (Refer to...)Figure 7 In one embodiment, step 104 includes:

[0122] Step 701: Based on the positive correlation between the sample stress corrosion results and the sample loading stress, construct the first formula;

[0123] Step 702: Based on the quadratic relationship between the sample stress corrosion results and the sample indentation depth, construct the second formula;

[0124] Step 703: Determine the stress corrosion prediction model based on the first formula and the second formula.

[0125] For example, the first formula is G = k1 * y + b1, where G represents the sample stress corrosion result data, y represents the sample loading stress, and k1 and b1 are coefficients. The second formula is G = k2 * x. 2 +k3*x+b2, G represents the sample stress corrosion result data, x represents the sample indentation depth, and k2, k3, and b2 are all coefficients.

[0126] In step 703, a stress corrosion prediction model can be obtained by integrating the first and second formulas, for example, G = k1*y + k2*x 2 +k3*x+b3. Where b3 is a coefficient. It should be noted that k1, k2, k3, and b3 need to conform to different numerical ranges at different confidence levels. For example, at a 95% confidence level, k1 should be within [1.531, 2.291], k2 within [-1.797, 0.2214], k3 within [2.165, 4.382], and b3 within [-1.005, 1.088].

[0127] The advantage of the embodiments of steps 701 to 703 is that different mapping relationships first determine the corresponding formulas, and then all formulas are fused to obtain the stress corrosion prediction model, making the model construction process relatively simple and easy to implement.

[0128] In another embodiment, the influence of the interaction between sample loading stress and sample indentation depth on the sample stress corrosion results data also needs to be considered. In the specific implementation of this embodiment, refer to... Figure 8 Step 104 may also include:

[0129] Step 801: Integrate the first formula and the second formula to obtain the first integrated formula;

[0130] Step 802: Based on the sample loading stress and the sample indentation depth, construct a third formula. The third formula is used to indicate the multiplicative relationship between the sample loading stress and the sample indentation depth.

[0131] Step 803: Determine the stress corrosion prediction model based on the first integrated formula and the third formula.

[0132] For example, the first integrated formula is G = k1*y + k2*x 2 Given that the first formula is +k3*x+b3 and the third formula is G=k4*x*y, then the stress corrosion prediction model obtained by integrating the first and third formulas is G=k1*y+k2*x 2 +k3*x+k4*x*y+b4. Where b4 is the coefficient. For example, the third formula is G=k4*x 2 The stress corrosion prediction model obtained by adding the first and third integrated formulas is G = k1*y + k2*x. 2 +k3*x+k4*x 2 *y+b4. The coefficients in the stress corrosion prediction model can be estimated from experimental data. For details on how to estimate them, please refer to the example in Table 1 below.

[0133] The benefit of this implementation is that it can fully consider the interaction between sample loading stress and sample indentation depth on the sample stress corrosion results data, further improving the prediction accuracy and universality of the stress corrosion prediction model.

[0134] In one embodiment, step 803 includes:

[0135] By integrating the first and third formulas, we obtain the second integrated formula;

[0136] Obtain the environmental factors of sample corrosion;

[0137] By multiplying the sample corrosion environment factor and the second integrated formula, a stress corrosion prediction model is obtained.

[0138] For example, the second integrated formula is G = k1*y + k2*x 2 Given that k3*x + k4*x*y + b4, and the sample corrosion environment factor is β, the obtained stress corrosion prediction model is G = β*(k1*y + k2*x). 2 +k3*x+k4*x*y+b4).

[0139] The benefit of this implementation is that it can fully reflect the impact of corrosive environmental factors on the stress corrosion results data of the samples, and further improve the prediction accuracy and universality of the stress corrosion prediction model.

[0140] In one embodiment, the crack length of the sample cross-section is positively correlated with the sample loading stress; the crack length of the sample cross-section and the sample indentation depth exhibit a quadratic relationship; different corrosion environments (e.g., different corrosive media) are addressed by introducing a sample corrosion environment factor β; the sample indentation type is incorporated into the model formula as a piecewise function to reflect its influence. The sample loading stress corresponds to a linear function, and the sample indentation depth corresponds to a quadratic function. Introducing the interaction term of these two variables, the stress corrosion prediction model is shown in the following formula:

[0141] L=β*(p0+p1x+p2y+p3x 2 +p4xy+ε).

[0142] Where L is the crack length of the sample cross section, x is the dent depth of the sample, y is the loading stress of the sample, β is the corrosion environment factor of the sample, p0, p1, p2, p3, and p4 are all coefficients, and ε is the random error.

[0143] Ultimately, a multi-factor coupled stress corrosion prediction model was constructed, incorporating factors such as sample indentation depth, sample loading stress, and sample indentation type. Overall, using stress corrosion results data and multiple input variables, regression analysis was used to determine the parameters in the general formula of the prediction model. A comprehensive evaluation of goodness of fit and minimum error was then performed to finalize the prediction model. Table 1 shows the estimated values ​​and confidence intervals of the coefficients of the prediction model constructed using the experimental data (including stress corrosion results data and multiple input variables) of this embodiment.

[0144]

[0145] Table 1

[0146] In Table 1, R 2 R represents the prediction accuracy of the stress corrosion prediction model, and RMSE represents the root mean square error of the stress corrosion prediction model. 2 The larger the value, the higher the prediction accuracy of the stress corrosion prediction model. The smaller the RMSE, the smaller the root mean square error of the stress corrosion prediction model, thus indicating higher prediction accuracy. At p0 = -0.827, p1 = 3.274, p2 = 1.911, p3 = -0.7877, and p4 = -3.627, R... 2 =0.82; RMSE =0.0782. Each coefficient is within the confidence interval of its corresponding regression coefficient and has a 95% confidence level.

[0147] In step 105 of some embodiments, the target stress corrosion result data of the dented heat transfer tube is predicted using a stress corrosion prediction model. Specifically, if the sample stress corrosion result data includes the sample oxide film thickness, then the target stress corrosion result data includes the target oxide film thickness; if the sample stress corrosion result data includes the sample cross-sectional crack length, then the target stress corrosion result data includes the target cross-sectional crack length; and if the sample stress corrosion result data includes the sample surface crack length, then the target stress corrosion result data includes the target surface crack length.

[0148] In one embodiment, if the input variable includes the sample indentation type, the stress corrosion prediction model includes candidate stress corrosion prediction models corresponding to the sample indentation type. In this embodiment, step 105 includes:

[0149] Type detection is performed on the dented heat transfer tube to determine the target dent type;

[0150] If the target dent type is consistent with the sample dent type, the target stress corrosion result data is obtained by predicting the heat transfer tube with dent using the candidate stress corrosion prediction model corresponding to the sample dent type.

[0151] In one example, detecting the dents on a dented heat transfer tube reveals that the target dent type is triangular prism. If the sample dent type includes triangular prisms, the heat transfer tube can be predicted using a candidate stress corrosion prediction model corresponding to the triangular prism type, ultimately yielding the target stress corrosion result data.

[0152] The advantage of the above embodiments is that they fully demonstrate the different effects of different types of indentations on stress corrosion prediction, thereby further improving the accuracy of prediction.

[0153] In one embodiment, reference is made to Figure 9 Step 105 may also include:

[0154] Step 901: Obtain the correspondence between the sample nondestructive testing signal and multiple input variables;

[0155] Step 902: Based on the correspondence, perform variable transformation on the stress corrosion prediction model to obtain the signal stress corrosion prediction model;

[0156] Step 903: Perform non-destructive testing on the dented heat transfer tube to obtain the target non-destructive testing signal;

[0157] Step 904: Input the target non-destructive testing signal into the signal stress corrosion prediction model to predict corrosion and obtain the target stress corrosion result data.

[0158] In step 901, the dent distribution characteristics (such as dent contour and dent depth) of the target sample (e.g., heat transfer tube sample) prepared above can be used, combined with common non-destructive testing methods currently used in the manufacturing, installation, and operation phases of nuclear power heat transfer tubes, to prepare calibration sample tubes. The dent depth range of the calibration sample tubes must cover the dent defects of all samples used for corrosion testing. Non-destructive testing (NDT) refers to the use of different NDT techniques to evaluate the quality of materials or components. These techniques may include ultrasonic testing, X-ray testing, eddy current testing, etc. These techniques can detect defects, cracks, or other undesirable conditions in materials or components. Taking eddy current testing as an example, pre-fabrication defects of all calibration sample tubes are tested, and eddy current signal impedance diagrams are recorded to obtain the correspondence between the sample eddy current signal and multiple input variables, such as the correspondence between the sample eddy current signal and the dent depth, applied stress, and dent type of the calibration sample tube.

[0159] In step 902, based on the obtained correspondence, the input variables in the stress corrosion prediction model are equivalently transformed into sample non-destructive testing signals, thereby obtaining the signal stress corrosion prediction model.

[0160] In steps 903 and 904, for example, if the nondestructive testing is specifically eddy current testing, the input variable is converted into a sample eddy current testing signal. Using the signal stress corrosion prediction model, during eddy current testing of heat transfer tubes in nuclear power plant steam generators, the potential stress corrosion cross-sectional crack length of the dented heat transfer tube can be quantitatively assessed directly using the actual eddy current signal. This allows for a subsequent integrity assessment to determine whether the dented heat transfer tube needs to be plugged. Furthermore, based on the abnormal signal characteristics of nondestructive testing results during the manufacturing and operation phases of the heat transfer tube, quantitative crack data (such as oxide film thickness, cross-sectional crack length, and surface crack length) can be predicted using the stress corrosion prediction model. Based on the predicted quantitative crack data, the prediction results are used as input parameters according to specifications to conduct an integrity assessment of the defective heat transfer tube, achieving the final evaluation and analysis of the heat transfer tube's service performance.

[0161] The benefits of this embodiment include: 1. It proposes a method for constructing a stress corrosion prediction model, which is simple to construct, has high prediction accuracy, reduces the experimental cycle, and greatly compresses experimental costs, providing an optimized solution for stress corrosion prediction and evaluation of typical components in related industries. 2. The proposed method of first converting non-destructive (eddy current testing) detection signals into input parameters for the stress corrosion prediction model, and then directly detecting and evaluating the crack initiation and propagation trend of stress corrosion online, can improve the efficiency and economy of inspection and maintenance of heat transfer tubes in nuclear power plant steam generators.

[0162] The various technical features in the above embodiments can be combined arbitrarily, as long as there is no conflict or contradiction between the combinations of features. However, due to space limitations, they are not described one by one. Therefore, the arbitrary combination of various technical features in the above embodiments is also within the scope of this specification.

[0163] Please see Figure 10 This application also provides a stress corrosion prediction device for a dented heat transfer tube, which can realize the stress corrosion prediction method for the dented heat transfer tube described above. Figure 10 This is a block diagram of a module structure for a stress corrosion prediction device for a dented heat transfer tube provided in an embodiment of this application. The device includes:

[0164] The acquisition module 1001 is used to acquire sample stress corrosion result data and multiple candidate stress corrosion influencing factors that cause the sample stress corrosion results;

[0165] The filtering module 1002 is used to filter input variables from multiple candidate stress corrosion influencing factors;

[0166] The module 1003 is used to draw a box plot based on the sample stress corrosion result data and input variables, and to determine the mapping relationship between the sample stress corrosion result data and the input variables based on the distribution pattern of the quartile values ​​in the box plot.

[0167] Module 1004 is used to construct a stress corrosion prediction model based on the mapping relationship between sample stress corrosion result data and input variables.

[0168] Prediction module 1005 is used to predict the target stress corrosion result data of the dented heat transfer tube through the stress corrosion prediction model.

[0169] It should be noted that the specific implementation of the stress corrosion prediction device for the dented heat transfer tube is basically the same as the specific implementation of the stress corrosion prediction method for the dented heat transfer tube described above, and will not be repeated here.

[0170] This application also provides an electronic device, which includes: a memory, a processor, a program stored in the memory and executable on the processor, and a data bus for communication between the processor and the memory. When the program is executed by the processor, it implements the stress corrosion prediction method for the dented heat transfer tube described above. This electronic device can be any smart terminal, including tablet computers, in-vehicle computers, etc.

[0171] Please see Figure 11 , Figure 11 The hardware structure of an electronic device according to another embodiment is illustrated. The electronic device includes:

[0172] The processor 1101 can be implemented using a general-purpose CPU (Central Processing Unit), microprocessor, application-specific integrated circuit (ASIC), or one or more integrated circuits, and is used to execute relevant programs to implement the technical solutions provided in the embodiments of this application.

[0173] The memory 1102 can be implemented as a read-only memory (ROM), static storage device, dynamic storage device, or random access memory (RAM). The memory 1102 can store the operating system and other application programs. When the technical solutions provided in the embodiments of this specification are implemented through software or firmware, the relevant program code is stored in the memory 1102 and called and executed by the processor 1101 to execute the stress corrosion prediction method for the dented heat transfer tube of this application embodiment.

[0174] Input / output interface 1103 is used to implement information input and output;

[0175] The communication interface 1104 is used to enable communication and interaction between this device and other devices. Communication can be achieved through wired means (such as USB, network cable, etc.) or wireless means (such as mobile network, WIFI, Bluetooth, etc.).

[0176] Bus 1105 transmits information between various components of the device (e.g., processor 1101, memory 1102, input / output interface 1103, and communication interface 1104);

[0177] The processor 1101, memory 1102, input / output interface 1103 and communication interface 1104 are connected to each other within the device via bus 1105.

[0178] This application embodiment also provides a storage medium, which is a computer-readable storage medium for computer-readable storage. The storage medium stores one or more programs, which can be executed by one or more processors to implement the above-described stress corrosion prediction method for dented heat transfer tubes.

[0179] Memory, as a non-transitory computer-readable storage medium, can be used to store non-transitory software programs and non-transitory computer-executable programs. Furthermore, memory may include high-speed random access memory, and may also include non-transitory memory, such as at least one disk storage device, flash memory device, or other non-transitory solid-state storage device. In some embodiments, memory may optionally include memory remotely located relative to the processor, and these remote memories can be connected to the processor via a network. Examples of such networks include, but are not limited to, the Internet, intranets, local area networks, mobile communication networks, and combinations thereof.

[0180] The embodiments described in this application are for the purpose of more clearly illustrating the technical solutions of the embodiments of this application, and do not constitute a limitation on the technical solutions provided by the embodiments of this application. As those skilled in the art will know, with the evolution of technology and the emergence of new application scenarios, the technical solutions provided by the embodiments of this application are also applicable to similar technical problems.

[0181] Those skilled in the art will understand that the technical solutions shown in the figures do not constitute a limitation on the embodiments of this application, and may include more or fewer steps than shown, or combine certain steps, or different steps.

[0182] The device embodiments described above are merely illustrative. The units described as separate components may or may not be physically separate; that is, they may be located in one place or distributed across multiple network units. Some or all of the modules can be selected to achieve the purpose of this embodiment according to actual needs.

[0183] Those skilled in the art will understand that all or some of the steps, functional modules / units in the systems and devices disclosed above can be implemented as software, firmware, hardware, and suitable combinations thereof. The terms “first,” “second,” “third,” “fourth,” etc. (if present) in the specification and accompanying drawings of this application are used to distinguish similar objects and are not necessarily used to describe a specific order or sequence. It should be understood that such data can be interchanged where appropriate so that the embodiments of this application described herein can be implemented in orders other than those illustrated or described herein. Furthermore, the terms “comprising” and “having,” and any variations thereof, are intended to cover non-exclusive inclusion; for example, a process, method, system, product, or device that comprises a series of steps or units is not necessarily limited to those steps or units explicitly listed, but may include other steps or units not explicitly listed or inherent to such processes, methods, products, or devices.

[0184] It should be understood that in this application, "at least one (item)" means one or more, and "more than" means two or more. "And / or" is used to describe the relationship between related objects, indicating that three relationships can exist. For example, "A and / or B" can represent three cases: only A exists, only B exists, and both A and B exist simultaneously, where A and B can be singular or plural. The character " / " generally indicates that the preceding and following related objects are in an "or" relationship. "At least one (item) of the following" or similar expressions refer to any combination of these items, including any combination of single or plural items. For example, at least one (item) of a, b, or c can represent: a, b, c, "a and b", "a and c", "b and c", or "a and b and c", where a, b, and c can be single or multiple.

[0185] In the several embodiments provided in this application, it should be understood that the disclosed apparatus and methods can be implemented in other ways. For example, the apparatus embodiments described above are merely illustrative; for instance, the division of the units described above is only a logical functional division, and in actual implementation, there may be other division methods. For example, multiple units or components may be combined or integrated into another system, or some features may be ignored or not executed. Furthermore, the coupling or direct coupling or communication connection shown or discussed may be through some interfaces; the indirect coupling or communication connection between apparatuses or units may be electrical, mechanical, or other forms.

[0186] The units described above as separate components may or may not be physically separate. The components shown as units may or may not be physical units; that is, they may be located in one place or distributed across multiple network units. Some or all of the units can be selected to achieve the purpose of this embodiment according to actual needs.

[0187] Furthermore, the functional units in the various embodiments of this application can be integrated into one processing unit, or each unit can exist physically separately, or two or more units can be integrated into one unit. The integrated unit can be implemented in hardware or as a software functional unit.

[0188] If the integrated unit is implemented as a software functional unit and sold or used as an independent product, it can be stored in a computer-readable storage medium. Based on this understanding, the technical solution of this application, in essence, or the part that contributes to the prior art, or all or part of the technical solution, can be embodied in the form of a software product. This computer software product is stored in a storage medium and includes multiple instructions to cause a computer device (which may be a personal computer, server, or network device, etc.) to execute all or part of the steps of the methods of the various embodiments of this application. The aforementioned storage medium includes various media capable of storing programs, such as USB flash drives, portable hard drives, read-only memory (ROM), random access memory (RAM), magnetic disks, or optical disks.

[0189] The preferred embodiments of the present application have been described above with reference to the accompanying drawings, but this does not limit the scope of the claims of the present application. Any modifications, equivalent substitutions, and improvements made by those skilled in the art without departing from the scope and substance of the embodiments of the present application shall be within the scope of the claims of the present application.

Claims

1. A method for predicting stress corrosion of a dented heat transfer tube, characterized in that, The method includes: Obtain sample stress corrosion results data and multiple candidate stress corrosion influencing factors that cause the sample stress corrosion results; Input variables were selected from multiple candidate stress corrosion influencing factors, including sample loading stress and sample indentation depth; Box plots are drawn based on the sample stress corrosion results data and the input variables. The mapping relationship between the sample stress corrosion results data and the input variables is determined based on the distribution pattern of the quartile values ​​in the box plots. The sample stress corrosion results data includes the crack length of the sample cross section. The mapping relationship includes a positive correlation between the sample stress corrosion results data and the sample loading stress, and a quadratic curve relationship between the sample stress corrosion results data and the sample indentation depth. Based on the mapping relationship between the sample stress corrosion results data and the input variables, a stress corrosion prediction model is constructed, including: constructing a first formula based on the positive correlation between the sample stress corrosion results data and the sample loading stress; constructing a second formula based on the quadratic curve relationship between the sample stress corrosion results data and the sample indentation depth; integrating the first formula and the second formula to obtain a first integrated formula; constructing a third formula based on the sample loading stress and the sample indentation depth, the third formula indicating the multiplicative relationship between the sample loading stress and the sample indentation depth; integrating the first integrated formula and the third formula to obtain a second integrated formula; obtaining the sample corrosion environment factor; and multiplying the sample corrosion environment factor and the second integrated formula to obtain the stress corrosion prediction model, the stress corrosion prediction model being as follows: L=β (p0+p1x+p2y+p3x) 2 +p4xy+ε); where L is the crack length of the sample cross section, x is the indentation depth of the sample, y is the loading stress of the sample, β is the corrosion environment factor of the sample, p0, p1, p2, p3, and p4 are all coefficients, and ε is the random error; The stress corrosion prediction model is used to predict the target stress corrosion results of the dented heat transfer tube.

2. The method according to claim 1, characterized in that, The acquisition of sample stress corrosion result data and multiple candidate stress corrosion influencing factors that cause the sample stress corrosion results include: Multiple candidate factors influencing stress corrosion were identified. Based on multiple candidate stress corrosion influencing factors, indentations were created on the initial sample to obtain the target sample; The target sample is placed in a preset corrosion environment, and corrosion state data of the target sample is acquired at predetermined intervals. Statistical analysis was performed on all the acquired corrosion state data to obtain the stress corrosion result data of the sample.

3. The method according to claim 2, characterized in that, Several of the candidate stress corrosion influencing factors include sample indentation type and sample indentation depth; The step of creating a dent in the initial sample based on multiple candidate stress corrosion influencing factors to obtain the target sample includes: The punch is determined based on the type of indentation in the sample. Obtain the impact mode, and obtain the mapping relationship between the first energy and the dent depth corresponding to the impact mode; By using the mapping relationship between the first energy and the indentation depth, the indentation depth of the sample is mapped to obtain the target energy; The target sample is obtained by applying the target energy to the initial sample using the impact method and the punch.

4. The method according to claim 3, characterized in that, The first energy-dent depth mapping relationship includes candidate energy-dent depth mapping relationships corresponding to multiple candidate dent types; The step of mapping the sample indentation depth using the mapping relationship between the first energy and the indentation depth to obtain the target energy includes: Based on the sample dent type, the candidate energy and dent depth mapping relationship corresponding to multiple candidate dent types is filtered to obtain the second energy and dent depth mapping relationship; By utilizing the second energy-dimple depth mapping relationship, the sample dimple depth is mapped to obtain the target energy.

5. The method according to any one of claims 1 to 4, characterized in that, The input variables include the sample dent type, and the stress corrosion prediction model includes candidate stress corrosion prediction models corresponding to the sample dent type. The data predicting the target stress corrosion result of the dented heat transfer tube using the stress corrosion prediction model includes: The type of the dented heat transfer tube is detected to obtain the target dent type; If the target dent type is consistent with the sample dent type, then the dented heat transfer pipe is predicted using the candidate stress corrosion prediction model corresponding to the sample dent type, and the target stress corrosion result data is obtained.

6. The method according to any one of claims 1 to 4, characterized in that, The data predicting the target stress corrosion result of the dented heat transfer tube using the stress corrosion prediction model includes: Obtain the correspondence between the sample non-destructive testing signal and multiple input variables; Based on the aforementioned correspondence, the stress corrosion prediction model is transformed to obtain the signal stress corrosion prediction model. The dented heat transfer tube was subjected to non-destructive testing to obtain the target non-destructive testing signal; The target non-destructive testing signal is input into the signal stress corrosion prediction model to predict corrosion and obtain the target stress corrosion result data.

7. A stress corrosion prediction device for a dented heat transfer tube, characterized in that, The device includes: The acquisition module is used to acquire sample stress corrosion result data and multiple candidate stress corrosion influencing factors that cause the sample stress corrosion results; The filtering module is used to filter input variables from multiple candidate stress corrosion influencing factors, including sample loading stress and sample indentation depth; The determination module is used to draw a box plot based on the sample stress corrosion result data and the input variables, and to determine the mapping relationship between the sample stress corrosion result data and the input variables based on the distribution law of the quartile values ​​in the box plot. The sample stress corrosion result data includes the crack length of the sample cross section, and the mapping relationship includes a positive correlation between the sample stress corrosion result data and the sample loading stress, and a quadratic curve relationship between the sample stress corrosion result data and the sample indentation depth. A construction module is used to construct a stress corrosion prediction model based on the mapping relationship between the sample stress corrosion result data and the input variables. This includes: constructing a first formula based on the positive correlation between the sample stress corrosion result data and the sample loading stress; constructing a second formula based on the quadratic curve relationship between the sample stress corrosion result data and the sample indentation depth; integrating the first and second formulas to obtain a first integrated formula; constructing a third formula based on the sample loading stress and the sample indentation depth, the third formula indicating the multiplicative relationship between the sample loading stress and the sample indentation depth; integrating the first and third integrated formulas to obtain a second integrated formula; obtaining a sample corrosion environment factor; and multiplying the sample corrosion environment factor and the second integrated formula to obtain the stress corrosion prediction model, as shown in the following formula: L=β (p0+p1x+p2y+p3x) 2 +p4xy+ε); where L is the crack length of the sample cross section, x is the indentation depth of the sample, y is the loading stress of the sample, β is the corrosion environment factor of the sample, p0, p1, p2, p3, and p4 are all coefficients, and ε is the random error; The prediction module is used to predict the target stress corrosion result data of the dented heat transfer pipe through the stress corrosion prediction model.

8. An electronic device, characterized in that, The electronic device includes a memory and a processor, the memory storing a computer program, and the processor executing the computer program to implement the method according to any one of claims 1 to 6.

9. A computer-readable storage medium storing a computer program, characterized in that, When the computer program is executed by a processor, it implements the method of any one of claims 1 to 6.

Citation Information

Patent Citations

  • Stress corrosion prediction method and device, equipment and storage medium

    CN117763951A